Orginal Article

Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials

  • Tao ZHANG ,
  • Wei YAN ,
  • Zhuoming XIE ,
  • Shu MIAO ,
  • Junfeng YANG ,
  • Xianping WANG ,
  • Qianfeng FANG ,
  • Changsong LIU
Expand
  • 1 Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031, China
    2 Experiment Center of Anhui San Lian University, Hefei 230031, China

Received date: 2018-02-28

  Online published: 2018-05-09

Supported by

Supported by National Key Research and Development Program of China (No.2017YFA0402800), National Magnetic Confinement Fusion Program (No.2015GB112000) and National Natural Science Foundation of China (Nos.11735015, 11575241 and 51771184)

Abstract

Tungsten (W) plays an important role in the defense industry, aerospace and nuclear industry due to its excellent properties such as high melting point (3410 ℃), high density (19.35 g/cm3), high hardness, high elastic modulus, high thermal conductivity, low expansion coefficient and low vapor pressure. However, its disadvantages, such as low temperature brittleness (ductile brittle transition temperature usually above 400 ℃), low tensile strength, recrystallization embrittlement, high thermal load induced cracking and irradiation embrittlement, affected seriously its processing and servicing performance. Focusing on these problems, carbides/oxide dispersion strengthened W alloys were studied widely. The mechanical properties and other service properties of W were significantly improved by nano scale carbide/oxide dispersion strengthening and microstructure optimization. This article mainly reviews carbide and oxide dispersion strengthening design and the corresponding W-based materials preparation, microstructure and properties of regulation and service performance evaluation, introduces the latest progress of the research and development of the authors' team, and looks forward to the future development trend and the problems to be solved.

Cite this article

Tao ZHANG , Wei YAN , Zhuoming XIE , Shu MIAO , Junfeng YANG , Xianping WANG , Qianfeng FANG , Changsong LIU . Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials[J]. Acta Metall Sin, 2018 , 54(6) : 831 -843 . DOI: 10.11900/0412.1961.2018.00071

