Recent Progresses in Competitive Grain Growth During Directional Solidification
Received date: 2017-12-20
Online published: 2018-03-14
Supported by
Supported by National Natural Science Foundation of China (Nos.51371151 and 51571165)
Competitive growth between different structures including phases, dendrites and grains is a common phenomenon existing in various microstructure evolution processes. The overgrowth outcome of competitive growth has a paramount influence on final solidification microstructures and mechanical behaviors of materials. The competitive grain growth during directional solidification is a key factor for microstructures controlling, especially for the preparation of single crystal turbine blades. In recent years, the competitive grain growth during directional solidification becomes a hot spot due to an increasing demand for the single crystal preparation and inconsistent experimental results with the classical Walton-Chalmers model. In this paper, the mechanism of competitive grain growth based on the classical Walton-Chalmers model and its challenges were firstly discussed, and then some recent research progresses in converging growth and diverging growth in two dimensional spaces, and non-uniplanar growth in three dimensional spaces were reviewed. Furthermore, the recent works of our group on competitive grain growth during directional solidification by using the phase field method were introduced. Finally, the outlooks of future studies on competitive grain growth during directional solidification are presented.
Jincheng WANG , Chunwen GUO , Junjie LI , Zhijun WANG . Recent Progresses in Competitive Grain Growth During Directional Solidification[J]. Acta Metall Sin, 2018 , 54(5) : 657 -668 . DOI: 10.11900/0412.1961.2017.00543
| [1] | Fu H Z, Guo J J, Liu L, et al.Directional Solidification and Processing of Advanced Materials [M]. Beijing: Science Press, 2009: 1(傅恒志, 郭景杰, 刘林等. 先进材料定向凝固 [M]. 北京: 科学出版社, 2009: 1) |
| [2] | Fu H Z, He G, Li J G.Observation of competitive growth in a directionally solidified nickel base single crystal superalloy[J]. Acta Metall. Sin., 1997, 33: 1233(傅恒志, 何国, 李建国. 单晶高温合金定向凝固过程中晶体竞争生长观察[J]. 金属学报, 1997, 33: 1233) |
| [3] | Hu Z Q, Liu L R, Jin T.Development of the Ni-base single crystal superalloys[J]. Aeroengine, 2005, 31: 1(胡壮麒, 刘丽荣, 金涛. 镍基单晶高温合金的发展[J]. 航空发动机, 2005, 31: 1) |
| [4] | D'Souza N, Jennings P A, Yang X L, et al. Seeding of single-crystal superalloys—Role of constitutional undercooling and primary dendrite orientation on stray-grain nucleation and growth[J]. Metall. Mater. Transact., 2005, 36B: 657 |
| [5] | Yan Y H, Liu J W, Jia Z H, et al.Simulation and experimental studies on grain selection behavior of DD5 single crystal superalloy[J]. Mater. Sci. Forum, 2017, 878: 42 |
| [6] | Zhang H, Xu Q Y, Sun C B, et al.Simulation and experimental studied on grain selection behavior of single crystal superalloy: I. Starter block[J]. Acta Metall. Sin., 2013, 49: 1508(张航, 许庆彦, 孙长波等. 单晶高温合金螺旋选晶过程的数值模拟与实验研究I.引晶段[J]. 金属学报, 2013, 49: 1508) |
