Thermophysical Properties and Atomic Distribution of Undercooled Liquid Cu
Received date: 2017-02-20
Online published: 2017-05-11
Supported by
Supported by National Natural Science Foundation of China (Nos.51474175 and 51522102) and Science and Technology Program of Shaanxi Province (No.2015GY138)
Cu is commonly used in the field of electricity and electronics because of its high ductility, and electrical and thermal conductivity. The thermophysical properties and the atomic structure of liquid Cu, especially for undercooled state, are of practical significance in both application and fundamental researches. The major approaches to obtain thermophysical properties of undercooled metals are containerless techniques based on electrostatic levitation, electromagnetic levitation and ultrasonic levitation et al. However, the strong volatility of liquid Cu results in great difficulties to measure the thermophysical properties. Accordingly, computational prediction is becoming an expected method to obtain the thermophysical data of liquid Cu. The molecular dynamics (MD) simulation, in combination with a resonable potential model, has been extensively employed in studying the physical properties of several metals as a powerful approach. In this work, the atomic distribution and thermophysical properties including melting temperature, density, specific heat and self-diffusion coefficient of liquid Cu were studied by molecular dynamics simulation. Mishin's and Zhou's embedded-atom method potentials, and the modified embedded-atom method potential proposed by Baskes were used over the temperature range of 800~2400 K, reaching the maximum undercooling of 556 K. The simulated results are in good agreement with the reported experimental results. The crystal-liquid-crystal sandwich structure has been used to calculate the melting point. The melting point calculated by Baskes' potential model is 1341 K, just a difference of 1.11% from the experimental value. The density at the melting point calculated by Mishin's potential is 7.86 g/cm3, with a difference less than 2% compared with the reported data. It is found that the enthalpy of liquid Cu increases linearly with the increase of temperature. The specific heat is obtained to be 31.89 J/(molK) by Mishin's potential, which is constant in the corresponding temperature range. The self-diffusion coefficient is exponentially dependent on the temperature. The maximum error between the reported value and the present value of the self-diffusion coefficient calculated by Mishin's potential is only 4.93%. The pair distribution function was applied to investigate the atomic structure of liquid Cu, which suggests that the simulated system is still ordered in short range and disordered in long range for both normal liquid and undercooled state. It is found that the atomic ordered degree is weakened with the increase of temperature, and it is kept within 3~4 atom neighbor distance.
Jianglei ZHU , Qing WANG , Haipeng WANG . Thermophysical Properties and Atomic Distribution of Undercooled Liquid Cu[J]. Acta Metall Sin, 2017 , 53(8) : 1018 -1024 . DOI: 10.11900/0412.1961.2017.00053
| [1] | Iida T, Guthrie R I L, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2006: 97, 218(Iida T, Guthrie R I L著, 冼爱平, 王连文译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2006: 97, 218) |
| [2] | Yan E H, Sun L X, Xu F, et al.Prediction of the solidification path of Al-6.32Cu-25.13Mg alloy by a unified microsegregation model coupled with Thermo-Calc[J]. Acta Metall. Sin., 2016, 52: 632(闫二虎, 孙立贤, 徐芬等. 基于Thermo-Calc和微观偏析统一模型对Al-6.32Cu-25.13Mg合金凝固路径的预测[J]. 金属学报, 2016, 52: 632) |
| [3] | Kim T H, Kelton K F.Structural study of supercooled liquid transition metals[J]. J. Chem. Phys., 2007, 126: 054513 |
| [4] | Wang H P, Yang S J, Hu L, et al.Molecular dynamics prediction and experimental evidence for density of normal and metastable liquid zirconium[J]. Chem. Phys. Lett., 2016, 653: 112 |
| [5] | Yan J H, Jian Z Y, Zhu M, et al.Solidification characteristics and microstructure of high undercooled Al-70%Si alloy[J]. Acta Metall. Sin., 2016, 52: 931(严军辉, 坚增运, 朱满等. 深过冷Al-70%Si合金的凝固特性与微观组织[J]. 金属学报, 2016, 52: 931) |
| [6] | Lü P, Wang H P.Direct formation of peritectic phase but no primary phase appearance within Ni83.25Zr16.75peritectic alloy during free fall[J]. Sci. Rep., 2016, 6: 22641 |