References

[1] Wurster S, Baluc N, Battabyal M.Recent progress in R&D on tungsten alloys for divertor structural and plasma facing materials[J]. J. Nucl. Mater., 2013, 442: S181
[2] Xie Z M, Liu R, Miao S, et al.High thermal shock resistance of the hot rolled and swaged bulk W-ZrC alloys[J]. J. Nucl. Mater., 2016, 469: 209
[3] Wesemann I, Spielmann W, Heel P, et al.Fracture strength and microstructure of ODS tungsten alloys[J]. Int. J. Refract. Met. Hard Mater., 2010, 28: 687
[4] Ueda Y, Schmid K, Balden M, et al.Baseline high heat flux and plasma facing materials for fusion[J]. Nucl. Fusion, 2017, 57: 092006
[5] Li X Y, Liu W, Xu Y C, et al.Radiation resistance of nano-crystalline iron: Coupling of the fundamental segregation process and the annihilation of interstitials and vacancies near the grain boundaries[J]. Acta Mater., 2016, 109: 115
[6] Li X Y, Liu W, Xu Y C, et al.Energetic and kinetic behaviors of small vacancy clusters near a symmetric Σ5 (310)/[001] tilt grain boundary in bcc Fe[J]. J. Nucl. Mater., 2013, 440: 250
[7] Kim Y, Lee K H, Kim E P, et al.Fabrication of high temperature oxides dispersion strengthened tungsten composites by spark plasma sintering process[J]. Int. J. Refract. Met. Hard Mater., 2009, 27: 842
[8] Kim Y, Hong M H, Lee S H, et al.The effect of yttrium oxide on the sintering behavior and hardness of tungsten[J]. Met. Mater. Int., 2006, 12: 245
[9] Aguirre M V, Martín A, Pastor J Y, et al.Mechanical properties of Y2O3-doped W-Ti alloys[J]. J. Nucl. Mater., 2010, 404: 203
[10] Vieider G, Merola M, Bonal J P, et al.European development of the ITER divertor target[J]. Fusion Eng. Des., 1999, 46: 221
[11] Yar M A, Wahlberg S, Bergqvist H, et al.Spark plasma sintering of tungsten-yttrium oxide composites from chemically synthesized nanopowders and microstructural characterization[J]. J. Nucl. Mater., 2011, 412: 227
[12] Battabyal M, Sch?ublin R, Sp?tig P, et al.W-2wt.%Y2O3 composite: Microstructure and mechanical properties[J]. Mater. Sci. Eng., 2012, A538: 53
[13] Battabyal M, Sch?ublin R, Sp?tig P, et al.Microstructure and mechanical properties of a W-2wt.%Y2O3 composite produced by sintering and hot forging[J]. J. Nucl. Mater., 2013, 442: S225
[14] Battabyal M, Sp?tig P, Baluc N.Effect of ion-irradiation on the microstructure and microhardness of the W-2Y2O3 composite materials fabricated by sintering and hot forging[J]. Fusion Eng. Des., 2013, 88: 1668
[15] Dong Z, Liu N, Ma Z Q, et al.Synthesis of nanosized composite powders via a wet chemical process for sintering high performance W-Y2O3 alloy[J]. Int. J. Refr. Met. Hard Mater., 2017, 69: 266
[16] Tan X Y, Luo L M, Chen H Y, et al.Mechanical properties and microstructural change of W-Y2O3 alloy under helium irradiation[J]. Sci. Rep., 2015, 512: 755
[17] Lian Y Y, Liu X, Feng F, et al, Mechanical properties and thermal shock performance of W-Y2O3 composite prepared by high-energy-rate forging[J]. Phys. Scr., 2017, (T170): 014044
[18] Xie Z M, Liu R, Miao S, et al.Effect of high temperature swaging and annealing on the mechanical properties and thermal conductivity of W-Y2O3[J]. J. Nucl. Mater., 2015, 464: 193
[19] Liu R, Xie Z M, Fang Q F, et al.Nanostructured yttria dispersion-strengthened tungsten synthesized by sol-gel method[J]. J. Alloys Compd., 2016, 657: 73
[20] Zhao M Y, Zhou Z J, Zhong M, et al.Thermal shock behavior of fine grained W-Y2O3 materials fabricated via two different manufacturing technologies[J]. J. Nucl. Mater., 2016, 470: 236
[21] Xie Z M, Liu R, Zhang T, et al.Achieving high strength/ductility in bulk W-Zr-Y2O3 alloy plate with hybrid microstructure[J]. Mater. Des., 2016, 107: 144
[22] Kurishita H, Kobayashi S, Nakai K.Development of ultra-fine grained W-(0.25-0.8)wt%TiC and its superior resistance to neutron and 3 MeV He-ion irradiations[J]. J. Nucl. Mater., 2008, 377: 34
[23] Kurishita H, Arakawa H, Matsuo S, et al.Development of nanostructured tungsten based materials resistant to recrystallization and/or radiation induced embrittlement[J]. Mater. Trans., 2013, 54: 456
[24] Kurishita H, Matsuo S, Arakawa H, et al.Current status of nanostructured tungsten-based materials development[J]. Phys. Scr., 2014, 159: 014032
[25] Ishijima Y, Kannari S, Kurishita H, et al.Processing of fine-grained W materials without detrimental phases and their mechanical properties at 200-432 K[J]. Mater. Sci. Eng., 2008, A473: 7
