Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process

  • Xiangru GUO ,
  • Chaoyang SUN ,
  • Chunhui WANG ,
  • Lingyun QIAN ,
  • Fengxian LIU
Expand
  • 1 School of Mechanical and Engineering, University of Science and Technology Beijing, Beijing 100083, China
    2 Beijing Key Laboratory of Lightweight Metal Forming, University of Science and Technology Beijing, Beijing 100083, China
    3 Applied Mechanics Lab., School of Aerospace Engineering, Tsinghua University, Beijing 100084, China

Received date: 2017-12-22

  Online published: 2018-05-09

Supported by

Supported by National Natural Science Foundation of China (No.51575039) and Joint Fund of National Natural Science Foundation of China and Chinese Academy of Engineering Physics (No.U1730121)

Abstract

Microelectromechanical systems (MEMS) have become increasingly prevalent in engineering applications. In these MEMS, a lot of micro-components, such as thin films, nanowires, micro-beams and micropillars, are utilized. The characteristic geometrical size of those components is at the same scale as that of grain, the mechanical behavior of crystal materials exhibits significant size effect and discontinuous deformation. In addition, those MEMS are often subjected to high strain rate at work, such as collision and impact loading. The coupling deformation characteristics of small scale crystals and high strain rate makes their mechanical behavior more complicated. Accordingly, investigation of the effect of the strain rate on crystal materials at micron scale is significant for both the academia and industry. In this work, a plastic deformation model of fcc crystal under axial compression was developed based on three-dimensional discrete dislocation dynamics (3D-DDD), which considered the influence of externally applied stress, interaction force between dislocation segments, dislocation line tension and image force from free surface on dislocation movement during the process of plastic deformation. It was applied to simulate the plastic deformation process of a Ni single crystal micropillar during compression under different loading strain rates. 3D-DDD and theoretical analysis are carried out to extensively investigate the effect of strain rate on flow stress and deformation mechanisms during plastic deformation process of crystal materials. The results show that the flow stress and the dislocation density increased with the loading strain rate. In the case of low strain rate, the flow stress was dominated by the activation stress of Freak-Read (FR) source in plastic deformation. With the increase of strain rate, the contribution of activation stress of FR source to the flow stress decreases and the effective stress gradually dominated the flow stress. Under high strain rate loading, with the increase of the initial FR source, the dislocation density also increased at the same strain correspondingly, which makes it easier to meet the requirement of the loading strain rate, so the flow stress is smaller. In addition, under the low strain rate loading, a few activated FR sources can meet the requirement of the plastic deformation, a single slip deformation come up as a result. While, as the loading strain rate increases, more and more activated FR sources would be needed to coordinate the plastic deformation, the deformation mechanisms of the single crystal micropillar transformed from single slip to multiple slip.

Cite this article

Xiangru GUO , Chaoyang SUN , Chunhui WANG , Lingyun QIAN , Fengxian LIU . Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process[J]. Acta Metall Sin, 2018 , 54(9) : 1322 -1332 . DOI: 10.11900/0412.1961.2017.00553

