Effect of Electrolyte Temperature on Microstructures of Direct-Current Electrodeposited Nanotwinned Cu
Received date: 2017-06-01
Online published: 2017-11-08
Supported by
Supported by National Natural Science Foundation of China (Nos.51420105001, 51371171, 51471172 and 51401211) and Key Research Program of Frontier Sciences, Chinese Academy of Sciences
Nanotwinned (NT) metals are promising structural materials due to their excellent combination of strength and ductility. These superior properties are strongly dependent on the microstructures i.e. the twin length (grain size), the twin thickness and the twin orientation. Understanding the synthesis process and growth mechanism of NT metals is essential for their structure design. In this work, the effect of electrolyte temperature on the microstructures of highly oriented NT Cu samples, including twin thickness and twin length (grain size), are systematically studied. The NT Cu samples were prepared by means of the direct-current electrodeposition at 293, 298, 303, 308 and 313 K, respectively, while other deposition parameters such as current density, concentration of additive and pH value were kept constant. With decreasing the temperature from 313 K to 293 K, the average grain size decreases from 27.6 μm to 2.8 μm and the average twin thickness decreases from 111 nm to 28 nm, which results in an increment of hardness from 0.7 GPa to 1.5 GPa. This is because with decreasing the temperature, the overpotential of cathode for depositing metal elevates, leading to the nucleation rate of both the grain and twin enhanced.
Zhao CHENG , Shuai JIN , Lei LU . Effect of Electrolyte Temperature on Microstructures of Direct-Current Electrodeposited Nanotwinned Cu[J]. Acta Metall Sin, 2018 , 54(3) : 428 -434 . DOI: 10.11900/0412.1961.2017.00208
| [1] | Lu L, Shen Y S, Chen X H, et al.Ultrahigh strength and high electrical conductivity in copper[J]. Science, 2004, 304: 422 |
| [2] | Lu L, Chen X H, Huang X, et al.Revealing the maximum strength in nanotwinned copper[J]. Science, 2009, 323: 607 |
| [3] | You Z S, Lu L, Lu K.Tensile behavior of columnar grained Cu with preferentially oriented nanoscale twins[J]. Acta Mater., 2011, 59: 6927 |
| [4] | Pan Q S, Lu Q H, Lu L.Fatigue behavior of columnar-grained Cu with preferentially oriented nanoscale twins[J]. Acta Mater., 2013, 61: 1383 |
| [5] | Pan Q S, Lu L.Strain-controlled cyclic stability and properties of Cu with highly oriented nanoscale twins[J]. Acta Mater., 2014, 81: 248 |
| [6] | Chen K C, Wu W W, Liao C N, et al.Observation of atomic diffusion at twin-modified grain boundaries in copper[J]. Science, 2008, 321: 1066 |
| [7] | Chen X H, Lu L, Lu K.Grain size dependence of tensile properties in ultrafine-grained Cu with nanoscale twins[J]. Scr. Mater., 2011, 64: 311 |
| [8] | Lu K, Lu L, Suresh S.Strengthening materials by engineering coherent internal boundaries at the nanoscale[J]. Science, 2009, 324: 349 |
| [9] | Zhang X, Misra A, Wang H, et al.Enhanced hardening in Cu/330 stainless steel multilayers by nanoscale twinning[J]. Acta Mater., 2004, 52: 995 |
| [10] | Zhang X, Anderoglu O, Hoagland R G, et al.Nanoscale growth twins in sputtered metal films[J]. JOM, 2008, 60(9): 75 |
| [11] | Liu C M, Lin H W, Lu C L, et al.Effect of grain orientations of Cu seed layers on the growth of <111>-oriented nanotwinned Cu[J]. Sci. Rep., 2014, 4: 6123 |
