Orginal Article

Galvanic Series of Metals and Effect of Alloy Compositions on Corrosion Resistance in Sanya Seawater

  • Mindong CHEN ,
  • Fan ZHANG ,
  • Zhiyong LIU ,
  • Chaohui YANG ,
  • Guoqing DING ,
  • Xiaogang LI
Expand
  • 1 Key Laboratory for Corrosion and Protection, Ministry of Education, Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China
    2 Qingdao Marine Corrosion Research Institute, Central Iron & Steel Research Insititute, Qingdao 266071, China;
    3 Ningbo Institute of Material Technology & Engineering, Chinese Academy of Sciences, Ningbo 315201, China;

Received date: 2017-12-06

  Online published: 2018-05-03

Supported by

Supported by National Basic Research Program of China (No.2014CB643300) and National Key Research and Development Program of China (No.2016YFB0300604)

Abstract

With the development of ocean engineering, various metallic materials have been applied to the marine environment. It is an urgent requirement to study the galvanic series and alloy composition optimization of metallic materials in the tropical marine environment. In this work, open circuit potentials (OCP) and galvanic series of 36 kinds of metallic materials in Sanya seawater were studied. By considering the response of OCP to tidal changes, the anti-corrosion effects of alloying elements were also analyzed. The results show that the OCP of metallic materials in Sanya seawater has a large range. The galvanic series order of metallic materials from high to low in Sanya seawater is: nickel alloy, duplex stainless steel, austenitic stainless steel and pure copper, ferritic stainless steel, martensitic stainless steel, copper alloy, low alloy steel, carbon steel, cast iron, aluminum alloy and aluminum anode. Low-carbon high-alloy content carbon steel and high Cr, Ni contents stainless steel have higher OCP. The potential fluctuations of carbon steel with tidal changes involves two phases: (1) under the dynamics control, the OCP of carbon steel is more negative at high tide; (2) under the diffusion control, the OCP is more positive at high tide. The potential fluctuations of metallic materials reflect the effect of the corrosion product film on the change of ionization balance, and metals with less potential fluctuations have better inhibition on ion diffusion. In Sanya seawater, the carbon steel, which has more alloying content and less carbon content, has less potential fluctuations with the tidal changes and has good oxygen diffusion resistance. The potential fluctuations of austenitic stainless steel with tidal changes are less than that of ferritic stainless steel and martensitic stainless steel. After 2700 h immersion, austenitic stainless steel and martensitic stainless steel, which have a higher content of Mo, have more stable OCP. In other words, the corrosion film gets a better corrosion resistance. The OCP of aluminum anode in Sanya seawater environment increases when the oxygen content is brought up. The OCP of Zn-containing or Ga-containing aluminum anode remains relatively stable. Al bronze and T2 copper have less potential fluctuations with tidal changes, and perform good corrosion resistance in Sanya seawater.

Cite this article

Mindong CHEN , Fan ZHANG , Zhiyong LIU , Chaohui YANG , Guoqing DING , Xiaogang LI . Galvanic Series of Metals and Effect of Alloy Compositions on Corrosion Resistance in Sanya Seawater[J]. Acta Metall Sin, 2018 , 54(9) : 1311 -1321 . DOI: 10.11900/0412.1961.2017.00521