| [7] | Zhang H, Xu Q Y, Sun C B, et al.Simulation and experimental studies on grain selection behavior of single crystal superalloy: II. Spiral part[J]. Acta Metall. Sin., 2013, 49: 1521(张航, 许庆彦, 孙长波等. 单晶高温合金螺旋选晶过程的数值模拟与实验研究II.螺旋段[J]. 金属学报, 2013, 49: 1521) |
| [8] | Gao S F, Liu L, Wang N, et al.EBSD studies of grain evolution and grain selection behavior during the preparation of Ni-based single crystal superalloy DD3[J]. Acta Metall. Sin., 2011, 47: 1251(高斯峰, 刘林, 王柠等. 镍基单晶高温合金DD3制备过程中晶粒演化和选晶行为的EBSD研究[J]. 金属学报, 2011, 47: 1251) |
| [9] | Wang N, Liu L, Gao S F, et al.Simulation of grain selection during single crystal casting of a Ni-base superalloy[J]. J. Alloys Compd., 2014, 586: 220 |
| [10] | Yang X L, Dong H B, Wang W, et al.Microscale simulation of stray grain formation in investment cast turbine blades[J]. Mater. Sci. Eng., 2004, A386: 129 |
| [11] | Zhang X L, Zhou Y Z, Jin T, et al.Study on the tendency of stray grain formation of Ni-based single crystal superalloys[J]. Acta Metall. Sin., 2012, 48: 1229(张小丽, 周亦胄, 金涛等. 镍基单晶高温合金杂晶形成倾向性的研究[J]. 金属学报, 2012, 48: 1229) |
| [12] | Yang X L, Ness D, Lee P D, et al. Simulation of stray grain formation during single crystal seed melt-back and initial withdrawal in the Ni-base superalloy CMSX4 [J]. Mater. Sci. Eng., 2005, A413-414: 571 |
| [13] | Trempa M, Reimann C, Friedrich J, et al.Mono-crystalline growth in directional solidification of silicon with different orientation and splitting of seed crystals[J]. J. Cryst. Growth, 2012, 351: 131 |
| [14] | Deng P R, Li J G.Orientation control of crystal growth for TbFe1.9 alloy in a magnetic field[J]. Rare Met. Mater. Eng., 2006, 35: 1311(邓沛然, 李建国. 磁场中TbFe1.9晶体生长的取向控制[J]. 稀有金属材料与工程, 2006, 35: 1311) |
| [15] | Stanford N, Djakovic A, Shollock B, et al.Defect grains in the melt-back region of cmsx-4 single crystal seeds [A]. Proceedings of the 10th International Symposium on Superalloys[C]. Warrendale, PA: TMS, 2004: 719 |
| [16] | Meng X B, Li J G, Chen Z Q, et al.Effect of platform dimension on the dendrite growth and stray grain formation in a Ni-base single-crystal superalloy[J]. Metall. Mater. Trans., 2013, 44A: 1955 |
| [17] | Yang C, Liu L, Zhao X, et al.Formation of stray grains during directional solidification of a superalloy AM3[J]. Appl. Phys., 2014, 114A: 979 |
| [18] | Bogdanowicz W, Albrecht R, Sieniawski J, et al.The subgrain structure in turbine blade roots of CMSX-4 superalloy[J]. J. Cryst. Growth, 2014, 401: 418 |
| [19] | Walton D, Chalmers B.The origin of the preferred orientation in the columnar zone of ingots[J]. Trans. Am. Inst. Min. Metall. Eng., 1959, 215: 447 |
| [20] | Rappaz M, Gandin C A.Modelling of microstructure formation in solidification processes[J]. Acta Metall. Mater., 1993, 41: 345 |
| [21] | Gandin C A, Rappaz M.A coupled finite element-cellular automaton model for the prediction of dendritic grain structures in solidification processes[J]. Acta Metall. Mater., 1994, 42: 2233 |
| [22] | Li J J, Wang Z J, Wang Y Q, et al.Phase-field study of competitive dendritic growth of converging grains during directional solidification[J]. Acta Mater., 2012, 60: 1478 |
| [23] | Esaka H.Dendrite growth and spacing in succinonitrile-acetone alloys [D]. Lausanne, Switzerland: EPFL, 1986 |
