Orginal Article

Effect of Si and Mn Contents on the Microstructure and Mechanical Properties of Ultra-High Strength Press Hardening Steel

  • Kuanhui HU ,
  • Xinping MAO ,
  • Guifeng ZHOU ,
  • Jing LIU ,
  • Zhifen WANG
Expand
  • 1 College of Materials and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China
    2 Wuhan Branch of Baosteel Central Research Institute (R&D Center of Wuhan Iron & Steel Co., Ltd.),Wuhan 430080, China;

Received date: 2017-11-20

  Online published: 2018-04-19

Abstract

It is very important to find out the mechanism of composition in steel. Many efforts have been put on the study of the effect of Si and Mn elements on the microstructure and mechanical properties of middle Mn steel, transformation induced plasticity (TRIP) steel and quenching and partitioning (Q&P) steel. But fewer studies were focused on the mechanism of Si and Mn contents in a press hardening steel. In this work, the microstructures after hot rolled and the fine martensite structure after hot stamping in ultra-high strength press hardening steel (PHS) with different Si and Mn contents were studied by OM, SEM, EBSD and TEM. The results showed that there are a great influence of Si and Mn contents on the microstructure and mechanical properties of PHS after hot rolled. The yield strength of the PHS increases from 552 MPa to 751 MPa, the ultimate tensile strength (UTS) increases from 757 MPa to 1124 MPa, and the microstructures are different with the Mn content rose from 0.57% to 1.21% and the other components remained the same. The UTS of the steels goes up as the Si content goes up from 0.25% to 0.38%, and the yield strength and the elongation show a fluctuation trend. After simulating hot stamping process at 950 ℃ and holding 5 min, the microstructure of the steels with different compositions is martensite, but it is different in the fine martensite structure and the average size of sub-grain; after hot stamping process, the comprehensive mechanical properties of the steel B with 0.30%C, 0.34%Si and 1.21%Mn are the most outstanding, the yield strength is 1161 MPa, the UTS is 1758 MPa, and the elongation is 6.5%; after hot stamping process, the microstructure of the steel B is fine lath martensite, and there is a large amount of dislocation in the martensite lath, and precipitates a small number of carbide. The mechanical properties of the ultra-high strength press hardening steels designed in this work is not obvious correlation before and after hot stamping process, and it is just a slight difference in martensite fine structure which is beneficial to controlling the performance stability of the mass industrial production.

Cite this article

Kuanhui HU , Xinping MAO , Guifeng ZHOU , Jing LIU , Zhifen WANG . Effect of Si and Mn Contents on the Microstructure and Mechanical Properties of Ultra-High Strength Press Hardening Steel[J]. Acta Metall Sin, 2018 , 54(8) : 1105 -1112 . DOI: 10.11900/0412.1961.2017.00487

