Orginal Article

Microstructure Evolution of Hot-Dip Al-10%Si Coating During the Austenitization of 22MnB5 Hot Stamping Steel

  • Xunhua YUAN ,
  • Qifu ZHANG
Expand
  • National Engineering Laboratory of Advanced Coating Technology for Metals, New Metallurgy Hi-Tech Group Co., Ltd., Beijing 100081, China

Received date: 2017-03-09

  Online published: 2017-07-18

Supported by

Supported by National Natural Science Foundation of China (No.51071052) and National Science and Technology Pillar Program during the Twelfth Five-Year Plan Period (No.2012BAJ13B03)

Abstract

Hot stamping is an alternative technology to produce ultra-high strength steel (UHSS) with a tensile strength above 1 GPa for automotive bodies. At present, the hot-dip Al-10%Si (mass fraction) coating is used as a shield coating for the hot stamping steels, which protects the steels from surface oxidation and decarburization, and enhances their corrosion resistance. However, the microstructure evolution and compounds of hot-dip Al-10%Si coating during austenitization of 22MnB5 hot stamping steel are not clear yet. In this work, the thermo-mechanically induced microstructure evolution of hot-dip Al-10%Si coating is observed using SEM after austenitization of 22MnB5 hot stamping steel at 900 ℃ for different times, and the elemental depth profiles are analyzed in hot-dip Al-10%Si coating by EDS and GD-OES. The results show that before austenitization, the hot-dip Al-10%Si coating consisted of an aluminum matrix, pure silicon, and the intermetallic compound Fe2SiAl7, which was formed by eutectic reaction, there was a thin layer, which was composed of Fe2Al5 and FeAl3 between the intermetallic compound Fe2SiAl7 and the steel substrate. When 22MnB5 hot stamping steel was austenitized at 900 ℃, the ternary eutectic phase Al+Si+τ6 was transformed into an Al-Fe-Si ternary intermetallic compound or Fe-Al binary intermetallic compound gradually in the hot-dip Al-10%Si coating. When the austenitizing time was 2 min, the Al-10%Si coating was composed of the intermetallic compound Fe2SiAl7, Fe2Al5 and FeAl2 phases; when the austenitizing time was 5 min, the Al-10%Si coating was composed of FeAl2, Fe2SiAl2 and Fe5SiAl4 phases; when the austenitizing time was 8 min, the Al-10%Si coating was composed of FeAl2 and Fe5SiAl4 phases. Because the diffusion rate of Al atoms was much larger than that of Fe atoms in the diffusion layer of intermetallic compound Fe2SiAl2 and coating/steel substrate, the amount of Al atoms which diffused and reacted from the coating to the grain boundaries or grain of steel substrate was much larger than that of the Fe atoms which diffused from the steel substrate to the Al-10%Si coating, also the number of vacancies which diffused from the steel substrate to the Al-10%Si coating was much larger than the other way round. Due to this imbalance, the Kirkendall void was formed in the interface between the diffusion reaction layer and the Al-10%Si the coating. The hot-dip Al-10%Si coating can be used as the protective layer, since it has a stable Al2O3 film formed on its surface, and its thermal oxidation was very limited, during the 22MnB5 hot stamping steel austenitizing. But the protective performances of Al-10%Si coating could be poor, because the high temperature ductility of brittle intermetallic compound was low, which induced a lot of micro cracks that were perpendicular to the interface of coating/steel substrate, and penetrated the whole coating during the diffusion process of hot-dip Al-10%Si coating.

Cite this article

Xunhua YUAN , Qifu ZHANG . Microstructure Evolution of Hot-Dip Al-10%Si Coating During the Austenitization of 22MnB5 Hot Stamping Steel[J]. Acta Metall Sin, 2017 , 53(11) : 1495 -1503 . DOI: 10.11900/0412.1961.2017.00077

