In Vitro Corrosion Resistance of Ta2N Nanocrystalline Coating in Simulated Body Fluids
Received date: 2017-06-21
Online published: 2017-12-19
Supported by
Supported by National Natural Science Foundation of China (Nos.51374130 and 51675267) and State Key Program of National Natural Science Foundation of China (No.51635004)
Due to its combination of outstanding characteristics, such as superior biocompatibility, excellent mechanical properties as well as good corrosion resistance, Ti-6Al-4V alloy has gained much attention as one of the most popular load-bearing biomedical metals in the area of orthopedic and dental. Unfortunately, Ti-6Al-4V alloy suffers from the localized corrosion damage in human body ?uids containing high chloride ion concentrations, which leads to the release of metal ions into the human body. The released ions (e.g., Al and V) are found to not only cause allergic and toxic reactions but also exhibit potential negative effects on osteoblast behavior. To improve the corrosion resistance of Ti-6Al-4V alloy in simulated body ?uids, a 40 μm thick Ta2N nanocrystalline coating with an average grain size of 12.8 nm was engineered onto a Ti-6Al-4V substrate using a double cathode glow discharge technique. The hardness and elastic modulus of the Ta2N coating were determined to be (32.1±1.6) GPa and (294.8±4.2) GPa, respectively, and the adhesion strength of the coating deposited on Ti-6Al-4V substrate was found to be 56 N. There is no evidence of crack formation within the coating under loads ranging from 0.49 N to 9.8 N, implying that the Ta2N nanocrystalline coating has a high contact damage resistance. Moreover, the corrosion resistance of the Ta2N nanocrystalline coating is significantly greater than that of Ti-6Al-4V alloy when tested in naturally aerated Ringer's solution at 37 ℃. This is due to that the passive film developed on the coating has superior compactness compared with that formed on the uncoated Ti-6Al-4V alloy. XPS analysis indicated that at a low polarized potential, the passive film consisted of TaOxNy, which would be converted to Ta2O5 at a higher polarized potential. The analysis of Mott-Schottky curves suggested that the passive film formed on the coating exhibits n-type semiconductor properties and, as such, the density and diffusivity of carrier for the coating was considerably lower than that for the uncoated Ti-6Al-4V alloy.
Jiang XU , Xike BAO , Shuyun JIANG . In Vitro Corrosion Resistance of Ta2N Nanocrystalline Coating in Simulated Body Fluids[J]. Acta Metall Sin, 2018 , 54(3) : 443 -456 . DOI: 10.11900/0412.1961.2017.00246
| [1] | Geetha M, Singh A K, Asokamani R, et al.Ti based biomaterials, the ultimate choice for orthopaedic implants—A review[J]. Prog. Mater. Sci., 2009, 54: 397 |
| [2] | Zaffe D, Bertoldi C, Consolo U.Element release from titanium devices used in oral and maxillofacial surgery[J]. Biomaterials, 2003, 24: 1093 |
| [3] | Matusiewicz H.Potential release of in vivo trace metals from metallic medical implants in the human body: From ions to nanoparticles—A systematic analytical review[J]. Acta Biomater., 2014, 10: 2379 |
| [4] | Rahilly G, Price N.Current products and practice nickel allergy and orthodontics[J]. J. Orthod., 2003, 30: 171 |
| [5] | Kumazawa R, Watari F, Takashi N, et al.Effects of Ti ions and particles on neutrophil function and morphology[J]. Biomaterials, 2002, 23: 3757 |
| [6] | Souto R M, Laz M M, Reis R L.Degradation characteristics of hydroxyapatite coatings on orthopaedic TiAlV in simulated physiological media investigated by electrochemical impedance spectroscopy[J]. Biomaterials, 2003, 24: 4213 |
| [7] | Leit?o E, Sa C, Silva R A, et al.Electrochemical and surface modifications on N+-ion implanted Ti-6Al-4V immersed in HBSS[J]. Corros. Sci., 1995, 37: 1861 |
| [8] | Jiang P L, Lin L X, Zhang F, et al.Electrochemical construction of micro-nano spongelike structure on titanium substrate for enhancing corrosion resistance and bioactivity[J]. Electrochim. Acta, 2013, 107: 16 |
| [9] | Liu G H, Wang J, Yang S H, et al.Effect of a porous tantalum rod on early and intermediate stages of necrosis of the femoral head[J]. Biomed. Mater., 2010, 5: 065003 |
| [10] | Zitter H, Plenk H Jr.The electrochemical behavior of metallic implant materials as an indicator of their biocompatibility[J]. Biomed. J. Mater. Res, 1987, 21: 881 |