References

[1] Naderi M, Durrenberger L, Molinari A, et al.Constitutive relationships for 22MnB5 boron steel deformed isothermally at high temperatures[J]. Mater. Sci. Eng., 2008, A478: 130
[2] Merklein M, Lechler J, Geiger M.Characterisation of the flow properties of the quenchenable ultra high strength steel 22MnB5[J]. CIRP Ann., 2006, 55: 229
[3] Turetta A, Bruschi S, Ghiotti A.Investigation of 22MnB5 formability in hot stamping operations[J]. J. Mater. Process. Technol., 2006, 177: 396
[4] Xing Z W, Bao J, Yang Y Y.Numerical simulation of hot stamping of quenchable boron steel[J]. Mater. Sci. Eng., 2009, A499: 28
[5] Min J Y, Lin J P, Li J Y, et al.Investigation on hot forming limits of high strength steel 22MnB5[J]. Comput. Mater. Sci., 2010, 49: 326
[6] Liu H S, Liu W, Bao J, et al.Numerical and experimental investigation into hot forming of ultra high strength steel sheet[J]. J. Mater. Eng. Perform., 2011, 20: 1
[7] Naderi M, Ketabchi M, Abbasi M, et al.Analysis of microstructure and mechanical properties of different boron and non-boron alloyed steels after being hot stamped[J]. Procedia Eng., 2011, 10: 460
[8] Li H Z, Wu X, Li G Y.Prediction of forming limit diagrams for 22MnB5 in hot stamping process[J]. J. Mater. Eng. Perform., 2013, 22: 2131
[9] Liu H S, Lei C X, Xing Z W.Cooling system of hot stamping of quenchable steel BR1500HS: Optimization and manufacturing methods[J]. Int. J. Adv. Manuf. Technol., 2013, 69: 211
[10] Wang X N, Ma F W, Liu Q, et al.Research on holding pressure and cooling process during hot forming of ultra-high strength steel 22MnB5 [A]. Proceedings of the FISITA 2012 World Automotive Congress[C]. Berlin: Springer-Verlag, 2013: 123
[11] Li F F, Fu M W, Lin J P, et al.Experimental and theoretical study on the hot forming limit of 22MnB5 steel[J]. Int. J. Adv. Manuf. Technol., 2014, 71: 297
[12] Shi D Y, Hu P, Ying L.Comparative study of ductile fracture prediction of 22MnB5 steel in hot stamping process[J]. Int. J. Adv. Manuf. Technol., 2016, 84: 895
[13] Min J Y, Lin J P, Min Y A, et al.On the ferrite and bainite transformation in isothermally deformed 22MnB5 steels[J]. Mater. Sci. Eng., 2012, A550: 375
[14] So H, Fa?mann D, Hoffmann H, et al.An investigation of the blanking process of the quenchable boron alloyed steel 22MnB5 before and after hot stamping process[J]. J. Mater. Process. Technol., 2012, 212: 437
[15] Karbasian H, Tekkaya A E.A review on hot stamping[J]. J. Mater. Process. Technol., 2010, 210: 2103
[16] Venturato G, Novella M, Bruschi S.Effects of phase transformation in hot stamping of 22MnB5 high strength steel[J]. Procedia Eng., 2017, 183: 316
[17] Mori K, Bariani P F, Behrens B A, et al.Hot stamping of ultra-high strength steel parts[J]. CIRP Ann., 2017, 66: 755
[18] Lu J, Song Y L, Hua L, et al.Influence of thermal deformation conditions on the microstructure and mechanical properties of boron steel[J]. Mater. Sci. Eng., 2017, A701: 328
[19] Zhao Z Z, Tong T T, Zhao A M, et al.Effect of Mn and Si on the microstructure and mechanical properties of medium manganese hot-rolled high-strength steel[J]. J. Univ. Sci. Technol. Beijing, 2014, 36(suppl.1): 133(赵征志, 佟婷婷, 赵爱民等. Mn和Si对中锰热轧高强钢组织和性能的影响[J]. 北京科技大学学报, 2014, 36(增刊): 133)
[20] Li L F, Yang W Y, Sun Z Q.Influence of Mn content on dynamic recrystallization of ferrite in low carbon steels[J]. Acta Metall. Sin., 2004, 40: 1257(李龙飞, 杨王玥, 孙祖庆. Mn含量对低碳钢中铁素体动态再结晶的影响[J]. 金属学报, 2004, 40: 1257)
[21] Li Z D, Miyamoto G, Yang Z G, et al.Effects of Mn and Si additions on pearlite-austenite phase transformation in Fe-0.6C steel[J]. Acta Metall. Sin., 2010, 46: 1066(李昭东, 宫本五郎, 杨志刚等. Mn 和Si对Fe-0.6C钢中珠光体-奥氏体相变的影响[J]. 金属学报, 2010, 46: 1066)
[22] Yin H X, Zhao A M, Zhao Z Z, et al.Effects of Mn content on microstructure and mechanical properties of a low carbon medium-manganese TRIP steel[J]. Mater. Sci. Technol., 2014, 22(3): 11(尹鸿祥, 赵爱民, 赵征志等. Mn含量对低碳中锰TRIP钢组织性能的影响[J]. 材料科学与工艺, 2014, 22(3): 11)
[23] Chen L S, Zhang J Y, Tian Y Q, et al.Effects of Mn partitioning on microstructure and mechanical properties of low-carbon Q&P steel[J]. Heat Treat. Met., 2015, 40(9): 130(陈连生, 张健杨, 田亚强等. Mn配分行为对低碳高强Q&P钢组织与性能的影响[J]. 金属热处理, 2015, 40(9): 130)
[24] Wang H, Shi W, He Y L, et al.Study of Mn and P solute distributions and their effect on the tensile behavior in ultra low carbon bake hardening steels[J]. Acta Metall. Sin., 2011, 47: 263(王华, 史文, 何燕霖等. Mn和P在超低碳烘烤硬化钢中的分布形态及其对拉伸行为的影响研究[J]. 金属学报, 2011, 47: 263)
[25] Shi W, Li L, Zhou Y, et al.Effect of Mn content on microstructures and mechanical properties of cold rolled 0.15C-0.6Si-Mn TRIP steels[J]. Heat Treat. Met., 2002, 27(8): 9(史文, 李麟, 周媛等. Mn含量对0.15C-0.6Si-Mn TRIP钢组织和力学性能的影响[J]. 金属热处理, 2002, 27(8): 9)
[26] Wang L J, Yu W, Wu H B, et al.Effects of Si on tempering stability of retained austenite and mechanical properties of ultra-high strength steels[J]. Trans. Mater. Heat Treat., 2002, 31: 31(王立军, 余伟, 武会宾等. Si对超高强钢残留奥氏体回火稳定性与力学性能的影响[J]. 材料热处理学报, 2010, 31: 31)
[27] Huang B X, Wang C Z, Wang X D, et al.Effect of nitrogen on martensitic transformation and mechanical properties of TWIP steel[J]. Acta Metall. Sin., 2012, 48: 769(黄宝旭, 王长征, 王晓东等. N对TWIP钢马氏体相变及力学性能的影响[J]. 金属学报, 2012, 48: 769)
Outlines

/