Orginal Article

Brazing of Coated Al Foil Filler to AlN Ceramic

  • Xiaoyi ZHANG ,
  • Hailong SHANG ,
  • Bingyang MA ,
  • Rongbin LI ,
  • Geyang LI
Expand
  • 1 State Key Laboratory of Metal Matrix Composites, Shanghai JiaoTong University, Shanghai 200240, China
    2 Shanghai Dianji University, Shanghai 201306, China

Received date: 2017-05-02

  Online published: 2018-01-30

Supported by

Supported by National Natural Science Foundation of China (Nos.51401120 and 51671125) and Natural Science Foundation of Shanghai (No.16ZR1412800)

Abstract

The wettabilities of molten metals on ceramics are poor normally. In order to improve the wettability, all existing ceramic brazing methods introduce a compound transition layer formed by the reaction of active metal and ceramic. The transition layer between brazing seam and ceramic however creates negative effect on the properties of brazing joints. Although Al is the scarce metal which can wet some ceramics such as AlN and Al2O3 without reaction, the difficulty of removing oxide layer on surface prevents it being ceramic brazing filler. This work proposed a kind of coated Al foil filler able to remove its own Al2O3 film and an elevating temperature brazing process to enhance Al/AlN joint strength. Removing Al2O3 film effect of vapor deposited Ni/Al double layer film on Al foil and the effect of brazing temperature on improving joint strength were studied. The results showed that due to buried by Ni/Al double layer film, Al2O3 film on Al foil original surface broken and was swept in Al-1%Ni (atomic fraction) alloy liquid during heating and melting process. As a result, the direct brazing of Al to AlN without interface reaction transition layer was realized. The joint strength was significantly enhanced by elevating brazing temperature. When brazing at 680 ℃, the joint fractured along the interface between Al seam and AlN and the sheer strength was 79 MPa because of Al liquid not wetting AlN. With the elevating of brazing temperature, the wettability and interface strength of Al/AlN improved. The fracture gradually transferred to brazing seam from interface. The joint strength increased and reached to the maximum value of 146 MPa at 840 ℃.

Cite this article

Xiaoyi ZHANG , Hailong SHANG , Bingyang MA , Rongbin LI , Geyang LI . Brazing of Coated Al Foil Filler to AlN Ceramic[J]. Acta Metall Sin, 2018 , 54(4) : 575 -580 . DOI: 10.11900/0412.1961.2017.00159