References

[1] Kang Y L.Lightweight vehicle, advanced high strength steel and energy-saving and emission reduction[J]. Iron Steel, 2008, 43(6): 1(康永林. 汽车轻量化先进高强钢与节能减排[J]. 钢铁, 2008, 43(6): 1)
[2] Jenner F.Investigation of the intermetallic coating formed during processing of aluminum-coated boron heat-treatable steels [A]. Proceedings of the XIth International Congress and Exposition[C]. Orlando: Society for Experimental Mechanics, 2008: 37
[3] Barcellona A, Palmeri D.Effect of plastic hot deformation on the hardness and continuous cooling transformations of 22MnB5 microalloyed boron steel[J]. Metall. Mater. Trans, 2009, 40A: 1160
[4] Abdulhay B, Bourouga B, Dessain C, et al.Experimental study of heat transfer in hot stamping process[J]. Int. J. Mater. Form., 2009, 2: 255
[5] Ma N, Shen G Z, Zhang Z H, et al.Material performance of hot-forming high strength steel and its application in vehicle body[J]. Chin. J. Mech. Eng., 2011, 47(8): 60(马宁, 申国哲, 张宗华等. 高强度钢板热冲压材料性能研究及在车身设计中的应用[J]. 机械工程学报, 2011, 47(8): 60)
[6] Nakagawa K, Nakagaito T, Yokata T, et al.Effect of depth of crack on fatigue property in Zn-Ni coated press hardened steel [A]. 5th International Conference on Proceedings on Hot Sheet Metal Forming of High-Performance Steel[C]. Toronto: Association for Iron & Steel Technology, 2015: 77
[7] Kolleck R, Veit R, Merklein M, et al.Investigation on induction heating for hot stamping of boron alloyed steels[J]. CIRP Ann. Manuf. Technol., 2009, 58(1): 275
[8] Naganathan A.Hot stamping of manganese boron steel [D]. Columbus: Ohio State University, 2010: 31
[9] Han Q H, Bi W Z, Jin X Y, et al.Low temperature hot forming of medium-Mn steel [A]. 5th International Conference on Hot Sheet Metal Forming of High-Performance Steel[C]. Toronto: Association for Iron & Steel Technology, 2015: 381
[10] Xu W L, Guan S R, Ai J, et al.Introduction of sheet metal hot-forming[J]. J. Plast. Eng., 2009, 16(4): 39(徐伟力, 管曙荣, 艾键等. 钢板热冲压新技术介绍[J]. 塑性工程学报, 2009, 16(4): 39)
[11] Liu H S, Liu W, Bao J, et al.Numerical and experimental investigation into hot forming of ultra high strength steel sheet[J]. J. Mater. Eng. Perform., 2011, 20: 1
[12] Naderi M, Ketabchi M, Abbasi M, et al.Semi-hot stamping as an improved process of hot stamping[J]. J. Mater. Sci. Technol., 2011, 27: 369
[13] Naderi M, Ketabchi M, Abbasi M, et al.Analysis of microstructure and mechanical properties of different high strength carbon steels after hot stamping[J]. J. Mater. Process. Technol., 2011, 211: 1117
[14] Liu H P, Jin X J, Dong H, et al.Martensitic microstructural transformations from the hot stamping, quenching and partitioning process[J]. Mater. Charact., 2011, 62: 223
[15] Sengoku A, Takebayashi H, Matsumura K.Microstructural and phase evolution of galvannealed coating during hot stamping heating [A]. 5th International Conference on Proceedings on Hot Sheet Metal Forming of High-Performance Steel[C]. Toronto: Association for Iron & Steel Technology, 2015: 363
[16] Suehiro M, Kusumi K, Miyakoshi T, et al.Properties of aluminum-coated steels for hot-forming[J]. Nippon Steel Tech. Rep., 2003, 88: 16
[17] Maki J, Kurosaki M, Kusumi K, et al.Effect of heating condition and hot forming on corrosion resistance of hot stamped aluminized steels [A]. 3th International Conference on Proceedings on Hot Sheet Metal Forming of High-Performance Steel[C]. Kassel: Association for Iron & Steel Technology, 2011: 449
[18] Dosdat L, Petitjean J, Vietoris T, et al.Corrosion resistance of different metallic coatings on press-hardened steels for automotive[J]. Steel Res. Int., 2011, 82: 726
[19] Fan D W, De Cooman B C. State-of-the-knowledge on coating systems for hot stamped parts[J]. Steel Res. Int., 2012, 83: 412
[20] Grigorieva R, Drillet P, Mataigne J M, et al. Phase transformations in the Al-Si coating during the austenitization step [J]. Solid State Phenom., 2011, 172-174: 784
[21] Luther F, Koll T, Braun M.Laboratory study on the performance of zinc and aluminum based coatings for a direct hot press forming process [A]. 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet[C]. Genova: Associazione Italiana Di Metallurgia, 2011: 379
[22] Fan D W, Kim H S, Oh J K, et al.Coating degradation in hot press forming[J]. ISIJ Int., 2010, 50: 561
[23] Chang Y Y, Tsaur C C, Rock J C.Microstructure studies of an aluminide coating on 9Cr-1Mo steel during high temperature oxidation[J]. Surf. Coat. Technol., 2006, 200: 6588
[24] Borsetto F, Ghiotti A, Bruschi S. Investigation of the high strength steel Al-Si coating during hot stamping operations [J]. Key Eng. Mater., 2009, 410-411: 289
[25] Young D J.High temperature oxidation and corrosion of metals[M]. Oxford, UK: Elsevier, 2008: 16
[26] Liu B J.Hot Dip Aluminizing Steel [M]. Beijing: Metallurgical Industry Press, 1995: 12(刘邦津. 钢材的热浸镀铝 [M]. 北京: 冶金工业出版社, 1995: 12)
[27] Paul A, Van Dal M J H, Kodentsov A A, et al. The kirkendall effect in multiphase diffusion[J]. Acta Mater., 2004, 52: 623
[28] Maitra T, Gupta S P.Intermetallic compound formation in Fe-Al-Si ternary system: Part II[J]. Mater. Charact., 2002, 49: 293
[29] Grigorieva R, Drillet P, Mataigne J M, et al.Study of phase transformations in Al-Si coating during the austenitization step [A]. 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet[C]. Genova: Associazione Italiana Di Metallurgia, 2011: 331
Outlines

/