References

[1] Fu M W, Wang J L, Korsunsky A M.A review of geometrical and microstructural size effects in micro-scale deformation processing of metallic alloy components[J]. Int. J. Mach. Tool. Manuf., 2016, 109: 94
[2] Kimberley J, Cooney R S, Lambros J, et al.Failure of Au RF-MEMS switches subjected to dynamic loading[J]. Sensor. Actuators, 2009, 154A: 140
[3] Kimberley J, Lambros J, Chasiotis I, et al.Mechanics of energy transfer and failure of ductile microscale beams subjected to dynamic loading[J]. J. Mech. Phys. Solids, 2010, 58: 1125
[4] Dimiduk D M, Uchic M D, Parthasarathy T A.Size-affected single-slip behavior of pure nickel microcrystals[J]. Acta Mater., 2005, 53: 4065
[5] Kiener D, Minor A M.Source-controlled yield and hardening of Cu(100) studied by in situ transmission electron microscopy[J]. Acta Mater., 2011, 59: 1328
[6] Nicola L, Xiang Y, Vlassak J J, et al.Plastic deformation of freestanding thin films: Experiments and modeling[J]. J. Mech. Phys. Solids, 2006, 54: 2089
[7] Ramachandramoorthy R, Gao W, Bernal R, et al.High strain rate tensile testing of silver nanowires: Rate-dependent brittle-to-ductile transition[J]. Nano Lett., 2016, 16: 255
[8] Seo J H, Yoo Y, Park N Y, et al.Superplastic deformation of defect-free Au nanowires via coherent twin propagation[J]. Nano Lett., 2011, 11: 3499
[9] Uchic M D, Shade P A, Dimiduk D M.Plasticity of micrometer-scale single crystals in compression[J]. Annu. Rev. Mater. Res., 2009, 39: 361
[10] Greer J R, Oliver W C, Nix W D.Size dependence of mechanical properties of gold at the micron scale in the absence of strain gradients[J]. Acta Mater., 2005, 53: 1821
[11] Liu Z L, You X C, Zhuang Z.A mesoscale investigation of strain rate effect on dynamic deformation of single-crystal copper[J]. Int. J. Solids Struct., 2008, 45: 3674
[12] Kiener D, Guruprasad P J, Keralavarma S M, et al.Work hardening in micropillar compression: In situ experiments and modeling[J]. Acta Mater., 2011, 59: 3825
[13] Jennings A T, Li J, Greer J R.Emergence of strain-rate sensitivity in Cu nanopillars: Transition from dislocation multiplication to dislocation nucleation[J]. Acta Mater., 2011, 59: 5627
[14] Liang Z Y, De Hosson J T M, Huang M X. Size effect on deformation twinning in face-centred cubic single crystals: Experiments and modelling[J]. Acta Mater., 2017, 129: 1
[15] Zhang J Y, Liang X, Zhang P, et al.Emergence of external size effects in the bulk-scale polycrystal to small-scale single-crystal transition: A maximum in the strength and strain-rate sensitivity of multicrystalline Cu micropillars[J]. Acta Mater., 2014, 66: 302
[16] Gray III G T. High-strain-rate deformation: Mechanical behavior and deformation substructures induced[J]. Ann. Rev. Mater. Res., 2012, 42: 285
[17] Shen Y F, Jia N, Misra R D K, et al. Softening behavior by excessive twinning and adiabatic heating at high strain rate in a Fe-20Mn-0.6C TWIP steel[J]. Acta Mater., 2016, 103: 229
[18] Khan A S, Liu J, Yoon J W, et al.Strain rate effect of high purity aluminum single crystals: Experiments and simulations[J]. Int. J. Plast., 2015, 67: 39
[19] Li N, Wang Y D, Lin P R, et al.Localized amorphism after high-strain-rate deformation in TWIP steel[J]. Acta Mater., 2011, 59: 6369
[20] Zhang J Y, Liu G, Sun J.Strain rate effects on the mechanical response in multi- and single-crystalline Cu micropillars: Grain boundary effects[J]. Int. J. Plast., 2013, 50: 1
[21] Oh S H, Legros M, Kiener D, et al.In situ observation of dislocation nucleation and escape in a submicrometre aluminium single crystal[J]. Nat. Mater., 2009, 8: 95
[22] Greer R J.Bridging the gap between computational and experimental length scales: A review on nanoscale plasticity[J]. Rev. Adv. Mater. Sci., 2006, 13: 59
[23] Shan Z W, Mishra R K, Syed Asif S A, et al. Mechanical annealing and source-limited deformation in submicrometre-diameter Ni crystals[J]. Nat. Mater., 2008, 7: 115
[24] Armstrong R W, Arnold W, Zerilli F J.Dislocation mechanics of copper and iron in high rate deformation tests[J]. J. Appl. Phys., 2009, 105: 023511
[25] Guo X R, Sun C Y, Li R, et al.A dislocation density based model for twinning induced softening of TWIP steel[J]. Comput. Mater. Sci., 2017, 139: 8
[26] Sun C Y, Guo N, Fu M W, et al.Modeling of slip, twinning and transformation induced plastic deformation for TWIP steel based on crystal plasticity[J]. Int. J. Plast., 2016, 76: 186
[27] Fan H D, Li Z H, Huang M S.Size effect on the compressive strength of hollow micropillars governed by wall thickness[J]. Scr. Mater., 2012, 67: 225
[28] Hu J Q, Liu Z L, Van Der Giessen E, et al. Strain rate effects on the plastic flow in submicron copper pillars: Considering the influence of sample size and dislocation nucleation[J]. Extreme Mech. Lett., 2017, 17: 33
[29] Gurrutxaga-Lerma B, Balint D S, Dini D, et al.The mechanisms governing the activation of dislocation sources in aluminum at different strain rates[J]. J. Mech. Phys. Solids, 2015, 84: 273
[30] Yu Y, Pan X X.Meso-scale simulation of Frank-Read dislocation sources[J]. Acta Metall. Sin., 2009, 45: 1309(余勇, 潘晓霞. Frank-Read位错源的细观级模拟[J]. 金属学报, 2009, 45: 1309)
[31] Gillis P P, Kratochvil J.Dislocation acceleration[J]. Philos. Mag., 1970, 21: 425
[32] Ghoniem N M, Tong S H, Sun L Z.Parametric dislocation dynamics: A thermodynamics-based approach to investigations of mesoscopic plastic deformation[J]. Phys. Rev., 2000, 61B: 913
[33] Zhou C Z, Biner S B, LeSar R. Discrete dislocation dynamics simulations of plasticity at small scales[J]. Acta Mater., 2010, 58: 1565
[34] Cai W, Arsenlis A, Weinberger C R, et al.A non-singular continuum theory of dislocations[J]. J. Mech. Phys. Solids, 2006, 54: 561
[35] Liu Z L, Liu X M, Zhuang Z, et al.A multi-scale computational model of crystal plasticity at submicron-to-nanometer scales[J]. Int. J. Plast., 2009, 25: 1436
[36] Cui Y N, Po G, Ghoniem N.Controlling strain bursts and avalanches at the nano-to micrometer scale[J]. Phys. Rev. Lett., 2016, 117: 155502
[37] Cui Y N, Lin P, Liu Z L, et al.Theoretical and numerical investigations of single arm dislocation source controlled plastic flow in FCC micropillars[J]. Int. J. Plast., 2014, 55: 279
[38] El-Awady J A. Unravelling the physics of size-dependent dislocation-mediated plasticity[J]. Nat. Commun., 2015, 6: 5926
Outlines

/