References

[1] Hou B R, Li X G, Ma X M, et al.The cost of corrosion in China[J]. npj Mater. Degrad., 2017, 1: 4
[2] Sun F L, Ren S, Li Z, et al.Comparative study on the stress corrosion cracking of X70 pipeline steel in simulated shallow and deep sea environments[J]. Mater. Sci. Eng., 2017, A685: 145
[3] Li T, Li X G, Dong C F, et al.Characterization of atmospheric corrosion of 2A12 aluminum alloy in tropical marine environment[J]. J. Mater. Eng. Perform., 2010, 19: 591
[4] Ma Y T, Li Y, Wang F H.The effect of β-FeOOH on the corrosion behavior of low carbon steel exposed in tropic marine environment[J]. Mater. Chem. Phys., 2008, 112: 844
[5] Wu J J, Zhang D, Wang P, et al.The influence of Desulfovibrio sp. and Pseudoalteromonas sp. on the corrosion of Q235 carbon steel in natural seawater[J]. Corros. Sci., 2016, 112: 552
[6] Matsukawa Y, Chuta H, Miyashita M, et al.Galvanic series of metals conventionally used in tap water with and without flow and its comparison to that in seawater[J]. Corrosion, 2011, 67: 1389
[7] Tewary N K, Kundu A, Nandi R, et al.Microstructural characterisation and corrosion performance of old railway girder bridge steel and modern weathering structural steel[J]. Corros. Sci., 2016, 113: 57
[8] Liu M, Cheng X Q, Li X G, et al.Corrosion behavior and durability of low-alloy steel rebars in marine environment[J]. J. Mater. Eng. Perform., 2016, 25: 4967
[9] Mu X, Wei J, Dong J H, et al.In situ corrosion monitoring of mild steel in a simulated tidal zone without marine fouling attachment by electrochemical impedance spectroscopy[J]. J. Mater. Sci. Technol., 2014, 30: 1043
[10] Gao L F, Du M.Pitting corrosion behavior of 304 stainless steel in desalination seawater[J]. Corros. Sci. Prot. Technol., 2017, 29: 8(高丽飞, 杜敏. 304不锈钢在淡化海水中的点蚀行为[J]. 腐蚀科学与防护技术, 2017, 29: 8)
[11] Thierry D, Leballeur C, Larché N.Galvanic series in seawater as a function of temperature, oxygen content and chlorination[J]. Corrosion, 2018, 74: 147
[12] Sun F L, Li X G, Lu L, et al.Corrosion behavior of copper alloys in deep ocean environment of South China Sea[J]. Acta Metall. Sin., 2013, 49: 1211(孙飞龙, 李晓刚, 卢琳等. 铜合金在中国南海深海环境下的腐蚀行为研究[J]. 金属学报, 2013, 49: 1211)
[13] Basumatary J, Wood R J K. Synergistic effects of cavitation erosion and corrosion for nickel aluminium bronze with oxide film in 3.5% NaCl solution [J]. Wear, 2017, 376-377: 1286
[14] Mameng S H, Pettersson R, Leygraf C.Effect of stainless steel composition on atmospheric corrosion resistance at a marine site in Dubai[J]. Corrosion, 2017, 73: 880
[15] Sun F L, Li X G, Lu L, et al.Corrosion behavior of 5052 and 6061 aluminum alloys in deep ocean environment of South China Sea[J]. Acta Metall. Sin., 2013, 49: 1219(孙飞龙, 李晓刚, 卢琳等. 5052和6061铝合金在中国南海深海环境下的腐蚀行为研究[J]. 金属学报, 2013, 49: 1219)
[16] Fin?gar M.Galvanic series of different stainless steels and copper-and aluminium-based materials in acid solutions[J]. Corros. Sci., 2013, 68: 51
[17] Song W X.Metallography [M]. 2nd Ed., Beijing: Metallurgical Industry Press, 1989: 421(宋维锡. 金属学[M]. 第二版. 北京: 冶金工业出版社, 1989: 421)
[18] Hernandez-Sandoval J, Gonzalez-Lopez R, Hernandez-Rodriguez M A L, et al. Localized corrosion in an electrical submergible pump (ESP)[J]. Eng. Fail. Anal., 2015, 53: 124
[19] Bokati K S, Dehghanian C, Yari S.Corrosion inhibition of copper, mild steel and galvanically coupled copper-mild steel in artificial sea water in presence of 1H-benzotriazole, sodium molybdate and sodium phosphate[J]. Corros. Sci., 2017, 126: 272
[20] Li X G, Zhang D W, Liu Z Y, et al.Materials science: Share corrosion data[J]. Nature, 2015, 527: 441
[21] Morcillo M, Díaz I, Chico B, et al.Weathering steels: From empirical development to scientific design. A review[J]. Corros. Sci., 2014, 83: 6
[22] Zhou Y L, Chen J, Xu Y, et al.Effects of Cr, Ni and Cu on the corrosion behavior of low carbon microalloying steel in a Cl- containing environment[J]. J. Mater. Sci. Technol., 2013, 29: 168
