Research Progress in Biodegradable Metals forStent Application
Received date: 2017-07-04
Online published: 2017-07-25
Supported by
Supported by National Key Research and Development Program of China (No.2016YFC1102402) and National Natural Science Foundation of China (No.51431002)
During the last two decades, a great amount of researches have been focused on biodegradable metals. Technologies from alloy design to melting, manufacturing and processing, from micro-tube to stent laser processing and drug eluting coating have been improved and optimized continuously. Biodegradable metallic stent has evolved from a concept to a real product and generated three branches of material system. A large amount of animal tests and clinical tests have been carried out to investigate biodegradable magnesium stents. Results of clinical study have indicated that the magnesium stent is feasible, with favourable safety and performance outcomes. More importantly, Biotronik won CE Mark for Magmaris bioresorbable stent in 2016. Researches of biodegradable iron stents are still in the stage of animal tests. The nitrided iron stent possesses excellent mechanical properties. Results showed a good long-term biocompatibility of nitrided iron stent in rabbit and porcine model. Biodegradable zinc stent has only been introduced in recent years. Only a few in vivo studies have been reported with zinc wires implanted in rats. Results showed a good degradation behavior and biocompatibility of zinc wires. In this paper, the current research status of biodegradable metallic stents is reviewed, and the future research and development in mechanical property optimization, drug eluting and intelligence is proposed.
Yufeng ZHENG , Hongtao YANG . Research Progress in Biodegradable Metals forStent Application[J]. Acta Metall Sin, 2017 , 53(10) : 1227 -1237 . DOI: 10.11900/0412.1961.2017.00270
| [1] | Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1 |
| [2] | Zheng Y F, Wu Y H.Revolutionizing metallic biomaterials[J]. Acta. Metall. Sin., 2017, 53: 257(郑玉峰,吴远浩. 处在变革中的医用金属材料[J]. 金属学报,2017, 53: 257) |
| [3] | Yu Y, Zhang W C, Duan X R.Study on microstructure and properties of thin tube of AZ31 magnesium alloy by extrusion technology[J]. Powder Metall. Technol., 2013, 31 : 201(于洋, 张文丛, 段祥瑞. AZ31镁合金细管静液挤压工艺及组织性能分析[J]. 粉末冶金技术, 2013, 31 : 201) |
| [4] | Liu F, Chen C X, Niu J L, et al.The processing of Mg alloy micro-tubes for biodegradable vascular stents[J]. Mater. Sci. Eng., 2015, C48: 400 |
| [5] | Liu X W, Sun J K, Yang Y H, et al.In vitro investigation of ultra-pure Zn and its mini-tube as potential bioabsorbable stent material[J]. Mater. Lett., 2015, 161: 53 |
| [6] | Grogan J A, Leen S B, Mchugh P E.Comparing coronary stent material performance on a common geometric platform through simulated bench testing[J]. J. Mech. Behav. Biomed. Mater., 2012, 12: 129 |
| [7] | Lin W J, Qin L, Qi H P, et al.Long-term in vivo corrosion behavior, biocompatibility and bioresorption mechanism of a bioresorbable nitrided iron scaffold[J]. Acta Biomater., 2017, 54: 454 |
| [8] | Haude M, Ince H, Abizaid A, et al.Sustained safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de novo coronary lesions: 12-month clinical results and angiographic findings of the BIOSOLVE-II first-in-man trial[J]. Eur. Heart J., 2016, 37: 2701 |
| [9] | Bowen P K, Shearier E R, Zhao S, et al.Biodegradable metals for cardiovascular stents: From clinical concerns to recent Zn-alloys[J]. Adv. Healthc. Mater., 2016, 5: 1121 |
| [10] | Zheng Y F, Liu B, Gu X N.Research progress in biodegradable metallic materials for medical application[J]. Mater. Rev., 2009, 23(1): 1(郑玉峰, 刘彬, 顾雪楠. 可生物降解性医用金属材料的研究进展[J]. 材料导报, 2009, 23(1): 1) |
| [11] | Sigel H.Metal Ions in Biological System[M]. New York: Marcel Dekker Inc, 1986: 1 |