[26] Zhong F L, Yu F W, Chen J L.W-TiC alloy plasma facing materials and heat flux performance test under electron beam facility[J]. Rare Met. Mater. Eng., 2010, 39: 3(种法力, 于福文, 陈俊凌. W-TiC合金面对等离子体材料及其电子束热负荷实验研究[J]. 稀有金属材料与工程, 2010, 39: 3)
[27] Yan Q Z, Zhang X F, Wang T N, et al.Effect of hot working process on the mechanical properties of tungsten materials[J]. J. Nucl. Mater., 2013, 442(suppl.1): S233
[28] Lang S T, Yan Q Z, Sun N B, et al.Effects of TiC content on microstructure, mechanical properties, and thermal conductivity of W-TiC alloys fabricated by a wet-chemical method[J]. Fusion Eng. Des., 2017, 121: 366
[29] Miao S, Xie Z M, Zhang T, et al.Mechanical properties and thermal stability of rolled W-0.5wt% TiC alloys[J]. Mater. Sci. Eng., 2016, A671: 87
[30] Ueda Y, Oya M, Hamaji Y, et al.Surface erosion and modification of toughened, fine-grained, recrystallized tungsten exposed to TEXTOR edge plasma[J]. Phys. Scr., 2014, 159: 014038.
[31] Oya M, Lee H T, Ohtsuka Y, et al.Deuterium retention in various toughened, fine-grained recrystallized tungsten materials under different irradiation conditions[J]. Phys. Scr., 2014, 159: 014048
[32] Roosta M, Baharvandi H.The change occurred in W/ZrC composite properties by using nano reactants[J]. Int. J. Refract. Met. Hard Mater., 2013, 37: 29
[33] Zhang T Q, Wang Y J, Zhou Y, et al.Effect of ZrC particle size on microstructure and room temperature mechanical properties of ZrCp/W composites[J]. Mater. Sci. Eng., 2010, A527: 4021
[34] Li P F, Fan J L, Zhang M, et al.Effect of sintering temperature on properties and microstructure of tungsten composites reinforced by ZrC-Y2O3 particles[J]. Chin. J. Nonferrous Met., 2016, 26: 1952(李鹏飞, 范景莲, 章曼等. 烧结温度对ZrC-Y2O3复合增强细晶钨组织与性能的影响[J]. 中国有色金属学报, 2016, 26: 1952)
[35] Fan J L, Han Y, Li P F, et al.Micro/nano composited tungsten material and its high thermal loading behavior[J]. J. Nucl. Mater., 2014, 455: 717
[36] Xie Z M, Liu R, Fang Q F, et al.Microstructure and mechanical properties of nano-size zirconium carbide dispersion strengthened tungsten alloys fabricated by spark plasma sintering method[J]. Plasma Sci. Technol., 2015, 17: 1066
[37] Xie Z M, Zhang T, Liu R, et al.Grain growth behavior and mechanical properties of zirconium micro-alloyed and nano-size zirconium carbide dispersion strengthened tungsten alloys[J]. Int. J. Refract. Met. Hard Mater., 2015, 51: 180
[38] Xie Z M, Liu R, Miao S, et al.High thermal shock resistance of the hot rolled and swaged bulk W-ZrC alloys[J]. J. Nucl. Mater., 2016, 469: 209
[39] Xie Z M, Liu R, Miao S, et al.Extraordinary high ductility/strength of the interface designed bulk W-ZrC alloy plate at relatively low temperature[J]. Sci. Rep., 2015, 5: 16014
[40] Ding H L, Xie Z M, Fang Q F, et al.Determination of the DBTT of nanoscale ZrC doped W alloys through amplitude-dependent internal friction technique[J]. Mater. Sci. Eng., 2018, A716: 268
[41] Deng H W, Xie Z M, Wang Y K, et al.Mechanical properties and thermal stability of pure W and W-0.5 wt%ZrC alloy manufactured with the same technology[J]. Mater. Sci. Eng., 2018, A715: 117
[42] Pintsuk G, Kurishita H, Linke J, et al.Thermal shock response of fine-and ultra-fine-grained tungsten-based materials[J]. Phys. Scr., 2011, T145: 014060
[43] Zhang X, Yan Q.The thermal crack characteristics of rolled tungsten in different orientations[J]. J. Nucl. Mater., 2014, 444: 428
[44] Liu X, Lian Y Y, Greuner H, et al.Irradiation effects of hydrogen and helium plasma on different grade tungsten materials[J]. Nucl. Mater. Energy, 2017, 12: 1134
[45] Xie Z M, Miao S, Liu R, et al.Recrystallization and thermal shock fatigue resistance of nanoscale ZrC dispersion strengthened W alloys as plasma-facing components in fusion devices[J]. J. Nucl. Mater., 2017, 496: 41
[46] Miao S, Xie Z M, Zeng L F, et al.The mechanical properties and thermal stability of a nanostructured carbide dispersion strengthened W-0.5 wt.%Ta-0.01 wt.%C alloy[J]. Fusion Eng. Des., 2017, 125: 490
[47] Miao S, Xie Z M, Zeng L F, et al.Mechanical properties, thermal stability and microstructure of fine-grained W-0.5 wt.% TaC alloys fabricated by an optimized multi-step process[J]. Nucl. Mater. Energy, 2017, 13: 12
[48] Xie Z M, Miao S, Zhang T, et al.Recrystallization behavior and thermal shock resistance of the W-1.0wt% TaC alloy[J]. J. Nucl. Mater., 2018, 501: 282
[49] Wang Y K, Miao S, Xie Z M, et al.Thermal stability and mechanical properties of HfC dispersion strengthened W alloys as plasma-facing components in fusion devices[J]. J. Nucl. Mater., 2017, 492: 260
Outlines

/