Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation
Received date: 2016-08-26
Online published: 2017-04-07
Electroslag remelting (ESR) is duly an important process for the production of high quality special steels and superalloys. Conventional ESR research has long been known as trial and error approach, which is excessively expensive and time-consuming, due to the complex process mechanism involving interactions of multiple physical fields, simultaneous phase transformations and chemical reactions. As the alternative way of study, ESR numerical simulation has been profoundly developed. Till now, systematically formulated model could demonstrate so many aspects of the process including electromagnetic field, fluid flow, heat and mass transfer, electrode melting, ingot solidification, slag/metal interface phenomenon, solidification structure parameters, ingot elements distribution, etc. There is a trend of multi-scale combined simulation, trying to bridge the gap between macro- and micro-scopes, thus could realize the control of solidified structure. Numerical modeling and simulation of ESR process have been widely accepted for its superiority of low cost, high speed, flexible adaptability and systematic results. Through combination of simulation and experiment, the ESR R&D process can be significantly promoted. Further, with the newly developed control technology supported by theoretical models, high precision and perfect quality control are expected to achieve. In this work, a mathematical model and the calculating code for the simulation of practical ESR process were developed based on multi-physics coupling calculation. The model considers many features of the process including the heat of the dropping liquid metal from the electrode, the naturally formed melt pool and the growing of the ingot, the cooling shrinkage of the solidified ingot away from the mould boundary, the changed slag skull thickness along the ingot growing direction, the matching between melt rate and input melting parameters, the specific boundary conditions, etc. The model covers physics of electromagnetic field, fluid flow, heat transfer, and melting and solidification during the remelting process, giving the characteristic information about distributions of temperature and liquid phase volume fraction, shape and size of melt pool and mushy zone, etc. highly concerned with the process control. Using history of temperature distributions and evolution, the model can compute various solidification parameters closely related to the ingot quality. The model realizes predictions for the unknown ESR process with steady state mode calculation and also analysis in transient mode of the whole ESR process from the melting start point of electrode to the end of cooling stage of ingot within the mould. Electromagnetic fields and steady and transient process simulations were carried out and discussed here for the practical IN718 alloy ESR process. The simulated melt pool profile and its depth size approximate to the experimental result of the ingot dissection analysis, and the predicted secondary dendrite spacing distribution coincides with the pictures of dendrite structure analysis fairly well. The model could be applied to the process analysis and optimization, and provide important technical support for the R&D of new product and technology.
Qing LI , Zixing WANG , Shuyuan XIE . Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation[J]. Acta Metall Sin, 2017 , 53(4) : 494 -504 . DOI: 10.11900/0412.1961.2016.00386
| [1] | Hernandez-Morales B, Mitchell A.Review of mathematical models of fluid flow, heat transfer, and mass transfer in electroslag remel-ting process[J]. Ironmak. Steelmak., 1999, 26: 423 |
| [2] | Kelkar K M, Patankar S V, Mitchell A.Computational modeling of the electroslag remelting (ESR) process used for the production of ingots of high-performance alloys [A]. Proceedings of the 2005 International Symposium on Liquid Metal Processing and Casting[C]. Materials Park, OH, USA: Wiley-TMS, 2005: 137 |
| [3] | Rückert A, Pfeifer H.Numerical modelling of the electroslag remelting process[J]. METAL 2007-Hradec nad Moravici, 2007, 5: 22 |
| [4] | Mackenbrock A, Maronnier V, K?ser O, et al.Numerical simulation of the protective gas electroslag remelting process and its industrial validation[J]. BHM Berg- und Hüttenm?nnische Monatshefte, 2007, 152: 345 |
