Structure and Visible-Light Induced Photocatalytic Activity of Zinc Cyanamide-Based Photocatalysts
Received date: 2017-04-11
Online published: 2017-05-19
Supported by
Supported by National Natural Science Foundation of China (No.21501023) and National Undergraduate Innovation and Entrepreneurship Training Program (No.201610145019)
Semiconductor-based photocatalytic technology, using abundant and renewable sunlight as an induced light source represents an emerging successful technology to solve the global energy and environmental challenges. Considerable efforts have been paid to develop novel photocatalysts with good response to sunlight and high quantum conversion efficiency. In this work, single ZnNCN microparticles have been prepared by the ligand exchange reaction between zinc salt, ammonia and cyanamide. And Ag2NCN/ZnNCN hetero structure has been also fabricated using the same ligand exchange process but mixing the silver salt with zinc salt together. Some means, such as XRD, SEM, infrared spectroscopy (FT-IR) and ultraviolet visible spectrometer (UV-Vis) were used to characterize the samples. The results showed that the single ZnNCN was flower-like particles with wide band gap (Eg=4.71 eV). Compared with single ZnNCN, the Ag2NCN/ZnNCN composite particles presented different morphology with rough surface, and physical interaction was existed between two kinds of metal cyanamide for Ag2NCN/ZnNCN composites. Because of the heterostructure, the light response spectrum for Ag2NCN/ZnNCN composite particles was extended to the visible light region, and the band gap was changed to 2.05 eV. The photocatalytic activity of Ag2NCN/ZnNCN composite particles in the degradation of Rhodamine B under Xenon irradiation was investigated, meanwhile, single ZnNCN and the mixture of Ag2NCN and ZnNCN was also applied in the photocatalysis under same conditions for comparison. The apparently enhanced photocatalytic activity of Ag2NCN/ZnNCN heterostructure was observed, and a first-order kinetic was discussed.
Fengming RONG , Yu WANG , Xia ZHANG . Structure and Visible-Light Induced Photocatalytic Activity of Zinc Cyanamide-Based Photocatalysts[J]. Acta Metall Sin, 2018 , 54(1) : 76 -82 . DOI: 10.11900/0412.1961.2017.00126
| [1] | Fujishima A, Honda K.Electrochemical photolysis of water at a semiconductor electrode[J]. Nature, 1972, 238: 37 |
| [2] | Carey J H, Lawrence J, Tosine H M.Photodechlorination of PCB's in the presence of titanium dioxide in aqueous suspensions[J]. Bull. Environ. Contam. Toxicol., 1976, 16: 697 |
| [3] | Zhang T T, Qi Y, Liu G, et al.Growth mechanism and photocatalytic activity of NaNbO3 with controllable morphology[J]. Acta Metall. Sin., 2017, 53: 376(张婷婷, 祁阳, 刘刚等. 形貌可控NaNbO3的生长机理和光催化性能[J]. 金属学报, 2017, 53: 376) |
| [4] | Feng X W, Chen H, Jiang F.In-situ ethylenediamine-assisted synthesis of a magnetic iron-basedmetal-organic framework MIL-53(Fe) for visible light photocatalysis[J]. J. Colloid Interface Sci., 2017, 494: 32 |
| [5] | Pu Y C, Chou H Y, Kuo W S, et al.Interfacial charge carrier dynamics of cuprous oxide-reduced graphene oxide (Cu2O-rGO) nanoheterostructures and their related visible-light-driven photocatalysis[J]. Appl. Catal., 2017, 204B: 21 |
| [6] | Martins L M D R S, Alegria E C B A, Hughes D L, et al. Syntheses and properties of hydride-cyanamide and derived hydrogen-cyanamide complexes of molybdenum (IV). Crystal structure of [MoH2-(NCNH2)2(Ph2PCH2CH2PPh2)2][BF4]2[J]. Dalton Trans., 2003, 19: 3743 |
| [7] | Liu X H,Mü1ller P, Kroll P, et al. Synthesis, structure determination, and quantum-chemical characterization of an alternate HgNCN polymorph[J]. Inorg. Chem., 2002, 41: 4259 |
