Incipient Melting Behavior and Its Influences on the Mechanical Properties of a Directionally Solidified Ni-Based Superalloy with High Boron Content

  • Hongwei ZHANG ,
  • Xuezhi QIN ,
  • Xiaowu LI ,
  • Lanzhang ZHOU
Expand
  • 1 Department of Materials Physics and Chemistry, School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2016-11-07

  Online published: 2017-04-01

Supported by

Supported by National Natural Science Foundation of China (No.51001101) and National High Technology Research and Development Program of China (No.2012AA03A501)

Abstract

A new directionally solidified Ni-based superalloy is developed for industrial gas turbine applications, which has high strength and excellent hot corrosion resistance at high temperatures. The high strength of the alloy is primarily derived from precipitation hardening by ordered L12 γ′ phase. To achieve a uniform distribution of precipitated γ′ particles for optimized mechanical properties, the suitable heat treatments are used. However, the heat treatment temperature in Ni-based superalloys is limited by the problem of incipient melting. Incipient melting microstructrue evolution during heat treatment has been hardly reported. Therefore, the behaviors of incipient melting and its effect on mechanical properties in the new directionally solidified superalloy DZ444 with high boron have been investigated in this work. The results show that some interdendritic regions of the as-cast DZ444 sample exhibit many of γ′/γ eutectic, MC carbides and multi-phase eutectic-like constituent which are composed of boride, Ni5Hf and η phases. During solution treatments, incipient melting does not occur in boride or Ni5Hf phase with low melting point firstly, but appears in γ matrix around multi-phase eutectic-like constituent which is affected significantly by borides. Compared to DZ444 alloy with the normal boron content, incipient melting occurs at the lower temperature in the range between 1160 ℃ and 1170 ℃. Incipient melting can occur significantly with the increase of the solid solution temperature or time. Incipient melting consists of typical γ dentrites and a lot of tiny precipitation particles after the water quenching (WQ) method following solution treatment. However, incipient melting forms multi-phase eutectic-like constituent, γ matrix and γ′/γ eutectic successively during air cooling (AC) following solution treatment, and the morphology of multi-phase eutectic-like constituent is similar to that of as-cast alloy. Firstly, a so-called incipiently melted circle (IMC) forms around multi-phase eutectic-like constituent; with the increase of the solid solution temperature or time, IMC extends inwards which makes γ matrix and multi-phase eutectic-like constituent in this circle melt successively. Finally, a incipiently melted pool forms gradually. Incipient melting is limited to the IMC below 1200 ℃ and the area of incipient melting changes with temperature or time correspondingly. However, incipiently melted region (IMR) expands outwards continuously which makes γ matrix outside the incipiently melted circle melt when the temperature is higher than 1210 ℃. Especially, IMR swallows up plenty of γ matrix, and many matrix islands, regions unmelted, exist in IMR above 1250 ℃ which destroys the continuity of the matrix significantly. The incipient melting has a minor effect on the tensile properties, nevertheless, decreases the creep-rupture properties remarkably. The degradation of mechanical properties mainly results from the increasing of the incipient melting area fraction and size.

Cite this article

Hongwei ZHANG , Xuezhi QIN , Xiaowu LI , Lanzhang ZHOU . Incipient Melting Behavior and Its Influences on the Mechanical Properties of a Directionally Solidified Ni-Based Superalloy with High Boron Content[J]. Acta Metall Sin, 2017 , 53(6) : 684 -694 . DOI: 10.11900/0412.1961.2016.00495