| [5] | Weber V, Jardy A, Dussoubs B, et al.A comprehensive model of the electroslag remelting process: Description and validation[J]. Metall. Mater. Trans., 2009, 40B: 271 |
| [6] | Wei J H, Ren Y L.Mathematical simulation of magnetic field in ESR system[J]. Acta Metall. Sin., 1995, 31: 51 |
| [6] | (魏季和, 任永莉. 电渣重熔体系内磁场的数学模拟[J]. 金属学报, 1995, 31: 51) |
| [7] | Geng M P, Sun D X.Process Control and Simulation in Electroslag Casting [M]. Beijing: Metallurgical Industry Press, 2008: 21 |
| [7] | (耿茂鹏, 孙达昕. 电渣熔铸过程控制与模拟仿真 [M]. 北京: 冶金工业出版社, 2008: 21) |
| [8] | Li B K, Wang B, Tsukihashi F.Modeling of electromagnetic field and liquid metal pool shape in an electroslag remelting process with two series-connected electrodes[J]. Metall. Mater. Trans., 2014, 45B: 1122 |
| [9] | Wang Q, He Z, Li B K, et al.A general coupled mathematical model of electromagnetic phenomena, two-phase flow, and heat transfer in electroslag remelting process including conducting in the mold[J]. Metall. Mater. Trans., 2014, 45B: 2425 |
| [10] | Kharicha A, Mackenbrock A, Ludwig A, et al.Selected numerical investigations on ESR process [A]. Proceedings of the 2007 International Symposium on Liquid Metal Processing and Casting[C]. Nancy, France: Wiley-TMS, 2007: 107 |
| [11] | Fezi K, Yanke J, Krane M J M. Macrosegregation during electroslag remelting of alloy 625[J]. Metall. Mater. Trans., 2015, 46B: 766 |
| [12] | Wei J H, Ren Y L.Mathematical modelling of slag flow field in ESR system[J]. Acta Metall. Sin., 1994, 30: 481 |
| [12] | (魏季和, 任永莉. 电渣重熔体系内熔渣流场的数学模拟[J]. 金属学报, 1994, 30: 481) |
| [13] | Liu F B, Chen X, Jiang Z H, et al.Mathematical modeling of electroslag remelting process[J]. J. Northeast. Univ.(Nat. Sci.), 2014, 35: 539 |
| [13] | (刘福斌, 陈旭, 姜周华等. 电渣重熔过程的数值模拟[J]. 东北大学学报(自然科学版), 2014, 35: 539) |
| [14] | Chang L Z, Li Z B.Dynamic simulation on temperature field of slab ingot during electroslag remelting[J]. Spec. Steel, 2007, 28(5): 34 |
| [14] | (常立忠, 李正邦. 电渣重熔板锭过程中温度场的动态模拟[J]. 特殊钢, 2007, 28(5): 34) |
| [15] | Bai H J, Li Y, Li B K.Effect of electromagnetic stirring on temperature field of ESR ingot[J]. Spec. Steel, 2008, 29(1): 7 |
| [15] | (白海军, 厉英, 李宝宽. 电磁搅拌对电渣重熔钢锭温度场的影响[J]. 特殊钢, 2008, 29(1): 7) |
| [16] | Wei J H, Mitchell A.Changes in composition during A. C. ESR—I. Theoretical development[J]. Acta Metall. Sin., 1984, 20: B261 |
| [16] | (魏季和, Mitchell A.交流电渣重熔过程中的成分变化——I.理论传质模型[J]. 金属学报, 1984, 20: B261) |
| [17] | Nastac L, Sundarraj S, Yu K O, et al.The stochastic modeling of solidification structures in alloy 718 remelt ingots[J]. JOM, 1998, 50(3): 30 |
| [18] | Li B K, Wang Q, Wang F, et al.A coupled cellular automaton-finite-element mathematical model for the multiscale phenomena of electroslag remelting H13 die steel ingot[J]. JOM, 2014, 66: 1153 |
| [19] | Bertram L A, Williamson R L, Melgaard D K, et al.Dynamic control of remelting processes [P]. US Pat., 6115404, 2000 |
| [20] | Xie D X, Yao Y Y, Bai B D, et al.The Finite Element Analysis of Three-dimensional Eddy Current Field [M]. Beijing: China Machine Press, 2001: 12 |
| [20] | (谢德馨, 姚缨英, 白保东等. 三维涡流场的有限元分析 [M]. 北京: 机械工业出版社, 2001: 12) |
| [21] | Tao W Q.Numerical Heat Transfer [M]. 2nd Ed., Xi'an: Xi'an Jiaotong University Press, 2001: 242, 273, 347, 351, 353 |
| [21] | (陶文铨. 数值传热学 [M]. 第2版. 西安: 西安交通大学出版社, 2001: 242, 273, 347, 351, 353) |
| [22] | Bai Y F.Coupled modeling and numerical calculation for transport phenomena in electromagnetic directional solidification of titanium alloy in cold crucible [D]. Harbin: Harbin Institute of Technology, 2006 |
| [22] | (白云峰. 钛合金冷坩埚电磁定向凝固传输过程耦合模型与数值计算 [D]. 哈尔滨: 哈尔滨工业大学, 2006) |
| [23] | Sun D L, Qu Z G, He Y L, et al.Inner doubly-iteration efficient algorithm for linked-equations based on three-dimensional non-staggered grid[J]. Chin. Sci. Bull., 2008, 53: 3014 |
| [23] | (孙东亮, 屈治国, 何雅玲等. 基于三维同位网格的高效稳定的分离式算法IDEAL[J]. 科学通报, 2008, 53: 3014) |
| [24] | Wang F J.Computational Fluid Dynamics Analysis——Principle and Application of CFD Software [M]. Beijing: Tsinghua University Press, 2004: 11, 50 |
| [24] | (王福军. 计算流体动力学分析——CFD软件原理与应用 [M]. 北京: 清华大学出版社, 2004: 11, 50) |
| [25] | Auburtin P, Wang T, Cockcroft S L, et al.Freckle formation and freckle criterion in superalloy castings[J]. Metall. Mater. Trans., 2000, 31B: 801 |
/
| 〈 |
|
〉 |