Investigation on the Change of Thermoelectric Power of Al-Fe Hypoeutectic Alloy Melt Caused by AC Magnetic Field

  • Jianfeng ZHANG ,
  • Qing LAN ,
  • Qichi LE
Expand
  • 1 College of Sciences, Northeastern University, Shenyang 110819, China
    2 Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China

Received date: 2017-10-10

  Online published: 2017-12-21

Supported by

Supported by China Postdoctoral Science Foundation Funded Project (No.2015M571320) and Fundamental Research Funds for the Central Universities (No.N150504002)

Abstract

A lot of studies have shown that electromagnetic field can significantly refine the metal solidification structure, thus improve the deformation properties and functional performance of metallic materials. However, the mechanism of how electromagnetic field affects melt structure remains unclear, so an intensive study of the effects of electromagnetic field on melt structure is very important for an in-depth understanding of the essence of melt solidification under external electromagnetic field. The effect of alternating current (AC) magnetic field with different exciting currents, magnetic frequencies and loading time on the thermoelectric potential difference (U) and melt microstructure of Al-0.99%Fe (mass fraction) hypoeutectic alloy at different temperatures was investigated in this work. The results showed that AC magnetic field would lead to a decrease in U of liquid Al-0.99%Fe hypoeutectic alloy. When the magnetic field was removed, the decreased thermoelectric potential difference experienced a rapid recovery process and a poor recovery process to increase to the initial value. The influence of AC magnetic field on U was different at different temperatures. With the increase of the magnetic frequency, the influence of AC magnetic field on U decreased. And the influence of AC magnetic field on U increased with the increase of the exciting current and loading time, however, there was a saturated loading time. There was a correlation between the change of U of Al-0.99%Fe hypoeutectic alloy and the change of size of the primary α-Al phase caused by AC magnetic field, therefore, the change of thermoelectric potential difference could be used to characterize the effect of AC magnetic field on the microstructure of the alloy melt of Al-0.99%Fe hypoeutectic alloy.

Cite this article

Jianfeng ZHANG , Qing LAN , Qichi LE . Investigation on the Change of Thermoelectric Power of Al-Fe Hypoeutectic Alloy Melt Caused by AC Magnetic Field[J]. Acta Metall Sin, 2018 , 54(7) : 1042 -1050 . DOI: 10.11900/0412.1961.2017.00421

