Orginal Article

Effects of MgO Modified HA Nanoparticles on the Microstructure and Properties of Mg-Zn-Zr/m-HA Composites

  • Haoran ZHENG ,
  • Minfang CHEN ,
  • Zhen LI ,
  • Chen YOU ,
  • Debao LIU
Expand
  • 1 School of Materials Science and Engineering, Tianjin University of Technology, Tianjin 300384, China
    2 Tianjin Key Lab for Photoelectric Materials & Devices, Tianjin University of Technology, Tianjin 300384, China

Received date: 2017-06-26

  Online published: 2017-08-04

Supported by

Supported by National Natural Science Foundation of China (No.51371126), Major Science and Technology Projects of Tianjin (No.15ZXQXSY00080) and Science and Technology Developing Foundation of Tianjin High Education (No.20110301)

Abstract

Magnesium metal matrix composites (MMCs) are hot research spots in recent years because of their adjustable mechanical and corrosion properties. However, the agglomerate particles in MMCs limit its applications in many areas. In order to solve this problem, MgO surface modified hydroxyapatite ceramic nanorods (m-HA) were prepared and added as reinforcement in this work. Mg-3Zn-0.8Zr alloy (MZZ), Mg-3Zn-0.8Zr composites with unmodified (MZZH) and modified (MZZMH) nanorods were produced by high shear mixing technology. Effects of m-HA nanorods on the microstructure, mechanical properties and corrosion properties of Mg-Zn-Zr/m-HA composites were investigated. The results showed that the addition of HA nanorods refined the grain size of MZZ alloy and gave a raise to the mechanical properties and electrochemical corrosion resistance of MZZ alloy. The grain size of MZZMH was smaller than that of MZZH and the distribution of m-HA nanorods in the matrix was more uniform than that of HA nanorods. Moreover, the as-extruded MZZMH composite exhibited a yield tensile strength of 291 MPa and ultimate tensile strength of 325 MPa, greater than that of MZZH. The corrosion potential of MZZMH was approximately 59 mV greater than that of MZZH. The corrosion rate of MZZMH was 5 mm/a after immersion 7 d in SBF, lower than that of MZZH. The corrosion resistance of MZZMH was better than that of MZZH due to the different corrosion mechanism. Surface corrosion products of MZZMH was alternating Mg(OH)2 and Ca-P compound at the early stage of immersion, but surface corrosion layer of MZZH specimen was always Mg(OH)2. The mechanical properties and corrosion resistance of Mg-Zn-Zr/m-HA composites were improved by the addition of m-HA.

Cite this article

Haoran ZHENG , Minfang CHEN , Zhen LI , Chen YOU , Debao LIU . Effects of MgO Modified HA Nanoparticles on the Microstructure and Properties of Mg-Zn-Zr/m-HA Composites[J]. Acta Metall Sin, 2017 , 53(10) : 1364 -1376 . DOI: 10.11900/0412.1961.2017.00249

