Chemical Units in Solid Solutions andAlloy Composition Design
Received date: 2017-11-02
Online published: 2018-03-07
Supported by
Supported by National Natural Science Foundation of China (No.11674045)
Industrial alloys all have specific chemical compositions as standardized in specifications. Understanding the structural origin of special compositions for these solid-solution alloys is significant to shortening the development of new industrial alloys. It is well accepted that all alloys are based on solid solutions characterized by chemical short-range ordering. Previously it was only possible to describe the deviation of solute distribution from average mode in a statistical manner. The lack of an accurate structural tool to address the characteristic short-range-order structures constitutes the major obstacle in establishing an effective structural model that allows precise composition design for alloys. Since alloys with good comprehensive performance do have specific chemical compositions, their compositions should correspond to molecule-like specific structural units. After a long effort of more than a decade, we have developed a new structural tool, so-called the cluster-plus-glue-atom model, to address any short-range-ordered structures. In particular, solid solutions can be understood as being constructed from the packing of special chemical units covering only the nearest-neighbor cluster and a few glue atoms located at the next outer shell, expressed in molecule-like cluster formula [cluster] (glue atoms). Such units represent the smallest particles that are representative of the whole structures, just like molecules do for chemical substances. After introducing Friedel oscillation, the cluster-plus-glue-atom model is turned into the cluster-resonance model that provides also the inter-cluster packing modes. Ideal atomic density is hence obtained which is only proportional to the number of atoms in the unit and the cube of the cluster radius. The calculation of chemical unit is then possible and is conducted in typical binary Cu-based industrial alloys. The calculated formulas give chemical composition that highly agree with the most popular alloy specifications. The work demonstrates its high potential for developing chemically complex alloys.
Chuang DONG , Dandan DONG , Qing WANG . Chemical Units in Solid Solutions andAlloy Composition Design[J]. Acta Metall Sin, 2018 , 54(2) : 293 -300 . DOI: 10.11900/0412.1961.2017.00462
| [1] | Tammann G.über eine farblose form des quecksilberjodides[J]. Z. Anorg. Chem., 1919, 109: 213 |
| [2] | Johansson C, Linde J.R?ntgenographische bestimmung der atomanordnung in den mischkristallreihen Au-Cu und Pd-Cu[J]. Ann. Phys., 1925, 383: 439 |
| [3] | Bradley A J, Jay A.The formation of superlattices in alloys of iron and aluminium[J]. Proc. R. Soc. London, 1932, 136A: 210 |
| [4] | Bragg W L, Williams E J.The effect of thermal agitation on atomic arrangement in alloys[J]. Proc. R. Soc. London, 1934, 145A: 699 |
| [5] | Williams E J.The effect of thermal agitation on atomic arrangement in alloys. III[J]. Proc. R. Soc. London, 1935, 152A: 231 |
| [6] | Bethe H A.Statistical theory of superlattices[J]. Proc. R. Soc. London, 1935, 150A: 552 |
| [7] | Cowley J M.An approximate theory of order in alloys[J]. Phys. Rev., 1950, 77: 669 |
| [8] | Cowley J M.Short-and long-range order parameters in disordered solid solutions[J]. Phys. Rev., 1960, 120: 1648 |
| [9] | Cowley J.Short-range order and long-range order parameters[J]. Phys. Rev., 1965, 138: A1384 |
| [10] | Dong C, Wang Q, Qiang J B, et al.From clusters to phase diagrams: Composition rules of quasicrystals and bulk metallic glasses[J]. J. Phys, 2007, 40D: R273 |
