Mechanical Properties of Biomedical Ultrafine Grained Mg-3Sn-0.5Mn Alloy Processed by Equal-Channel Angular Pressing
Received date: 2017-07-18
Online published: 2017-08-29
Supported by
Supported by National Natural Science Foundation of China (No.51301049)
Mg alloy has attracted researchers' attention as applied for novel biomedical material because of its super corrosion property and well biocompatibility. Ultra-fine grain (UFG) Mg alloy has certain advantages in the development of medical devices because of its good plasticity and corrosion resistance. Equal channel angular pressing (ECAP) was performed on Mg-3Sn-0.5Mn alloy successfully. The microstructure and grain size were observed and measured by OM and TEM. The mechanical property was tested by microhardness and tensile test, the texture oriented was experimented by XRD, and the corrosion property was tested by electrochemical experiment. After 4 passes ECAP at 320 ℃, the average grain size of Mg-3Sn-0.5Mn alloy reached 1.65 μm, and local grain size reached 0.8 μm. The grain refinement was caused by severe plastic deformation and recrystallization. The elongation increased from 22.2% to 58.6%, the tensile strength decreased from 242.8 MPa to 195.6 MPa after 4 passes deformation. The mechanical tests showed an improvement in the elongation after 4 passes, which were about 3 times higher than in the as-extruded sample, whereas the tensile strength decreased slightly. The texture of Mg-3Sn-0.5Mn alloy changed obviously which contributed to the actuating of the slip system. This change of texture contributed to the improvement of fracture elongation and decrease of tensile strength. The mechanical property of Mg-3Sn-0.5Mn alloy after ECAP was affected by the texture orientation and grain strengthening.
Yu PAN , Diantao ZHANG , Yuning TAN , Zhen LI , Yufeng ZHENG , Li LI . Mechanical Properties of Biomedical Ultrafine Grained Mg-3Sn-0.5Mn Alloy Processed by Equal-Channel Angular Pressing[J]. Acta Metall Sin, 2017 , 53(10) : 1357 -1363 . DOI: 10.11900/0412.1961.2017.00300
| [2] | Agarwal S, Curtin J, Duffy B, et al.Biodegradable magnesium alloys for orthopaedic applications: A review on corrosion, biocompatibility and surface modifications[J]. Mater. Sci. Eng., 2016, C68: 948 |
| [3] | Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1 |
| [4] | Cheng M Q, Wahafu T, Jiang G F, et al.A novel open-porous magnesium scaffold with controllable microstructures and properties for bone regeneration[J]. Sci. Rep., 2016, 6: 24134 |
| [5] | Hou L D, Li Z, Pan Y, et al.In vitro and in vivo studies on biodegradable magnesium alloy[J]. Prog. Nat. Sci. Mater. Int., 2014, 24: 466 |
| [6] | Hou L D, Li Z, Zhao H, et al.Microstructure, mechanical properties, corrosion behavior and biocompatibility of as-extruded biodegradable Mg-3Sn-1Zn-0.5Mn alloy[J]. J. Mater. Sci. Technol., 2016, 32: 874 |
| [7] | Chen Y J, Xu Z G, Smith C, et al.Recent advances on the development of magnesium alloys for biodegradable implants[J]. Acta Biomater., 2014, 10: 4561 |
| [8] | Amerstorfer F, Fischerauer S F, Fischer L, et al.Long-term in vivo degradation behavior and near-implant distribution of resorbed elements for magnesium alloys WZ21 and ZX50[J]. Acta Biomater., 2016, 42: 440 |
| [9] | Cheng P F, Han P, Zhao C L, et al.Magnesium inference screw supports early graft incorporation with inhibition of graft degradation in anterior cruciate ligament reconstruction[J]. Sci. Rep., 2016, 6: 26434 |
