Evolution of Interfacial Intermetallic Compounds in Ni/Sn-xCu/Ni Micro Solder Joints Under Thermomigration During Soldering
Received date: 2016-12-22
Online published: 2017-04-18
Supported by
Supported by National Natural Science Foundation of China (No.51675080) and Key Laboratory of Advanced Display and System Applications, Ministry of Education (Shanghai University) (No.P201601)
The effect of Cu content on the evolution of intermetallic compounds (IMCs) in Ni/Sn-xCu/Ni (x= 0.3, 0.7, 1.5, mass fraction, %) micro solder joints during soldering at 240 ℃ under a temperature gradient of 1045 ℃/cm was investigated. Asymmetrical growth and transformation of interfacial IMCs and asymmetrical dissolution of Ni substrate were clearly observed. In Ni/Sn-0.3Cu/Ni micro solder joints, though the interfacial IMC remained as the initial (Ni, Cu)3Sn4, asymmetrical IMC growth between cold and hot ends occurred, i.e., the (Ni, Cu)3Sn4 IMC at the cold end was obviously thicker than that at the hot end. In Ni/Sn-0.7Cu/Ni and Ni/Sn-1.5Cu/Ni micro solder joints, the interfacial IMC gradually transformed from the initial (Cu, Ni)6Sn5 into (Ni,Cu)3Sn4. Meanwhile, the transformation at the cold end lagged behind the hot end, namely asymmetrical transformation phenomenon occurred. Moreover, the transformations at the cold and hot ends in the Ni/Sn-1.5Cu/Ni micro solder joints both lagged behind those in the Ni/Sn-0.7Cu/Ni micro solder joints. Based on the analysis of the Cu and Ni atomic fluxes for the IMC growth at both cold and hot ends, the thermomigration (TM) direction was confirmed to be from the hot end towards the cold end. The Cu concentration in the micro solder joints had a significant effect on the main TM element, and thus affected the growth and transformation behavior of the interfacial IMCs at the two ends. In addition, TM promoted the diffusion of Ni atoms into solder at the hot end, which accelerated the dissolution of the hot end Ni substrate. Most of the dissolved Ni atoms migrated to the cold end and participated in interfacial reaction locally. On the contrary, TM inhibited the diffusion of Ni atoms at the hot end, resulting in no obvious dissolution of the cold end Ni substrate.
Ning ZHAO , Jianfeng DENG , Yi ZHONG , Luqiao YIN . Evolution of Interfacial Intermetallic Compounds in Ni/Sn-xCu/Ni Micro Solder Joints Under Thermomigration During Soldering[J]. Acta Metall Sin, 2017 , 53(7) : 861 -868 . DOI: 10.11900/0412.1961.2016.00569
| [1] | Chen C, Hsiao H Y, Chang Y W, et al.Thermomigration in solder joints[J]. Mater. Sci. Eng., 2012, R73: 85 |
| [2] | Ouyang F Y, Jhu W C.Comparison of thermomigration behaviors between Pb-free flip chip solder joints and microbumps in three dimensional integrated circuits: Bump height effect[J]. J. Appl. Phys., 2013, 113: 043711 |
| [3] | Guo M Y, Lin C K, Chen C, et al.Asymmetrical growth of Cu6Sn5 intermetallic compounds due to rapid thermomigration of Cu in molten SnAg solder joints[J]. Intermetallics, 2012, 29: 155 |
| [4] | Huang A T, Gusak A M, Tu K N, et al.Thermomigration in SnPb composite flip chip solder joints[J]. Appl. Phys. Lett., 2006, 88: 141911 |
| [5] | Ouyang F Y, Jhu W C, Chang T C.Thermal-gradient induced abnormal Ni3Sn4 interfacial growth at cold side in Sn2.5Ag alloys for three-dimensional integrated circuits[J]. J. Alloys Compd., 2013, 580: 114 |
| [6] | Wang B, Wu F S, Wu Y P, et al.Microstructural evolution of the intermetallic compounds in the high density solder interconnects with reduced stand-off heights[J]. Solder. Surf. Mt. Technol., 2011, 23: 229 |
