Orginal Article

Wettability Improvement and Brazing of Si3N4by Sputtered Al

  • Geliang LIU ,
  • Bingyang MA ,
  • Hailong SHANG ,
  • Fan CHEN ,
  • Rongbin LI ,
  • Geyang LI
Expand
  • 1 State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong University, Shanghai 200240, China
    2 Shanghai Dianji University, Shanghai 201306, China

Received date: 2017-01-20

  Online published: 2017-05-15

Supported by

Supported by National Natural Science Foundation of China (Nos.51401120 and 51671125) and Natural Science Foundation of Shanghai (No.16ZR1412800)

Abstract

In the present technology, the brazing of Si3N4 needs a reactive transition layers to resolve the non-wetting problem of usual metal fillers. Aluminum could wet Si3N4 without reaction but the brazing is very difficult due to wetting temperature above 1000 ℃. In this work, the wetting effect of sputtered Al films on Si3N4 and its physics essence were revealed. Based on this, the brazing of Si3N4 ceramic with Al or Al-Ni film fillers was realized near their melting temperature. The results showed that the seams of brazing joints with direct sputtered Al on Si3N4 film were well-stacked and less defects, and well metallurgically bonded to ceramic without reactive transition layers. The shear strength of pure Al/Si3N4 joint reached 106 MPa. The strength increased to 148 MPa with adding 1.0%Ni into film filler due hypoeutectic structure in the seam. With further increasing Ni content to 3.0%, the eutectic structure of the seam slightly decreased the strength of joint to 132 MPa. These joints above all fractured in joint seams. Moreover, the Al-1.0%Ni film filler first sputtered Ni layer was compared. Its brazing joint fractured at the interface between seam and ceramic and the shear strength decreased to only 81 MPa. This comparsion revealed the "wetting" effect of the bombardment of energetic sputtered Al particles. This effect still existed after filler melting and the direct brazing of Si3N4 ceramic without reactive transition layers was realized.

Cite this article

Geliang LIU , Bingyang MA , Hailong SHANG , Fan CHEN , Rongbin LI , Geyang LI . Wettability Improvement and Brazing of Si3N4by Sputtered Al[J]. Acta Metall Sin, 2017 , 53(12) : 1645 -1650 . DOI: 10.11900/0412.1961.2017.00026

