Very High Cycle Fatigue Failure Mechanism of TC17 Alloy
1 The authors contributed equally to this work.
Received date: 2016-12-15
Online published: 2017-06-13
Supported by
Supported by National Natural Science Foundation of China (No.11372201)
Titanium alloys have been widely used in bearing force components in aeronautical structures, such as blades and beams to withstand the high frequency dynamic loads, which requires an outstanding fatigue resistance performance in very high cycle regime during their service life. In this work, very high cycle fatigue failure property of TC17 alloy used as aircraft engine blade material was studied by ultrasonic fatigue test and electromagnetic resonance fatigue test under 110 Hz and 20 kHz sinusoidal load, and crack initiation mechanism of different failure mode was analyzed. The results showed that, fatigue failure modes of TC17 alloy could be divided into surface induced failure and interior induced failure. Surface induced failure was caused by the machine defect and surface slide trace that triggered by the asymmetric loading. Interior induced failure was caused by slid fracture of primary α phase under asymmetric loading. Fatigue resistance of TC17 alloy was influenced by the fatigue crack initiation mechanism but concerned little about the loading frequency. The variation of the fatigue failure mechanism resulted in the S-N curves presenting bilinear. A fatigue strength predicted model is established based on the parameter of the weak crystal orientation area, which is in good agreement with the fatigue test result.
Hanqing LIU , Chao HE , Zhiyong HUANG , Qingyuan WANG . Very High Cycle Fatigue Failure Mechanism of TC17 Alloy[J]. Acta Metall Sin, 2017 , 53(9) : 1047 -1054 . DOI: 10.11900/0412.1961.2016.00561
| [1] | Sakai T, Sato Y, Nagano Y, et al.Effect of stress ratio on long life fatigue behavior of high carbon chromium bearing steel under axial loading[J]. Int. J. Fatigue, 2006, 28: 1547 |
| [2] | Furuya Y, Takeuchi E.Gigacycle fatigue properties of Ti-6Al-4V alloy under tensile mean stress[J]. Mater. Sci. Eng., 2014, A598: 135 |
| [3] | Schuller R, Karr U, Irrasch D, et al.Mean stress sensitivity of spring steel in the very high cycle fatigue regime[J]. J. Mater. Sci., 2015, 50: 5514 |
| [4] | Liu X L, Sun C Q, Hong Y S.Effects of stress ratio on high-cycle and very-high-cycle fatigue behavior of a Ti-6Al-4V alloy[J]. Mater. Sci. Eng., 2015, A622: 228 |
| [5] | Mughrabi H.On ‘multi-stage’ fatigue life diagrams and the relevant life-controlling mechanisms in ultrahigh-cycle fatigue[J]. Fatigue Fract. Eng. Mater. Struct., 2002, 25: 755 |
| [6] | Lei Z Q, Hong Y S, Xie J J, et al.Effects of inclusion size and location on very-high-cycle fatigue behavior for high strength steels[J]. Mater. Sci. Eng., 2012, A558: 234 |
| [7] | Marines I, Dominguez G, Baudry G, et al.Ultrasonic fatigue tests on bearing steel AISI-SAE 52100 at frequency of 20 and 30 kHz[J]. Int. J. Fatigue, 2003, 25: 1037 |
| [8] | Wang Q Y, Bathias C, Kawagoishi N, et al.Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength[J]. Int. J. Fatigue, 2002, 24: 1269 |
| [9] | Phung N L, Favier V, Ranc N, et al.Very high cycle fatigue of copper: evolution, morphology and locations of surface slip markings[J]. Int. J. Fatigue, 2014, 63: 68 |
| [10] | Stanzl-Tschegg S E, Sch?nbauer B. Mechanisms of strain localization, crack initiation and fracture of polycrystalline copper in the VHCF regime[J]. Int. J. Fatigue, 2010, 32: 886. |
| [11] | Huang Z Y, Liu H Q, Wang C, et al.Fatigue life dispersion and thermal dissipation investigations for titanium alloy TC17 in very high cycle regime[J]. Fatigue Fract. Eng. Mater. Struct., 2015, 38: 1285 |
| [12] | Bantounas I, Dye D, Lindley T C.The role of microtexture on the faceted fracture morphology in Ti-6Al-4V subjected to high-cycle fatigue[J]. Acta Mater., 2010, 58: 3908 |
| [13] | Jha S K, Szczepanski C J, John R, et al.Deformation heterogeneities and their role in life-limiting fatigue failures in a two-phase titanium alloy[J]. Acta Mater., 2015, 82: 378 |
| [14] | Efstathiou C, Sehitoglu H, Lambros J.Multiscale strain measurements of plastically deforming polycrystalline titanium: Role of deformation heterogeneities[J]. Int. J. Plast., 2010, 26: 93 |
| [15] | Drugan W J, Willis J R.A micromechanics-based nonlocal constitutive equation and estimates of representative volume element size for elastic composites[J]. J. Mech. Phys. Solids, 1996, 44: 497 |
| [16] | Gusev A A.Representative volume element size for elastic composites: a numerical study[J]. J. Mech. Phys. Solids, 1997, 45: 1449 |
| [17] | Ren Z Y, Zheng Q S.Effects of grain sizes, shapes, and distribution on minimum sizes of representative volume elements of cubic polycrystals[J]. Mech. Mater., 2004, 36: 1217 |
| [18] | Ranganathan S I, Ostoja-Starzewski M.Scale-dependent homogenization of inelastic random polycrystals[J]. J. Appl. Mech., 2008, 75: 883 |
| [19] | Stroh A N.The formation of cracks as a result of plastic flow[J]. Proc. R. Soc. London, 1954, 223: 404 |
| [20] | Echlin M L P, Stinville J C, Miller V M, et al. Incipient slip and long range plastic strain localization in microtextured Ti-6Al-4V titanium[J]. Acta Mater., 2016, 114: 164 |
| [21] | Britton T B, Birosca S, Preuss M, et al.Electron backscatter diffraction study of dislocation content of a macrozone in hot-rolled Ti-6Al-4V alloy[J]. Scr. Mater., 2010, 62: 639 |
| [22] | Bridier F, Villechaise P, Mendez J.Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales[J]. Acta Mater., 2008, 56: 3951 |
| [23] | Wang Q Y, Berard J Y, Rathery S, et al.Technical note High-cycle fatigue crack initiation and propagation behaviour of high-strength sprin steel wires[J]. Fatigue Fract. Eng. Mater. Struct., 2003, 22: 673 |
| [24] | Hong Y S, Lei Z Q, Sun C Q, et al.Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels[J]. Int. J. Fatigue, 2014, 58: 144 |
| [25] | Yoshinaka F, Nakamura T, Takaku K.Effects of vacuum environment on small fatigue crack propagation in Ti-6Al-4V[J]. Int. J. Fatigue, 2016, 91: 29 |
| [26] | Sugano M, Kanno S, Satake T.Fatigue behavior of titanium in vacuum[J]. Acta Metall., 1989, 37: 1811 |
| [27] | Murakam Y, Nomoto T, Ueda T.Factors influencing the mechanism of superlong fatigue failure in steels[J]. Fatigue Fract. Eng. Mater. Struct., 1999, 22: 581 |
| [28] | Murakami Y, Endo M.Effects of defects, inclusions and in homogeneities on fatigue strength[J]. Int. J. Fatigue, 1994, 16: 163 |
/
| 〈 |
|
〉 |