Orginal Article

Point Defect Concentrations and Interactions in D019-Ti3Al from First-Principles Calculations

  • Huijin TAO ,
  • Shan ZHOU ,
  • Yu LIU ,
  • Jian YIN ,
  • Hao XU
Expand
  • 1 School of Materials Science and Engineering, Central South University, Changsha 410083, China
    2 Key Laboratory of Nonferrous Metal Materials Science and Engineering,Ministry of Education, Central South University, Changsha 410083, China
    3 State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China

Received date: 2016-10-20

  Online published: 2017-03-31

Supported by

Supported by National Natural Science Foundation of China (Nos.51302322 and 21373273), Open-End Fund for the Valuable and Precision Instruments of Central South University (Nos.CSUZC201708 and CSUZC201613), Education Reform Project of Central South University (Nos.2016jy03 and 2016CLYJG02) and Open Foundation of Guangdong Provincial Key Laboratory for Technology and Application of Metal Toughening, Guangdong Institute of Materials and Processing (No.GKL201605)

Abstract

The intermetallics D019-Ti3Al has low specific density and high thermal resistance for both bulk and coating applications in engineering area. The point defects such as thermal vacancy, compostion vacancy and antisite defect have great influence on the properties of D019-Ti3Al, but are usally neglected. According to available research data from both theory and experiment, it is commonly considered that the thermal vacancies in D019-Ti3Al provide paths for atomic migration and diffusion, the antisite defects play an important role in the disordering of D019-Ti3Al, and the interaction between composition vacancy and antisite defect may have important influence on atomic diffusion and dislocation movement. So it is necessary to explore the mechanism of interaction between composition vacancy and antisite defect for more accurate understanding of the atomic diffusion, dislocation movement and plastic deform in D019-Ti3Al. In this work, the formation enthalpy, equilibrium concentration, and binding energy of composition vacancy and antisite defect in D019-Ti3Al intermetallics were calculated by using both the Wagner-Schottky model of point defect thermodynamics and the plane wave pseudopotential method in first-principles. Results suggest that, in the whole composition range of interest, the point defect concentrations increase with the increase of temperature. In particular, the concentrations of antisite defects are higher than those of vacancies, and the vacancy concentration of Ti is higher than that of Al. At the stoichiometric composition, the concentrations of antisite defects of Ti and Al are very close. At the Ti-rich side of component, the antisite defect of Ti dominates in concentration, while at the Al-rich side, that of Al dominates in concentration. For the calculated results of 3 types of point defect pairs, AlTi-TiAl, TiAl-TiAl and VAl-AlTi, they may have the strong trend to aggregate, while others may show the tend to diffuse into the matrix.

Cite this article

Huijin TAO , Shan ZHOU , Yu LIU , Jian YIN , Hao XU . Point Defect Concentrations and Interactions in D019-Ti3Al from First-Principles Calculations[J]. Acta Metall Sin, 2017 , 53(6) : 751 -759 . DOI: 10.11900/0412.1961.2016.00464