| [11] | Leng Y X, Sun H, Yang P, et al. Biomedical properties of tantalum nitride films synthesized by reactive magnetron sputtering [J]. Thin. Solid Films, 2001, 398-399: 471 |
| [12] | Kokubo T, Takadama H.How useful is SBF in predicting in vivo bone bioactivity[J]. Biomaterials, 2006, 27: 2907 |
| [13] | Zhang Y M, Chai F, Hornez J C, et al.The corrosion and biological behaviour of titanium alloys in the presence of human lymphoid cells and MC3T3-E1 osteoblasts[J]. Biomed. Mater, 2009, 4: 015004 |
| [14] | Lei W W, Liu D, Zhang J, et al.Direct synthesis and characterization of single-phase tantalum nitride (Ta2N) nanocrystallites by dc arc discharge[J]. J. Alloys Compd., 2008, 459: 298 |
| [15] | Cheng H, Hon M.Texture formation in titanium nitride films prepared by chemical vapor deposition[J]. J. Appl. Phys., 1996, 79: 8047 |
| [16] | Xu J, Li Z Y, Xu S, et al.A nanocrystalline zirconium carbide coating as a functional corrosion-resistant barrier for polymer electrolyte membrane fuel cell application[J]. J. Power Sources, 2015, 297: 359 |
| [17] | Musil J, Jirout M.Toughness of hard nanostructured ceramic thin films[J]. Surf. Coat. Technol., 2007, 201: 5148 |
| [18] | Hogmark S, Jacobson S, Larsson M.Design and evaluation of tribological coatings[J]. Wear, 2000, 246: 20 |
| [19] | Kannan A R S, Muralidharan S, Sarangapani K B, et al. Corrosion and anodic behaviour of zinc and its ternary alloys in alkaline battery electrolytes[J]. J. Power Sources, 1995, 57: 93 |
| [20] | Sun S, Podlaha E J.Electrodeposition of Mo-rich, MoNi alloys from an aqueous electrolyte[J]. J. Electrochem. Soc., 2012, 159: D97 |
| [21] | Alves V A, Reis R Q, Santos I C B, et al. In situ impedance spectroscopy study of the electrochemical corrosion of Ti and Ti-6Al-4V in simulated body fluid at 25 ℃ and 37 ℃[J]. Corros. Sci., 2009, 51: 2473 |
| [22] | Jiang Z L, Dai X, Middleton H.Effect of silicon on corrosion resistance of Ti-Si alloys[J]. Mater. Sci. Eng., 2011, B176: 79 |
| [23] | Vasilescu C, Drob S I, Moreno J M C, et al. Long-term corrosion resistance of new Ti-Ta-Zr alloy in simulated physiological fluids by electrochemical and surface analysis methods[J]. Corros. Sci., 2015, 93: 310. |
| [24] | Macdonald D D, Urquidi-Macdonald M.Theory of steady-state passive films[J]. J. Electrochem. Soc., 1990, 137: 2395 |
| [25] | Chang C C, Jeng J S, Chen J S.Microsteuctural and electrical characteristics of reactively sputtered Ta-N thin films[J]. Thin Solid Films, 2002, 413: 46 |
| [26] | Lamour P, Fioux P, Ponche A, et al.Direct measurement of the nitrogen content by XPS in self-passivated TaNx thin films[J]. Surf. Interface Anal., 2008, 40: 1430 |
| [27] | Olefjord I, Wegrelius L.The influence of nitrogen on the passivation of stainless steels[J]. Corros. Sci., 1996, 38: 1203 |
| [28] | Feng Z C, Cheng X Q, Dong C F, et al.Passivity of 316L stainless steel in borate buffer solution studied by Mott-Schottky analysis, atomic absorption spectrometry and X-ray photoelectron spectroscopy[J]. Corros. Sci., 2010, 52: 3646 |
| [29] | Jovic V D, Barsoum M W.Corrosion behavior and passive film characteristics formed on Ti, Ti3SiC2, and Ti4AlN3 in H2SO4 and HCl[J]. J. Electrochem. Soc., 2004, 151: B71 |
| [30] | Kerrec O, Devilliers D, Grout H, et al.Dielectric properties of anodic oxide films on tantalum[J]. Electrochim. Acta, 1995, 40: 719 |
| [31] | Silva R A, Walls M, Rondot B, et al.Electrochemical and microstructural studies of tantalum and its oxide films for biomedical applications in endovascular surgery[J]. J. Mater. Sci. Mater. Med., 2002, 13: 495 |
| [32] | Schneider M, Schroth S, Schilm J, et al.Micro-EIS of anodic oxide films on titanium for capacitor applications[J]. Electrochim. Acta, 2009, 54: 2663 |
| [33] | Macdonald D D.The point defect model for the passive state[J]. J. Electrochem. Soc., 1992, 139: 3434 |
| [34] | Kong D S, Lu W H, Feng Y Y, et al.Studying on the point-defect-conductive property of the semiconducting anodic films on titanium[J]. J. Electrochem. Soc., 2009, 156: C39 |
| [35] | Guo H X, Lu B T, Luo J T.Study on passivation and erosion-enhanced corrosion resistance by Mott-Schottky analysis[J]. Electrochim. Acta, 2006, 52: 1108 |
| [36] | Mandonald D D.The history of the point defect model for the passive state: A brief review of film growth aspects[J]. Electrochim. Acta, 2011, 56: 1761 |
| [37] | Ye W, Li Y, Wang F H.Effects of nanocrystallization on the corrosion behavior of 309 stainless steel[J]. Electrochim. Acta, 2006, 51: 4426 |
/
| 〈 |
|
〉 |