Effect of Austenitization Temperature on the Dry Sliding Wear Properties of a Medium Carbon Quenching and Partitioning Steel
Received date: 2017-04-14
Online published: 2018-01-22
Supported by
Supported by National Natural Science Foundation of China (No.51071101)
The quenching and partitioning (Q&P) process is a promising method to create novel martensitic steels with improved balance of strength and ductility by retaining considerable amount of austenite in martensitic matrix. This kind of microstructure provides suitable condition to study wear and abrasion mechanism since the effect of retained austenite on the wear property of martensitic steel is still controversial by now. Selecting traditional quenching and tempering (Q&T) sample with identical composition Fe-0.4C-1.5Mn-1.5Si as reference, the dry sliding wear property of Q&P samples with different austenitization temperatures was studied. The results show that the volume fraction of retained austenite in Q&P samples with full austenitization at 860 or 1000 °C respectively is nearly the same (about 14.37% in the former and about 13.79% in the later), and the corresponding carbon concentration (mass fraction) in retained austenite is relatively high (1.37% in the former and 1.38% in the later). Under the conditions of low loading (50 N) and slide speed (40 mm/s), it is not easy to induce martensitic transformation because of very strong mechanical stability, leading to the low friction and wear resistance of samples. The slight better wear resistance of samples with low austenitization temperature can be attributed to microstructural refinement. When the austenitization temperature was 800 ℃, the intercritical Q&P samples were obtained. Microstructure analysis indicates there exist the highest volume fraction of retained austenite (about 22.28%) and a small volume fraction of ferrite (about 6.75%) in martensitic matrix, which results in the lowest microhardness among present four kinds of samples. However, the mechanical stability of retained austenite in this kind of sample is weak due to the low carbon concentration (about 1.06%). The obvious martensitic transformation accompanying sliding wear contributes to extra hardening and provides additional compressive stress on the touching surface caused by volume expansion. Therefore, the intercritical Q&P samples exhibit the best wear resistance. Based on the experimental results, it is true that the mechanical stability instead of the amount of retained austenite in martensitic steel plays a critical role in improving wear resistance.
Jilan YANG , Yuankai JIANG , Jianfeng GU , Zhenghong GUO , Haiyan CHEN . Effect of Austenitization Temperature on the Dry Sliding Wear Properties of a Medium Carbon Quenching and Partitioning Steel[J]. Acta Metall Sin, 2018 , 54(1) : 21 -30 . DOI: 10.11900/.0412.1961.2017.00129
| [1] | Speer J G, Matlock D K, De Cooman B C, et al. Carbon partitioning into austenite after martensite transformation[J]. Acta Mater., 2003, 51: 2611 |
| [2] | Santofimia M J, Nguyen-Minh T, Zhao L, et al.New low carbon Q&P steels containing film-like intercritical ferrite[J]. Mater. Sci. Eng., 2010, A527: 6429 |
| [3] | Santofimia M J, Zhao L, Petrov R, et al.Microstructural development during the quenching and partitioning process in a newly designed low-carbon steel[J]. Acta Mater., 2011, 59: 6059 |
| [4] | Wang L, Speer J G.Quenching and partitioning steel heat treatment[J]. Metall. Microstruct. Anal., 2013, 2: 268 |
| [5] | Zhao C, Tang D, Jiang H T, et al.Process simulation and microstructure analysis of low carbon Si-Mn quenched and partitioned steel[J]. J. Iron Steel Res. Int., 2008, 15: 82 |
| [6] | Speer J G,Rizzo Assun??o F C R,Matlock D K,et al. The "quenching and partitioning" process: Background and recent progress[J]. Mater. Res., 2005, 8: 417 |
| [7] | Zhang K, Xu W Z, Guo Z H, et al.Effects of novel Q-P-T and traditional Q-T processes on the microstructure and mechanical properties of martensitic steels with different carbon content[J]. Acta Metall. Sin., 2011, 47: 489(张珂, 许为宗, 郭正洪等. 新型Q-P-T和传统Q-T工艺对不同C含量马氏体钢组织和力学性能的影响[J]. 金属学报, 2011, 47: 489) |
| [8] | Weng Y Q, Dong H, Gan Y.Advanced Steels [M]. Beijing: Metallurgical Industry Press, 2011: 67 |