References

[1] Tao H J, Sun S P, Zhang C C, et al.First principles study of point defect concentrations in L10-TiAl intermetallic composite[J]. Chin. J. Nonferrous Met., 2014, 24: 2789
[1] (陶辉锦, 孙顺平, 张铖铖等. 金属间化合物L10-TiAl点缺陷浓度的第一原理[J]. 中国有色金属学报, 2014, 24: 2789)
[2] Filimonov V Y, Korchagin M A, Dietenberg I A, et al.High temperature synthesis of single-phase Ti3Al intermetallic compound in mechanically activated powder mixture[J]. Powder Technol., 2013, 235: 606
[3] Liu Y L, Liu L M, Wang S Q, et al.First-principles study of shear deformation in TiAl and Ti3Al[J]. Intermetallics, 2007, 15: 428
[4] Liu Y L, Zhang L, Wang S Q, et al.Shear deformation in Ti3Al: Atomic, dynamic and static simulations[J]. Model. Simul. Mater. Sci. Eng., 2008, 16: 085008
[5] Yoo M H, Zou J, Fu C L. Mechanistic modeling of deformation and fracture behavior in TiAl and Ti3Al [J]. Mater. Sci. Eng., 1995, A192-193: 14
[6] Karkina L E, Yakovenkova L I.Dislocation core structure and deformation behavior of Ti3Al[J]. Model. Simul. Mater. Sci. Eng., 2012, 20: 065003
[7] Fu C L, Zou J, Yoo M H.Elastic constants and planar fault energies of Ti3Al, and interfacial energies at the Ti3Al/TiAl interface by first-principles calculations[J]. Scr. Metall. Mater., 1995, 33: 885
[8] Wang L, Shang J X, Wang F H, et al.First principles study of α2-Ti3Al (0001) surface and γ-TiAl (111)/α2-Ti3Al (0001) interfaces[J]. Appl. Surf. Sci., 2013, 276: 198
[9] Xie Z C, Gao T H, Guo X T, et al.Molecular dynamics simulation of nanocrystal formation and deformation behavior of Ti3Al alloy[J]. Comput. Mater. Sci., 2015, 98: 245
[10] Piao Y X, Li W.Effect of Nb on valence electron structures and embrittlement of Ti3Al[J]. Chin. J. Rare Met., 2000, 24: 47
[10] (朴英锡, 李文. 铌对Ti3Al价电子结构及其脆性的影响[J]. 稀有金属, 2000, 24: 47)
[11] Chen C L, Lu W, Sun D, et al.Deformation-induced α2 →γ phase transformation in TiAl alloys[J]. Mater. Charact., 2010, 61: 1029
[12] Al-Kassab T, Yuan Y, Kluthe C, et al.Investigation of the ordering and atomic site occupancies of Nb-doped TiAl/Ti3Al intermetallics[J]. Surf. Interface Anal., 2007, 39: 257
[13] Wei Y, Zhou H B, Zhang Y, et al.Effects of O in a binary-phase TiAl-Ti3Al alloy: From site occupancy to interfacial energetic[J]. J. Phys.: Condens Matter, 2011, 23: 225504
[14] Zhang E L, Wang H W, Zeng S Y.Microstructure characteristics of in situ carbide reinforced titanium aluminide (Ti3Al) matrix Composites[J]. J. Mater. Sci. Lett., 2001, 20: 1733
[15] Bratanich T I, Skorokhod V V, Kopylova L I, et al.Ti3Al destructive hydrogenation[J]. Int. J. Hydrogen Energy, 2011, 36: 1276
[16] Rüsing J, Herzig C.Concentration and temperature dependence of titanium self-diffusion and interdiffusion in the intermetallic phase Ti3Al[J]. Intermetallics, 1996, 4: 647
[17] Shirai Y, Murakami T, Ogawa N, et al.Vacancies and their clusters in Ti3Al studied by positron lifetime spectrometry[J]. Intermetallics, 1996, 4: 31
[18] Mishin Y, Herzig C.Diffusion in the Ti-Al system[J]. Acta Mater., 2000, 48: 589
[19] Semenova O, Krachler R, Ipser H.Estimation of point defect formation energies in the D019-type intermetallic compound Ti3Al[J]. Solid State Sci., 2002, 4: 1113
[20] Fr?bel U, Appel F.Strain ageing in γ (TiAl)-based and α2 (Ti3Al) titanium aluminides[J]. Intermetallics, 2006, 14: 1187
[21] Kresse G, Joubert D.From ultrasoft pseudopotentials to the projector augmented-wave method[J]. Phys. Rev., 1999, 59B: 1758
[22] Perdew J P, Burke K, Ernzerhof M.Generalized gradient approximation made simple[J]. Phys. Rev. Lett., 1996, 77: 3865
[23] Monkhorst H J, Pack J D.Special points for Brillouin-zone integrations[J]. Phys. Rev., 1976, 13B: 5188
[24] Bl?chl P E, Jepsen O, Andersen O K.Improved tetrahedron method for Brillouin-zone integrations[J]. Phys. Rev., 1994, 49B: 16223
[25] Novoselova T, Malinov S, Sha W, et al.High-temperature synchrotron X-ray diffraction study of phases in a gamma TiAl alloy[J]. Mater. Sci. Eng., 2004, A371: 103
[26] Yoo M H, Fu C L.Physical constants, deformation twinning, and microcracking of titanium aluminides[J]. Metall. Mater. Trans., 1998, 29A: 49
[27] Wagner C, Schottky W.Theorie der geordneten Mischphasen[J]. Z. Phys. Chem., 1930, 11B: 163
[28] Sun S P, Li X P, Yu Y, et al.First-principle calculation of point defects concentration in L12-Al3Li intermetallic[J]. Chin. J. Nonferrous Met., 2013, 23: 370
[28] (孙顺平, 李小平, 于赟等. L12-Al3Li金属间化合物点缺陷浓度的第一原理计算[J]. 中国有色金属学报, 2013, 23: 370)
[29] Benedek R, van de Walle A, Gerstl S S A, et al. Partitioning of solutes in multiphase Ti-Al alloys[J]. Phys. Rev., 2005, 71B: 094201
[30] Würschum R, Kümmerle E A, Badura-Gergen K, et al.Thermal vacancy formation and positron-vacancy interaction in Ti3Al at high temperatures[J]. J. Appl. Phys., 1996, 80: 724
[31] Fu C L, Wang X D. The effect of electronic structure on the defect properties of FeAl [J]. Mater. Sci. Eng., 1997, A239-240: 761
[32] Parlinski K, Jochym P T, Kozubsk R, et al.Atomic modelling of Co, Cr, Fe, antisite atoms and vacancies in B2-NiAl[J]. Intermetallics, 2003, 11: 157
Outlines

/