Incomplete Bainite Transformation Accompanied with Cementite Precipitation in Fe-1.5(3.0)%Si-0.4%C Alloys
Received date: 2017-07-03
Online published: 2017-12-04
Supported by
Supported by National Natural Science Foundation of China (No.51471094)
Steels containing bainite microstructure are widely applied in various industrial areas. Incomplete bainite transformation is frequently used to control volume fraction of retained austenite as well as its stability and is also closely related to bainite growth mechanism. It is generally accepted that incomplete bainite transformation could occur when carbide precipitation is absent. On the other hand, some new studies revealed that carbide with very fine size were observed in “carbide-free” bainite in Si added steels. Our previous study on bainite isothermal transformation kinetics together with its microstructural evolution with Fe-1.5(3.0)%Si-0.4%C alloys (mass fraction) at 400~500 ℃ found incomplete bainite transformation phenomenon for the 3.0Si alloy at 450 ℃ and for two alloys at 400 ℃. In contrast with the generally accepted view, cementite precipitation with Si depletion was observed at the beginning of incomplete transformation stage. Further analysis on three dimension atom probe results revealed that the carbide volume fraction as well as amount of C atoms in carbide hardly changes during incomplete transformation stage. Thermodynamic analysis revealed that small chemical driving force for cementite precipitation and/or the necessity of Si partition are two factors accounting for the extremely slow cementite precipitation kinetics. It is thus proposed that incomplete bainite transformation and carbide precipitation could co-exist. Conditions for incomplete bainite transformation are modified as follows. Firstly, bainitic ferrite growth is stopped before reaching equilibrium fraction. In addition, carbide precipitation should be absent or its kinetics should be slow enough.
Huidong WU , Goro MIYAMOTO , Zhigang YANG , Chi ZHANG , Hao CHEN , Tadashi FURUHARA . Incomplete Bainite Transformation Accompanied with Cementite Precipitation in Fe-1.5(3.0)%Si-0.4%C Alloys[J]. Acta Metall Sin, 2018 , 54(3) : 367 -376 . DOI: 10.11900/0412.1961.2017.00262
| [1] | De Cooman B C. Structure-properties relationship in TRIP steels containing carbide-free bainite[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 285 |
| [2] | Jacques P J.Transformation-induced plasticity for high strength formable steels[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 259 |
| [3] | Zaefferer S, Ohlert J, Bleck W.A study of microstructure, transformation mechanisms and correlation between microstructure and mechanical properties of a low alloyed TRIP steel[J]. Acta Mater., 2004, 52: 2765 |
| [4] | Aaronson H I, Reynolds W T Jr, Purdy G R. The incomplete transformation phenomenon in steel[J]. Metall. Mater. Trans., 2006, 37A: 1731 |
| [5] | Bhadeshia H K D H, Christian J W. Bainite in steels[J]. Metall. Trans., 1990, 21A: 767 |
| [6] | Aaronson H I, Reynolds W T, Shiflet G J, et al.Bainite viewed three different ways[J]. Metall. Trans., 1990, 21A: 1343 |
| [7] | Fielding L C D. The bainite controversy[J]. Mater. Sci. Technol., 2013, 29: 383 |
| [8] | Reynolds W T, Liu S K, Li F Z, et al.An investigation of the generality of incomplete transformation to bainite in Fe-C-X alloys[J]. Metall. Trans., 1990, 21A: 1479 |
| [9] | Reynolds W T, Li F Z, Shui C K, et al.The incomplete transformation phenomenon in Fe-C-Mo alloys[J]. Metall. Trans., 1990, 21A: 1433 |
| [10] | Liu Z Q, Miyamoto G, Yang Z G, et al.Carbon enrichment in austenite during bainite transformation in Fe-3Mn-C Alloy[J]. Metall. Mater. Trans., 2013, 46A: 1544 |
| [11] | Xia Y, Miyamoto G, Yang Z G, et al.Direct measurement of carbon enrichment in the incomplete bainite transformation in Mo added low carbon steels[J]. Acta Mater., 2015, 91: 10 |
| [12] | Hofer C, Leitner H, Winkelhofer F, et al.Structural characterization of "carbide-free" bainite in a Fe-0.2C-1.5Si-2.5 Mn steel[J]. Mater. Charact., 2015, 102: 85 |
| [13] | Quidort D, Brechet Y J M. Isothermal growth kinetics of bainite in 0.5%C steels[J]. Acta Mater., 2001, 49: 4161 |
| [14] | Tsuzaki K, Kodai A, Maki T.Formation mechanism of bainitic ferrite in an Fe-2pct Si-0.6pct C alloy[J]. Metall. Mater. Trans., 1994, 25A: 2009 |
| [15] | Papadimitrou G D, Génin J M R. Kinetic and thermodynamic aspects of the bainite reaction in a silicon steel [A]. Phase Transformation in Solids[C]. Greece: Materials Research Society, 1983: 746 |
| [16] | Toji Y, Matsuda H, Herbig M, et al.Atomic-scale analysis of carbon partitioning between martensite and austenite by atom probe tomography and correlative transmission electron microscopy[J]. Acta Mater., 2014, 65: 215 |
| [17] | Wu H D, Miyamoto G, Yang Z G, et al.Incomplete bainite transformation in Fe-Si-C alloys[J]. Acta Mater., 2017, 133: 1 |
| [18] | Hillert M.Paraequilibrium [R]. Stockholm: Swedish Inst. Met. Res., 1953 |
| [19] | Coates D E.Diffusion-controlled precipitate growth in ternary systems I[J]. Metall. Trans., 1972, 3: 1203 |
| [20] | Zener C.Kinetics of the decomposition of austenite[J]. Trans. Am. Inst. Min. Metall. Eng., 1946, 167: 550 |
| [21] | Andrews K W.Empirical formulae for calculation of some transformation temperatures[J]. J. Iron Steel Inst., 1965, 203: 721 |
| [22] | Cullity B D.Elements of X-Ray Diffraction [M]. Massachusetts: Addition-Wesley Publishing Company Inc., 1956: 199 |
| [23] | Miller M K, Russell K F, Thompson G B.Strategies for fabricating atom probe specimens with a dual beam FIB[J]. Ultramicroscopy, 2005, 102: 287 |
| [24] | Miyamoto G, Shinbo K, Furuhara T.Quantitative measurement of carbon content in Fe-C binary alloys by atom probe tomography[J]. Scr. Mater., 2012, 67: 999 |
| [25] | Caballero F G, Miller M K, Garcia-Mateo G.Opening previously impossible avenues for phase transformation in innovative steels by atom probe tomography[J]. Mater. Sci. Technol., 2014, 30: 1034 |
| [26] | Kobayashi A.Incomplete bainite transformation in Fe-11Ni-0.2C alloy [D]. Japan: Kyoto University, 1994 |
| [27] | Hehemann R F, Kinsman K R, Aaronson H I.Debate on the bainite reaction[J]. Metall. Trans., 1972, 3: 1077 |
| [28] | Huang D H, Thomas G.Metallography of bainitic transformation in silicon containing steels[J]. Metall. Trans., 1977, 8A: 1661 |
| [29] | Spanos G, Fang H S, Aaronson H I.A mechanism for the formation of lower bainite[J]. Metall. Trans., 1990, 21A: 1381 |
| [30] | Yada H.Discussion of “A mechanism for the formation of lower bainite[J]. Metall. Mater. Trans., 1991, 22A: 1674 |
| [31] | Franke P, Inden G.An assessment of the Si mobility and the application to phase transformations in silicon steels[J]. Z Metallkd., 1997, 88: 795 |
/
| 〈 |
|
〉 |