Orginal Article

Strengthening Mechanism of 600 MPa Grade Nb-Ti Microalloyed High Formability Crossbeam Steel

  • Yajun HUI ,
  • Hui PAN ,
  • Kun LIU ,
  • Wenyuan LI ,
  • Yang YU ,
  • Bin CHEN ,
  • Yang CUI
Expand
  • 1 Sheet Metal Research Institute, Shougang Research Institute of Technology, Beijing 100043, China
    2 Beijing Key Laboratory of Green Recyclable Process for Iron & Steel Production, Shougang Group, Beijing 100043, China

Received date: 2017-02-13

  Online published: 2017-04-21

Abstract

Automobile beam steel with high strength is the development trend of the automotive industry, which will help to conserve resources and protect the environment. The crossbeam as an important part of the frame, its strength also affects the overall strength of the frame, which will affect the safety performance of vehicles. At present, the crossbeam steel of heavy-duty vehicles is mainly Q235B and Q345C. About 3% of the crossbeams occur cracking problems when heavy-duty vehicles drive about 10000 km or about half a year or so. The strength increasing will cause the cracking in the forming process. Therefore, it is of great significance to develop a high strength crossbeam steel with high fatigue and high formability. In this work, the microstructure, properties and strengthening mechanism of 600 MPa grade Nb-Ti microalloyed high formability crossbeam steel were investigated by OM, SEM and TEM. The results show that the finish rolling temperature has a considerable influence on the microstructure and mechanical strength, with the decreasing of finish rolling temperature, the ferrite grain size and the size of precipitates decreases gradually; dislocation density, the number of precipitates and the ratio of Nb/Ti increase gradually; both the yield strength and tensile strength increase monotonously, while the elongation has an optimum temperature. The optimal mechanical properties were obtained when the finish rolling temperature is 840 ℃, and the yield strength, tensile strength, elongation and impact energy at -60 ℃ reached 541 MPa, 615 MPa, 31.0% and 117 J, respectively. The NrT and PTT curves of (Nb, Ti)C precipitated in the austenite showed that the nucleation rate of uniform nucleation and dislocation linear nucleation increases and the nucleation time is shortened with the decrease of temperature in the experimental temperature range, which is consistent with the observation result that the size of precipitates decreases with the reduction of the finish rolling temperature, while the number of precipitates increases. The grain refinement strengthening and dislocation strengthening are the main strengthening modes of the steel, the grain refinement strengthening accounts for 46%~48% of the yield strength, the dislocation strengthening accounts for 18%~25%, while the precipitation strengthening only contributes 2% of the yield strength.

Cite this article

Yajun HUI , Hui PAN , Kun LIU , Wenyuan LI , Yang YU , Bin CHEN , Yang CUI . Strengthening Mechanism of 600 MPa Grade Nb-Ti Microalloyed High Formability Crossbeam Steel[J]. Acta Metall Sin, 2017 , 53(8) : 937 -946 . DOI: 10.11900/0412.1961.2017.00038