References

[1] Zhang J, Zhang A B, Tan Y N, et al.Effect of Re on microstructure and properties of directionally solidified superalloy[J]. J. Aeronaut. Mater., 2010, 30(3): 24
[1] (张俊, 张爱斌, 谭永宁等. Re对定向凝固Ni基高温合金组织及性能的影响[J]. 航空材料学报, 2010, 30(3): 24)
[2] Zhou P J, He X M.Influences of minor alloying elements on the eutectic volume of Ni-Base superalloy[J]. Foundry, 2012, 61: 868
[2] (周鹏杰, 何向明. 微量元素对镍基高温合金共晶数量的影响[J]. 铸造, 2012, 61: 868)
[3] Ojo O A, Richards N L, Chaturvedi M C.On incipient melting during high temperature heat treatment of cast Inconel 738 superalloy[J]. J. Mater. Sci., 2004, 39: 7401
[4] Seo S M, Kim I S, Lee J H, et al.Eta phase and Boride formation in directionally solidified Ni-base superalloy IN792+Hf[J]. Metall. Mater. Trans., 2007, 38A: 883
[5] Shulga A V.Boron and carbon behavior in the cast Ni-base superalloy EP962[J]. J. Alloys Compd., 2007, 436: 155
[6] Wu B P, Li L H, Wu J T, et al.Effect of boron addition on the microstructure and stress-rupture properties of directionally solidified superalloys[J]. Int. J. Miner. Metall. Mater., 2014, 21: 1120
[7] Zhen B L, Zhang S J.The phase composition and the rules of the phase precipitation in Hf-bearing nickel base superalloys[J]. Cent. Iron Steel Res. Inst. Tech. Bull., 1981, (1): 65
[7] (甄宝林, 张绍津. 加铪镍基合金相的组成和析出规律[J]. 钢铁研究总院学报, 1981, (1): 65)
[8] Baldan A.Electron microprobe investigation of lower melting regions in the as-cast structure of DS200+Hf single crystal[J]. J. Mater. Sci., 1990, 25: 4341
[9] Ojo O A, Zhang H R.Analytical electron microscopy study of Boron-Rich grain boundary microconstituent in directionally solidified Rene 80 superalloy[J]. Metall. Mater. Trans., 2008, 39A: 2799
[10] Sidhu R K, Ojo O A, Chaturvedi M C.Sub-solidus melting of directionally solidified Rene 80 superalloy during solution heat treatment[J]. J. Mater. Sci., 2008, 43: 3612
[11] Zheng Y R.Incipient melting and its control in a directionally solidified nickel-base superalloy DZ22[J]. Acta Aeronaut. Astronaut. Sin., 1986, 7: 482
[11] (郑运荣. DZ22定向高温合金的初熔及其控制[J]. 航空学报, 1986, 7: 482)
[12] Zheng Y R, Cai Y L, Wang L B.Factors influenced incipient melting in Hf-bearing DS Ni-base superalloys[J]. Acta Metall. Sin., 1983, 19: A190
[12] (郑运荣, 蔡玉林, 王罗宝. 影响含Hf定向凝固合金初熔的某些因素[J]. 金属学报, 1983, 19: A190)
[13] Chen R Z, Wang L B, Wang Y P.Influence of solution temperature on microstructure and properties of directionally solidified super-alloy DZ22[J]. Acta Aeronaut. Astronaut. Sin., 1988, 9: A368
[13] (陈荣章, 王罗宝, 王玉屏. 固溶温度对定向凝固高温合金DZ22的组织和性能的影响[J]. 航空学报, 1988, 9: A368)
[14] Jahangiri M R, Boutorabi S M A, Arabi H. Study on incipient melting in cast Ni base IN939 superalloy during solution annealing and its effect on hot workability[J]. Mater. Sci. Technol., 2012, 28: 1402
[15] Guo J T.Materials Science and Engineering for Superalloys (Book 3) [M]. Beijing: Science Press, 2008: 3
[15] (郭建亭. 高温合金材料学(下册) [M]. 北京: 科学出版社, 2008: 3)
[16] Versnyder F I, Shank M E.The development of columnar grain and single crystal high temperature materials through directional solidification[J]. Mater. Sci. Eng., 1970, A6: 213
[17] Zheng Y R, Zhang D T.Color Metallographic Investigation of Superalloys and Steels [M]. Beijing: National Defense Industry Press, 1999: 141
[17] (郑运荣, 张德堂. 高温合金与钢的彩色金相研究 [M]. 北京: 国防工业出版社, 1999: 141)
[18] Zhao Y S, Zhang J, Luo Y S, et al.Effects of Hf and B on high temperature low stress creep behavior of a second generation Ni-based single crystal superalloy DD11[J]. Mater. Sci. Eng., 2016, A672: 143
[19] Caldwell E C, Fela F J, Fuchs G E.The segregation of elements in high-refractory-content single-crystal nickel-based superalloys[J]. JOM, 2004, 56(9): 44
[20] Collier J P, Keefe P W, Tien J K.The effects of replacing the refractory elements W, Nb and Ta with Mo in nickel-base superalloys on microstructural, microchemistry, and mechanical properties[J]. Metall. Trans., 1986, 17A: 651
[21] Huang Y Y, Mao Z G, Noebe R D, et al.The effects of refractory elements on Ni-excesses and Ni-depletions at γ(f.c.c.)/γ’(L12) interfaces in model Ni-based superalloys: Atom-probe tomographic experiments and first-principles calculations[J]. Acta Mater., 2016, 121: 288
[22] Zhang Z L, Ma J B, Dai Y B, et al.Effects of refractory elements on the structure and dynamics of molten Ni: An ab initio molecular dynamics study[J]. Comp. Mater. Sci., 2013, 77: 254
[23] Ma Y Q, Yu X F, Sun W R.Study on the initial melting characteristics of γ+γ’ eutectics in K417G alloy and influencing factors[J]. Foundry, 2014, 63: 185
[23] (马亚芹, 于兴福, 孙文儒. K417G合金γ+γ’共晶初熔特性及影响因素研究[J]. 铸造, 2014, 63: 185)
[24] Liang Y J, Li J, Li A, et al.Solidification path of single-crystal nickel-base superalloys with minor carbon additions under laser rapid directional solidification conditions[J]. Scr. Mater., 2017, 127: 58
[25] Wang H F, Su H J, Zhang J, et al.Effect of melt thermal history on solidification behavior and microstructural characteristics of a third-generation Ni-based single crystal superalloy[J]. J. Alloys Compd., 2016, 688: 430
[26] Shi Z X, Dong J X, Zhang M C, et al.Solidification characteristics and segregation behavior of Ni-based superalloy K418 for auto turbocharger turbine[J]. J. Alloys Compd., 2013, 571: 168
[27] Zhang Y J, Huang Y J, Yang L, et al.Evolution of microstructures at a wide range of solidification cooling rate in a Ni-based superalloy[J]. J. Alloys Compd., 2013, 570: 70
[28] Wang F, Ma D, Zhang J, et al.Effect of solidification parameters on the microstructures of superalloy CMSX-6 formed during the downward directional solidification process[J]. J. Cryst. Growth, 2014, 389: 47
[29] Zheng Y R, Cai Y L.Phase transformations in hafnium-bearing cast nickel-base superalloys [A]. Superalloys[C], 1980: 465
Outlines

/