Optimization and Controlling on the Microstructure, Texture and Properties of an Advanced Al-Mg-Si-Cu-Zn Alloy Sheet
Received date: 2016-10-27
Online published: 2017-04-20
Supported by
Supported by National Key Research and Development Program of China (No.2016YFB0300801), National Natural Science Foundation of China (Nos.51301016 and 51571023), National High Technical Research and Development Program of China (No.2013AA032403) and Beijing Natural Science Foundation (No.2172038)
To reduce the weight of car body, Al-Mg-Si-Cu series alloys have been widely used to produce outer body panels of automobiles due to their favorable high-strength-to-weight ratio, corrosion resistance and good formability. Moreover, the strength of Al-Mg-Si-Cu series alloys can be enhanced by artificial ageing treatments. However, their formability and final strengths still need to be further improved compared to steels, which are the major obstacles to wide-scale application of aluminum in the automotive fields. In this work, both the effect of different thermomechanical processes on formability, microstructure and texture of Al-Mg-Si-Cu-Zn alloy, and the influence of ageing treatment on its precipitation behavior were studied through mechanical property tests, OM, SEM, TEM and EBSD measurements. The results reveal that both the strengths and strain-hardening component n value of the T4P treated alloys are not affected by the two thermomechanical processes, but the
Yi CHEN , Mingxing GUO , Long YI , Bo YUAN , Gaojie LI , Linzhong ZHUANG , Jishan ZHANG . Optimization and Controlling on the Microstructure, Texture and Properties of an Advanced Al-Mg-Si-Cu-Zn Alloy Sheet[J]. Acta Metall Sin, 2017 , 53(8) : 907 -917 . DOI: 10.11900/0412.1961.2016.00480
| [1] | Engler O, Hirsch J. Recrystallization textures and plastic anisotropy in Al-Mg-Si sheet alloys [J]. Mater. Sci. Forum, 1996, 217-222: 479 |
| [2] | Bennett T A, Petrov R H, Kestens L A I, et al. The effect of particle-stimulated nucleation on texture banding in an aluminium alloy[J]. Scr. Mater., 2010, 63: 461 |
| [3] | Troeger L P, Starke Jr E A. Particle-stimulated nucleation of recrystallization for grain-size control and superplasticity in an Al-Mg-Si-Cu alloy[J]. Mater. Sci. Eng., 2000, 293A: 19 |
| [4] | Guo M X, Sha G, Cao L Y, et al.Enhanced bake-hardening response of an Al-Mg-Si-Cu alloy with Zn addition[J]. Mater. Chem. Phys., 2015, 162: 15 |
| [5] | Peng X Y, Guo M X, Wang X F, et al.Influence of particles with different sizes on microstructure, texture and mechanical properties of Al-Mg-Si-Cu series alloys[J]. Acta Metall. Sin., 2015, 51: 169(彭祥阳, 郭明星, 汪小锋等. 不同尺寸粒子对Al-Mg-Si-Cu系合金组织、织构和力学性能的影响[J]. 金属学报, 2015, 51: 169) |
| [6] | Esmaeili S, Lloyd D J, Poole W J.A yield strength model for the Al-Mg-Si-Cu alloy AA6111[J]. Acta Mater., 2003, 51: 2243 |
| [7] | Hirth S M, Marshall G J, Court S A, et al. Effects of Si on the aging behaviour and formability of aluminium alloys based on AA6016 [J]. Mater. Sci. Eng., 2001, A319-321: 452 |
| [8] | Esmaeili S, Lloyd D J.Effect of composition on clustering reactions in AlMgSi(Cu) alloys[J]. Scr. Mater., 2004, 50: 155 |
| [9] | Gupta A K, Lloyd D J.Study of precipitation kinetics in a super purity Al-0.8 Pct Mg-0.9 Pct Si alloy using differential scanning calorimetry[J]. Metall. Mater. Trans., 1999, 30A: 879 |
