Experimental and Finite Element Simulation of Milling Process for γ-TiAl Intermetallics
Received date: 2016-06-23
Online published: 2017-04-07
γ-TiAl intermetallics are attractive candidates for applications in aircraft turbine engines due to their low density and good mechanical properties at high temperature. However, the low room temperature ductility makes the machinability of these materials poorer compared to the conventional alloys. In this work, a meso-model of γ-TiAl intermetallic was developed using ABAQUS finite element software. The surface morphology and edge fracture mechanism of different material models were analyzed, and the effects of cutting parameters on the surface roughness and size of edge fracture were investigated. The results indicate that the cracks and pits occur between the lamellar and lamellar with different material properties. At the same time, due to the low ductility of γ-TiAl intermetallic, the negative shear angle begins to form at the exit of workpiece, then the edge fracture is formed. In addition, for both surface roughness and size of edge fracture, the experimental data are slightly higher than the simulated data obtained by the hexagonal lamellar model, and smaller than those obtained by the rectangular lamellar model. With the increasing of cutting depth, the surface roughness and the size of edge fracture increase gradually, on the contrary, the cutting speed has a small effect on them. Therefore, in order to obtain a fine surface quality during machining of γ-TiAl intermetallic, the cutting speed can be adopted as higher as possible, but not the cutting depth.
Key words: γ-TiAl intermetallics; milling process; meso-model; finite element
Li ZHOU , Chao CUI , Qing JIA , Yingshi MA . Experimental and Finite Element Simulation of Milling Process for γ-TiAl Intermetallics[J]. Acta Metall Sin, 2017 , 53(4) : 505 -512 . DOI: 10.11900/0412.1961.2016.00256
| [1] | Klocke F, Lung D, Arft M, et al.On high-speed turning of a third-generation gamma titanium aluminide[J]. Int. J. Adv. Manuf. Technol., 2013, 65: 155 |
| [2] | Boyer R R.An overview on the use of titanium in the aerospace industry[J]. Mater. Sci. Eng., 1996, A213: 103 |
| [3] | Liu R C, Wang Z, Liu D, et al.Microstructure and tensile properties of Ti-45.5Al-2Cr-2Nb-0.15B alloy processed by hot extrusion[J]. Acta Metall. Sin., 2013, 49: 641 |
| [3] | (刘仁慈, 王震, 刘冬等. Ti-45.5Al-2Cr-2Nb-0.15B合金热挤压组织与拉伸性能研究[J]. 金属学报, 2013, 49: 641) |
| [4] | Aspinwall D K, Dewes R C, Mantle A L.The machining of γ-TiAl intermetallic alloys[J]. CIRP Ann.-Manuf. Technol., 2005, 54: 99 |
| [5] | Peng Y B, Chen F, Wang M Z, et al.Relationship between mechanical properties and lamellar orientation of PST crystals in Ti-45Al-8Nb alloy[J]. Acta Metall. Sin., 2013, 49: 1457 |
| [5] | (彭英博, 陈锋, 王敏智等. Ti-45Al-8Nb合金PST晶体片层取向与力学性能的关系[J]. 金属学报, 2013, 49: 1457) |
| [6] | Kad B K, Dao M, Asaro R J. Numerical simulations of stress-strain behavior in two-phase α2+γ lamellar TiAl alloys [J]. Mater. Sci. Eng., 1995, A192-193: 97 |
| [7] | Su J L, Lin G F, Zheng S H.Effects of grain size and lamellar thickness on yield strength of fully lamellar γ-TiAl based alloys[J]. J. Aeronaut. Mater., 2009, 29(4): 1 |
| [7] | (苏继龙, 林高飞, 郑书河. 晶粒尺寸和片层厚度对全片层γ-TiAl基合金屈服强度的影响[J]. 航空材料学报, 2009, 29(4): 1) |
| [8] | Su J L, Hu G K.Micromechanical study on yield stress and the effects of twinning for γ-TiAl-based PST crystals[J]. Acta Metall. Sin., 2005, 41: 1243 |
