Orginal Article

Numerical Simulation of Microstructure Evolution During the Solid Phase Transformation of Ti-6Al-4V Alloy in Investment Casting

  • Heng SHAO ,
  • Yan LI ,
  • Hai NAN ,
  • Qingyan XU
Expand
  • 1 Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China
    2 Beijing Institute of Aeronautical Materials, Beijing 100095, China。

Received date: 2016-12-28

  Online published: 2017-06-08

Supported by

Supported by China-EU (European Union) Science & Technology Cooperation in Aviation, Horizon 2020 Framework Programme for Research and Innovation (2014-2020) of EU, National Basic Research Program of China (No.2011CB706801), National Natural Science Foundation of China (Nos.51171089 and 51374137), National Science and Technology Major Project (No.2012ZX04012011) and High Technology Research and Development Program of China (No.2007AA04Z141)

Abstract

Investment casting is widely used in producting complex thin-wall titanium alloy components. In this process, the βα phase transformation decides the final microstructures of these components. However most of present studies on phase transformation of titanium alloys focus on the microstructure evolution in heat treatment process or after deformation rather than in casting process now. It is a main reason only this work aims at the solid phase transformation of Ti-6Al-4V alloy in investment casting. In this work, the growth model of edge of α phase plates based on multi component Zener-Hiller model, and the growth model of broad face of α phase plates based on diffusion and conservation of multi components were established. The growth competition of different colonies, which consist of α phase plates in same orientation, was simulated and the microstructures and their evolution with temperature were obtained. The comparison between simulated microstructures and their evolution with temperature and experimental data indicated that the proportion of undercooling degree caused by impurities in the alloy is about 45% of the total undercooling degree in broad face of α phase plates and a much smaller portion in edge of α phase plates. The comparison also showed that the enthalpy change of solid phase transformation of titanium alloy is about 70 kJ/kg. The simulated and experimental morphologies look like similar and the simulated growth rate is also in good accordance with experiment inferred growth rate.

Cite this article

Heng SHAO , Yan LI , Hai NAN , Qingyan XU . Numerical Simulation of Microstructure Evolution During the Solid Phase Transformation of Ti-6Al-4V Alloy in Investment Casting[J]. Acta Metall Sin, 2017 , 53(9) : 1140 -1152 . DOI: 10.11900/0412.1961.2016.00579

References

[1] Cui C X, Hu B M, Zhao L C, et al.Titanium alloy production technology, market prospects and industry development[J]. Mater. Des., 2011, 32: 1684
[2] Li Y H, Sun Z Q, Li X L, et al.Recent progress of biomedical porous titanium for bone implants[J]. J. Optoelect. Adv. Mater., 2014, 16: 513
[3] Zhou L.Review of titanium industry progress in America, Japan and China[J]. Rare Met. Mater. Eng., 2003, 32: 577(周廉. 美国、日本和中国钛工业发展评述[J]. 稀有金属材料与工程, 2003, 32: 577)
[4] Williams J C, Starke E A Jr. Progress in structural materials for aerospace systems[J]. Acta Mater., 2003, 51: 5775
[5] Filip R, Kubiak K, Ziaja W, et al.The effect of microstructure on the mechanical properties of two-phase titanium alloys[J]. J. Mater. Process. Technol., 2003, 133: 84
[6] Jovanovi? M T, Tadi? S, Zec S, et al.The effect of annealing temperatures and cooling rates on microstructure and mechanical properties of investment cast Ti-6Al-4V alloy[J]. Mater. Des., 2006, 27: 192
[7] Sui Y W, Li B S, Liu A H, et al.Microstructures and hardness of Ti-6Al-4V alloy staging castings under centrifugal field[J]. Trans. Nonferrous Met. Soc. China, 2008, 18: 291
[8] Ahmed T, Rack H J.Phase transformations during cooling in α+β titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 206
[9] Lütjering G.Influence of processing on microstructure and mecha-nical properties of (α+β) titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 32
[10] Bhattacharyya D, Viswanathan G B, Denkenberger R, et al.The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy[J]. Acta Mater., 2003, 51: 4679
[11] Bhattacharyya D, Viswanathan G B, Fraser H L.Crystallographic and morphological relationships between β phase and the Widmanst?tten and allotriomorphic α phase at special β grain boundaries in an α/β titanium alloy[J]. Acta Mater., 2007, 55: 6765
[12] Whittaker R, Fox K, Walker A.Texture variations in titanium alloys for aeroengine applications[J]. Mater. Sci. Technol., 2010, 26: 676
[13] He D, Zhu J C, Zaefferer S, et al.Influences of deformation strain, strain rate and cooling rate on the Burgers orientation relationship and variants morphology during βα phase transformation in a near α titanium alloy[J]. Mater. Sci. Eng., 2012, A549: 20
[14] Katzarov I, Malinov S, Sha W.Finite element modeling of the morphology of β to α phase transformation in Ti-6Al-4V alloy[J]. Metall. Mater. Trans., 2002, 33A: 1027
[15] Yang M, Wang G, Teng C Y, et al.3D phase field simulation of effect of interfacial energy anisotropy on sideplate growth in Ti-6Al-4V[J]. Acta Metall. Sin., 2012, 48: 148(杨梅, 王刚, 滕春禹等. Ti-6Al-4V中界面能对α相片层生长的影响三维相场模拟[J]. 金属学报, 2012, 48: 148)
[16] Shi R, Zhou N, Niezgoda S R, et al.Microstructure and transformation texture evolution during α precipitation in polycrystalline α/β titanium alloys——A simulation study[J]. Acta Mater., 2015, 94: 224
[17] Song K J, Wei Y H, Dong Z B, et al.Numerical simulation of β to α phase transformation in heat affected zone during welding of TA15 alloy[J]. Comp. Mater. Sci., 2013, 72: 93
[18] Jacot A, Rappaz M.A pseudo-front tracking technique for the modelling of solidification microstructures in multi-component alloys[J]. Acta Mater., 2002, 50: 1909
[19] Shi R, Ma N, Wang Y.Predicting equilibrium shape of precipitates as function of coherency state[J]. Acta Mater., 2012, 60: 4172
[20] Carman A, Zhang L C, Ivasishin O M, et al.Role of alloying elements in microstructure evolution and alloying elements behaviour during sintering of a near-β titanium alloy[J]. Mater. Sci. Eng., 2011, A528: 1686
[21] Lutjering G, Williams J C.Titanium[M]. Berlin: Springer-Verlag, 2003: 44
[22] Hillert M, H?glund L, ?gren J.Diffusion-controlled lengthening of Widmanst?tten plates[J]. Acta Mater., 2003, 51: 2089
[23] Nastac L.Numerical modeling of solidification morphologies and segregation patterns in cast dendritic alloys[J]. Acta Mater., 1999, 47: 4253
[24] Shao H, Li Y, Nan H, et al.Research on the interfacial heat transfer coeffecient between casting and ceramic shell in investment casting process of Ti6Al4V alloy[J]. Acta Metall. Sin., 2015, 51: 976(邵珩, 李岩, 南海等. 熔模铸造条件下Ti6Al4V合金铸件与陶瓷型壳间界面换热系数研究[J]. 金属学报, 2015, 51: 976)
[25] Liu Z, Welsch G.Literature survey on diffusivities of oxygen, aluminum, and vanadium in alpha titanium, beta titanium, and in rutile[J]. Metall. Trans., 1988, 19A: 1121
[26] Mills K C.Recommended Values of Thermophysical Properties for Selected Commercial Alloys [M]. Cambridge: Woodhead Publishing Ltd., 2002: 211
Outlines

/