Recent Advances on Biodegradable MgYREZrMagnesium Alloy
Received date: 2017-07-03
Online published: 2017-08-29
Supported by
Supported by National Natural Science Foundation of China (Nos.81401773 and 31500777)
In recent years, magnesium and its alloys as biodegradable materials have attracted much attention. Biodegradable MgYREZr, mainly WE43 alloy, with good integrated properties has been studied in favor. In this paper, the microstructure, mechanical properties, biodegradable property and biocompatibility of biodegradable MgYREZr alloy were reviewed, as well as the clinical results of the bone fixation screws developed in Germany using the alloy with similar composition to WE43. MgYREZr alloy presents uniform microstructure and higher mechanical properties after large plastic deformation with the grain size of less than 1 μm. The RE elements can be dissolved and stabilize the corrosion layer, which can decrease the degradation rate of the alloy accompanying with optimized heat treatment. The animal tests showed biocompatibility and good bioactivity. Clinical tests showed the MgYREZr alloy screws presented equivalent to titanium screws for the treatment of mild hallux valgus deformities, however resorption cysts was revealed by X-rays when the acute scaphoid fractures were treated with a double-threaded screw made of MgYREZr, and it was only after 6 months that the fractures were consolidated enough to allow physical work. So for different clinical cases, the degradation and biological behaviors of MgYREZr alloys need to be further studied in vitro and in vivo. To control the degradation rates to meet the different clinical requirements is still a major obstacle for biodegradable MgYREZr alloys to enlarge their clinical application.
Lili TAN , Junxiu CHEN , Xiaoming YU , Ke YANG . Recent Advances on Biodegradable MgYREZrMagnesium Alloy[J]. Acta Metall Sin, 2017 , 53(10) : 1207 -1214 . DOI: 10.11900/0412.1961.2017.00266
| [1] | Staiger M P, Pietak A M, Huadmai J, et al.Magnesium and its alloys as orthopedic biomaterials: A review[J]. Biomaterials, 2006, 27: 1728 |
| [2] | Zhang W J, Li M H, Chen Q, et al.Effects of Sr and Sn on microstructure and corrosion resistance of Mg-Zr-Ca magnesium alloy for biomedical applications[J]. Mater. Des., 2012, 39: 379 |
| [3] | Witte F, Fischer J, Nellesen J, et al.In vitro and in vivo corrosion measurements of magnesium alloys[J]. Biomaterials, 2006, 27: 1013 |
| [4] | Song G L.Control of biodegradation of biocompatable magnesium alloys[J]. Corros. Sci., 2007, 49: 1696 |
| [5] | Kraus T, Fischerauer S F, H?nzi A C, et al.Magnesium alloys for temporary implants in osteosynthesis: In vivo studies of their degradation and interaction with bone[J]. Acta Biomater., 2012, 8: 1230 |
| [6] | Zhou P, Gong H R.Phase stability, mechanical property, and electronic structure of an Mg-Ca system[J]. J. Mech. Behav. Biomed. Mater., 2012, 8: 154 |
| [7] | Jin W H, Wu G S, Feng H Q, et al.Improvement of corrosion resistance and biocompatibility of rare-earth WE43 magnesium alloy by neodymium self-ion implantation[J]. Corros. Sci., 2015, 94: 142 |
| [8] | Zong Y, Yuan G Y, Zhang X B, et al.Comparison of biodegradable behaviors of AZ31 and Mg-Nd-Zn-Zr alloys in Hank's physiological solution[J]. Mater. Sci. Eng., 2012, B177: 395 |
| [9] | Zhang J Y, Kang Z X, Wang F.Mechanical properties and biocorrosion resistance of the Mg-Gd-Nd-Zn-Zr alloy processed by equal channel angular pressing[J]. Mater. Sci. Eng., 2016, C68: 194 |
| [10] | Mao L, Shen L, Chen J H, et al.Enhanced bioactivity of Mg-Nd-Zn-Zr alloy achieved with nanoscale MgF2 surface for vascular stent application[J]. ACS Appl. Mater. Interfaces, 2015, 7: 5320 |
| [11] | Zhao D W, Huang S B, Lu F Q, et al.Vascularized bone grafting fixed by biodegradable magnesium screw for treating osteonecrosis of the femoral head[J]. Biomaterials, 2016, 81: 84 |
| [12] | Lee J W Han H S, Han K J, et al. Long-term clinical study and multiscale analysis of in vivo biodegradation mechanism of Mg alloy[J]. Proc. Natl. Acad. Sci. USA, 2016, 113: 716 |
