Effect of Graphite Flake Size on the Strength and Thermal Conductivity of Graphite Flakes/Al Composites

  • Xiaoyun LIU ,
  • Wenguang WANG ,
  • Dong WANG ,
  • Bolv XIAO ,
  • Dingrui NI ,
  • Liqing CHEN ,
  • Zongyi MA
Expand
  • 1 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
    2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2017-01-13

  Online published: 2017-04-05

Supported by

Supported by National Natural Science Foundation of China (Nos.U1508216 and 51271051)

Abstract

Graphite flakes reinforced Al matrix composites (Gf /Al) with low density, good machining property and high thermal conductivity are considered an excellent heat sink materials used in electronic industry. When the composites are manufactured by liquid method such as liquid infiltration, it is easy to achieve a high thermal conductivity composite. However, the Al4C3 phase would be formed in the composite, which will decrease the corrosion properties of the composites. The powder metallurgy technique could avoid the formation of the Al4C3 phase. In this work, three seized graphite flakes (150, 300, 500 μm) were used to investigate the effect of the graphite flake size on the strength and thermal conductivity of Gf/Al alloy composites. The 50%Gf /Al alloy (volume fraction) composites were fabricated by the powder metallurgy technique. The density of all the three Gf /Al alloy composites were similar to the theoretical density. The graphite flakes had a well bonding with Al alloy matrix without cracks and pores. The (001)Gf basal plane of the graphite flakes were almost parallel to the circular plane (xy plane) of the composites ingot. However, for the small graphite flakes, their (001)Gf basal plane was not well parallel to the xy plane of the composite ingot due to the powder metallurgy process. For the large graphite flakes, they exhibited a good orientation in the xy plane of the composite ingot. The strength of the Gf /Al alloy composites decreased with the increase of the graphite flake size. For the 150 μm graphite flake, the bending strength of the Gf /Al alloy composite was 82 MPa. However, for the 500 μm graphite flake, the bending strength of the composite decreased to 39 MPa. Due to the low strength between the layers of the graphite flake, the cracks were prone to expand in the graphite flake. As the size of the graphite flake increased, this phenomenon became more obviously. It is easy to observe that the graphite flakes peeled off on the fracture surfaces. When the size of the graphite flake increased from 150 μm to 500 μm, the thermal conductivity increased by 63%. The highest thermal conductivity was 604 W/(mK). The interfacial thermal conductance (hc) of the composites were calculated by the Maxwell-Garnett type effective medium approximation model. The hc of 300 and 500 μm graphite flake Gf /Al alloy composites were slightly lower than the theoretical value (calculated by the acoustic mismatch model). However, the hc of the 150 μm graphite flake Gf /Al alloy composite was lower than that of the theoretical value. Besides the size of the graphite flakes, the shape, distribution and defect of the graphite flakes also influenced the thermal conductivity of the composites.

Cite this article

Xiaoyun LIU , Wenguang WANG , Dong WANG , Bolv XIAO , Dingrui NI , Liqing CHEN , Zongyi MA . Effect of Graphite Flake Size on the Strength and Thermal Conductivity of Graphite Flakes/Al Composites[J]. Acta Metall Sin, 2017 , 53(7) : 869 -878 . DOI: 10.11900/0412.1961.2017.00015

