Orginal Article

Deformation Characteristics and Mechanical Properties of Single Crystal Copper During Equal Channel Angular Pressing by Route A

  • Tingbiao GUO ,
  • Qi LI ,
  • Chen WANG ,
  • Feng ZHANG ,
  • Zhi JIA
Expand
  • 1 State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China
    2 Key Laboratory of Non-Ferrous Metal Alloys and Processing, Ministry of Education, Lanzhou University of Technology, Lanzhou 730050, China

Received date: 2016-12-30

  Online published: 2017-05-22

Supported by

Supported by National Natural Science Foundation of China (No.51261016)

Abstract

The single crystal copper has got more and more attention in the important areas of the national economy due to its good conductivity and thermal conductivity and elongation. Whereas the lower strength limits its application and strengthening methods of single crystal copper are of great concern. The traditional strengthening methods, such as solid solution strengthening, fine grain strengthening and deformation strengthening, can seriously damage the conductivity of single crystal copper. As an effective method for severe plastic deformation (SPD), equal channel angular pressing (ECAP) can effectively improve the material strength and keep its excellent performance by controlling the deformation and strain. Deformation texture of the single crystal copper (99.999%) during ECAP by A route was investigated by XRD, EBSD and TEM, the mechanical properties and conductivity were tested, and the mechanism of texture evolution and influence factors of mechanical and electrical properties during deformation process were analyzed. The results show that equiaxed deformation structure with small sizes appeared in single crystal copper after two passes extruded. After four passes of deformation, deformation band structure with same (110) orientation was formed. And the grain orientation of the highly refined grains gradually tended to the (111) surface, the {111}<110>, {111}<112> textures and the little {001}<100> recrystallization texture formed. The scattering of electrons by grain boundaries (GBs) can effectively get reduced and conductivity increases slightly, at the same time, the work hardening rate of the material is significantly improved when {hkl}<110> texture with stable orientation forms under medium and low strains. A large number of low-angle grain boundaries (LAGBs) are formed in the initial deformation stage of single crystal copper. With the increase of strain, the LAGBs gradually change to the high-angle grain boundaries (HAGBs). Dislocation accumulation and GB density increase that dislocation movement is obstructed during deformation process. The tensile strength increases from 168 MPa to 400 MPa, the elongation decreases from 63% to 27.3% after three passes deformation. With the extrusion process, the tensile strength increases slowly, whereas the elongation increases slightly. When the extrusion pass is less than eight times, hardness increases continuously, and recrystallization occurs after eighth passes extrusion that hardness tends to be unstable.

Cite this article

Tingbiao GUO , Qi LI , Chen WANG , Feng ZHANG , Zhi JIA . Deformation Characteristics and Mechanical Properties of Single Crystal Copper During Equal Channel Angular Pressing by Route A[J]. Acta Metall Sin, 2017 , 53(8) : 991 -1000 . DOI: 10.11900/0412.1961.2016.00582