| [7] | Li X P, Zhou M B, Xia J M, et al.Effect of the cross-interaction on the formation and evolution of intermetallic compounds in Cu(Ni)/Sn-Ag-Cu/Cu(Ni)BGA structure solder joints[J]. Acta Metall. Sin., 2011, 47: 611 |
| [7] | (李勋平, 周敏波, 夏建民等. 界面耦合作用对Cu(Ni)/Sn-Ag-Cu/Cu(Ni)BGA焊点界面IMC形成与演化的影响[J]. 金属学报, 2011, 47: 611) |
| [8] | Zhao N, Zhong Y, Huang M L, et al.Growth kinetics of Cu6Sn5 intermetallic compound at liquid-solid interfaces in Cu/Sn/Cu interconnects under temperature gradient[J]. Sci. Rep., 2015, 5: 13491 |
| [9] | Gu X, Yung K C, Chan Y C, et al.Thermomigration and electromigration in Sn8Zn3Bi solder joints[J]. J. Mater. Sci. Mater. Electron., 2011, 22: 217 |
| [10] | Chen W Y, Chiu T C, Lin K L, et al.Electrorecrystallization of intermetallic compound in the Sn0.7Cu solder joint[J]. Intermetallics, 2012, 26: 40 |
| [11] | Zhao N, Deng J F, Zhong Y, et al.Abnormal intermetallic compound evolution in Ni/Sn/Ni and Ni/Sn-9Zn/Ni micro solder joints under thermomigration[J]. J. Electron. Mater., 2017, 46: 1931 |
| [12] | Zhao N, Pan X M, Ma H T, et al.Study of the liquid structure of Sn-Cu solders[J]. Acta Metall. Sin., 2008, 44: 467 |
| [12] | (赵宁, 潘学民, 马海涛等. Sn-Cu钎料液态结构的研究[J]. 金属学报, 2008, 44: 467) |
| [13] | Chen W T, Ho C E, Kao C R.Effect of Cu concentration on the interfacial reactions between Ni and Sn-Cu solders[J]. J. Mater. Res., 2002, 17: 263 |
| [14] | Chiu M Y, Wang S S, Chuang T H.Intermetallic compounds formed during interfacial reactions between liquid Sn-8Zn-3Bi solders and Ni substrates[J]. J. Electron. Mater., 2002, 31: 494 |
| [15] | Ho C E, Tsai R Y, Lin Y L, et al.Effect of Cu concentration on the reactions between Sn-Ag-Cu solders and Ni[J]. J. Electron. Mater., 2002, 31: 584 |
| [16] | Chen W T, Ho C E, Kao C R.Effect of Cu concentration on the interfacial reactions between Ni and Sn-Cu solders[J]. J. Mater. Res., 2002, 17: 263 |
| [17] | Chen S W, Wang C H.Interfacial reactions of Sn-Cu/Ni couples at 250 ℃[J]. J. Mater. Res., 2006, 21: 2270 |
| [18] | Peralta-Martinez M V, Wakeham W A. Thermal conductivity of liquid tin and indium[J]. Int. J. Thermophys., 2001, 22: 395 |
| [19] | Yu D Q, Wu C M L, He D P, et al. Effects of Cu contents in Sn-Cu solder on the composition and morphology of intermetallic compounds at a solder/Ni interface[J]. J. Mater. Res., 2005, 20: 2205 |
| [20] | Zhao N, Zhong Y, Huang M L, et al.Dissolution and precipitation kinetics of Cu6Sn5 intermetallics in Cu/Sn/Cu micro interconnects under temperature gradient[J]. Intermetallics, 2016, 79: 28 |
| [21] | Qu L, Zhao N, Ma H T, et al.In situ study on the effect of thermomigration on intermetallic compounds growth in liquid-solid interfacial reaction[J]. J. Appl. Phys., 2014, 115: 204907 |
| [22] | Yang Y S, Yang C J, Ouyang F Y.Interfacial reaction of Ni3Sn4 intermetallic compound in Ni/SnAg solder/Ni system under thermomigration[J]. J. Alloys Compd., 2016, 674: 331 |
| [23] | Zhao N, Zhong Y, Huang M L, et al.In situ study on interfacial reactions of Cu/Sn-9Zn/Cu solder joints under temperature gradient[J] J. Alloys Compd., 2016, 682: 1 |
| [24] | Laurila L, Vuorinen V, Kivilahti J K.Analyses of interfacial reactions at different levels of interconnection[J]. Mater. Sci. Semicond. Proc., 2004, 7: 307 |
| [25] | Wang C H, Lai W H, Chen S W.Dissolution and interfacial reactions of (Cu,Ni)6Sn5 intermetallic compound in molten Sn-Cu-Ni solders[J]. J. Electron. Mater., 2014, 43: 195 |
/
| 〈 |
|
〉 |