| [13] | Kalb H, Rzany A, Hensel B.Impact of microgalvanic corrosion on the degradation morphology of WE43 and pure magnesium under exposure to simulated body fluid[J]. Corros. Sci., 2012, 57: 122 |
| [14] | Xu H, Liu J A, Xie S S.Magnesium Alloy Fabrication and Processing Technology [M]. Beijing: Metallurgical Industry Press, 2007: 64(徐河, 刘静安, 谢水生. 镁合金制备与加工技术 [M]. 北京: 冶金工业出版社, 2007: 64) |
| [15] | Windhagen H, Radtke K, Weizbauer A, et al.Biodegradable magnesium-based screw clinically equivalent to titanium screw in hallux valgus surgery: Short term results of the first prospective, randomized, controlled clinical pilot study[J]. Biomed. Eng. Online, 2013, 12: 62 |
| [16] | Rzychoń T, Kie?bus A.Microstructure of WE-43 casting magnesium alloys[J]. J. Achiev. Mater. Manuf. Eng., 2007, 21: 31 |
| [17] | Nie J F, Muddle B C.Precipitation in magnesium alloy WE54 during isothermal ageing at 250 ℃[J]. Scr. Mater., 1999, 40: 1089 |
| [18] | Apps P J, Karimzadeh H, King J F, et al.Phase compositions in magnesium-rare earth alloys containing yttrium, gadolinium or dysprosium[J]. Scr. Mater., 2003, 48: 475 |
| [19] | Hornberger H, Witte F, Hort N, et al.Effect of fetal calf serum on the corrosion behaviour of magnesium alloys[J]. Mater. Sci. Eng., 2011, B176: 1746 |
| [20] | Witte F, Hort N, Vogt C, et al.Degradable biomaterials based on magnesium corrosion[J]. Curr. Opin. Solid State Mater. Sci., 2008, 12: 63 |
| [21] | Kutniy K V, Papirov I I, Tikhonovsky M A, et al.Influence of grain size on mechanical and corrosion properties of magnesium alloy for medical implants[J]. Materialwiss. Werkstofftech., 2009, 40: 242 |
| [22] | Gu X N, Zhou W R, Zheng Y F, et al.Corrosion fatigue behaviors of two biomedical Mg alloys-AZ91D and WE43-In simulated body fluid[J]. Acta Biomater., 2010, 6: 4605 |
| [23] | Ezechieli M, Ettinger M, K?nig C, et al.Biomechanical characteristics of bioabsorbable magnesium-based (MgYREZr-alloy) interference screws with different threads[J]. Knee Surg. Sports Traumatol., 2014, 24: 3976 |
| [24] | Ascencio M, Pekguleryuz M, Omanovic S.An investigation of the corrosion mechanisms of WE43 Mg alloy in a modified simulated body fluid solution: The influence of immersion time[J]. Corrosion Sci., 2014, 87: 489 |
| [25] | Zhou X H, Jiang L, Wu P P, et al.Effect of aggressive ions on degradation of WE43 magnesium alloy in physiological environment[J]. Int. J. Electrochem. Sci., 2014, 9: 304 |
| [26] | Li N, Guo C, Wu Y H, et al.Comparative study on corrosion behaviour of pure Mg and WE43 alloy in static, stirring and flowing Hank's solution[J]. Corros. Eng. Sci. Technol., 2013, 47: 346 |
| [27] | Ben-Hamu G, Eliezer D, Shin K S, et al.The relation between microstructure and corrosion behavior of Mg-Y-RE-Zr alloys[J]. J. Alloys Compd., 2007, 431: 269 |
| [28] | Witte F, Kaese V, Haferkamp H, et al.In vivo corrosion of four magnesium alloys and the associated bone response[J]. Biomaterials, 2005, 26: 3557 |
| [29] | Witte F, Abeln I, Switzer E, et al.Evaluation of the skin sensitizing potential of biodegradable magnesium alloys[J]. J. Biomed. Mater. Res., 2008, 86A: 1041 |
| [30] | Waizy H, Diekmann J, Weizbauer A, et al.In vivo study of a biodegradable orthopedic screw (MgYREZr-alloy) in a rabbit model for up to 12 months[J]. J. Biomater. Appl., 2013, 28: 667 |
| [31] | Diekmann J, Bauer S, Weizbauer A, et al.Examination of a biodegradable magnesium screw for the reconstruction of the anterior cruciate ligament: A pilot in vivo study in rabbits[J]. Mater. Sci. Eng., 2016, C59: 1100 |
| [32] | Herbert T J, Fisher W E, Leicester A W.The Herbert bone screw: A ten year perspective[J]. J. Hand Surg., 1992, 17: 415 |
| [33] | Biber R, Pauser J, Ge?lein M, et al.Magnesium-based absorbable metal screws for intra-articular fracture fixation[J]. Case Rep. Orthop., 2016, 2016: 9673174 |
| [34] | Meier R, Panzica M.First results with a resorbable MgYREZr compression screw in unstable scaphoid fractures show extensive bone cysts[J]. Handchir. Mikrochir. Plast. Chir., 2017, 49: 37 |
| [35] | Plaass C, Ettinger S, Sonnow L, et al.Early results using a biodegradable magnesium screw for modified chevron osteotomies[J]. J. Orthop. Res., 2016, 34: 2207 |
/
| 〈 |
|
〉 |