[23] Huang G Q.Study of the corrosion potential of metals in seawater[J]. Corros. Prot., 2000, 21(1): 8(黄桂桥. 金属在海水中的腐蚀电位研究[J]. 腐蚀与防护, 2000, 21(1): 8)
[24] Liu D Y, Wei K J.Corrosion potentials of metals in natural sea water of South China Sea[J]. Corros. Sci. Prot. Technol., 1991, 11: 330(刘大扬, 魏开金. 金属在南海海域腐蚀电位研究[J]. 腐蚀科学与防护技术, 1999, 11: 330)
[25] Mu X, Wei J, Dong J H, et al.The effect of sacrificial anode on corrosion protection of Q235B steel in simulated tidal zone[J]. Acta Metall. Sin., 2014, 50: 1294(穆鑫, 魏洁, 董建华等. 牺牲阳极保护对Q235B钢在模拟海洋潮差区间腐蚀行为的影响[J]. 金属学报, 2014, 50: 1294)
[26] Ding G Q, Yang C H, Huang G Q, et al.Corrosion potential of metals in natural river water[J]. Equip. Environ. Eng., 2017, 14(2): 31(丁国清, 杨朝晖, 黄桂桥等. 金属材料在天然河水中的腐蚀电位研究[J]. 装备环境工程, 2017, 14(2): 31)
[27] Hao W K, Liu Z Y, Wu W, et al.Electrochemical characterization and stress corrosion cracking of E690 high strength steel in wet-dry cyclic marine environments[J]. Mater. Sci. Eng., 2018, A710: 318
[28] Dexter S C, Gao G Y.Effect of seawater biofilms on corrosion potential and oxygen reduction of stainless steel[J]. Corrosion, 1988, 44: 717
[29] Liu B, Duan J Z, Hou B R.Microbiologically influenced corrosion of 316L SS by marine biofilms in seawater[J]. J. Chin. Soc. Corros. Protect., 2012, 32: 48(刘彬, 段继周, 侯保荣. 天然海水中微生物膜对316L不锈钢腐蚀行为研究[J]. 中国腐蚀与防护学报, 2012, 32: 48)
[30] Fischer D A, Daille L, Aguirre J, et al.Corrosion of stainless steel in simulated tide of fresh natural seawater of South East Pacific[J]. Int. J. Electrochem. Sci., 2016, 11: 6873
[31] Katkar V A, Gunasekaran G.Galvanic corrosion of AA6061 with other ship building materials in seawater[J]. Corrosion, 2015, 72: 400
[32] Ju H, Duan J Z, Yang Y, et al.Mapping the galvanic corrosion of three coupled metal alloys using coupled multielectrode array: Influence of chloride ion concentration[J]. Materials, 2018, 11: 634
[33] Guo J, Yang S W, Shang C J, et al.Influence of carbon content and microstructure on corrosion behaviour of low alloy steels in a Cl- containing environment[J]. Corros. Sci., 2009, 51: 242
[34] Wang Z F, Liu J R, Wu L X, et al.Study of the corrosion behavior of weathering steels in atmospheric environments[J]. Corros. Sci., 2013, 67: 1
[35] Sedriks A J.Plenary lecture—1986: Effects of alloy composition and microstructure on the passivity of stainless steels[J]. Corrosion, 1986, 42: 376
[36] Wu J S, Pang K, Peng D D, et al.Corrosion behaviors of carbon steels in artificially simulated and accelerated marine environment[J]. Int. J. Electrochem. Sci., 2017, 12: 1216
[37] Melchers R E.Effect of small compositional changes on marine immersion corrosion of low alloy steels[J]. Corros. Sci., 2004, 46: 1669
[38] Cheng X Q, Jin Z, Liu M, et al.Optimizing the nickel content in weathering steels to enhance their corrosion resistance in acidic atmospheres[J]. Corros. Sci., 2017, 115: 135
[39] Xing P, Lu L, Li X G.Oxygen-concentration cell induced corrosion of E690 steel for ocean platform[J]. Chin. J. Mater. Res., 2016, 30: 241(邢佩, 卢琳, 李晓刚. 海洋用高强钢E690氧浓差腐蚀行为研究[J]. 材料研究学报, 2016, 30: 241)
[40] Ghahari M, Krouse D, Laycock N, et al.Synchrotron X-ray radiography studies of pitting corrosion of stainless steel: Extraction of pit propagation parameters[J]. Corros. Sci., 2015, 100: 23
[41] Le Bozec N, Compère C, L'Her M, et al. Influence of stainless steel surface treatment on the oxygen reduction reaction in seawater[J]. Corros. Sci., 2001, 43: 765
[42] Zhang T, Yang Y G, Shao Y W, et al.Advances of the analysis methodology for electrochemical noise[J]. J. Chin. Soc. Corros. Protect., 2014, 34: 1(张涛, 杨延格, 邵亚薇等. 电化学噪声分析方法的研究进展[J]. 中国腐蚀与防护学报, 2014, 34: 1)
[43] Li X G, Dong C F, Xiao K, et al.Corrosion behavior and mechanism of typical materials in Xisha ocean atmosphere environment [M]. Beijing: Science Press, 2014: 123(李晓刚, 董超芳, 肖葵等. 西沙海洋大气环境下典型材料腐蚀/老化行为与机理 [M]. 北京: 科学出版社, 2014: 123)
[44] Li J, Mayer J W, Colgan E G.Oxidation and protection in copper and copper alloy thin films[J]. J. Appl. Phys., 1991, 70: 2820
Outlines

/