Orginal Article

Dual-Cluster Characteristic and Composition Optimization of Finemet Soft Magnetic Nanocrystalline Alloys

  • Yaoxiang GENG ,
  • Xin LIN ,
  • Jianbing QIANG ,
  • Yingmin WANG ,
  • Chuang DONG
Expand
  • 1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China
    2 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
    3 Key Lab of Materials Modification by Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China

Received date: 2016-12-05

  Online published: 2017-04-25

Supported by

Supported by National Natural Science Foundation of China (Nos.51671045 and 51601073), International Magnetic Confined Fusion Energy Development (Nos.2013GB107003 and 2015GB105003), Fundamental Research Funds for the Central Universities (No.DUT16ZD209) and Fund of the State Key Laboratory of Solidification Processing in NWPU (No.SKLSP201607)

Abstract

The development of nanocrystalline Fe-Si-B-Nb-Cu alloys, commercially known as Finemet, has established a new approach to obtain soft-magnetic materials with high magnetic flux density. The material consists of α-Fe(Si) nanocrystals embedded in an amorphous matrix, which is made by means of partial crystallization. The composition and local structure of the precursor amorphous alloys are crucial for the formation of the unique nanocrystalline structure. The present study is devoted to understanding the composition characteristics and developing new compositions of Finemet alloys. Using the “cluster-plus-glue-atom” model and noticing the crystallization characteristic of Finemet alloy, a “dual-cluster” amorphous structure model is proposed. In this model, the precursor amorphous structure of Finemet alloy is considered to contain a mixture of the [(Si, B)-B2(Fe, Nb)8]Fe cluster derived from the Fe-B-Si-Nb bulk glassy alloys, and the [Si-Fe14](Cu1/13Si12/13)3 cluster from Fe3Si phase. A series of new Finemet nanocrystalline alloy compositions are designed by mixing [(Si, B)-B2(Fe, Nb)8]Fe and [Si-Fe14](Cu1/13Si12/13)3 cluster formulas with a ratio of 1∶1. Thermal analysis results show that [(Si0.8B0.2)-B2Fe7.2Nb0.8]Fe+[Si-Fe14](Cu1/13Si12/13)3 (alloy composition: Fe74B7.33Si15.23Nb2.67Cu0.77) amorphous alloy exhibits a maximal temperature interval of about 192 K between the first and second crystallization peaks. Magnetic measurement results show that the Fe74B7.33Si15.23Nb2.67Cu0.77 nanocrystalline alloy exhibits optimal soft magnetic properties with a saturation magnetization Bs about 1.26 T, a coercive force Hc about 0.5 A/m and an effective permeability μe about 8.5×105 at 1 kHz after isothermal annealing at 813 K for 60 min. The soft magnetic properties of the new composition nanocrystalline alloys are better than that of the typical Finemet nanocrystalline alloy (Fe73.5Si13.5B9Cu1Nb3).

Cite this article

Yaoxiang GENG , Xin LIN , Jianbing QIANG , Yingmin WANG , Chuang DONG . Dual-Cluster Characteristic and Composition Optimization of Finemet Soft Magnetic Nanocrystalline Alloys[J]. Acta Metall Sin, 2017 , 53(7) : 833 -841 . DOI: 10.11900/0412.1961.2016.00546

