Preparation and Properties of Biological Functional Magnesium Coating on Ti6Al4V Substrate
Received date: 2017-07-10
Online published: 2017-11-09
Supported by
Supported by National Natural Science Foundation of China (Nos.51631009, 81500897 and 81400528) and National Key Research and Development Program of China (No.2016YFC1101804)
Currently, metallic biomaterials used in orthopedics are normally bioinert which is hard to integrate with the bone tissue inducing aseptic loosening and easy to get infection, which is the main reason of implantation failure. Mg base metals are considered to be a new generation of revolutionary metallic biomaterials due to its similar density and mechanical properties with natural bone, good biocompatibility, degradability in the body as well as the biological functional ability to promote new bone tissue formation. In addition, the degradation of Mg may increase the local pH which can inhibit the growth of bacteria. In this work, pure Mg coating was deposited on Ti6Al4V substrate by arc ion plating. The effects of different working pressures on the surface quality and properties of Mg coating were investigated. The degradation, antibacterial and biosafety properties were studyied. The results showed that the pure Mg coating can be deposited on the surface of Ti6Al4V substrate and the coating was uniform and smooth. The immersion test in vitro showed that the degradation was very fast because of galvanic corrosion, and the whole process was finished in about one week. The results of antimicrobial experiments showed that the Mg coating can kill staphylococcus aureus and showed good antibacterial function. The results of cytotoxicity test showed that Mg coating promoted rabbit bone marrow mesenchymal stem cells (rBMSCs) growth and proliferation.
Key words: Ti alloy; pure Mg coating; bioproperty
Xiaoming YU , Lili TAN , Zongyuan LIU , Ke YANG , Zhonglin ZHU , Yangde LI . Preparation and Properties of Biological Functional Magnesium Coating on Ti6Al4V Substrate[J]. Acta Metall Sin, 2018 , 54(6) : 943 -949 . DOI: 10.11900/0412.1961.2017.00285
| [1] | Ge J H, Wang Y J, Zheng Y D.Advances in biodegradable and bioabsorbable bone-repaired materials[J]. New Chem. Mater., 2003, 31: 34(葛建华, 王迎军, 郑裕东. 可降解及可吸收性骨科材料研究进展[J]. 化工新型材料 2003, 31: 34) |
| [2] | Geetha M, Singh A K, Asokamani R, et al.Ti based biomaterials, the ultimate choice for orthopaedic implants—A review[J]. Prog. Mater. Sci., 2009, 54: 397 |
| [3] | Niinomi M.Mechanical properties of biomedical titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 231 |
| [4] | Witte F, Kaese V, Haferkamp H, et al.In vivo corrosion of four magnesium alloys and the associated bone response[J]. Biomaterials, 2005, 26: 3557 |
| [5] | Witte F.The history of biodegradable magnesium implants: A review[J]. Acta Bio., 2015, 23: S28 |
| [6] | Zhao D W, Witte F, Lu F Q, et al.Current status on clinical applications of magnesium-based orthopaedic implants: A review from clinical translational perspective[J]. Biomaterials, 2016, 112: 287 |
| [7] | Tan L L, Yu X M, Wan P, et al.Biodegradable materials for bone repairs: A review[J]. J. Mater. Sci. Technol., 2013, 29: 503 |
| [8] | Ren L, Lin X, Tan L L, et al.Effect of surface coating on antibacterial behavior of magnesium based metals[J]. Mater. Lett., 2011, 65: 3509 |
| [9] | Robinson D A, Griffith R W, Shechtman D, et al.In vitro antibacterial properties of magnesium metal against Escherichia coli, Pseudomonas aeruginosa and Staphylococcus aureus[J]. Acta Biomater., 2010, 6: 1869 |