| [24] | D'Souza N, Ardakani M G, Wagner A, et al. Morphological aspects of competitive grain growth during directional solidification of a nickel-base superalloy, CMSX4[J]. J. Mater. Sci., 2002, 37: 481 |
| [25] | Wagner A, Shollock B A, McLean M. Grain structure development in directional solidification of nickel-base superalloys[J]. Mater. Sci. Eng., 2004, A374: 270 |
| [26] | Ardakani M G, D'Souza N, Wagner A, et al. Competitive grain growth and texture evolution during directional solidification of superalloys [A]. Superalloys 2000[C]. Warrendale, PA: TMS, 2000: 219 |
| [27] | He G, Li J G, Mao X M, et al.Investigation on competitive growth mechanism of crystals during unidirectional solidification[J]. J. Synth. Cryst., 1995, 24(4): 278(何国, 李建国, 毛协民等. 定向凝固晶粒宏观竞争生长机制的实验研究[J]. 人工晶体学报, 1995, 24: 278) |
| [28] | Liu Z Y, Lei Y, Fu H Z.A study on mechanism of misoriented grain growth in single-crystal manufacture of DD8 nickel based superalloy[J]. Acta Metall. Sin., 2000, 36: 1(刘志义, 雷毅, 傅恒志. DD8镍基高温合金单晶制备中的杂晶长大机制[J]. 金属学报, 2000, 36: 1) |
| [29] | Seo S M, Kim I S, Lee J H, et al.Grain structure and texture evolutions during single crystal casting of the Ni-base superalloy CMSX-4[J]. Met. Mater. Int., 2009, 15: 391 |
| [30] | Zhou Y Z, Volek A, Green N R.Mechanism of competitive grain growth in directional solidification of a nickel-base superalloy[J]. Acta Mater., 2008, 56: 2631 |
| [31] | Zhou Y Z, Green N R.Competitive grain growth in directional solidification of a nickel-base superalloy [A]. Superalloys[M]. Warrendale, PA: TMS, 2008: 317 |
| [32] | Zhou Y Z, Jin T, Sun X F.Structure evolution in directionally solidified bicrystals of nickel base superalloys[J]. Acta Metall. Sin., 2010, 46: 1327(周亦胄, 金涛, 孙晓峰. 双晶镍基高温合金定向凝固过程的结构演化[J]. 金属学报, 2010, 46: 1327) |
| [33] | Epishin A I, Nolze G.Investigation of the competitive grain growth during solidification of single crystals of nickel-based superalloys[J]. Crystallogr. Rep., 2006, 51: 710 |
| [34] | Zhou Y Z, Sun X F.Effect of solidification rate on competitive grain growth in directional solidification of a nickel-base superalloy[J]. Sci. China: Tech. Sci., 2012, 56: 1327 |
| [35] | Lu Q, Li J G, Jin T, et al.Competitive growth in bi-crystal of Ni-based superalloys during directional solidification[J]. Acta Metall. Sin., 2011, 47: 641(卢琦, 李金国, 金涛等. 镍基双晶高温合金定向凝固过程中的竞争生长[J]. 金属学报, 2011, 47: 641) |
| [36] | Zhao X B.Crystal orientation of single crystal superalloys under high thermal gradient directional solidification [D]. Xi'an: Northwestern Polytechnical University, 2010(赵新宝. 高梯度定向凝固单晶高温合金晶体取向研究 [D]. 西安: 西北工业大学, 2010) |
| [37] | Yu H L, Lin X, Li J J, et al.Research on diverged bi-crystal competitive growth in directional solidification[J]. Acta Metall. Sin., 2013, 49: 58(宇红雷, 林鑫, 李俊杰等. 定向凝固发散双晶的竞争生长研究[J]. 金属学报, 2013, 49: 58) |
| [38] | Yang C, Liu L, Zhao X B, et al.Competitive grain growth mechanism in three dimensions during directional solidification of a nickel-based superalloy[J]. J. Alloys Compd., 2013, 578: 577 |
| [39] | Yu H L, Li J J, Lin X, et al.Anomalous overgrowth of converging dendrites during directional solidification[J]. J. Cryst. Growth, 2014, 402: 210 |
