Orginal Article

Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating

  • Chengyang JIANG ,
  • Yingfei YANG ,
  • Zhengyi ZHANG ,
  • Zebin BAO ,
  • Shenglong ZHU ,
  • Fuhui WANG
Expand
  • 1 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3 China National South Aviation Industry Co., Ltd., Zhuzhou 412002, China

Received date: 2017-09-08

  Online published: 2018-01-29

Supported by

Supported by National Natural Science Foundation of China (Nos.51671202 and 51301184), Defense Industrial Technology Development Program (No.JCKY2016404C001) and Liaoning BaiQianWan Talents Program

Abstract

Prior to practical service, hot-section components (e.g. airfoils and vanes) of a gas turbine engine are necessarily coated by a protective metallic coating (such as aluminide diffusion coating, modified aluminide coating and MCrAlY overlay etc.) to resist high temperature oxidation and hot corrosion. Among the modified aluminide coatings, the coating with Pt-modification has attracted great attention and is widely used in applications requiring high reliability and extended service life since it possesses superior oxidation/corrosion resistance at high temperature. The presence of Pt in aluminide coating is favorable for increasing bonding strength of oxide scale, enlarging phase region of β-NiAl and confining detrimental effect of sulphur etc. Although Pt-modification has exhibited visible benefits for acquiring better high-temperature performance, it is far from satisfaction to develop an ideal aluminide diffusion coating. Reactive elements such as Y, Hf, Zr or their oxides have been employed to modify the nickel aluminide coating system, with an aim to further improve scale adhesion and promote exclusive formation of α-Al2O3 simultaneously. In this work, a Zr-doped PtAl2+(Ni, Pt)Al dual-phase aluminide coating was prepared on a Ni-based single crystal superalloy by co-deposition of Pt-Zr through electroplating and subsequent aluminization treatments. The coating was mainly composed of three layers: the outmost layer consisted of double phases with PtAl2 particles dispersed in β-(Ni, Pt)Al domain, while the interlayer comprised β-(Ni, Pt)Al with small amount of Cr-precipitates, and the bottom layer was an inter-diffusion zone (IDZ). Zirconium was mainly distributed inside β-(Ni, Pt)Al solid solution in both the outmost layer and the interlayer. Compared with normal PtAl2+(Ni, Pt)Al dual-phase coating, the hot corrosion behavior of the Zr-doped PtAl2+(Ni, Pt)Al coating was assessed in a salt mixture of Na2SO4/NaCl (75:25, mass ratio) at 850 ℃ in static air. The results indicated that the Zr-doped PtAl2+(Ni, Pt)Al dual-phase coating exhibited superior hot corrosion resistance since Zr was confirmed able to capture and fix S and Cl to diminish their detrimental effects. Meanwhile, a pre-oxidation treatment did not effectively improve the overall hot corrosion resistance of normal PtAl2+(Ni, Pt)Al coating because the thin alumina scale formed during pre-oxidation was unable to prohibit the sustained inward-invasion of the mixed salt.

Cite this article

Chengyang JIANG , Yingfei YANG , Zhengyi ZHANG , Zebin BAO , Shenglong ZHU , Fuhui WANG . Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating[J]. Acta Metall Sin, 2018 , 54(4) : 581 -590 . DOI: 10.11900/0412.1961.2017.00376