| [12] | Bowman B A, Russell R M.Present Knowledge in Nutrition[M]. 8th Ed., Washington, DC: International Life Science Institute, 2001: 1 |
| [13] | Fawcett W, Haxby E, Male D A.Magnesium: Physiology and pharmacology[J]. Br. J. Anaesth., 1999, 83: 302 |
| [14] | Gu X N, Zheng Y F, Cheng Y, et al.In vitro corrosion and biocompatibility of binary magnesium alloys[J]. Biomaterials, 2009, 30: 484 |
| [15] | Ma J, Zhao N, Zhu D H.Biphasic responses of human vascular smooth muscle cells to magnesium ion[J]. J. Biomed. Mater. Res., 2016, 104A: 347 |
| [16] | Zhao N, Zhu D H.Endothelial responses of magnesium and other alloying elements in magnesium-based stent materials[J]. Metallomics, 2015, 7: 118 |
| [17] | Heublein B, Rohde R, Kaese V, et al.Biocorrosion of magnesium alloys: A new principle in cardiovascular implant technology?[J]. Heart, 2003, 89: 651 |
| [18] | Yue Y N, Wang L L, Yang N, et al.Effectiveness of biodegradable magnesium alloy stents in coronary artery and femoral artery[J]. J. Interv. Cardiol., 2015, 28: 358 |
| [19] | Li H W, Zhong H S, Xu K, et al.Enhanced efficacy of sirolimus-eluting bioabsorbable magnesium alloy stents in the prevention of restenosis[J]. J. Endovasc. Ther., 2011, 18: 407 |
| [20] | Mario C D, Griffiths H, Goktekin O, et al.Drug-eluting bioabsorb able magnesium stent[J]. J. Interv. Cardiol., 2004, 17: 391 |
| [21] | Maeng M, Jensen L O, Falk E, et al.Negative vascular remode-lling after implantation of bioabsorbable magnesium alloy stents in porcine coronary arteries: A randomised comparison with bare-metal and sirolimus-eluting stents[J]. Heart, 2009, 95: 241 |
| [22] | Waksman R, Pakala R, Kuchulakanti P K, et al.Safety and efficacy of bioabsorbable magnesium alloy stents in porcine coronary arteries[J]. Catheter. Cardiovasc. Interv., 2006, 68: 607 |
| [23] | Wittchow E, Adden N, Riedmueller J, et al.Bioresorbable drug-eluting magnesium-alloy scaffold: Design and feasibility in a porcine coronary model[J]. EuroIntervention, 2013, 8: 1441 |
| [24] | Zartner P, Buettner M, Singer H, et al.First biodegradable metal stent in a child with congenital heart disease: Evaluation of macro and histopathology[J]. Catheter. Cardiovasc. Interv., 2007, 69: 443 |
| [25] | Schranz D, Zartner P, Michel-Behnke I, et al.Bioabsorbable metal stents for percutaneous treatment of critical recoarctation of the aorta in a newborn[J]. Catheter. Cardiovasc. Interv., 2006, 67: 671 |
| [26] | Peeters P, Bosiers M, Verbist J, et al.Preliminary results after application of absorbable metal stents in patients with critical limb ischemia[J]. J. Endovasc. Ther., 2005, 12: 1 |
| [27] | Erbel R, Mario C D, Bartunek J, et al.Temporary scaffolding of coronary arteries with bioabsorbable magnesium stents: A prospective, non-randomised multicentre trial[J]. Lancet, 2007, 369: 1869 |
| [28] | Haude M, Erbel R, Erne P, et al.Safety and performance of the drug-eluting absorbable metal scaffold (DREAMS) in patients with de-novo coronary lesions: 12 month results of the prospective, multicentre, first-in-man BIOSOLVE-I trial[J]. Lancet, 2013, 381: 836 |
| [29] | Haude M, Ince H, Abizaid A, et al.Safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de-novo coronary artery lesions (BIOSOLVE-II): 6 month results of a prospective, multicentre, non-randomised, first-in-man trial[J]. Lancet, 2016, 387: 31 |
| [30] | Andrews N C.Disorders of iron metabolism[J]. New Engl. J. Med., 1999, 341: 1986 |
| [31] | Hermawan H, Dubé D, Mantovani D.Developments in metallic biodegradable stents[J]. Acta Biomater., 2010, 6: 1693 |
| [32] | Mueller P P, May T, Perz A, et al.Control of smooth muscle cell proliferation by ferrous iron[J]. Biomaterials, 2006, 27: 2193 |
| [33] | Zhu S F, Huang N, Xu L, et al.Biocompatibility of pure iron: in vitro assessment of degradation kinetics and cytotoxicity on endothelial cells[J]. Mater. Sci. Eng., 2009, C29: 1589 |