| [10] | Li Y, Liu G W, Zhai Z J, et al.Antibacterial properties of magnesium in an in vitro and in vivo model of implant-associated MRSA infection[J]. Antimicrob. Agent. Chemoth., 2014, 58: 3936 |
| [11] | Wang Q, Jin S, Lin X, et al.Cytotoxic effects of biodegradation of pure Mg and MAO-Mg on tumor cells of MG63 and KB[J]. J. Mater. Sci. Technol., 2014, 30: 487 |
| [12] | Qu X H, Jin F C, Hao Y Q, et al.Nonlinear association between magnesium intake and the risk of colorectal cancer[J]. Eur. J. Gastroen Hepat., 2013, 25: 309 |
| [13] | Li M, Ren L, Li L H, et al.Cytotoxic effect on osteosarcoma MG-63 cells by degradation of magnesium[J]. J. Mater. Sci. Technol., 2014, 30: 888 |
| [14] | Chen L, Fu X K, Pan H B, et al.Biodegradable Mg-Cu alloys with enhanced osteogenesis, angiogenesis, and long-lasting antibacterial effects[J]. Sci. Rep., 2016, 6: 273274 |
| [15] | Chen Z T, Mao X L, Tan L L, et al.Osteoimmunomodulatory properties of magnesium scaffolds coated with β-tricalcium phosphate[J]. Biomaterials, 2014, 35: 8553 |
| [16] | Zhai Z J, Qu X H, Li H W, et al.The effect of metallic magnesium degradation products on osteoclast-induced osteolysis and attenuation of NF-κB and NFATc1 signaling[J]. Biomaterials, 2014, 35: 6299 |
| [17] | Cheng M Q, Wahafu T, Jiang G F, et al.A novel open-porous magnesium scaffold with controllable microstructures and properties for bone regeneration[J]. Sci. Rep., 2016, 6: 24134 |
| [18] | Guo Y, Ren L, Liu C, et al.Effect of implantation of biodegradable magnesium alloy on BMP-2 expression in bone of ovariectomized osteoporosis rats[J]. Mater. Sci. Eng., 2013, C33: 4470 |
| [19] | Zeng J H, Ren L, Yuan Y J, et al.Short-term effect of magnesium implantation on the osteomyelitis modeled animals induced by Staphylococcus aureus[J]. J. Mater. Sci. Mater. Med., 2013, 24: 2405 |
| [20] | Wan P, Wu J Y, Tan L L, et al.Research on super-hydrophobic surface of biodegradable magnesium alloys used for vascular stents[J]. Mater. Sci. Eng., 2013, C33: 2885 |
| [21] | Zhao Y H, Wang X Q, Xiao J Q, et al.Ti-Cu-N hard nanocomposite films prepared by pulse biased arc ion plating[J]. Appl. Surf. Sci., 2011, 258: 370 |
| [22] | Zhao Y H, Lin G Q, Xiao J Q, et al.Ti/TiN multilayer thin films deposited by pulse biased arc ion plating[J]. Appl. Surf. Sci., 2011, 257: 2683 |
| [23] | Ren L, Lin X, Tan L L, et al.Effect of surface coating on antibacterial behavior of magnesium based metals[J]. Mater. Lett., 2011, 65: 3509 |
| [24] | Witte F, Fischer J, Nellesen J, et al.In vitro and in vivo corrosion measurements of magnesium alloys[J]. Biomaterials, 2006, 27: 1013 |
| [25] | Salunke P, Shanov V, Witte F.High purity biodegradable magnesium coating for implant application[J]. Mater. Sci. Eng., 2011, B176: 1711 |
| [26] | Song G, Atrens A.Understanding magnesium corrosion—A framework for improved alloy performance[J]. Adv. Eng. Mater., 2003, 5: 837 |
| [27] | Fukumoto S, Sugahara K, Yamamoto A, et al.Improvement of corrosion resistance and adhesion of coating layer for magnesium alloy coated with high purity magnesium[J]. Mater. Trans., 2003, 44: 518 |
| [28] | Tsubakino H, Yamamoto A, Fukumoto S, et al.High-purity magnesium coating on magnesium alloys by vapor deposition technique for improving corrosion resistance[J]. Mater. Trans., 2003, 44: 504 |
| [29] | Li X K, Gao P, Wan P, et al.Novel bio-functional magnesium coating on porous Ti6Al4V orthopaedic implants: In vitro and in vivo study[J]. Sci. Rep., 2017, 7: 40755 |
/
| 〈 |
|
〉 |