| [9] | Wang C Y, Shi J, Liu S, et al.Study on three-body impact-abrasion of steel treated by quenching-partitioning-tempering process[J]. Chin. J. Mater. Res., 2009, 23: 305(王存宇, 时捷, 刘苏等. 淬火-配分-回火工艺处理钢的三体冲击磨损性能研究[J]. 材料研究学报, 2009, 23: 305) |
| [10] | Liu S G, Dong S S, Yang F, et al.Application of quenching-partitioning-tempering process and modification to a newly designed ultrahigh carbon steel[J]. Mater. Des., 2014, 56: 37 |
| [11] | Wang C Y, Li X D, Chang Y, et al. Comparison of three-body impact abrasive wear behaviors for quenching-partitioning-tempering and quenching-tempering 20Si2Ni3 steels[J]. Wear, 2016, 362-363: 121 |
| [12] | Hu F, Wu K M, Hodgson P D.Effect of retained austenite on wear resistance of nanostructured dual phase steels[J]. Mater. Sci. Technol., 2016, 32: 40 |
| [13] | Kim H J, Kweon Y G.The effects of retained austenite on dry sliding wear behavior of carburized steels[J]. Wear, 1996, 193: 8 |
| [14] | Riviére J P, Brin C, Villain J P.Structure and topography modifications of austenitic steel surfaces after friction in sliding contact[J]. Appl. Phys., 2003, 76A: 277 |
| [15] | Zandrahimi M, Bateni M R, Poladi A, et al.The formation of martensite during wear of AISI 304 stainless steel[J]. Wear, 2007, 263: 674 |
| [16] | Molinari A, Pellizzari M, Gialanella S, et al.Effect of deep cryogenic treatment on the mechanical properties of tool steels[J]. J. Mater. Proc. Technol., 2001, 118: 350 |
| [17] | Wei X C, Li J, Meng H.Tribological characteristics of HSLA TRIP steel containing meta-stable retained austenite[J]. Tribology, 2006, 26: 49(韦习成, 李健, Meng H.含亚稳残余奥氏体HSLA TRIP钢的摩擦磨损性能研究[J]. 摩擦学学报, 2006, 26: 49) |
| [18] | Liu Y, Yu W P, Zhang J D, et al.Effect of deep cryogenic treatment on microstructure and mechanical properties of T8A steel[J]. Trans. Mater. Heat Treat., 2010, 31(10): 48(刘勇, 于文平, 张金东等. 深冷处理对T8A钢组织和力学性能的影响[J]. 材料热处理学报, 2010, 31(10): 48) |
| [19] | Wu H Y.Study on friction-induced martensite transformation of retained austenite and its wear resistance[J]. Hot Work. Technol., 2007, 36(16): 32(吴海燕. 残余奥氏体的摩擦诱发马氏体相变行为及其耐磨特性的研究[J]. 热加工工艺, 2007, 36(16): 32) |
| [20] | Arques J L, Prado J M.The dry wear resistance of a carbonitrided steel[J]. Wear, 1985, 103: 321 |
| [21] | Siepak J.The influence of contact stress on the wear of a carburized steel case with a high content of retained austenite[J]. Wear, 1982, 80: 301 |
| [22] | Jatczak C F.Retained Austenite and its Measurement by X-ray Diffraction [R]. SAE Technical Paper 800426. Detroit: Society of Automotive Engineers, Inc., 1980: 6 |
| [23] | Xiong Z L, Cai Q W, Jiang H T, et al.Research on mechanical stability of austenite in TRIP steels[J]. J. Mater. Eng., 2011, (3): 11(熊自柳, 蔡庆伍, 江海涛等. TRIP钢中奥氏体的力学稳定性研究[J]. 材料工程, 2011, (3): 11) |
| [24] | Huang F, Yang J L, Guo Z H, et al.Effect of partitioning treatment on the mechanical property of Fe-0.19C-1.47Mn-1.50Si steel with refined martensitic microstructure[J]. Metall. Mater. Trans., 2016, 47A: 1072 |
| [25] | Yao Y Q.The research on friction and wear properties of low-carbon low-alloy steels [D].Nanjing: Nanjing University of Science and Technology, 2013)(姚寅群.低碳低合金钢摩擦磨损性能研究 [D]. 南京: 南京理工大学, 2013) |
| [26] | Wang Y, Lei T Q, Liu J J.Tribo-metallographic behavior of high carbon steels in dry sliding: II. Microstructure and wear[J]. Wear, 1999, 231: 12 |
| [27] | Sun J S.Wear of Metals [M]. Beijing: Metallurgical Industry Press, 1992: 182(孙家枢. 金属的磨损 [M]. 北京: 冶金工业出版社, 1992: 182) |
| [28] | Xu Y L, Qin H Q, Pang Z G, et al.Wear resistance at high temperature of H13 steel after RE-N-C-S-V-Nb multi-element penetrating[J]. Surf. Technol., 2015, 44(4): 60(徐永礼, 覃海泉, 庞祖高等. RE-N-C-S-V-Nb多元共渗H13钢的高温耐磨性[J]. 表面技术, 2015, 44(4): 60) |
| [29] | Wang M S, Zhu Y F.The plastic induced martensite transformation of a medium manganese austenite steel[J].Phys. Tests. Chem. Anal. (Phys.Test.), 1991, A(1): 23(王明胜, 朱延福.奥氏体中锰钢的形变诱发马氏体[J]. 理化检验(物理分册), 1991, A(1): 23) |
| [30] | Society of Heat Treatment,Chinese Society of Mechanical Engineers. The Friction Wear and Heat Treatment of Metals [M]. Beijing: Mechanical Industry Press, 1988: 93(中国机械工程学会热处理学会. 金属的摩擦磨损与热处理 [M]. 北京: 机械工业出版社, 1988: 93) |
/
| 〈 |
|
〉 |