| [34] | Lin W J, Zhang D Y, Zhang G, et al.Design and characterization of a novel biocorrodible iron-based drug-eluting coronary scaffold[J]. Mater. Des., 2016, 91: 72 |
| [35] | Peuster M, Wohlsein P, Brügmann M, et al.A novel approach to temporary stenting: Degradable cardiovascular stents produced from corrodible metal-results 6-18 months after implantation into New Zealand white rabbits[J]. Heart, 2001, 86: 563 |
| [36] | Peuster M, Hesse C, Schloo T, et al.Long-term biocompatibility of a corrodible peripheral iron stent in the porcine descending aorta[J]. Biomaterials, 2006, 27: 4955 |
| [37] | Waksman R, Pakala R, Baffour R, et al.Short-term effects of biocorrodible iron stents in porcine coronary arteries[J]. J. Interv. Cardiol., 2008, 21: 15 |
| [38] | Pierson D, Edick J, Tauscher A, et al.A simplified in vivo approach for evaluating the bioabsorbable behavior of candidate stent materials[J]. J. Biomed. Mater. Res., 2012, 100B: 58 |
| [39] | Peuster M, Hesse C, Schloo T, et al.Long-term biocompatibility of a corrodible peripheral iron stent in the porcine descending aorta[J]. Biomaterials, 2006, 27: 4955 |
| [40] | Lin W J, Zhang D Y, Zhang G, et al.Design and characterization of a novel biocorrodible iron-based drug-eluting coronary scaffold[J]. Mater. Des., 2016, 91: 72 |
| [41] | Hermawan H, Purnama A, Dube D, et al.Fe-Mn alloys for metallic biodegradable stents: Degradation and cell viability studies[J]. Acta Biomater., 2010, 6: 1852 |
| [42] | Kaur K, Gupta R, Saraf S A, et al.Zinc: The metal of life[J]. Compr. Rev. Food. Sci. Food Saf., 2014, 13: 358 |
| [43] | Little P J, Bhattacharya R, Moreyra A E, et al.Zinc and cardiovascular disease[J]. Nutrition, 2010, 26: 1050 |
| [44] | Ma J, Zhao N, Zhu D H.Endothelial cellular responses to biodegradable metal zinc[J]. ACS Biomater. Sci. Eng., 2015, 1: 1174 |
| [45] | Ma J, Zhao N, Zhu D H.Bioabsorbable zinc ion induced biphasic cellular responses in vascular smooth muscle cells[J]. Sci. Rep., 2016, 6: 26661 |
| [46] | Bowen P K, Drelich J, Goldman J.Zinc exhibits ideal physiological corrosion behavior for bioabsorbable stents[J]. Adv. Mater., 2013, 25: 2577 |
| [47] | Bowen P K, Guillory II R J, Shearier E R, et al. Metallic zinc exhibits optimal biocompatibility for bioabsorbable endovascular stents[J]. Mater. Sci. Eng., 2015, C56: 467 |
| [48] | Bowen P K, Seitz J M, Guillory II R J, et al. Evaluation of wrought Zn-Al alloys (1, 3, 5 wt % Al) through mechanical and in vivo testing for stent applications [J]. J. Biomed. Mater. Res., 2017, B, doi: 10.1002/jbm.b.33850 |
| [49] | Guillory II R J, Bowen P K, Hopkins S P, et al. Corrosion characteristics dictate the long-term inflammatory profile of degradable zinc arterial implants[J]. ACS Biomater. Sci. Eng., 2016, 2: 2355 |
| [50] | Zhao S, Seitz J M, Eifler R, et al.Zn-Li alloy after extrusion and drawing: Structural, mechanical characterization, and biodegradation in abdominal aorta of rat[J]. Mater. Sci. Eng., 2017, C76: 301 |
| [51] | Drelich A, Zhao S, Guillory II R J, et al. Long-term surveillance of zinc implant in murine artery: Surprisingly steady biocorrosion rate[J]. Acta Biomater., 2017, 58: 539 |
| [52] | Yang H T, Wang C, Liu C Q, et al.Evolution of the degradation mechanism of pure zinc stent in the one-year study of rabbit abdominal aorta model, Biomaterials, 2017, doi: 10.1016/j.biomaterials.2017.08.022 |
| [53] | Nakazawa G, Granada J F, Alviar C L, et al.Anti-CD34 antibodies immobilized on the surface of sirolimus-eluting stents enhance stent endothelialization[J]. JACC Cardiovasc. Interv., 2010, 3: 68 |
| [54] | Swanson N, Hogrefe K, Javed Q, et al.Vascular endothelial growth factor (VEGF)-eluting stents: in vivo effects on thrombosis, endothelialization and intimal hyperplasia[J]. J. Invasive Cardiol., 2003, 15: 688 |
/
| 〈 |
|
〉 |