A New Method for Directly Testing the Mechanical Properties of Anisotropic Materials in Bi-Axial Stress State by Tube Bulging Test
Received date: 2017-03-07
Online published: 2017-06-14
Supported by
Supported by National Natural Science Foundation of China (Nos.51405102 and 51475121), China Postdoctoral Science Foundation (No.2015M570286), Fundamental Research Funds for the Central Universities (No.HIT.NSRIF.2016093) and Scientific Research Foundation of Harbin Institute of Technology at Weihai (No.HIT(WH)201414)
Due to the increasing demands for lightweight parts in various fields, such as bicycle, automotive, aircraft and aerospace industries, hydroforming processes have become popular in recent years. Since tubular materials during tube hydroforming are under a bi-axial even tri-axial stress state, which is different from that in the tensile test, it is necessary to test the mechanical properties of the material under bi-axial stress state. Tube bulging test is an advanced method for characterizing the mechanical properties of tubular materials under bi-axial stress state. But there are excessive physical quantities in the theoretical model of tube bulging test for testing the mechanical properties of tubes under bi-axial stress state which are difficult to be obtained during the experiment. In order to solve the problems, a method for directly testing the mechanical properties of tubes under bi-axial stress state was proposed in this work, which will be referred to as "one point method". Because of circular model is characterized by a dominant function expression, theoretical models of both the pole axial curvature radius and the pole thickness during bulging test are derived under supposing the geometrical models for bulging zone as circular. Thus, the mechanical properties of tubes under bi-axial stress state can be obtained only through measuring the bulging height at the pole point during the bulging test, which laid the foundation for the establishment of a simple and reliable method for testing the mechanical properties of the tube online. Based on the above proposed method, the extruded aluminum alloy tubes AA6061 were tested. The results showed that both the pole axial curvature radius and the pole thickness during bulging test can be expressed as display functions pertaining to the bulging height at the pole point. For the theoretical model of the pole axial curvature radius, as the bulging rate increases, the prediction accuracy increases at beginning, and decreases at the end when using circular as the theoretical geometrical models for bulging zone. The prediction accuracy is the highest as the bulging rate is about 13%, the prediction accuracy decreases after the bulging rate is more than 20%. Fortunately, the overall prediction error is small. The maximum error does not exceed ±0.9%. The prediction accuracy of the pole thickness using the theoretical model is almost unaffected by the specimen geometry. When the ratios of length to diameter and diameter to thickness change, the difference is very small, the prediction error is not more than 0.8%. This is very helpful to ensure the accuracy of mechanical testing under bi-axial loading conditions. Using the "one point method", the stress and strain components along the circumferential and axial directions can be simultaneously measured, this laid the foundation for further analysis of the anisotropic property impacting on the flow and subsequent yield under complex stress state.
Yanli LIN , Zhubin HE , Guannan CHU , Yongda YAN . A New Method for Directly Testing the Mechanical Properties of Anisotropic Materials in Bi-Axial Stress State by Tube Bulging Test[J]. Acta Metall Sin, 2017 , 53(9) : 1101 -1109 . DOI: 10.11900/0412.1961.2017.00074
| [1] | Chu E, Xu Y.Hydroforming of aluminum extrusion tubes for automotive applications. Part I: buckling, wrinkling and bursting analyses of aluminum tubes[J]. Int. J. Mech. Sci., 2004, 46: 263 |