| [7] | Demmel F, Hennet L, Brassamin S, et al.Nickel self-diffusion in a liquid and undercooled NiSi alloy[J]. Phys. Rev., 2016, 94B: 014206 |
| [8] | Hu L, Li L H, Yang S J, et al.Thermophysical properties and eutectic growth of electrostatically levitated and substantially undercooled liquid Zr91.2Si8.8 alloy[J]. Chem. Phys. Lett., 2015, 621: 91 |
| [9] | Perepezko J H, Imhoff S D.Crystallization control in highly undercooled liquids and glasses[J]. Int. J. Mater. Res., 2012, 103: 1083 |
| [10] | Johnson M L, Mauro N A, Vogt A J, et al.Structural evolution and thermophysical properties of ZrxNi100-x, metallic liquids and glasses[J]. J. Non-Cryst. Solids, 2014, 405: 211 |
| [11] | Ishikawa T, Okada J T, Paradis P F, et al.Thermophysical property measurements of liquid gadolinium by containerless methods[J]. Int. J. Thermophys., 2010, 31: 388 |
| [12] | Wunderlich R K, Fecht H J, Egry I, et al.Thermophysical properties of a Fe-Cr-Mo alloy in the solid and liquid phase[J]. Steel Res. Int., 2012, 83: 43 |
| [13] | Cho Y C, Kim B S, Yoo H, et al.Successful melting and density measurements of Cu and Ag single crystals with an electrostatic levitation (ESL) system[J]. CrystEngComm, 2014, 16: 7575 |
| [14] | Brillo J, Egry I.Density determination of liquid copper, nickel, and their alloys[J]. Int. J. Thermophys., 2003, 24: 1155 |
| [15] | Meyer A.Self-diffusion in liquid copper as seen by quasielastic neutron scattering[J]. Phys. Rev., 2010, 81B: 012102 |
| [16] | Yang H, Wang L, Yuan B, et al.Adhesion of an ultrasmall nanoparticle on a bilayer membrane is still size and shape dependent[J]. J. Mater. Sci. Technol., 2015, 31: 660 |
| [17] | Wu H N, Xu D S, Wang H, et al.Molecular dynamics simulation of tensile deformation and fracture of γ-TiAl with and without surface defects[J]. J. Mater. Sci. Technol., 2016, 32: 1033 |
| [18] | Chen F F, Zhang H F, Qin F X, et al.Molecular dynamics study of atomic transport properties in rapidly cooling liquid copper[J]. J. Chem. Phys., 2004, 120: 1826 |
| [19] | Wang H P, Wei B.Thermophysical properties of stable and metastable liquid copper and nickel by molecular dynamics simulation[J]. Appl. Phys., 2009, 95A: 661 |
| [20] | Han X J, Chen M, Guo Z Y.Thermophysical properties of undercooled liquid Au-Cu alloys from molecular dynamics simulations[J]. J. Phys.: Condens. Matter, 2004, 16: 705 |
| [21] | Lü Y J, Cheng H, Chen M.A molecular dynamics examination of the relationship between self-diffusion and viscosity in liquid metals[J]. J. Chem. Phys., 2012, 136: 214505 |
| [22] | Daw M S, Baskes M I.Embedded-atom method: derivation and application to impurities, surfaces, and other defects in metals[J]. Phys. Rev., 1984, 29B: 6443 |
| [23] | Stott M J, Zaremba E.Quasiatoms: An approach to atoms in nonuniform electronic systems[J]. Phys. Rev., 1980, 22B: 1564 |
| [24] | N?rskov J, Lang N D.Effective-medium theory of chemical binding: application to chemisorption[J]. Phys. Rev., 1980, 21B: 2131 |
| [25] | Baskes M I.Modified embedded-atom potentials for cubic materials and impurities[J]. Phys. Rev., 1992, 46B: 2727 |
| [26] | Baskes M I, Johnson R A.Modified embedded atom potentials for HCP metals[J]. Modell. Simul. Mater. Sci. Eng., 1994, 2: 147 |
| [27] | Baskes M I.Calculation of the behaviour of Si ad-dimers on Si(001)[J]. Modell. Simul. Mater. Sci. Eng., 1997, 5: 149 |
| [28] | Mishin Y, Mehl M J, Papaconstantopoulos D A, et al.Structural stability and lattice defects in copper: Ab initio, tight-binding, and embedded-atom calculations[J]. Phys. Rev., 2001, 63B: 224106 |
| [29] | Zhou X W, Johnson R A, Wadley H N G. Misfit-energy-increasing dislocations in vapor-deposited CoFe/NiFe multilayers[J]. Phys. Rev., 2004, 69B: 144113 |
| [30] | Plimpton S.Fast parallel algorithms for short-range molecular dynamics[J]. J. Comput. Phys., 1995, 117: 1 |
| [31] | Nasch P M, Steinemann S G.Density and thermal expansion of molten manganese, iron, nickel, copper, aluminum and tin by means of the gamma-ray attenuation technique[J]. Phys. Chem. Liq., 1995, 29: 43 |
| [32] | Assael M J, Kalyva A E, Antoniadis K D, et al.Reference data for the density and viscosity of liquid copper and liquid tin[J]. J. Phys. Chem. Ref. Data, 2010, 39: 033105 |
/
| 〈 |
|
〉 |