References

[1] Rapp R A.Hot corrosion of materials: A fluxing mechanism?[J]. Corros. Sci., 2002, 44: 209
[2] Padture N P, Gell M, Jordan E H.Thermal barrier coatings for gas-turbine engine applications[J]. Science, 2002, 296: 280
[3] Zeng C L, Wu W T, Guo J T.High temperature hot corrosion of NiAl-20%Fe with its surface aluminide coating[J]. Acta Metall. Sin., 1996, 32: 197(曾潮流, 吴维?, 郭建亭. 渗铝NiAl-20%Fe金属间合金的高温热腐蚀[J]. 金属学报, 1996, 32: 197)
[4] Rhys-Jones T N. Coatings for blade and vane applications in gas turbines[J]. Corros. Sci., 1989, 29: 623
[5] Guan H R, Lou H Y, Mao X Y, et al.Deterioration of aluminide coating on nickel-base superalloys[J]. Acta Metall. Sin., 1981, 17: 412(管恒荣, 楼翰一, 毛晓禹等. 两种高温合金渗Al防护层的退化过程[J]. 金属学报, 1981, 17: 412)
[6] Felten E J, Pettit F S.Development, growth, and adhesion of Al2O3 on platinum-aluminum alloys[J]. Oxid. Met., 1976, 10: 189
[7] Kohlscheen J, Stock H R.Deposition of silicon enriched nickel aluminide coatings on internally cooled airfoils[J]. Met. Finish., 2009, 107: 22
[8] Li M J, Sun X F, Guan H R, et al.High temperature hot-corrosion behavior of (Ni, Pd)Al coating[J]. Acta Metall. Sin., 2004, 40: 773(李猛进, 孙晓峰, 管恒荣等. (Ni, Pd)Al涂层的高温热腐蚀[J]. 金属学报, 2004, 40: 773)
[9] Li M J, Sun X F, Guan H R, et al.High temperature oxidation behavior of Pd-Ni-Al coating[J]. Acta Metall. Sin., 2003, 39: 755(李猛进, 孙晓峰, 管恒荣等. Pd-Ni-Al涂层的高温长期氧化行为[J]. 金属学报, 2003, 39: 755)
[10] Boone D H, Deb P, Purvis L I, et al.Surface morphology of platinum modified aluminide coatings[J]. J. Vac. Sci. Technol., 1985, 3A: 2557
[11] Deb P, Boone D H, Streiff R.Platinum aluminide coating structural effects on hot corrosion resistance at 900 ℃[J]. J. Vac. Sci. Technol., 1985, 3A: 2578
[12] Deb P, Boone D H, Manley II T F. Surface instability of platinum modified aluminide coatings during 1100 ℃ cyclic testing[J]. J. Vac. Sci. Technol., 1987, 5A: 3366
[13] Stringer J. The reactive element effect in high-temperature corrosion [J]. Mater. Sci. Eng., 1989, A120-121: 129
[14] Wei F I, Stott F H.The development of Cr2O3 scales on iron-chromium alloys containing reactive elements[J]. Corro. Sci., 1989, 29: 839
[15] Thanneeru R, Patil S, Deshpande S, et al.Effect of trivalent rare earth dopants in nanocrystalline ceria coatings for high-temperature oxidation resistance[J]. Acta Mater., 2007, 55: 3457
[16] Sánchez L, Bolívar F J, Hierro M P, et al.Effect of Ce and La additions in low temperature aluminization process by CVD-FBR on 12%Cr ferritic/martensitic steel and behaviour in steam oxidation[J]. Corros. Sci., 2008, 50: 2318
[17] Hong S J, Hwang G H, Han W K, et al.Effect of zirconium addition on cyclic oxidation behavior of platinum-modified aluminide coating on nickel-based superalloy[J]. Intermetallics, 2010, 18: 864
[18] Liu Q, Yang Y F, Bao Z B, et al.Oxidation property and failure mechanism of a single phase PtAl2 coating[J]. Acta Metall. Sin., 2014, 50: 1102(柳泉, 阳颖飞, 鲍泽斌等. PtAl2单相涂层的高温抗氧化性能及失效机制研究[J]. 金属学报, 2014, 50: 1102)
[19] Moretto P, Bressers J, Arrell D J.Evolution of a PtAl2 coating on the nickel-base alloy CMSX-6 subjected to thermo-mechanical fatigue[J]. Mater. Sci. Eng., 1999, A272: 310
[20] Smeggil J G.Some comments on the role of yttrium in protective oxide scale adherence[J]. Mater. Sci. Eng., 1987, 87: 261
[21] Smialek J L.Adherent Al2O3 scales formed on undoped nicrai alloys[J]. Metall. Mater. Trans., 1987, 18A: 164
[22] Smialek J L, Jayne D T, Schaeffer J C, et al.Effects of hydrogen annealing, sulfur segregation and diffusion on the cyclic oxidation resistance of superalloys: A review[J]. Thin Solid Films, 1994, 253: 285
[23] Lee W Y, Wright I G, Pint B A, et al.Effects of sulfur impurity on the scale adhesion behavior of a desulfurized Ni-based superalloy aluminized by chemical vapor deposition[J]. Metall. Mater. Trans., 1998, 29A: 833
[24] Eliaz N, Shemesh G, Latanision R M.Hot corrosion in gas turbine components[J]. Eng. Fail. Anal., 2002, 9: 31
[25] Barin I, translated by Cheng N L, Niu S T, Xu G Y, et al. Thermochemical Data of Pure Substances [M]. Beijing: Science Press, 2010: 563(Barin I 著, 程乃良, 牛四通, 徐桂英 等译. 纯物质热化学数据手册 [M]. 北京: 科学出版社, 2010: 563)
[26] Bao Z B, Wang Q M, Li W Z, et al.Preparation and hot corrosion behaviour of an Al-gradient NiCoCrAlYSiB coating on a Ni-base superalloy[J]. Corros. Sci., 2009, 51: 860
[27] Shinata Y.Accelerated oxidation rate of chromium induced by sodium chloride[J]. Oxid. Met., 1987, 27: 315
[28] Shinata Y. Nishi Y.NaCl-induced accelerated oxidation of chromium[J]. Oxid. Met., 1986, 26: 201
[29] Deodeshmukh V, Gleeson B.Effects of platinum on the hot corrosion behavior of Hf-modified γ′-Ni3Al +γ-Ni-based alloys[J]. Oxid. Met., 2011, 76: 43
Outlines

/