References

[1] Zhang P C, Wu H B, Tang D, et al.Dissolving behaviors of carbonitrides in Nb-V-Ti and V-Ti microalloying steels[J]. Acta Metall. Sin., 2007, 43: 753(张鹏程, 武会宾, 唐荻等. Nb-V-Ti和V-Ti微合金钢中碳氮化物的回溶行为[J]. 金属学报, 2007, 43: 753)
[2] Speer J G, Michael J R, Hansen S S.Carbonitride precipitation in niobium/vanadium microalloyed steels[J]. Metall. Trans., 1987, 18A: 211
[3] Zheng L X, Li W Y, Zhai D Y.Analysis on fracture of the ingot beam of the heavy-duty dump truck[J]. Metall. Equipm., 2010, (5): 28(郑利霞, 李文颖, 翟大勇. 自卸车元宝梁断裂分析[J]. 冶金设备, 2010, (5): 28)
[4] Wu C L, Ma W R, Wang S, et al. Girder shaped like shoe-shaped gold ingot and vehicle frame assembly with same [P]. China Patents, CN204341193U, 2015(吴辰龙, 马维忍, 王珊等. 一种元宝梁以及具有该元宝梁的车架总成 [P]. 中国专利, CN204341193U, 2015)
[5] Li Y J.Finite element analysis of static-dynamic stress of heavy truck[J]. Autom. Eng., 1989, (1): 35(李玉娟. 超重型汽车车架静动态应力的有限元分析[J]. 汽车工程, 1989, (1): 35)
[6] Zhang Y, Zhang L, Xu Z J, et al.Simulation of heavy vehicle frame based on assembled structures and analysis on the frame fracture[J]. Comput. Simul., 2005, 22(12): 218(张勇, 张力, 徐宗俊等. 基于组合结构的重车车架建模仿真及断裂分析[J]. 计算机仿真, 2005, 22(12): 218)
[7] Yu C W.Finite elements simulation and optimization of heavy-duty truck's frame structure [D]. Changchun: Jilin University, 2005(余传文. 重型载货汽车车架结构的有限元仿真及优化 [D]. 长春: 吉林大学, 2005)
[8] Zou L, Yu H C, Jing J H.Finite element analysis of the frame of 6×4 heavy dump truck[J]. J. Hefei Univ. Technol.(Nat. Sci), 2007, 30(Suppl.): 43(邹琳, 于海昌, 景俊鸿. 6×4重型自卸车车架有限元分析[J]. 合肥工业大学学报(自然科学版), 2007, 30(增刊): 43)
[9] Xu B, Shang L P, Chen X J, et al. Reinforced heavy duty car wing girder [P]. China Patents, CN202911799U, 2013(徐斌, 尚利平, 陈学军等. 一种强化重型汽车元宝梁 [P]. 中国专利, CN202911799U, 2013)
[10] Song W X.Metallography [M]. Beijing: Metallurgical Industry Press, 1980: 1(宋维锡. 金属学[M]. 北京: 冶金工业出版社, 1980: 1)
[11] Wang Y M, Li M Y, Wei G, et al.Controlled Rolling of Steel and Controlled Cooling [M]. Beijing: Metallurgical Industry Press, 1995: 1(王有铭, 李曼云, 韦光等. 钢材的控制轧制和控制冷却 [M]. 北京: 冶金工业出版社, 1995: 1)
[12] Yong Q L, Li Y F, Sun Z B, et al.Second-phase on grain coarsening time and temperature[J]. Iron Steel, 1993, 28(9): 45(雍岐龙, 李永福, 孙珍宝等. 第二相与晶粒粗化时间及粗化温度[J]. 钢铁, 1993, 28(9): 45)
[13] Smith R M, Dunne D P.Structural aspects of alloy carbonitride precipitation in microalloyed steels[J]. Mater. Forum, 1988, 11: 166
[14] Hong S G, Kang K B, Park C G.Strain-induced precipitation of Nb in Nb and Nb-Ti microalloyed HSLA steels[J]. Scr. Mater., 2002, 46: 163
[15] Yi H L, Du L X, Wang G D, et al.New Ti-bearing high strength steel[J]. Chin. J. Mech. Eng., 2008, 44(8): 50(衣海龙, 杜林秀, 王国栋等, 一种新型含钛高强度钢[J], 机械工程学报, 2008, 44(8): 50)
[16] Dutta B, Valdes E, Sellars C M.Mechanism and kinetics of strain induced precipitation of Nb(C, N) in austenite[J]. Acta Metall. Mater., 1992, 40: 653
[17] Poths R M, Higginson R L, Palmiere E J.Complex precipitation behaviour in a microalloyed plate steel[J]. Scr. Mater., 2001, 44: 147
[18] Craven A J, He K, Garvie L A J, et al. Complex heterogeneous precipitation in titanium-niobium microalloyed Al-killed HSLA steels——I. (Ti, Nb)(C, N) particles[J]. Acta Mater., 2000, 48: 3857
[19] Thillou V.Basic metal processing research institute report [R]. Pittsburgh, PA, USA: University of Pittsburgh, 1997
[20] Yong Q L.The Second Phase in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 175(雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 175)
[21] Yong Q L, Ma M T, Wu B R.Microalloyed steel——Physical and Mechanical Metallurgy [M]. Beijing: China Machine Press, 1989: 57(雍岐龙, 马鸣图, 吴宝榕. 微合金钢——物理和力学冶金 [M]. 北京: 机械工业出版社, 1989: 57)
[22] Wang R Z, Zhang H T.Strengthening mechanism of Nb and Ti complex microalloyed strip steel produced by thin slab casting and direct rolling process[J]. Acta Metall. Sin., 2007, 43: 1082(王瑞珍, 章洪涛. 薄板坯连铸连轧工艺生产的Nb、Ti复合微合金化热轧带钢的强化机制[J]. 金属学报, 2007, 43: 1082)
[23] Pickering F B.Physical Metallurgy and the Design of Steels [M]. London: Applied Science Publishing Ltd., 1978: 63
[24] Ashby M F.Strengthening Methods in Crystals[M]. London: Applied Science Publishers Ltd., 1971: 137
[25] Gladman T, Dulieu D, Mclvor I D.Microalloy' 75[M]. New York: Union Carbide Corporation, 1977: 32
Outlines

/