References

[1] Wang X L.From research to industrialization for amorphous and nanocrystalline soft magnetic alloys (1)[J]. Met. Funct. Mater., 1996, 3(5): 161
[1] (王新林. 非晶和纳米晶软磁合金从研究到产业化(一)[J]. 金属功能材料, 1996, 3(5): 161)
[2] Yoshizawa Y, Oguma S, Yamauchi K.New Fe-based soft magnetic alloys composed of ultrafine grain structure[J]. J. Appl. Phys., 1988, 64: 6044
[3] Chen G J, Wang X J.Recent advance in Finemet type nanocrystaline soft magnetie alloys[J]. Met. Funct. Mater., 2003, 10(4): 28
[3] (陈国钧, 王旭军. Finemet型FeCuNbSiB系纳米软磁合金的新进展[J]. 金属功能材料, 2003, 10(4): 28)
[4] Yoshizawa Y, Yamauchi K.Fe-based soft magnetic alloys composed of ultrafine grain structure[J]. Mater. Trans. JIM, 1990, 31: 307
[5] Ayers J D, Harris V G, Sprague J A, et al.On the formation of nanocrystals in the soft magnetic alloy Fe73.5Nb3Cu1Si13.5B9[J]. Acta Mater., 1998, 46: 1861
[6] Hono K, Ping D H, Ohnuma M, et al.Cu clustering and Si partitioning in the early crystallization stage of an Fe73.5Si13.5B9Nb3Cu1 amorphous alloy[J]. Acta Mater., 1999, 47: 997
[7] Wang Z R, Qiang J B, Wang Y M, et al.Composition design procedures of Ti-based bulk metallic glasses using the cluster-plus-glue-atom model[J]. Acta Mater., 2016, 111: 366
[8] Han G, Qiang J B, Li F W, et al.The e/a values of ideal metallic glasses in relation to cluster formulae[J]. Acta Mater., 2011, 59: 5917
[9] Luo L J, Chen H, Wang Y M, et al.24 electron cluster formulas as the ‘molecular’ units of ideal metallic glasses[J]. Philos. Mag., 2014, 94: 2520
[10] Geng Y X, Wang Y M, Qiang J B, et al.Composition formulas of Fe-B binary amorphous alloys[J]. J. Non-Cryst. Solids, 2016, 432: 453
[11] Geng Y X, Zhang Z J, Wang Z R, et al.Magnetic properties and a structure model for high Fe content Fe-B-Si-Zr bulk glassy alloys[J]. J. Non-Cryst. Solids, 2016, 450: 1
[12] Geng Y X, Zhang Z J, Wang Y M, et al.Structure-property correlation of high Fe-content Fe-B-Si-Hf bulk glassy alloys[J]. Acta Metall. Sin., 2017, 53: 369
[12] (耿遥祥, 张志杰, 王英敏等. 高Fe含量Fe-B-Si-Hf块体非晶合金的结构-性能关联[J]. 金属学报, 2017, 53: 369)
[13] Pang C, Jiang B B, Shi Y, et al.Cluster-plus-glue-atom model and universal composition formulas [cluster] (glue atom)x for BCC solid solution alloys[J]. J. Alloys Compd., 2015, 652: 63
[14] Geng Y X, Wang Y M, Qiang J B, et al.Fe-B-Si-Zr soft magnetic bulk glassy alloys[J]. Intermetallics, 2015, 67: 138
[15] Geng Y X.Composition design and properties investigation for Fe-B-Si based amorphous and nanocrystalline alloys [D]. Dalian: Dalian University of Technology, 2016
[15] (耿遥祥. Fe-B-Si系非晶/纳米晶合金的成分设计及性能研究[D]. 大连: 大连理工大学, 2016)
[16] Wang Q, Zha Q F, Liu E X, et al., Composition design of high-strength martensitic precipitation hardening stainless steels based on a cluster model[J]. Acta Metall. Sin., 2012, 48: 1201
[16] (王清, 查钱锋, 刘恩雪等. 基于团簇模型的高强度马氏体沉淀硬化不锈钢成分设计[J]. 金属学报, 2012, 48: 1201)
[17] Geng Y X, Wang Y M, Qiang J B, et al.Composition design and optimization of Fe-B-Si-Nb bulk amorphous alloys[J]. Acta Metall. Sin., 2016, 52: 1459
[17] (耿遥祥, 王英敏, 羌建兵等. Fe-B-Si-Nb块体非晶合金的成分设计与优化[J]. 金属学报, 2016, 52: 1459)
[18] Ma Y P, Dong D D, Dong C, et al.Composition formulas of binary eutectics[J]. Sci. Rep., 2015, 5: 17880
[19] Mondal K, Murty B S.On the parameters to assess the glass forming ability of liquids[J]. J. Non-Cryst. Solids, 2005, 351: 1366
[20] Makino A, Men H, Kubota T, et al. New Fe-metalloids based nanocrystalline alloys with high Bs of 1.9 T and excellent magnetic softness [J]. J. Appl. Phys., 2009, 105: 07A308
[21] McHenry M E, Willard M A, Laughlin D E. Amorphous and nanocrystalline materials for applications as soft magnets[J]. Prog. Mater. Sci., 1999, 44: 291
[22] Patterson A L.The Scherrer formula for X-ray particle size determination[J]. Phys. Rev., 1939, 56: 978
[23] Herzer G.Grain structure and magnetism of nanocrystalline ferromagnets[J]. IEEE Trans. Magn., 1989, 25: 3327
[24] Herzer G.Grain size dependence of coercivity and permeability in nanocrystalline ferromagnets[J]. IEEE Trans. Magn., 1990, 26: 1397
Outlines

/