Crystallization Behavior of Laser Solid Forming of Annealed Zr55Cu30Al10Ni5 Powder
Received date: 2016-09-18
Online published: 2017-05-10
Supported by
Supported by National Natural Science Foundation of China (Nos.51323008, 51271213 and 51475380), National High Technology Research and Development Program of China (No.2013AA031103), National Basic Research Program of China (No.2011CB610402) and Fundamental Research Funds for the Central Universities (No.3102015BJ(II)ZS013)
Laser solid forming (LSF) provides an innovative way in building the bulk metallic glasses (BMGs) due to its inherently rapid heating and cooling process and point by point additive manufacturing process, which can eliminate the limitation of critical casting size of BMGs. The annealed powder has been demonstrated to be applicable to the preparation of BMGs with high content of amorphous phase using LSF. In this work, the plasma rotating electrode processed (PREPed) Zr55Cu30Al10Ni5 (Zr55) powders annealed at 1000 K are used for LSF of Zr55 BMGs. The influences of powder size and laser processing parameter on the crystallization characteristic of the deposit are investigated, and the crystallization behavior of the remelted zone (RZ) and heat affected zone (HAZ) is analyzed. It is found that the microstructures of the pre-annealed Zr55 powders are composed of the Al5Ni3Zr2, CuZr2 and Al2Zr3 phases. As the heat input increases from 7.0 J/mm to 15.7 J/mm, the every deposited layer presents a periodic repeating gradient microstructure (amorphous, NiZr2 nanocrystal, CuZr2+ZrCu dendrite-like eutectic, CuZr2+ZrCu spherulite-like eutectic) from the molten pool to the HAZ. The size of the eutectic phase in the HAZ decreases as the increase of distance from the featureless amorphous zone. On condition that the laser heat input is less than 7.0 J/mm, the deposits contain a high content of amorphous phase. As the increase of laser heat input, the crystallization degree of HAZ does not increase obviously for the deposit prepared by the powder with size range of 75~106 μm. However, the crystallization degree of HAZ increases significantly for the deposit prepared by the powder with size range of 106~150 μm. That is because the lower overheating temperature and shorter existing time of the molten pool enhances the heredity of Al5Ni3Zr2 clusters and other intermetallic clusters in remelted alloy melt during LSF of coarser powder, which decreases the thermal stability of the already-deposited layer and induces the severe crystallization. It is deduced that the raw state of annealed powders has a minimal impact on the crystallization behavior of the Zr55 deposited layers when the content of Al5Ni3Zr2 phase is same in different sizes of annealed powders. The thermal history of RZ and HAZ during deposition is the primary factor to affect the crystallization behavior in the Zr55 deposits fabricated by different powder sizes.
Yuanyuan ZHANG , Xin LIN , Lei WEI , Yongming REN . Crystallization Behavior of Laser Solid Forming of Annealed Zr55Cu30Al10Ni5 Powder[J]. Acta Metall Sin, 2017 , 53(7) : 824 -832 . DOI: 10.11900/0412.1961.2016.00417
| [1] | Schroers J.Processing of bulk metallic glass[J]. Adv. Mater., 2010, 22: 1566 |
| [2] | Inoue A, Takeuchi A.Recent development and application products of bulk glassy alloys[J]. Acta Mater., 2011, 59: 2243 |
| [3] | Hu Q, Lin X, Yang G L, et al.Crystallization behavior of Zr55Al10Ni5Cu30 amorphous alloys with different morphologies and thermal history conditions[J]. Acta Metall. Sin., 2012, 48: 1467 |
| [3] | (胡桥, 林鑫, 杨高林等. 不同形态和热历史条件下Zr55Al10Ni5Cu30非晶合金的晶化行为[J]. 金属学报, 2012, 48: 1467) |
| [4] | Inoue A.Stabilization of metallic supercooled liquid and bulk amorphous alloys[J]. Acta Mater., 2000, 48: 279 |