References

[1] Cui W, Yan J C, Dai Y, et al.Building a nano-crystalline α-alumina layer at a liquid metal/sapphire interface by ultrasound[J]. Ultrason. Sonochem., 2015, 22: 108
[2] Ali M, Knowles K M, Mallinson P M, et al.Microstructural evolution and characterisation of interfacial phases in Al2O3/Ag-Cu-Ti/Al2O3 braze joints[J]. Acta Mater., 2015, 96: 143
[3] Yadav D P, Kaul R, Ganesh P, et al.Study on vacuum brazing of high purity alumina for application in proton synchrotron[J]. Mater. Des., 2014, 64: 415
[4] Laik A, Mishra P, Bhanumurthy K, et al.Microstructural evolution during reactive brazing of alumina to Inconel 600 using Ag-based alloy[J]. Acta Mater., 2013, 61: 126
[5] Xia H Y, Wu A P, Fan Y L, et al.Effects of ion implantation on the brazing properties of high purity alumina[J]. Surf. Coat. Technol., 2012, 206: 2098
[6] Ghosh S, Chakraborty R, Dandapat N, et al.Characterization of alumina-alumina/graphite/monel superalloy brazed joints[J]. Ceram. Int., 2012, 38: 663
[7] Ksiazek M, Sobczak N, Mikulowski B, et al.Wetting and bonding strength in Al/Al2O3 system[J]. Mater. Sci. Eng., 2002, A324: 162
[8] Prin G R, Baffie T, Jeymond M, et al.Contact angles and spreading kinetics of Al and Al-Cu alloys on sintered AlN[J]. Mater. Sci. Eng., 2001, A298: 34
[9] Sobczak N, Stobierski L, Radziwill W, et al.Wettability and interfacial reactions in Al/TiO2 [J]. Surf. Interface Anal., 2004, 36: 1067
[10] Ljungberg L, Warren R.Wetting of silicon nitride with selected metals and alloys [A]. Proceedings of the International Forum on Structural Ceramics Joining: Ceramic Engineering and Science Proceedings[C]. American: The American Ceramic Society, Inc., 2008, 10: 1655
[11] Naka M, Kubo M.Brazing of Si3N4 to metals with Al-Si filler metals (physics, process, instruments & measurement)[J]. Trans. JWRI, 1990, 19: 181
[12] Chen F, Shi K C, Sun S Y, et al.Direct brazing of Al/Al2O3 without wettability of molten metal[J]. J. Inorg. Mater., 2016, 31: 602(陈凡, 石恺成, 孙士阳等. 不基于熔态润湿的Al/Al2O3直接钎焊[J]. 无机材料学报, 2016, 31: 602)
[13] Zhao B W, Shang H L, Chen F, et al."Wetting" and brazing of AlN by sputtered Al[J]. Acta Phys. Sin., 2016, 65: 086801(赵博文, 尚海龙, 陈凡等. 溅射Al对AlN的“润湿”与钎焊[J]. 物理学报, 2016, 65: 086801)
[14] Mouradoff L, Tristant P, Desmaison J, et al.Interaction between liquid aluminium and non-oxide ceramics (AlN, Si3N4, SiC)[J]. Key Eng. Mater., 1995, 113: 177
[15] Eustathopoulos N, Nicholas M G, Drevet B.Wettability at High Temperatures[M]. New York: Pergamon, 1999: 294
[16] Li J G.Wetting of ceramic materials by liquid silicon, aluminium and metallic melts containing titanium and other reactive elements: A review[J]. Ceram. Int., 1994, 20: 391
[17] Nicholas M G, Mortimer D A, Jones L M, et al.Some observations on the wetting and bonding of nitride ceramics[J]. J. Mater. Sci., 1990, 25: 2679
[18] Naka M, Kubo M, Okamoto I.Joining of silicon nitride with Al-Cu alloys[J]. J. Mater. Sci., 1987, 22: 4417
[19] Naka M, Kubo M, Okamoto I.Wettability of silicon nitride by aluminium, copper and silver[J]. J. Mater. Sci. Lett., 1987, 6: 965
[20] Mouradoff L, Lachau-Durand A, Desmaison J, et al.Study of the interaction between liquid aluminum and silicon nitride[J]. J. Eur. Ceram. Soc., 1994, 13: 323
[21] Zhang Q, ?a??n T, van Duin A, et al. Adhesion and nonwetting-wetting transition in the Al/α-Al2O3 interface[J]. Phys. Rev., 2004, 69B: 045423
[22] Zheng W T.Thin Film Materials and Thin Film Technology [M]. Beijing: Chemical Industry Press, 2004: 72(郑伟涛. 薄膜材料与薄膜技术 [M]. 北京: 化学工业出版社, 2004: 72)
[23] Fujii H, Nakae H, Okada K.Interfacial reaction wetting in the boron nitride/molten aluminum system[J]. Acta Metall. Mater., 1993, 41: 2963
[24] Li G C, Ning X S, Chen K X, et al.Interaction of Si3N4 ceramics and liquid aluminum at interface without oxidation[J]. Rare Met. Mater. Eng., 2009, 38(S2): 186(李国才, 宁晓山, 陈克新等. 界面无氧化膜条件下氮化硅陶瓷和铝溶液的反应[J]. 稀有金属材料与工程, 2009, 38(S2): 186)
[25] Ning X S, Okamoto T, Miyamoto Y, et al.Reaction chemistry at joined interfaces between silicon nitride and aluminium[J]. J. Mater. Sci., 1991, 26: 4142
Outlines

/