References

[1] Sidhu S S, Kumar S, Batish A.Metal matrix composites for thermal management: A review[J]. Crit. Rev. Solid State Mater. Sci., 2016, 41: 132
[2] Mathias J D, Geffroy P M, Silvain J F.Architectural optimization for microelectronic packaging[J]. Appl. Therm. Eng., 2009, 29: 2391
[3] Rawal S P.Metal-matrix composites for space applications[J]. JOM, 2001, 53(4): 14
[4] Xia Y, Song Y Q, Cui S, et al.Progress in thermal management materials[J]. Mater. Rev., 2008, 22(1): 4
[4] (夏杨, 宋月清, 崔舜等. 热管理材料的研究进展[J]. 材料导报, 2008, 22(1): 4)
[5] Xue C, Yu J K.Enhanced thermal transfer and bending strength of SiC/Al composite with controlled interfacial reaction[J]. Mater. Des., 2014, 53: 74
[6] Liu X Y, Wang W G, Wang D, et al.Effect of nanometer TiC coated diamond on the strength and thermal conductivity of diamond/Al composites[J]. Mater. Chem. Phys., 2016, 182: 256
[7] Yoshida K, Morigami H.Thermal properties of diamond/copper composite material[J]. Microelectron. Reliab., 2004, 44: 303
[8] Fu H T, Huang Y, Wu H W, et al.Synthesis by vacuum infiltration, microstructure, and thermo-physical properties of graphite-aluminum composite[J]. ?Adv. Eng. Mater., 2016, 18: 1609
[9] Zhou S X, Chiang S, Xu J Z, et al.Modeling the in-plane thermal conductivity of a graphite/polymer composite sheet with a very high content of natural flake graphite[J]. Carbon, 2012, 50: 5052
[10] Li W J, Liu Y, Wu G H.Preparation of graphite flakes/Al with preferred orientation and high thermal conductivity by squeeze casting[J]. Carbon, 2015, 95: 545
[11] Kurita H, Miyazaki T, Kawasaki A, et al.Interfacial microstructure of graphite flake reinforced aluminum matrix composites fabricated via hot pressing[J]. Composites, 2015, 73A: 125
[12] Prieto R, Molina J M, Narciso J, et al.Thermal conductivity of graphite flakes-SiC particles/metal composites[J]. Composites, 2011, 42A: 1970
[13] Yang Y W, Huang Y, Wu H W, et al.Interfacial characteristic, thermal conductivity, and modeling of graphite flakes/Si/Al composites fabricated by vacuum gas pressure infiltration[J]. J. Mater. Res., 2016, 31: 1723
[14] Prieto R, Molina J M, Narciso J, et al.Fabrication and properties of graphite flakes/metal composites for thermal management applications[J]. Scr. Mater., 2008, 59: 11
[15] Chen J K, Huang I S.Thermal properties of aluminum-graphite composites by powder metallurgy[J]. Composites, 2013, 44B: 698
[16] Wang D, Xiao B L, Wang Q Z, et al.Friction stir welding of SiCp/2009Al composite plate[J]. Mater. Des., 2013, 47: 243
[17] Huang Y, Ouyang Q B, Guo Q, et al.Graphite film/aluminum laminate composites with ultrahigh thermal conductivity for thermal management applications[J]. Mater. Des., 2016, 90: 508
[18] Zhou C, Huang W, Chen Z, et al.In-plane thermal enhancement behaviors of Al matrix composites with oriented graphite flake alignment[J]. Composites, 2015, 70B: 256
[19] Wang D, Xiao B L, Wang Q Z, et al.Evolution of the microstructure and strength in the nugget zone of friction stir welded SiCp/Al-Cu-Mg composite[J]. J. Mater. Sci. Technol., 2014, 30: 54
[20] Xue C, Bai H, Tao P F, et al.Thermal conductivity and mechanical properties of flake graphite/Al composite with a SiC nano-layer on graphite surface[J]. Mater. Des., 2016, 108: 250
[21] Nan C W, Birringer R, Clarke D R, et al.Effective thermal conductivity of particulate composites with interfacial thermal resistance[J]. J. Appl. Phys., 1997, 81: 6692
[22] Wang Z T, Tian R Z.Aluminum Alloy and Its Processing Manual [M]. 3rd Ed., Changsha: Central South University Press, 2005: 314
[22] (王祝堂, 田荣璋. 铝合金机器加工手册 [M]. 长沙: 中南大学出版社, 2005: 314)
[23] Molina J M, Louis E.Anisotropy in thermal conductivity of graphite flakes-SiCp/matrix composites: implications in heat sinking design for thermal management applications[J]. Mater. Charact., 2015, 109: 107
[24] Shenogin S, Gengler J, Roy A, et al.Molecular dynamics studies of thermal boundary resistance at carbon-metal interfaces[J]. Scr. Mater., 2013, 69: 100
[25] Chu K, Jia C C, Liang X B, et al.Modeling the thermal conductivity of diamond reinforced aluminium matrix composites with inhomogeneous interfacial conductance[J]. Mater. Des., 2009, 30: 4311
[26] Zhou C, Ji G, Chen Z, et al.Fabrication, interface characterization and modeling of oriented graphite flakes/Si/Al composites for thermal management applications[J]. Mater. Des., 2014, 63: 719
Outlines

/