| [40] | Liu Z Y, Lin M, Yu D E, et al.Dependence of competitive grain growth on secondary dendrite orientation during directional solidification of a Ni-based superalloy[J]. Metall. Mater. Trans., 2013, 44A: 5113 |
| [41] | Hu S S, Liu L, Cui Q W, et al.Converging competitive growth in bi-crystal of Ni-based superalloy during directional solidification[J]. Acta Metall. Sin., 2016, 52: 897(胡松松, 刘林, 崔强伟等. 镍基高温合金定向凝固过程中的汇聚型双晶竞争生长[J]. 金属学报, 2016, 52: 897) |
| [42] | Hu S S, Yang W C, Cui Q W, et al.Effect of secondary dendrite orientations on competitive growth of converging dendrites of Ni-based bi-crystal superalloys[J]. Mater. Charact., 2017, 125: 152 |
| [43] | Eiken J.Dendritic growth texture evolution in Mg-based alloys investigated by phase-field simulation[J]. Int. J. Cast Met. Res., 2013, 22: 86 |
| [44] | Chen P, Tsai Y L, Lan C W.Phase field modeling of growth competition of silicon grains[J]. Acta Mater., 2008, 56: 4114 |
| [45] | Wang Y Q, Wang J C, Li J J.Phase field modeling of the growth and competition behavior of tilted dendrites in directional solidification[J]. Acta Phys. Sin., 2012, 61: 118103(王雅琴, 王锦程, 李俊杰. 定向倾斜枝晶生长规律及竞争行为的相场法研究[J]. 物理学报, 2012, 61: 118103) |
| [46] | Meng X B, Lu Q, Zhang X L, et al.Mechanism of competitive growth during directional solidification of a nickel-base superalloy in a three-dimensional reference frame[J]. Acta Mater., 2012, 60: 3965 |
| [47] | Takaki T, Shimokawabe T, Ohno M, et al.Unexpected selection of growing dendrites by very-large-scale phase-field simulation[J]. J. Cryst. Growth, 2013, 382: 21 |
| [48] | Takaki T, Ohno M, Shimokawabe T, et al.Two-dimensional phase-field simulations of dendrite competitive growth during the directional solidification of a binary alloy bicrystal[J]. Acta Mater., 2014, 81: 272 |
| [49] | Takaki T, Ohno M, Shibuta Y, et al.Two-dimensional phase-field study of competitive grain growth during directional solidification of polycrystalline binary alloy[J]. J. Cryst. Growth, 2016, 442: 14 |
| [50] | Takaki T, Sakane S, Ohno M, et al.Large-scale phase-field studies of three-dimensional dendrite competitive growth at the converging grain boundary during directional solidification of a bicrystal binary alloy[J]. ISIJ Int., 2016, 56: 1427 |
| [51] | Sakane S, Takaki T, Ohno M, et al.GPU-accelerated 3D phase-field simulations of dendrite competitive growth during directional solidification of binary alloy[J]. IOP Conf. Ser.: Mater. Sci. Eng., 2015, 84: 012063 |
| [52] | Tourret D, Karma A.Growth competition of columnar dendritic grains: a phase-field study[J]. Acta Mater., 2015, 82: 64 |
| [53] | Tourret D, Song Y, Clarke A J, et al.Grain growth competition during thin-sample directional solidification of dendritic microstructures: A phase-field study[J]. Acta Mater., 2017, 122: 220 |
| [54] | Guo C W, Li J J, Yu H L, et al.Branching-induced grain boundary evolution during directional solidification of columnar dendritic grains[J]. Acta Mater., 2017, 136: 148 |
| [55] | Viardin A, Zalo?nik M, Souhar Y, et al.Mesoscopic modeling of spacing and grain selection in columnar dendritic solidification: Envelope versus phase-field model[J]. Acta Mater., 2017, 122: 386 |
