Effect of High Magnetic Field on the Microstructure in Directionally Solidified Co-Al-W Alloy
Received date: 2017-05-03
Online published: 2017-07-21
Supported by
Supported by National Natural Science Foundation of China (Nos.51404148, 51690162 and U1560202), United Innovation Program of Shanghai Commercial Aircraft Engine (Nos.AR910 and AR911) and fund of the State Key Laboratory of Solidification Processing (No.SKLSP201602)
Recently, a new Co-Al-W-based alloy with ordered L12 structure has been attracted much attention of researchers, these alloys have higher melting point than Ni-base superalloys with morphologically identical microstructure, but grain defect formation caused by thermosolutal convection has become an important problem for its application. Magnetic field is always applied to damp the convection which reduces the formation of defects. However, there are hitherto few papers to investigate the effect of magnetic field on grain defects during Co-Al-W-based alloy directional solidification. In this work, The effect of high magnetic field on the solidification structure and macrosegregation in directionally solidified Co-Al-W-based alloy was investigated. The results showed that the application of longitudinal magnetic field can induce convection and cause deformation of the solid-liquid interface shape, forming the macrosegregation and the stray grains in the mushy zone at the pulling rate of 5 μm/s. With the increase of pulling rate, the macrosegregation and the stray grains disappeared gradually at 2 T magnetic field. While the transverse magnetic field was applied, the macrosegregation became serious and the number of the stray grains increased. The macrosegregation further became more serious and the columnar-to-equiaxed transition was induced after adding the Ta element. The main reason of undercooling nucleation and columnar-to-equiaxed transition (CET) was the microsegregation induced by thermoelectric magnetic convention.
Jianbo YU , Yuan HOU , Chao ZHANG , Zhibin YANG , Jiang WANG , Zhongming REN . Effect of High Magnetic Field on the Microstructure in Directionally Solidified Co-Al-W Alloy[J]. Acta Metall Sin, 2017 , 53(12) : 1620 -1626 . DOI: 10.11900/0412.1961.2017.00165
| [1] | Hunt J D.Steady state columnar and equiaxed growth of dendrites and eutectic[J]. Mater. Sci. Eng., 1984, 65: 75 |
| [2] | Gandin C A, Rappaz M.Coupled finite element-cellular automaton model for the prediction of dendritic grain structures in solidification processes[J]. Acta Metall. Mater., 1994, 42: 2233 |
| [3] | Nastac L.Numerical modeling of solidification morphologies and segregation patterns in cast dendritic alloys[J]. Acta Mater., 1999, 47: 4253 |
| [4] | Dong H B, Yang X L, Lee P D, et al.Simulation of equiaxed growth ahead of an advancing columnar front in directionally solidified Ni-based superalloys[J]. J. Mater. Sci., 2004, 39: 7207 |
| [5] | Dong H B, Lee P D.Simulation of the columnar-to-equiaxed transition in directionally solidified Al-Cu alloys[J]. Acta Mater., 2005, 53: 659 |
| [6] | Liu D R, Mangelinck-No?l N, Gandin C A, et al.Structures in directionally solidified Al-7wt.% Si alloys: Benchmark experiments under microgravity[J]. Acta Mater., 2014, 64: 253 |
| [7] | Spittle J A.Columnar to equiaxed grain transition in as solidified alloys[J]. Int. Mater. Rev., 2006, 51: 247 |
| [8] | Li X, Gagnoud A, Fautrelle Y, et al.Dendrite fragmentation and columnar-to-equiaxed transition during directional solidification at lower growth speed under a strong magnetic field[J]. Acta Mater., 2012, 60: 3321 |
| [9] | Li X, Fautrelle Y, Zaidat K, et al.Columnar-to-equiaxed transitions in al-based alloys during directional solidification under a high magnetic field[J]. J. Cryst. Growth, 2010, 312: 267 |
| [10] | Li X, Ren Z M, Shen Y, et al.Effect of thermoelectric magnetic force on the array of dendrites during directional solidification of Al-Cu alloys in a high magnetic field[J]. Philos. Mag. Lett., 2012, 92: 675 |
| [11] | Li X, Fautrelle Y, Ren Z M.Influence of thermoelectric effects on the solid-liquid interface shape and cellular morphology in the mushy zone during the directional solidification of Al-Cu alloys under a magnetic field[J]. Acta Mater., 2007, 55: 3803 |
| [12] | Li X, Gagnoud A, Fautrelle Y, et al.Effect of a transverse magnetic field on solidification structures in unmodified and Sr-modified Al-7wtpctSi alloys during directional solidification[J]. Metall. Mater. Trans., 2016, 47A: 1198 |
| [13] | Li X, Fautrelle Y, Ren Z M.Influence of an axial high magnetic field on the liquid-solid transformation in Al-Cu hypoeutectic alloys and on the microstructure of the solid[J]. Acta Mater., 2007, 55: 1377 |
| [14] | Li X, Gagnoud A, Ren Z M, et al.Investigation of thermoelectric magnetic convection and its effect on solidification structure during directional solidification under a low axial magnetic field[J]. Acta Mater., 2009, 57: 2180 |
| [15] | Li X, Fautrelle Y, Ren Z M.Morphological instability of cell and dendrite during directional solidification under a high magnetic field[J]. Acta Mater., 2008, 56: 3146 |
| [16] | Li X, Fautrelle Y, Ren Z M.Influence of a high magnetic field on columnar dendrite growth during directional solidification[J]. Acta Mater., 2007, 55: 5333 |
| [17] | Zhong H, Li C J, Ren Z M, et al.Effect of interdendritic thermoelectric magnetic convection on the evolution of tertiary dendrite during directional solidification[J]. J. Cryst. Growth, 2016, 439: 66 |
| [18] | Sato J, Omori T, Oikawa K, et al.Cobalt-base high-temperature alloys[J]. Science, 2006, 312: 90 |
| [19] | Omori T, Oikawa K, Sato J, et al.Partition behavior of alloying elements and phase transformation temperatures in Co-Al-W-base quaternary systems[J]. Intermetallics, 2013, 32: 274 |
| [20] | Pollock T M, Dibbern J, Tsunekane M, et al.New Co-based γ-γ′ high-temperature alloys[J]. JOM, 2010, 62(1): 58 |
| [21] | Xue F, Li Z Q, Feng Q. Mo effect on the microstructure in Co-Al-W-based superalloys [J]. Mater. Sci. Forum, 2010, 654-656: 420 |
| [22] | Shi L, Yu J J, Cui C Y, et al.Effect of Ta additions on microstructure and mechanical properties of a single-crystal Co-Al-W-base alloy[J]. Mater. Lett., 2015, 149: 58 |
| [23] | Pyczak F, Bauer A, G?ken M, et al.The effect of tungsten content on the properties of L12-hardened Co-Al-W alloys[J]. J. Alloys Compd., 2015, 632: 110 |
| [24] | Yan Y H, Coakley J, Vorontsov V A, et al.Alloying and the micromechanics of Co-Al-W-X quaternary alloys[J]. Mater. Sci. Eng., 2014, A613: 201 |
| [25] | Wang J, Ren Z M, Fautrelle Y, et al.Modification of liquid/solid interface shape in directionally solidifying Al-Cu alloys by a transverse magnetic field[J]. J. Mater. Sci., 2013, 48: 213 |
/
| 〈 |
|
〉 |