| [10] | Haude M, Ince H, Abizaid A, et al.Sustained safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de novo coronary lesions: 12-month clinical results and angiographic findings of the BIOSOLVE-II first-in-man trial[J]. Eur. Heart J., 2016, 37: 2701 |
| [11] | Haude M, Ince H, Abizaid A, et al.Safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de-novo coronary artery lesions (BIOSOLVE-II): 6 month results of a prospective, multicentre, non-randomised, first-in-man trial[J]. Lancet, 2016, 387: 31 |
| [12] | Zhao D W, Witte F, Lu F Q, et al.Current status on clinical applications of magnesium-based orthopaedic implants: A review from clinical translational perspective[J]. Biomaterials, 2017, 112: 287 |
| [13] | Ge Q, Dellasega D, Demir A G, et al.The processing of ultrafine-grained Mg tubes for biodegradable stents[J]. Acta Biomater., 2013, 9: 8604 |
| [14] | Mostaed E, Vedani M, Hashempour M, et al.Influence of ECAP process on mechanical and corrosion properties of pure Mg and ZK60 magnesium alloy for biodegradable stent applications[J]. Biomatter, 2014, 4: e28283 |
| [15] | Mostaed E, Hashempour M, Fabrizi A, et al.Microstructure, texture evolution, mechanical properties and corrosion behavior of ECAP processed ZK60 magnesium alloy for biodegradable applications[J]. J. Mech. Behav. Biomed. Mater., 2014, 37: 307 |
| [16] | Orlov D, Ralston K D, Birbilis N, et al.Enhanced corrosion resistance of Mg alloy ZK60 after processing by integrated extrusion and equal channel angular pressing[J]. Acta Mater., 2011, 59: 6176 |
| [17] | Sunil B R, Kumar T S S, Chakkingal U, et al. In vitro and in vivo studies of biodegradable fine grained AZ31 magnesium alloy produced by equal channel angular pressing[J]. Mater. Sci. Eng., 2016, C59: 356 |
| [18] | Su C W, Lu L, Lai M O.A model for the grain refinement mechanism in equal channel angular pressing of Mg alloy from microstructural studies[J]. Mater. Sci. Eng., 2006, A434: 227 |
| [19] | Balogh L, Figueiredo R B, Ungár T, et al.The contributions of grain size, dislocation density and twinning to the strength of a magnesium alloy processed by ECAP[J]. Mater. Sci. Eng., 2010, A528: 533 |
| [20] | Del Valle J A, Carre?o F, Ruano O A. Influence of texture and grain size on work hardening and ductility in magnesium-based alloys processed by ECAP and rolling[J]. Acta Mater., 2006, 54: 4247 |
| [21] | Yuan W, Panigrahi S K, Su J Q, et al.Influence of grain size and texture on Hall-Petch relationship for a magnesium alloy[J]. Scr. Mater., 2011, 65: 994 |
| [22] | Petch N J.The cleavage strength of polycrystals[J]. J. Iron Steel Inst., 1953, 174: 25 |
| [23] | Chokshi A H, Rosen A, Karch J, et al.On the validity of the hall-petch relationship in nanocrystalline materials[J]. Scr. Metall., 1989, 23: 1679 |
| [24] | Srinivasarao B, Dudamell N V, Pérez-Prado M T. Texture analysis of the effect of non-basal slip systems on the dynamic recrystallization of the Mg alloy AZ31[J]. Mater. Charact., 2013, 75: 101 |
| [25] | Wang L F, Mostaed E, Cao X Q, et al.Effects of texture and grain size on mechanical properties of AZ80 magnesium alloys at lower temperatures[J]. Mater. Des., 2016, 89: 1 |
| [26] | Xu W Q, Birbilis N, Sha G, et al.A high-specific-strength and corrosion-resistant magnesium alloy[J]. Nat. Mater., 2015, 14: 1229 |
| [27] | Zhao M C, Liu M, Song G L, et al.Influence of the β-phase morphology on the corrosion of the Mg alloy AZ91[J]. Corro. Sci., 2008, 50: 1939 |
/
| 〈 |
|
〉 |