| [5] | Somekawa H, Inoue A, Higashi K.Superplastic and diffusion bonding behavior on Zr-Al-Ni-Cu metallic glass in supercooled liquid region[J]. Scr. Mater., 2004, 50: 1395 |
| [6] | Ye X Y, Shin Y C.Synthesis and characterization of Fe-based amorphous composite by laser direct deposition[J]. Surf. Coat. Technol., 2014, 239: 34 |
| [7] | Yang G L, Lin X, Liu F C, et al.Laser solid forming Zr-based bulk metallic glass[J]. Intermetallics, 2012, 22: 110 |
| [8] | Pauly S, L?ber L, Petters R, et al.Processing metallic glasses by selective laser melting[J]. Mater. Today, 2013, 16: 37 |
| [9] | Bai Y W, Bian X F, Lv X Q, et al.Heredity of medium-range order structure from melts to amorphous solids[J]. J. Appl. Phys., 2012, 112: 083524 |
| [10] | Balla V K, Bandyopadhyay A.Laser processing of Fe-based bulk amorphous alloy[J]. Surf. Coat. Technol., 2010, 205: 2661 |
| [11] | Zhang Y Y, Lin X, Wei L, et al.Influence of powder size on the crystallization behavior during laser solid forming Zr55Cu30Al10Ni5 bulk amorphous alloy[J]. Intermetallics, 2016, 76: 1 |
| [12] | Zhang Y Y, Lin X, Yang H O, et al.Influence of powdered state on crystallization during laser solid forming Zr55Cu30Al10Ni5 bulk metallic glasses[J]. Acta Phys. Sin., 2015, 64: 0166402 |
| [12] | (张媛媛, 林鑫, 杨海欧等. 粉末状态对激光立体成形Zr55Cu30Al10Ni5块体非晶合金晶化行为的影响[J]. 物理学报, 2015, 64: 0166402) |
| [13] | Zhang Y Y, Lin X, Wang L L, et al.Microstructural analysis of Zr55Cu30Al10Ni5 bulk metallic glasses by laser surface remelting and laser solid forming[J]. Intermetallics, 2015, 66: 22 |
| [14] | Al-Jaroudi S S, Ul-Hamid A, Mohammed A R I, et al. Use of X-ray powder diffraction for quantitative analysis of carbonate rock reservoir samples[J]. Powder Technol., 2007, 175: 115 |
| [15] | Chokethawai K, McCartney D G, Shipway P H. Microstructure evolution and thermal stability of an Fe-based amorphous alloy powder and thermally sprayed coatings[J]. J. Alloys Compd., 2009, 480: 351 |
| [16] | Basu A, Samant A N, Harimkar S P, et al.Laser surface coating of Fe-Cr-Mo-Y-B-C bulk metallic glass composition on AISI 4140 steel[J]. Surf. Coat. Technol., 2008, 202: 2623 |
| [17] | Zhu W H, Gu Y Q.Fundamentals of Statistical Physics [M]. Beijing: Tsinghua University Press, 1983: 208 |
| [17] | (朱文浩, 顾毓沁. 统计物理学基础 [M]. 北京: 清华大学出版社, 1983: 208) |
| [18] | Sih S S, Barlow J W.Measurement and prediction of the thermal conductivity of powders at high temperature [A]. Proceedings of the 6th Annual SFF Symposium[C]. Austin: The University of Texas, 1994: 397 |
| [19] | Dai K, Shaw L.Thermal and mechanical finite element modeling of laser forming from metal and ceramic powders[J]. Acta Mater., 2004, 52: 69 |
| [20] | Mao J, Zhang H F, Fu H M, et al.Influence of casting temperature on the thermal stability of Zr-based metallic glasses[J]. J. Alloys Compd., 2010, 496: 595 |
| [21] | Miracle D B.The efficient cluster packing model——An atomic structural model for metallic glasses[J]. Acta Mater., 2006, 54: 4317 |
| [22] | Ye S L, Li X Y, Bian X F, et al.Remelting treatment and heredity phenomenon in the formation of Fe78Si9B13 amorphous alloy[J]. J. Alloys Compd., 2013, 562: 143 |
| [23] | Lipton J, Kurz W, Trivedi R.Rapid dendrite growth in undercooled alloys[J]. Acta Metall., 1987, 35: 957 |
| [24] | Trivedi R, Magnin P, Kurz W.Theory of eutectic growth under rapid solidification conditions[J]. Acta Metall., 1987, 35: 971 |
| [25] | Shao G.Thermodynamic and kinetic aspects of intermetallic amorphous alloys[J]. Intermetallics, 2003, 11: 313 |
| [26] | Smityhells C J.Metals Reference Book[M]. 5th Ed., London: Butterworth & Ltd., 1976: 186 |
| [27] | Schroers J, Johnson W L.History dependent crystallization of Zr41Ti14Cu12Ni10Be23 melts[J]. J. Appl. Phys., 2000, 88: 44 |
| [28] | Katakam S, Kumar V, Santhanakrishnan S, et al.Laser assisted Fe-based bulk amorphous coating: Thermal effects and corrosion[J]. J. Alloys Compd., 2014, 604: 266 |
/
| 〈 |
|
〉 |