References

[1] Hou L G, Liu M L, Wang X D, et al.Cryogenic processing high-strength 7050 aluminum alloy and controlling of the microstructures and mechanical properties[J]. Acta Metall. Sin., 2017, 53: 1075(侯陇刚, 刘明荔, 王新东等. 高强7050铝合金超低温大变形加工与组织、性能调控[J]. 金属学报, 2017, 53: 1075)
[2] Jia P, Wang E G, Lu H, et al.Effect of electromagnetic field on micro-structure and mechanical property for Inconel 625 superalloy[J]. Acta Metall. Sin., 2013, 49: 1573(贾鹏, 王恩刚, 鲁辉等. 电磁场对Inconel 625合金凝固组织及力学性能的影响[J]. 金属学报, 2013, 49: 1573)
[3] Li X, Ren Z M, Fautrelle Y.Phase distribution and phase structure control through a high gradient magnetic field during the solidification process[J]. Mater. Des., 2008, 29: 1796
[4] Gillon P.Uses of intense d.c. magnetic fields in materials processing[J]. Mater. Sci. Eng., 2000, A287: 146
[5] Chen DD, Zhang H T, Wang X J, et al.Investigation on microsegregation of Al-4.5%Cu alloy produced by low frequency electromagnetic casting[J]. Acta Metall. Sin., 2011, 47: 185(陈丹丹, 张海涛, 王向杰等. 低频电磁铸造Al-4.5%Cu合金微观偏析研究[J]. 金属学报, 2011, 47: 185)
[6] Liu X, Zhang J F, Li H Y, et al.Electrical resistivity behaviors of liquid Pb-Sn binary alloy in the presence of ultrasonic field[J]. Ultrasonics, 2015, 55: 6
[7] Xu X J, Deng A Y, Wang E G, et al.Evolvement mechanism of surface oscillation marks on round billet during soft-contact electromagnetic continuous casting[J]. Acta Metall. Sin., 2009, 45: 464(许秀杰, 邓安元, 王恩刚等. 电磁软接触连铸圆坯表面振痕演变机理[J]. 金属学报, 2009, 45: 464)
[8] Zhang H T, Nagaumi H, Zuo Y B, et al.Coupled modeling of electromagnetic field, fluid flow, heat transfer and solidification during low frequency electromagnetic casting of 7XXX aluminum alloys: Part 1: Development of a mathematical model and comparison with experimental results[J]. Mater. Sci. Eng., 2007, A448: 189
[9] Zhang T, Ren W L, Dong J W, et al.Effect of high magnetic field on the primary dendrite arm spacing and segregation of directionally solidified superalloy DZ417G[J]. J. Alloys Compd., 2009, 487: 612
[10] Li M J, Tamura T, Miwa K.Controlling microstructures of AZ31 magnesium alloys by an electromagnetic vibration technique during solidification: From experimental observation to theoretical understanding[J]. Acta Mater., 2007, 55: 4635
[11] Wang Q, Li Y X.Theoretical study of electrical transport properties of liquid metals and alloys[J]. Mater. Rev., 2001, 15(8): 7(王强, 李言祥. 液态金属电子输运性质的理论研究[J]. 材料导报, 2001, 15(8): 7)
[12] Wang Q, Lu K Q, Li Y X.The relationship between electrical resistivity, thermopower and temperature for liquid InSb[J]. Acta Phys. Sin., 2001, 50: 1355(王强, 陆坤权, 李言祥. 液态InSb电阻率和热电势与温度的关系[J]. 物理学报, 2001, 50: 1355)
[13] Yakubtsov I A.Effects of composition and microstructure on behaviors of electrical resistivity during continuous heating above room temperature in Mg-based alloys[J]. J. Alloys Compd., 2010, 492: 153
[14] Chung D D L. Thermal analysis by electrical resistivity measurement[J]. J. Therm. Anal. Calorim., 2001, 65: 153
[15] Richardsen T, Loh?fer G, Egry I.Electrical resistivity of undercooled liquid Cu-Ni alloys[J]. Int. J. Thermophys., 2002, 23: 1207
[16] Abdellah A B, Grosdidier B, Osman S M, et al.Spin-state dependence of electrical resistivity and thermoelectric power of molten Al-Mn alloys: Experiment and theory[J]. J. Alloys Compd., 2016, 658: 1010
[17] Zu F Q, Shen R R, Xi Y, et al.Electrical resistivity of liquid Sn-Sb alloy[J]. J. Phys. Condens. Matter, 2006, 18: 2817
[18] Gaffar M A, Gaber A, Mostafa M S, et al.The effect of Cu addition on the thermoelectric power and electrical resistivity of Al-Mg-Si balanced alloy: A correlation study[J]. Mater. Sci. Eng., 2007, A465: 274
[19] Deng Y B, Geng H R, Wang Z M, et al.Recent research progress on structure sensitive properties of metal melt based on liquid structure changing[J]. Met. World, 2010, (1): 49(邓延波, 耿浩然, 王致明等. 基于液态结构变化的金属熔体结构敏感物性的研究进展[J]. 金属世界, 2010, (1): 49)
[20] Giuseppe G, Giuseppe P P.Solid State Physics [M]. Amsterdam: Academic Press, 2006: 419
[21] Cong H R, Bian X F, Li H, et al.Medium-range order structure in liquid Al80Fe20 alloy[J]. Acta Phys. Chim. Sin., 2002, 18: 39(丛红日, 边秀房, 李辉等. 液态Al80Fe20合金的中程有序结构[J]. 物理化学学报, 2002, 18: 39)
[22] Anderson P W.Absence of diffusion in certain random lattices[J]. Phys. Rev., 1958, 109: 1492
Outlines

/