References

[1] Wingqvist G.AlN-based sputter-deposited shear mode thin film bulk acoustic resonator (FBAR) for biosensor applications—A review[J]. Surf. Coat. Technol., 2010, 205: 1279
[2] Naidich Y V, Zhuravlev V S, Gab I I, et al.Liquid metal wettability and advanced ceramic brazing[J]. J. Eur. Ceram. Soc., 2008, 28: 717
[3] Wang C B, Li S J, Li S Z, et al.Wettability and interfacial reactions for AlN/CuTi and AlN/SnTi systems[J]. Ceram. Int., 2012, 38: 1099
[4] Heo Y J, Kim H T, Kim K J, et al.Enhanced heat transfer by room temperature deposition of AlN film on aluminum for a light emitting diode package[J]. Appl. Therm. Eng., 2013, 50: 799
[5] Souza J C M, Nascimento R M, Martinelli A E. Characterization of dental metal-ceramic interfaces immersed in artificial saliva after substructural mechanical metallization with titanium[J]. Surf. Coat. Technol., 2010, 205: 787
[6] Yadav D P, Kaul R, Ganesh P, et al.Study on vacuum brazing of high purity alumina for application in proton synchrotron[J]. Mater. Des., 2014, 64: 415
[7] Asthana R, Singh M.Joining of partially sintered alumina to alumina, titanium, Hastealloy and C-SiC composite using Ag-Cu brazes[J]. J. Eur. Ceram. Soc., 2008, 28: 617
[8] Jarrige J, Joyeux T, Lecompte J P, et al.Comparison between two processes using oxygen in the Cu/AlN bonding[J]. J. Eur. Ceram. Soc., 2007, 27: 855
[9] Lang F, Yamaguchi H, Ohashi H, et al.Improvement in joint reliability of SiC power devices by a diffusion barrier between Au-Ge solder and Cu/Ni(P)-metalized ceramic substrates[J]. J. Electron. Mater., 2011, 40: 1563
[10] Wang Y, Yang Z W, Zhang L X, et al.Low-temperature diffusion brazing of actively metallized Al2O3 ceramic tube and 5A05 aluminum alloy[J]. Mater. Des., 2015, 86: 328
[11] Chen B, Xiong H P, Cheng Y Y, et al.Microstructure and property of AlN joint brazed with Au-Pd-Co-Ni-V brazing filler[J]. J. Mater. Sci. Technol., 2015, 31: 1034
[12] Su C Y, Pan C T, Lo M S.Microstructure and mechanical properties of AlN/Cu brazed joints[J]. J. Mater. Eng. Perform., 2014, 23: 3299
[13] Kozlova O, Braccini M, Voytovych R, et al.Brazing copper to alumina using reactive CuAgTi alloys[J]. Acta Mater., 2010, 58: 1252
[14] Ho H N, Wu S T.The wettability of molten aluminum on sintered aluminum nitride substrate[J]. Mater. Sci. Eng., 1998, A248: 120
[15] Jeurgens L P H, Sloof W G, Tichelaar F D, et al. Growth kinetics and mechanisms of aluminum-oxide films formed by thermal oxidation of aluminum[J]. J. Appl. Phys., 2002, 92: 1649
[16] Prin G R, Baffie T, Jeymond M, et al.Contact angles and spreading kinetics of Al and Al-Cu alloys on sintered AlN[J]. Mater. Sci. Eng., 2001, A298: 34
[17] Taranets N Y, Naidich Y V.Wettability of aluminum nitride by molten metals[J]. Powder Metall. Met. Ceram., 1996, 35: 282
[18] Sangghaleh A, Halali M.An investigation on the wetting of polycrystalline alumina by aluminium[J]. Mater. Process. Technol., 2008, 197: 156
[19] Lee S B, Kim Y M.Direct observation of in-plane ordering in the liquid at a liquid Al/α-Al2O3 interface[J]. Acta Mater., 2011, 59: 1383
[20] Strohmeier B R.An ESCA method for determining the oxide thickness on aluminum alloys[J]. Surf. Interface Anal., 1990, 15: 51
[21] Garcia-Cordovilla C, Louis E, Narciso J.Pressure infiltration of packed ceramic particulates by liquid metals[J]. Acta Mater., 1999, 47: 4461
[22] Chen F, Shi K C, Sun S Y, et al.Direct brazing of Al/Al2O3 without wettability of molten metal[J]. J. Inorg. Mater., 2016, 31: 602(陈凡, 石恺成, 孙士阳 等. 不基于熔态润湿的Al/Al2O3直接钎焊 [J]. 无机材料学报, 2016, 31: 602)
[23] Zhao B W, Shang H L, Chen F, et al."Wetting" and brazing of AlN by sputtered Al[J]. Acta Phys. Sin., 2016, 65: 086801(赵博文, 尚海龙, 陈凡等. 溅射Al对AlN的“润湿”与钎焊[J]. 物理学报, 2016, 65: 086801)
[24] Liu G L, Ma B Y, Shang H L, et al.Wettability improvement and brazing of Si3N4 by sputtered Al[J]. Acta Metall. Sin., 2017, 53: 1645(刘葛亮, 马冰洋, 尚海龙等. 溅射Al对Si3N4润湿性的改善与钎焊[J]. 金属学报, 2017, 53: 1645)
[25] Zhang Q, ?a??n T, van Duin A, et al. Adhesion and nonwetting-wetting transition in the Al/α-Al2O3 interface[J]. Phys. Rev., 2004, 69B: 045423
Outlines

/