Effect of La Content on Hydriding Kinetics of Ce-La Alloys
Received date: 2017-11-20
Online published: 2018-04-08
Supported by
Supported by National Natural Science Foundation of China (No.11504344)
Various metals, such as uranium and plutonium, have the potential to form hydride phases while environment develop so that they are exposed to low standard of hydrogen in a long time storage environment. The generation of hydride phases has safety implications, for instance the potential to cause unintended thermal excursions and to adversely alter mechanical properties. So the reaction of alloys between hydrogen is of signi?cant industrial interest. The hydrogenation kinetics characteristics of Ce-La alloys have the similarity with some actinide materials. Investigating the growth kinetics of Ce-La alloy hydride reaction sites is of fundamental importance to the development of predictive model of hydriding behavior. In this work, the effect of La content (0~10%, mass fraction) on hydriding kinetics of Ce-La alloys was studied by pressure consume curve, and the effects of La content on surface morphology and oxidation film structure of Ce-La alloy were observed by in situ OM, XRD and Raman spectra. The results show that doped La can shorten the induction period and accelerate the nucleation rate, so as to accelerate the hydriding rate. Furthermore, doped La can cause the lattice expansion and promote the formation of oxygen vacancy in the oxidation film. The apparent activation energies of pure Ce and Ce-10La alloy are 51.12 and 41.53 kJ/mol, respectively, suggesting that the diffusion barrier of hydrogen in the oxidation film of Ce-10La alloys is lower. The oxygen vacancy and the lattice expansion caused by doped La may promote the diffusion ability of hydrogen in the oxide film. Hydrogen diffusion through the oxide film decides the hydriding rate. So doped La accelerate the hydrogenation.
Key words: Ce-La alloy; La content; oxygen vacancy; hydriding kinetics
Shuaipeng WANG , Wenhua LUO , Gan LI , Haibo LI , Guangfeng ZHANG . Effect of La Content on Hydriding Kinetics of Ce-La Alloys[J]. Acta Metall Sin, 2018 , 54(8) : 1187 -1192 . DOI: 10.11900/0412.1961.2017.00488
| [1] | Zhan W C, Guo Y, Gong X Q, et al.Surface oxygen activation on CeO2 and its catalytic performances for oxidation reactions[J]. Sci. Sin.: Chim., 2012, 42: 433(詹望成, 郭耘, 龚学庆等. 二氧化铈表面氧的活化及对氧化反应的催化作用[J]. 中国科学: 化学, 2012, 42: 433) |
| [2] | Vinodkumar T, Rao B G, Reddy B M.Influence of isovalent and aliovalent dopants on the reactivity of cerium oxide for catalytic applications[J]. Catal. Today, 2015, 253: 57 |
| [3] | Brierley M, Knowles J, Montgomery N, et al.Microstructure of surface cerium hydride growth sites[J]. J. Vac. Sci. Technol., 2014, 32A: 031402 |
| [4] | Knowles J P, Rule G, Brierley M.The morphology and anisotropic growth kinetics of cerium hydride reaction sites[J]. Corros. Sci., 2013, 77: 31 |
| [5] | Sun B, Liu H F, Song H F, et al.Microdynamics simulations of the hydrogen-corrosion resistance of passivation layers on Pu surface[J]. Acta Phy-Chim. Sin., 2009, 31(suppl.1): 81(孙博, 刘海风, 宋海峰等. 钚表面钝化层抗氢蚀机理的微观动力学模拟[J]. 物理化学学报, 2015(增刊1): 81) |
| [6] | Mcgillivray G W, Knowles J P, Findlay I M, et al.The plutonium/hydrogen reaction: The pressure dependence of reaction initiation time and nucleation rate controlled by a plutonium dioxide over-layer[J]. J. Nucl. Mater., 2011, 412: 35 |
| [7] | Edelstein N M.Comparison of the electronic structure of the lanthanides and actinides[J]. J. Alloys Compd., 1995, 223: 197 |
| [8] | Ito M, Setoyama D, Matsunaga J, et al.Effect of electronegativity on the mechanical properties of metal hydrides with a fluorite structure[J]. J. Alloys Compd., 2006, 426: 67 |
| [9] | Haschke J M, Dinh L N.Chemistry and kinetics of the pyrophoric plutonium hydride-air reaction[J]. J. Alloys Compd., 2017, 698: 44 |
| [10] | Brill M, Bloch J, Shmariahu D, et al.The incipient kinetics of hydride growth on cerium surfaces[J]. J. Alloys Compd., 1995, 231: 368 |
| [11] | Hadano M, Urushihara N, Terada S, et al. Reaction kinetics of cerium thin films with H2, O2 and H2O systems at 298 K [J]. J. Alloys Compd., 2002, 330-332: 498 |
| [12] | Brierley M, Knowles J.Probing the cerium/cerium hydride interface using nanoindentation[J]. J. Alloys Compd., 2015, 645(suppl.1): S148 |
| [13] | Bach H T, Venhaus T J, Paglieri S N, et al. The effect of surface state on the kinetics of cerium-hydride formation [J]. J. Alloys Compd., 2007, 446-447: 567 |
| [14] | Zhang L Q, Cheng Y, Niu Z W, et al.First-principles investigations on structural, elastic, and thermodynamic properties of Ce-La alloys under high pressure[J]. Z. Naturforsch., 2014, 69A: 52 |
| [15] | Stakebake J L.Atmospheric oxidation of Pu-1wt.%Ga in the temperature range 150-500 ℃[J]. J. Less-Common Met., 1986, 123: 185 |
| [16] | Ganduglia-Pirovano M V, Hofmann A, Sauer J. Oxygen vacancies in transition metal and rare earth oxides: Current state of understanding and remaining challenges[J]. Surf. Sci. Rep., 2007, 62: 219 |
| [17] | Wheeler D W, Khan I.A Raman spectroscopy study of cerium oxide in a cerium-5wt.% lanthanum alloy[J]. Vib. Spectrosc., 2014, 70: 200 |
| [18] | McBride J R, Hass K C, Poindexter B D, et al. Raman and X-ray studies of Ce1-xRexO2-y, where Re=La, Pr, Nd, Eu, Gd, and Tb[J]. J. Appl. Phys., 1994, 76: 2435 |
| [19] | Weber W H, Hass K C, Mcbride J R.Raman study of CeO2: Second-order scattering, lattice dynamics, and particle-size effects[J]. Phys. Rev., 1993, 48B: 178 |
| [20] | Fernández-Torre D, Carrasco J, Ganduglia-Pirovano M V, et al. Hydrogen activation, diffusion, and clustering on CeO2(111): A DFT+U study[J]. J. Chem. Phys., 2014, 141: 014703 |
| [21] | Lim W F, Cheong K Y.Oxygen vacancy formation and annihilation in lanthanum cerium oxide as a metal reactive oxide on 4H-silicon carbide[J]. Phys. Chem. Chem. Phys., 2014, 16: 7015 |
| [22] | Tsunekawa S, Sivamohan R, Ito S, et al.Structural study on monosize CeO2-x nano-particles[J]. Nanostruct. Mater., 1999, 11: 141 |
| [23] | Uchida H, Terao K, Huang Y C.Current problems in the development and application of hydrogen storage materials[J]. Z. Phys. Chem., 1989, 164: 1275 |
/
| 〈 |
|
〉 |