| [10] | Cao L F, Rometsch P A, Couper M J.Effect of pre-ageing and natural ageing on the paint bake response of alloy AA6181A[J]. Mater. Sci. Eng., 2013, A571: 77 |
| [11] | Wolverton C.Solute-vacancy binding in aluminum[J]. Acta Mater., 2007, 55: 5867 |
| [12] | Saito T, Ehlers F J H, Lefebvre W, et al. HAADF-STEM and DFT investigations of the Zn-containing β″ phase in Al-Mg-Si alloys[J]. Acta Mater., 2014, 78: 245 |
| [13] | Ding X P, Cui H, Zhang J X, et al.The effect of Zn on the age hardening response in an Al-Mg-Si alloy[J]. Mater. Des., 2015, 65: 1229 |
| [14] | Yan L Z, Zhang Y A, Li X W, et al.Effect of Zn addition on microstructure and mechanical properties of an Al-Mg-Si alloy[J]. Prog. Nat. Sci. Mater. Int., 2014, 24: 97 |
| [15] | Cai Y H, Wang C, Zhang J S.Microstructural characteristics and aging response of Zn-containing Al-Mg-Si-Cu alloy[J]. Int. J. Miner. Metall. Mater., 2013, 20: 659 |
| [16] | Saito T, Wenner S, Osmundsen E, et al.The effect of Zn on precipitation in Al-Mg-Si alloys[J]. Philos. Mag., 2014, 94: 2410 |
| [17] | Fukui S, Kudo H.The earing in deep-drawing and a directionality in tension-test of sheet metal[J]. Rep. Inst. Sci. Technol. Univ. Tokyo, 1950, 4: 33 |
| [18] | Lankford W T, Snyder S C, Bauscher J A.New criteria for predicting the press performance of deep drawing sheets[J]. Trans. ASM, 1950, 42: 1197 |
| [19] | Inoue H, Takasugi T.Texture control for improving deep drawability in rolled and annealed aluminum alloy sheets[J]. Mater. Trans., 2007, 48: 2014 |
| [20] | Wang X F, Guo M X, Chapuis A, et al.The dependence of final microstructure, texture evolution and mechanical properties of Al-Mg-Si-Cu alloy sheets on the intermediate annealing[J]. Mater. Sci. Eng., 2015, A633: 46 |
| [21] | Liu W C, Man C S, Morris J G.Lattice rotation of the cube orientation to the β fiber during cold rolling of AA 5052 aluminum alloy[J]. Scr. Mater., 2001, 45: 807 |
| [22] | Lücke K, Engler O.Effects of particles on development of microstructure and texture during rolling and recrystallisation in fcc alloys[J]. Mater. Sci. Technol., 1990, 6: 1113 |
| [23] | Bennett T A, Petrov R H, Kestens L A I. Effect of particles on texture banding in an aluminium alloy[J]. Scr. Mater., 2010, 62: 78 |
| [24] | Engler O, Lücke K.Mechanisms of recrystallization texture formation in aluminium alloys[J] Scr. Metall. Mater., 1992, 27: 1527 |
| [25] | Kashihara K, Inagaki H.Effect of precipitation on development of recrystallization texture in a 6061 aluminum alloy[J]. Mater. Trans., 2009, 50: 528 |
| [26] | Engler O, Yang P, Kong X W.On the formation of recrystallization textures in binary Al-1.3%Mn investigated by means of local texture analysis[J]. Acta Mater., 1996, 44: 3349 |
| [27] | Ding L P, Jia Z H, Zhang Z Q, et al.The natural aging and precipitation hardening behaviour of Al-Mg-Si-Cu alloys with different Mg/Si ratios and Cu additions[J]. Mater. Sci. Eng., 2015, A627: 119 |
| [28] | Li Y, Guo M X, Jiang N, et al.Precipitation behaviors and preparation of an advanced Al-0.93Mg-0.78Si-0.20Cu-3.00Zn alloy for automotive application[J]. Acta Metall. Sin., 2016, 52: 191(李勇, 郭明星, 姜宁等. 汽车用新型Al-0.93Mg-0.78Si-0.20Cu-3.00Zn合金的制备及其时效析出行为研究[J]. 金属学报, 2016, 52: 191) |
| [29] | Wolverton C.Crystal structure and stability of complex precipitate phases in Al-Cu-Mg-(Si) and Al-Zn-Mg alloys[J]. Acta Mater., 2001, 49: 3129 |
/
| 〈 |
|
〉 |