References

[1] Fukuda Y, Oh-Ishi K, Furukawa M, et al.Influence of crystal orientation on the processing of copper single crystals by ECAP[J]. J. Mater. Sci., 2007, 42: 1501
[2] Sun L X, Tao N R, Lu K.A high strength and high electrical conductivity bulk CuCrZr alloy with nanotwins[J]. Scr. Mater., 2015, 99: 73
[3] Lu L, Chen X H, Huang X X, et al.Revealing the maximum strength in nanotwinned copper[J]. China Basic Sci., 2010, 12(1): 16(卢磊, 陈先华, 黄晓旭等. 纳米孪晶纯铜的极值强度及纳米孪晶提高金属材料综合强韧性[J]. 中国基础科学, 2010, 12(1): 16)
[4] Gao L, Chen R S, Han E H.Effects of rare-earth elements Gd and Y on the solid solution strengthening of Mg alloys[J]. J. Alloys Compd., 2009, 481: 379
[5] Lu K, Lu L, Suresh S.Strengthening materials by engineering coherent internal boundaries at the nanoscale[J]. Science, 2009, 324: 349
[6] Ning Y T, Zhang X H, Wu Y J.Strain strengthening of Cu-Ag alloy in situ filamentary composites[J]. Chin. J. Nonferrous Met., 2007, 17: 68(宁远涛, 张晓辉, 吴跃军. Cu-Ag合金原位纤维复合材料的应变强化效应[J]. 中国有色金属学报, 2007, 17: 68)
[7] Pry R H, Hennig R W.On the use of electrical resistivity as a measure of plastic deformation in copper[J]. Acta Metall., 1954, 2: 318
[8] Lu L, Lu K.Metallic materials with nano-scale twins[J]. Acta Metall. Sin., 2010, 46: 1422(卢磊, 卢柯. 纳米孪晶金属材料[J]. 金属学报, 2010, 46: 1422)
[9] Lu L, You Z S.Plastic deformation mechanisms in nanotwinned metals[J]. Acta Metall. Sin., 2014, 50: 129(卢磊, 尤泽升. 纳米孪晶金属塑性变形机制[J]. 金属学报, 2014, 50: 129)
[10] Shen Y F, Lu L, Lu Q H, et al.Tensile properties of copper with nano-scale twins[J]. Scr. Mater., 2005, 52: 989
[11] Lu L, Shen Y F, Chen X H, et al.Ultrahigh strength and high electrical conductivity in copper[J]. Science, 2004, 304: 422
[12] Shih H, Yu C Y, Kao P W, et al.Microstructure and flow stress of copper deformed to large plastic strains[J]. Scr. Mater., 2001, 45: 793
[13] Valiev R Z, Islamgaliev R K, Alexandrov I V.Bulk nanostructured materials from severe plastic deformation[J]. Prog. Mater. Sci., 2000, 45: 103
[14] Tao N R, Lu K.Structured metallic materials via plastic deformation[J]. Acta Metall. Sin., 2014, 50: 141(陶乃镕, 卢柯. 纳米结构金属材料的塑性变形制备技术[J]. 金属学报, 2014, 50: 141)
[15] Zhu C C, Ma A B, Jiang J H, et al.Effect of ECAP combined cold working on mechanical properties and electrical conductivity of Conform-produced Cu-Mg alloys[J]. J. Alloys Compd., 2014, 582: 135
[16] Purcek G, Yanar H, Demirtas M, et al.Optimization of strength, ductility and electrical conductivity of Cu-Cr-Zr alloy by combining multi-route ECAP and aging[J]. Mater. Sci. Eng., 2016, A649: 114
[17] Wu S D, An X H, Han W Z, et al.Microstructure evolution and mechanical properties of fcc metallic materials subjected to equal channel angular pressing[J]. Acta Metall. Sin., 2010, 46: 257(吴世丁, 安祥海, 韩卫忠等. 等通道转角挤压过程中fcc金属的微观结构演化与力学性能[J]. 金属学报, 2010, 46: 257)
[18] Fukuda Y, Oh-Ishi K, Furukawa M, et al.Influence of crystal orientation on ECAP of aluminum single crystals[J]. Mater. Sci. Eng., 2006, A420: 79
[19] Guo T B, Ding Y T, Yuan X F, et al.Microstructure and orientation evolution of unidirectional solidification pure copper during ECAP[J]. Rare Met. Mater. Eng., 2011, 40: 171
[20] Iwahashi Y, Horita Z, Nemoto M, et al.An investigation of microstructural evolution during equal-channel angular pressing[J]. Acta Metall., 1997, 45: 4733
[21] Hu J, Lin D L, Wang Y.EBSD analyses of the microstructural evolution and CSL characteristic grain boundary of coarse-grained NiAl alloy during plastic deformation[J]. Acta Metall. Sin., 2009, 45: 652(胡静, 林栋梁, 王燕. EBSD技术分析大晶粒NiAl合金高温塑性变形组织演变与CSL特征晶界分布[J]. 金属学报, 2009, 45: 652)
[22] He Y B, Pan Q L, Qin Y J, et al.Microstructure and mechanical properties of ultra-fine grain ZK60 magnesium alloy processed by equal channel angular pressing[J]. Chin. J. Nonferrous Met., 2010, 20: 2274(何运斌, 潘清林, 覃银江等. 等通道角挤压制备细晶ZK60镁合金的组织与力学性能[J]. 中国有色金属学报, 2010, 20: 2274)
[23] Wen Y N, Zhang J M.Surface energy calculation of the bcc metals by using the MAEAM[J]. Computat. Mater. Sci., 2008, 42: 281
[24] Guo T B, Ding Y T, Yuan X F, et al.Grain orientation evolution and texture fluctuation effect of pure copper during equal channel angular pressing[J]. Chin. J. Nonferrous Met., 2011, 21: 384(郭廷彪, 丁雨田, 袁训锋等. 等通道角挤压中纯铜的晶粒取向演变及织构起伏效应[J]. 中国有色金属学报, 2011, 21: 384)
[25] Xu J, Li J W, Shan D B, et al.Microstructural evolution and micro/meso-deformation behavior in pure copper processed by equal-channel angular pressing[J]. Mater. Sci. Eng., 2016, A664: 114
[26] Segal V M.Equal channel angular extrusion: From macromechanics to structure formation[J]. Mater. Sci. Eng., 1999, 271: 322
[27] Yun X B, Song B Y, Chen L.Ultra-fine grain copper prepared by continuous equal channel angular press[J]. Chin. J. Nonferrous Met., 2006, 16: 1563(运新兵, 宋宝韫, 陈莉. 连续等径角挤压制备超细晶铜[J]. 中国有色金属学报, 2006, 16: 1563)
[28] Yamakov V, Wolf D, Salazar M, et al.Length-scale effects in the nucleation of extended dislocations in nanocrystalline Al by molecular-dynamics simulation[J]. Acta Metall., 2001, 49: 2713
[29] An X H, Wu S D, Zhang Z F.Influence of stacking fault energy on the microstructures, tensile and fatigue properties of nanostructured Cu-Al alloys[J]. Acta Metall. Sin., 2014, 50: 191(安祥海, 吴世丁, 张哲峰. 层错能对纳米晶Cu-Al合金微观结构、拉伸及疲劳性能的影响[J]. 金属学报, 2014, 50: 191)
[30] Zheng W W, Sun Z Q.The rotation of the B2-ordered Fe3Al single crystal during room temperature tensile[J]. Acta Metall. Sin., 2000, 36: 1161(郑为为, 孙祖庆. B2结构Fe3Al单晶在室温拉伸过程中的取向转动[J]. 金属学报, 2000, 36: 1161)
Outlines

/