References

[1] Witte F, Fischer J, Nellesen J, et al.In vitro and in vivo corrosion measurements of magnesium alloys[J]. Biomaterials, 2006, 27: 1013
[2] Zhao Y C, Huang G S, Wang G G, et al.Influence of grain orientation on the corrosion behavior of rolled AZ31 magnesium alloy[J]. Acta Metall. Sin.(Engl. Lett.), 2015, 28: 1387
[3] Qin F X, Ji C, Dan Z H, et al.Corrosion behavior of MgZnCa bulk amorphous alloys fabricated by spark plasma sintering[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 793
[4] Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1
[5] Chaubey A K, Jha B B, Mishra B K.Microstructure and mechanical properties of Mg-7.4% Al alloy matrix composites reinforced by nanocrystalline Al-Ca intermetallic particles[J]. Acta Metall. Sin.(Engl. Lett.), 2015, 28: 444
[6] Wang Y, Wang H Y, Xiu K, et al.Fabrication of TiB2 particulate reinforced magnesium matrix composites by two-step processing method[J]. Mater. Lett., 2006, 60: 1533
[7] Soon L L, Zuhailawati H, Suhaina I, et al.Prediction of compressive strength of biodegradable Mg-Zn/HA composite via response surface methodology and its biodegradation[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 464
[8] Witte F, Feyerabend F, Maier P, et al.Biodegradable magnesium-hydroxyapatite metal matrix composites[J]. Biomaterials, 2007, 28: 2163
[9] Gao J H, Guan S K, Ren Z W, et al.Homogeneous corrosion of high pressure torsion treated Mg-Zn-Ca alloy in simulated body fluid[J]. Mater. Lett., 2011, 65: 691
[10] Zhao F Z, Feng X H, Yang Y S.Microstructure and mechanical properties of CNT-reinforced AZ91D composites fabricated by ultrasonic processing[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 652
[11] Lei T, Tang W, Cai S H, et al.On the corrosion behaviour of newly developed biodegradable Mg-based metal matrix composites produced by in situ reaction[J]. Corros. Sci., 2012, 54: 270
[12] Ratna Sunil B, Ganapathy C, Sampath Kumar T S, et al. Processing and mechanical behavior of lamellar structured degradable magnesium-hydroxyapatite implants[J]. J. Mech. Behav. Biomed. Mater., 2014, 40: 178
[13] Zhou D S, Qiu F, Wang H Y, et al.Manufacture of nano-sized particle-reinforced metal matrix composites: A review[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 798
[14] Gu X N, Wang X, Li N, et al.Microstructure and characteristics of the metal-ceramic composite (MgCa-HA/TCP) fabricated by liquid metal infiltration[J]. J. Biomed. Mater. Res., 2011, 99B: 127
[15] Ye X Y, Chen M F, Yang M, et al.In vitro corrosion resistance and cytocompatibility of nano-hydroxyapatite reinforced Mg-Zn-Zr composites[J]. J. Mater. Sci. Mater. Med., 2010, 21: 1321
[16] Liu D B, Zuo Y B, Meng W Y, et al.Fabrication of biodegradable nano-sized β-TCP/Mg composite by a novel melt shearing technology[J]. Mater. Sci. Eng., 2012, C32: 1253
[17] Li Z, Chen M F, Li W, et al.The synergistic effect of trace Sr and Zr on the microstructure and properties of a biodegradable Mg-Zn-Zr-Sr alloy[J]. J. Alloys Compd., 2017, 702: 290
[18] Li Z, Sun S Z, Chen M F, et al.In vitro and in vivo corrosion, mechanical properties and biocompatibility evaluation of MgF2-coated Mg-Zn-Zr alloy as cancellous screws[J]. Mater. Sci. Eng., 2017, C75: 1268
[19] He S Y, Sun Y, Chen M F, et al.Microstructure and properties of biodegradable β-TCP reinforced Mg-Zn-Zr composites[J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 814
[20] Jin X Y, Zhuang J Z, Zhi Z, et al.Hydrothermal synthesis of hydroxyapatite nanorods in the presence of sodium citrate and its aqueous colloidal stability evaluation in neutral pH[J]. J. Colloid Interface Sci., 2015, 443: 125
[21] Huang Y, Liu D B, Anguilano L, et al.Fabrication and characterization of a biodegradable Mg-2Zn-0.5Ca/1β-TCP composite[J]. Mater. Sci. Eng., 2015, C54: 120
[22] Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena[M]. 2nd Ed., Oxford: Elsevier, 2004: 20
[23] Song G L.Corrosion and Protection of Magnesium Alloys [M]. Beijing: Chemical Industry Press, 2006: 94(宋光铃. 镁合金腐蚀与防护 [M]. 北京: 化学工业出版社, 2006: 94)
[24] Bakhsheshi-Rad H R, Abdul-Kadir M R, Idris M H, et al. Relationship between the corrosion behavior and the thermal characteristics and microstructure of Mg-0.5Ca-xZn alloys[J]. Corros. Sci., 2012, 64: 184
[25] Argade G R, Kandasamy K, Panigrahi S K, et al.Corrosion behavior of a friction stir processed rare-earth added magnesium alloy[J]. Corros. Sci., 2012, 58: 321
[26] Shi Z M, Atrens A.An innovative specimen configuration for the study of Mg corrosion[J]. Corros. Sci., 2011, 53: 226
[27] King A D, Birbilis N, Scully J R.Accurate electrochemical measurement of magnesium corrosion rates; a combined impedance, mass-loss and hydrogen collection study[J]. Electrochim. Acta, 2014, 121: 394
[28] Wang Y, Fan Z, Zhou X, et al.Characterisation of magnesium oxide and its interface with α-Mg in Mg-Al-based alloys[J]. Phil. Mag. Lett., 2011, 91: 516
[29] Splinter S J, Rofagha R, McIntyre N S, et al. XPS characterization of the corrosion films formed on nanocrystalline Ni-P alloys in sulphuric acid[J]. Surf. Interface Anal., 1996, 24: 181
Outlines

/