| [12] | Liu T C, Liu C M, Hsiao H Y, et al.Fabrication and characterization of (111)-oriented and nanotwinned Cu by Dc electrodeposition[J]. Cryst. Growth Des., 2012, 12: 5012 |
| [13] | Jin S, Pan Q S, Lu L.Microstructure dependence of direct-current electrodeposited bulk Cu with preferentially oriented nanotwins on the current densities[J]. Acta Metall. Sin., 2013, 49: 635(金帅, 潘庆松, 卢磊. 电流密度对直流电解沉积纳米孪晶Cu微观结构的影响 [J]. 金属学报, 2013, 49: 635) |
| [14] | Hasegawa M, Mieszala M, Zhang Y C, et al.Orientation-controlled nanotwinned copper prepared by electrodeposition[J]. Electrochim. Acta, 2015, 178: 458 |
| [15] | Chan T C, Chueh Y L, Liao C N.Manipulating the crystallographic texture of nanotwinned Cu films by electrodeposition[J]. Cryst. Growth Des., 2011, 11: 4970 |
| [16] | Jin S, Cheng Z, Pan Q S, et al.Effect of electrolyte additive concentration on microstructure of direct-current electrodeposited nanotwinned Cu[J]. Acta Metall. Sin., 2016, 52: 973(金帅, 程钊, 潘庆松等. 添加剂浓度对直流电解沉积纳米孪晶Cu微观结构的影响 [J]. 金属学报, 2016, 52: 973) |
| [17] | Seo S, Jin S, Wang G, et al.The effect of copper dissolution in acidic electrolyte on the formation of nanotwin in pulse electrodeposited copper[J]. J. Electrochem. Soc., 2014, 161: D425 |
| [18] | Natter H, Hempelmann R.Nanocrystalline copper by pulsed electrodeposition: The effects of organic additives, bath temperature, and pH[J]. J. Phys. Chem., 1996, 100: 19525 |
| [19] | Kang J X, Zhao W Z, Zhang G F.Influence of electrodeposition parameters on the deposition rate and microhardness of nanocrystalline Ni coatings[J]. Surf. Coat. Technol., 2009, 203: 1815 |
| [20] | Liao C N, Lin C Y, Huang C L, et al.Morphology, texture and twinning structure of Cu films prepared by low-temperature electroplating[J]. J. Electrochem. Soc., 2013, 160: D3070 |
| [21] | Cohen-Atiya M, Mandler D. Studying thiol adsorption on Au, Ag and Hg surfaces by potentiometric measurements [J]. J. Electroanal. Chem., 2003, 550-551: 267 |
| [22] | Zhang Q B, Hua Y X, Dong T G, et al.Effects of temperature and current density on zinc electrodeposition from acidic sulfate electrolyte with [BMIM]HSO4 as additive[J]. J. Appl. Electrochem., 2009, 39: 1207 |
| [23] | Cifuentes L, Simpson J.Temperature dependence of the cathodic and anodic kinetics in a copper electrowinning cell based on reactive electrodialysis[J]. Chem. Eng. Sci., 2005, 60: 4915 |
| [24] | Nikoli? N D, Pavlovi? L J, Pavlovi? M G, et al.Effect of temperature on the electrodeposition of disperse copper deposits[J]. J. Serb. Chem. Soc., 2007, 72: 1369 |
| [25] | Gründer Y, Markovic N M, Thompson P, et al.Temperature effects on the atomic structure and kinetics in single crystal electrochemistry[J]. Surf. Sci., 2015, 631: 123 |
| [26] | Li D.Principles of Electrochemistry [M]. 3rd Ed., Beijing: Beijing University of Aeronautics and Astronautics Press, 2008: 286(李荻. 电化学原理 [M]. 第3版. 北京: 北京航空航天大学出版社, 2008: 286) |
| [27] | Mallik A.An analysis on the effect of temperature on electrocrystallization mechanism during deposition of Cu thin films[J]. Trans. Indian Inst. Met., 2013, 66: 79 |
| [28] | Milchev A, Montenegro M I.A galvanostatic study of electrochemical nucleation[J]. J. Electroanal. Chem., 1992, 333: 93 |
| [29] | Kanani N.Electroplating: Basic Principles, Processes and Practice[M]. Berlin: Elsevier, 2005: 150 |
| [30] | Bufford D C, Wang Y M, Liu Y, et al.Synthesis and microstructure of electrodeposited and sputtered nanotwinned face-centered-cubic metals[J]. MRS Bull., 2016, 41: 286 |
/
| 〈 |
|
〉 |