| [56] | Pieters R, Langer J S.Noise-driven sidebranching in the boundary-layer model of dendritic solidification[J]. Phys. Rev. Lett., 1986, 56: 1948 |
| [57] | Langer J S.Dendritic sidebranching in the three-dimensional symmetric model in the presence of noise[J]. Phys. Rev., 1987, 36A: 3350 |
| [58] | Barber M N, Barbieri A, Langer J S.Dynamics of dendritic sidebranching in the two-dimensional symmetric model of solidification[J]. Phys. Rev., 1987, 36A: 3340 |
| [59] | Dougherty A, Kaplan P D, Gollub J P.Development of side branching in dendritic growth[J]. Phys. Rev. Lett., 1988, 58: 1652 |
| [60] | Brener E, Temkin D.Noise-induced sidebranching in the three-dimensional nonaxisymmetric dendritic growth[J]. Phys. Rev., 1995, 51E: 351 |
| [61] | Pocheau A, Bodea S, Georgelin M.Self-organized dendritic sidebranching in directional solidification: Sidebranch coherence within uncorrelated bursts[J]. Phys. Rev., 2009, 80E: 031601. |
| [62] | Guo C W, Li J J, Ma Y, et al.Growth behaviors and forced modulation characteristics of dendritic sidebranches in directional solidification[J]. Acta Phys. Sin., 2015, 64: 148101(郭春文, 李俊杰, 马渊等. 定向凝固过程中枝晶侧向分枝生长行为与强制调控规律[J]. 物理学报, 2015, 64: 148101) |
| [63] | Esaka H, Tamura M, Shinozuka K.Analysis of yield rate in single crystal casting process using an engineering simulation model[J]. Mater. Trans., 2005, 44: 829 |
| [64] | Esaka H, Shinozuka K, Tamura M.Analysis of single crystal casting process taking into account the shape of pigtail[J]. Mater. Sci. Eng., 2005, A413: 151 |
| [65] | Pocheau A, Deschamps J, Georgelin M.Dendrite growth directions and morphology in the directional solidification of anisotropic materials[J]. JOM, 2007, 59(7): 71 |
| [66] | Ghmadh J, Debierre J M, Deschamps J, et al.Directional solidification of inclined structures in thin samples[J]. Acta Mater., 2014, 74: 255 |
| [67] | Deschamps J, Georgelin M, Pocheau A.Growth directions of microstructures in directional solidification of crystalline materials[J]. Phys. Rev., 2008, 78E: 011605 |
| [68] | Xing H, Ankit K, Dong X L, et al.Growth direction selection of tilted dendritic arrays in directional solidification over a wide range of pulling velocity: A phase-field study[J]. Int. J. Heat Mass Transfer, 2018, 117: 1107 |
| [69] | Xing H, Dong X L, Chen C L, et al.Phase-field simulation of tilted growth of dendritic arrays during directional solidification[J]. Int. J. Heat Mass Transfer, 2015, 90: 911 |
| [70] | George W L, Warren J A.A parallel 3D dendritic growth simulator using the phase-field method[J]. J. Comput. Phys., 2002, 177: 264 |
| [71] | Provatas N, Goldenfeld N, Dantzig J.Efficient computation of dendritic microstructures using adaptive mesh refinement[J]. Phys. Rev. Lett., 1997, 80: 3308 |
| [72] | Zhu C S, Li H, Feng L, et al.GPU accelerated phase-field simulation of convection effect on dendritic growth[J]. J. Comput. Theor. Nanosci., 2015, 12: 3591 |
| [73] | Yang C, Xu Q Y, Liu B C.GPU-accelerated three-dimensional phase-field simulation of dendrite growth in a nickel-based superalloy[J]. Comput. Mater. Sci., 2017, 136: 133 |
/
| 〈 |
|
〉 |