| [11] | Dong D D.Composition origin of metallic glasses and solid solution alloys: Short-range-order structural unit [D]. Dalian: Dalian University of Technology, 2017(董丹丹. 金属玻璃和固溶体合金的成分根源: 近程序结构单元 [D]. 大连: 大连理工大学, 2017) |
| [12] | Zhang J, Wang Q, Wang Y M, et al.Revelation of solid solubility limit Fe/Ni= 1/12 in corrosion resistant Cu-Ni alloys and relevant cluster model[J]. J. Mater. Res., 2010, 25: 328 |
| [13] | Li F W, Qiang J B, Wang Y M, et al.Revisiting Al-Ni-Zr bulk metallic glasses using the 'cluster-resonance' model[J]. Chin. Sci. Bull., 2011, 56: 3902 |
| [14] | Dong D D, Zhang S, Wang Z J, et al.Composition interpretation of binary bulk metallic glasses via principal cluster definition[J]. Mater. Des., 2016, 96: 115 |
| [15] | Luo L J, Chen H, Wang Y M, et al.24 electron cluster formulas as the 'molecular' units of ideal metallic glasses[J]. Philos. Mag., 2014, 94: 2520 |
| [16] | Dong D D, Dong C.Composition interpretation procedures of bulk metallic glasses via example of Cu64Zr36[J]. J. Non-Cryst. Solids, 2017, 460: 125 |
| [17] | Mackay A L, Finney J L.Structuration[J]. J. Appl. Crystallogr., 1973, 6: 284 |
| [18] | Chen H, Qiang J B, Wang Q, et al.A cluster-resonance criterion for Al-TM quasicrystal compositions[J]. Isr. J. Chem., 2011, 51: 1226 |
| [19] | Hume-Rothery W, Smallman R E, Haworth C W.The Structure of Metals and Alloys[M]. London: The Institute of Metals, 1969: 1 |
| [20] | Cahn R W.Homo or hetero?[J]. Nature, 1978, 271: 407 |
| [21] | Jones H.Notes on work at the University of Bristol, 1930-7[J]. Proc. R. Soc. London, 1980, 371A: 52 |
| [22] | Friedel J.Electronic structure of primary solid solutions in metals[J]. Adv. Phys., 1954, 3: 446 |
| [23] | Li Z Z.Solid State Theory [M]. Beijing: Higher Education Press, 2002: 1(李正中. 固体理论[M]. 北京: 高等敎育出版社, 2002: 1) |
| [24] | Friedel J.Metallic alloys[J]. Il Nuovo Cimento (1955-1965), 1958, 7: 287 |
| [25] | Dong D D, Zhang S, Wang Z R, et al.Nearest-neighbor coordination polyhedral clusters in metallic phases defined using Friedel oscillation and atomic dense packing[J]. J. Appl. Crystallogr., 2015, 48: 2002 |
| [26] | Waseda Y, Suzuki K.Atomic distribution and magnetic moment in liquid iron by neutron diffraction[J]. Phys. Status Solidi, 1970, 39B: 669 |
| [27] | Mauro N A, Bendert J C, Vogt A J, et al.High energy x-ray scattering studies of the local order in liquid Al[J]. J. Chem. Phys., 2011, 135: 044502 |
| [28] | Abrikosov I A, Niklasson A M N, Simak S I, et al. Order-N Green's function technique for local environment effects in alloys[J]. Phys. Rev. Lett., 1996, 76: 4203 |
| [29] | Stolz U, Arpshofen I, Sommer F, et al.Determination of the enthalpy of mixing of liquid alloys using a high-temperature mixing calorimeter[J]. J. Phase Equil., 1993, 14: 473 |
| [30] | Baker H, Okamoto H.Alloy phase diagrams[M]. ASM International: ASM Handbook, 1992, 3: 501 |
| [31] | Metals A S F, Davis J R. Properties and selection: Nonferrous alloys and special-purpose materials[M]. ASM International: ASM Handbook, 2009: 1 |
| [32] | Reinhard L, Sch?nfeld B, Kostorz G, et al.Short-range order in α-brass[J]. Phys. Rev., 1990, 41: 1727 |
| [33] | Gaskell P H.On the density of transition metal-metalloid glasses[J]. Acta Metall., 1981, 29: 1203 |
| [34] | Aalders J, Van Dijk C, Radelaar S.Neutron scattering study of short-range clustering in CuNi (Fe) alloys[J]. J. Phys. Met. Phys., 1984, 14F: 2801 |
| [35] | Massalski T.The Al-Cu (aluminum-copper) system[J]. Bull. Alloy Phase Diagr., 1980, 1: 27 |
| [36] | Takeuchi A, Inoue A.Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element[J]. Mater. Trans., 2005, 46: 2817 |
| [37] | Koo Y M, Cohen J B.The structure of GP zones in Cu-10.9at.% Be[J]. Acta Metall., 1989, 37: 1295 |
| [38] | Chakrabarti D J, Laughlin D E, Tanner L E.The Be-Cu (beryllium-copper) system[J]. Bull. Alloy Phase Diagr., 1987, 8: 269 |
/
| 〈 |
|
〉 |