| [8] | (苏继龙, 胡更开. γ-TiAl基PST晶体的屈服应力及孪晶影响的细观力学研究[J]. 金属学报, 2005, 41: 1243) |
| [9] | Inui H, Oh M H, Nakamura A, et al.Room-temperature tensile deformation of polysynthetically twinned (PST) crystals of TiAl[J]. Acta Metall. Mater., 1992, 40: 3095 |
| [10] | Lin J G, Zhou Y J, Zhang Y G, et al.Microstructure and high-temperature compression behavior of Ti-48Al PST crystals[J]. J. Aeronaut. Mater., 1998, 18(1): 1 |
| [10] | (林建国, 周亚建, 张永刚等. Ti-48Al合金PST晶体显微组织及高温压缩性能[J]. 航空材料学报, 1998, 18(1): 1) |
| [11] | Zheng R T, Zhang Y G, Chen C Q, et al.Influence of grain boundary on the fracture toughness of full lamellar γ-TiAl alloys[J]. Rare Met. Mater. Eng., 2003, 32: 1003 |
| [11] | (郑瑞廷, 张永刚, 陈昌麒等. 晶界对全片层组织γ-TiAl合金断裂韧性的影响[J]. 稀有金属材料与工程, 2003, 32: 1003) |
| [12] | Fu L F, Lin J G, Cao G X, et al.Relationship between yield strength and microstructure of a fully lamellar TiAl-based alloy[J]. Rare Met. Mater. Eng., 2001, 30: 178 |
| [12] | (付连峰, 林建国, 曹国鑫等. 全片层TiAl基合金的屈服强度与显微组织关系[J]. 稀有金属材料与工程, 2001, 30: 178) |
| [13] | Priarone P C, Rizzuti S, Rotella G, et al.Tool wear and surface quality in milling of a gamma-TiAl intermetallic[J]. Int. J. Adv. Manuf. Technol., 2012, 61: 25 |
| [14] | Pérez R G V. Wear mechanisms of WC inserts in face milling of gamma titanium aluminides[J]. Wear, 2005, 259: 1160 |
| [15] | Priarone P C, Rizzuti S, Settineri L, et al.Effects of cutting angle, edge preparation, and nano-structured coating on milling performance of a gamma titanium aluminide[J]. J. Mater. Process. Technol., 2012, 212: 2619 |
| [16] | Kolahdouz S, Hadi M, Arezoo B, et al.Investigation of surface integrity in high speed milling of gamma titanium aluminide under dry and minimum quantity lubricant conditions[J]. Proc. CIRP, 2015, 26: 367 |
| [17] | Klocke F, Settineri L, Lung D, et al.High performance cutting of gamma titanium aluminides: Influence of lubricoolant strategy on tool wear and surface integrity[J]. Wear, 2013, 302: 1136 |
| [18] | Hood R, Aspinwall D K, Sage C, et al.High speed ball nose end milling of γ-TiAl alloys[J]. Intermetallics, 2013, 32: 284 |
| [19] | Mantle A L, Aspinwall D K.Surface integrity of a high speed milled gamma titanium aluminide[J]. J. Mater. Process. Technol., 2001, 118: 143 |
| [20] | Hood R, Aspinwall D K, Soo S L, et al.Workpiece surface integrity when slot milling γ-TiAl intermetallic alloy[J]. CIRP Ann.-Manuf. Technol., 2014, 63: 53 |
| [21] | Fu Z T, Yang W Y, Zeng S Q, et al.Identification of constitutive model parameters for nickel aluminum bronze in machining[J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 1105 |
| [22] | Wu Q, Zhang Y D, Zhang H W.Corner-milling of thin walled cavities on aeronautical components[J]. Chin. J. Aeronaut., 2009, 22: 677 |
| [23] | Dong H Y, Ke Y L.Study on machining deformation of aircraft monolithic component by FEM and experiment[J]. Chin. J. Aeronaut., 2006, 19: 247 |
| [24] | Wang S.An optimal method for elastoplastic finite element analysis[J]. Acta Mech. Solida Sin., 1990, 11: 272 |
| [24] | (王苏. 弹塑性有限元的一种最优化方法[J]. 固体力学学报, 1990, 11: 272) |
| [25] | Gasik M M.Elastic properties of lamellar Ti-Al alloys[J]. Comp. Mater. Sci., 2009, 47: 206 |
| [26] | Zhou L, Wang Y, Ma Z Y, et al.Finite element and experimental studies of the formation mechanism of edge defects during machining of SiCp/Al composites[J]. Int. J. Mach. Tool. Manu., 2014, 84: 9 |
/
| 〈 |
|
〉 |