| [8] | Cunha S M P R M, da Silvaab M F C G, Pombeiro A J L. Activation of cyanamide by a molybdenum(0) diphosphinic centre. Formation of cyanoimide and its reactivity with electrophiles[J]. J. Chem. Soc. Dalton Trans., 2002, 43: 1791 |
| [9] | Cunha S M P R M, da Silva M F C G, Pombeiro A J L. Mixed dinitrogen-organocyanamide complexes of molybdenum(0) and their protic conversion into hydrazide and amidoazavinylidene derivatives[J]. Inorg. Chem., 2003, 42: 2157 |
| [10] | Deb S K, Yoffe A D.Inorganic cyanamides. Physical and optical properties, and decomposition[J]. Trans. Faraday Soc., 1959, 55: 106 |
| [11] | Liu X H, Dronskowski R, Kremer R K, et al.Characterization of the magnetic and structural properties of copper carbodiimide, CuNCN, by neutron diffraction and first-principles evaluations of its spin exchange interactions[J]. J. Phys. Chem., 2008, 112C: 11013 |
| [12] | Liu X H, Stork L, Speldrich M, et al.FeNCN and Fe(NCNH)2: Synthesis, structure, and magnetic properties of a nitrogen-based pseudo-oxide and -hydroxide of divalent iron[J]. Chem. Eur. J. 2009, 15: 1558 |
| [13] | Liu X H, Krott M, Müller P, et al.Synthesis, crystal structure, and properties of MnNCN, the first carbodiimide of a magnetic transition metal[J]. Inorg. Chem., 2005, 44: 3001 |
| [14] | Krott M, Liu X H, Fokwa B P T, et al.. Synthesis, crystal-structure determination and magnetic properties of two new transition-metal carbodiimides: CoNCN and NiNCN[J]. Inorg. Chem., 2007, 46: 2204 |
| [15] | Cao R, Tatsumi K.Use of dipotassium cyanamide for the synthesis of cyanoimido (NCN2-) complexes of tungsten and cobalt[J]. Chem. Commun., 2002, 18: 2144 |
| [16] | Becker M, Nuss J, Jansen M.Synthese und charakterisierung von Natriumcyanamid[J]. Z. Anorg. Allg. Chem., 2000, 626: 2505 |
| [17] | Becker M, Jansen M.Synthesis of potassium cyanamide, and crystal structure determination by pareto optimisation of the cost functions 'lattice energy' and 'powder intensities'[J]. Solid State Sci., 2000, 2: 711 |
| [18] | Liu X H, Decker A D, Schmitz D, et al.Crystal structure refinement of lead cyanamide and the stiffness of the cyanamide anion[J]. Z. Anorg. Allg. Chem., 2000, 626: 103 |
| [19] | Becker M, Jansen M.Synthese und charakterisierung von quecksilbercyanamid[J]. Z. Anorg. Allg. Chem., 2000, 626: 1639 |
| [20] | Liao W P, Hu C H, Kremer R K, et al.Formation of complex three-and one-dimensional interpenetrating networks within carbodiimide chemistry:NCN2--coordinated rare-earth-metal tetrahedra and condensed alkali-metal iodide octahedra in two novel lithium europium carbodiimide iodidesLiEu2(NCN)I3 and LiEu4(NCN)3I3[J]. Inorg. Chem., 2004, 43: 5884 |
| [21] | Becker M, Nuss J, Jansen M.Crystal structure and spectroscopic data of silver cyanamide (in German) [J].Z.Naturforsch., 2000, 55B:383 |
| [22] | Zhao W, Liu Y F, Liu J J, et al.Controllable synthesis of silver cyanamide as a new semiconductor photocatalyst under visible-light irradiation[J]. J. Mater. Chem., 2013, 1A: 7942 |
| [23] | Meng H, Li X X, Zhang X, et al.Fabrication of nanocomposites composed of silver cyanamide and titania for improved photocatalytic hydrogen generation[J]. Dalton Trans., 2015, 44: 19948 |
| [24] | Li X, Zhang X, Zhu Z F, et al.Synthesis of TiO2/Ag2NCN composite catalysts and their photocatalytic activity under visible light irradiation[J]. Chem. J. Chin Univ., 2015, 36: 361(李霞, 张霞, 朱泽峰等. TiO2/Ag2NCN复合光催化剂的制备与可见光催化性能[J]. 高等学校化学学报, 2015, 36: 361) |
| [25] | Kaye K M, Grantham W, Hyett G.A facile route to thin films of zinc carbodiimide using aerosol-assisted CVD[J]. Chem. Vap. Deposition, 2015, 21: 281 |
| [26] | Pesika N S, Stebe K J, Searson P C.Determination of the particle size distribution of quantum nanocrystals from absorbance spectra[J]. Adv. Mater., 2003, 15: 1289 |
/
| 〈 |
|
〉 |