| [2] | Liu J A.Make great efforts to develop aluminum parts industry and promote the modernization progress of automobile industry[J]. Alum. Fabricat., 2005, (3): 8(刘静安. 大力发展铝合金零部件产业促进汽车工业的现代化进程[J]. 铝加工, 2005, (3): 8) |
| [3] | Zhu J F.Aluminum alloy used for automobile outer panel at abroad[J]. Metall. Inform. Rev., 2005, (1): 25(朱久发. 国外汽车面板用铝合金材料[J]. 冶金信息导刊, 2005, (1): 25) |
| [4] | Zhong Q, Shi Y, Liu B.The application of aluminum alloy in automotive light weighting[J]. Adv. Mater. Ind., 2015, (2): 23(钟奇, 施毅, 刘博. 铝合金在汽车轻量化中的应用[J]. 新材料产业, 2015, (2): 23) |
| [5] | Zhang L X, Chen W Z, Zhang W C, et al.Microstructure and mechanical properties of thin ZK61 magnesium alloy sheets by extrusion and multi-pass rolling with lowered temperature[J]. J. Mater. Process. Technol., 2016, 237: 65 |
| [6] | Kuwabara T, Yoshida K, Narihara K, et al.Anisotropic plastic deformation of extruded aluminum alloy tube under axial forces and internal pressure[J]. Int. J. Plast., 2005, 21: 101 |
| [7] | Jansson M, Nilsson L, Simonsson K.On constitutive modeling of aluminum alloys for tube hydroforming applications[J]. Int. J. Plast., 2005, 21: 1041 |
| [8] | Kuwabara T, Sugawara F.Multiaxial tube expansion test method for measurement of sheet metal deformation behavior under biaxial tension for a large strain range[J]. Int. J. Plast., 2013, 45: 103 |
| [9] | Fuchizawa S, Narazaki M.Bulge test for determining stress-strain characteristics of thin tubes [A]. Advanced Technology of Plasticity Proceedings of Fourth ICTP[C]. Beijing China: ICTP, 1993: 488 |
| [10] | Hwang Y M, Lin Y K, Altan T.Evaluation of tubular materials by a hydraulic bulge test[J]. Int. J. Mach. Tool Manuf., 2007, 47: 343 |
| [11] | Hwang Y M, Lin Y K.Evaluation of flow stresses of tubular materials considering anisotropic effects by hydraulic bulge tests[J]. J. Eng. Mater. Technol., 2007, 129: 414 |
| [12] | Hwang Y M, Wang C W.Flow stress evaluation of zinc copper and carbon steel tubes by hydraulic bulge tests considering their anisotropy[J]. J. Mater. Process. Technol., 2009, 209: 4423 |
| [13] | Bortot P, Ceretti E, Giardini C.The determination of flow stress of tubular material for hydroforming applications[J]. J. Mater. Process. Technol., 2008, 203: 381 |
| [14] | Velasco R, Boudeau N.Tube bulging test: Theoretical analysis and numerical validation[J]. J. Mater. Process. Technol., 2008, 205: 51 |
| [15] | He Z B, Yuan S J, Lin Y L, et al.Analytical model for tube hydro-bulging test, Part I: Models for stress components and bulgingzone profile[J]. Int. J. Mech. Sci., 2014, 87: 297 |
| [16] | He Z B, Yuan S J, Lin Y L, et al.Analytical model for tube hydro-bulging tests, Part II: Linear model for pole thickness and its application[J]. Int. J. Mech. Sci., 2014, 87: 307 |
| [17] | Yang L F, Guo C.Determination of stress-strain relationship of tubular material with hydraulic bulge test[J]. Thin Wall. Struct., 2008, 46: 147 |
| [18] | Tirosh J, Neubrger A, Shirizly A.On tube expansion by internal fluid pressure with additional compressive stress[J]. Int. J. Mech. Sci., 1996, 38: 839 |
| [19] | Strano M, Altan T.An inverse energy approach to determine the flow stress of tubular materials for hydroforming applications[J]. J. Mater. Process. Technol., 2004, 146: 92 |
| [20] | Li S G.Foundamental study on tube hydroforming process [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2007(李泷杲. 金属薄壁管液压成形应用基础研究 [D]. 南京: 南京航空航天大学, 2007) |
| [21] | Hosford W F.Comments on anisotropic yield criteria[J]. Int. J. Mech. Sci., 1985, 27: 423 |
| [22] | Logan R, Hosford W F.Upper-bound anisotropic yield locus calculations assuming <111>-pencil glide[J]. Int. J. Mech. Sci., 1980, 22: 430 |
| [23] | Barlat F, Brem J C, Yoon J W, et al.Plane stress yield function for aluminum alloy sheets——Part 1: Theory[J]. Int. J. Plast., 2003, 19: 1297 |
| [24] | Banabic D.Sheet Metal Forming Processes: Constitutive Modelling and Numerical Simulation[M]. Berlin: Springer, 2010: 77 |
| [25] | Hu W L, Lin Y L, Yuan S J, et al. Constitutive models for regression of various experimental stress-strain relations [J]. Int. J. Mech. Sci., 2015, 101-102: 1 |
/
| 〈 |
|
〉 |