Effect of Mn, Ni, Mo Contents on Microstructure Transition and Low Temperature Toughness of Weld Metal for K65 Hot Bending Pipe
Received date: 2016-09-08
Online published: 2017-03-30
To increase transport efficiency and to lower the costs of pipeline construction, longitudinally submerged arc welded (LSAW) pipes with larger diameters and thicker walls have been increasingly used by the pipeline industry. For example, in Russia, the LSAW pipeline in the Bovanenkovo-Ukhta project was recently constructed with K65 steel (the highest grade of the Russian natural gas pipeline), which is similar in specifications and yield strength requirement (550 MPa grade) to API X80 but has a stricter low temperature toughness value of 60 J at -40 ℃ (compared to -20 ℃ for API X80 grade) due to the extreme Arctic environment. Although weld metal with acicular ferrite (AF) has been developed to meet the requirement of low temperature toughness, the main objective of the present work was to clarify the microstructural evolution and the resulting changes in mechanical properties after the bending process. Hot bending pipes are necessary links in the construction of pipeline lying, which make more strin gent standards for the strength and low temperature toughness. That puts forward a challenge especially to the weld bead because of the deterioration of toughness during the hot bending process. In this work, submerged arc welding wire with high strength and toughness was developed for K65 hot bending pipes, and the alloying elements of Mn, Ni, Mo were considered to estimate the microstructure evolution and the effect of low temperature toughness for the weld metal. The results showed the low temperature toughness at -40 ℃ reached 90~185 J and 65~124 J for weld metal of straight seam pipe and hot bending pipe respectively, which reflect the excellent role of alloying elements of Mn, Ni, Mo. Microstructure characterization revealed that the weld metal, which originally consisted mainly of AF in the as-deposited condition, became predominantly composed of bainitic ferrite (BF) after hot bending. In addition, the large size cementite along the grain boundary was also the reason for the deterioration of toughness. It is found that reaustenisation caused a small austenite grain-sized matrix, which brought about a very high volume fraction of bainite. However, the low temperature toughness for hot bending pipe was improved to 124 J for the weld metal with 0.2%Mo, in which about 67.1% of high angle grain boundary were found. It is clear that the process of reaustenitisation during the bending process plays an important role in successful microstructural design for the steel weld metals.
Liming DONG , Li YANG , Jun DAI , Yu ZHANG , Xuelin WANG , Chengjia SHANG . Effect of Mn, Ni, Mo Contents on Microstructure Transition and Low Temperature Toughness of Weld Metal for K65 Hot Bending Pipe[J]. Acta Metall Sin, 2017 , 53(6) : 657 -668 . DOI: 10.11900/0412.1961.2016.00403
| [1] | Gao H L.The challenges for pipeline projects & development trend of pipeline steel[J]. Weld. Pipe Tube, 2010, 33(10): 5 |
| [1] | (高惠临. 管道工程面临的挑战与管线钢的发展趋势[J]. 焊管, 2010, 33(10): 5) |
| [2] | Stalheim D G.The use of high temperature processing (HTP) for high strength oil and gas transmission pipeline application [A]. Proceedings of the 5th steels Conference[C]. Iron Steel, 2005, 40: 699 |
| [3] | Niu J, Liu Y L, Feng Y R, et al.Low temperature embrittlement of X80 steel weld after heat treatment[J]. Hot Work. Technol., 2010, 39(19): 15 |
| [3] | (牛靖, 刘迎来, 冯耀荣等. 热处理状态下X80钢焊缝的低温脆化[J]. 热加工工艺, 2010, 39(19): 15) |
| [4] | Keehan E, Karlsson L, Andren H O, et al. New developments with C-Mn-Ni high-strength steel weld metals, Part A——Microstructure [J]. Weld. J., 2006,85: 200.s |
| [5] | Keehan E, Karlsson L, Andrén H O.Influence of carbon, manganese and nickel on microstructure and properties of strong steel weld metals: Part 1——Effect of nickel content[J]. Sci. Technol. Weld. Join., 2006, 11: 1 |
| [6] | Keehan E, Karlsson L, Andrén H O, et al.Influence of carbon, manganese and nickel on microstructure and properties of strong steel weld metals: Part 2——Impact toughness gain resulting from manganese reductions[J]. Sci. Technol. Weld. Join., 2006, 11: 9 |
| [7] | Bhole S D, Nemade J B, Collins L, et al.Effect of nickel and molybdenum additions on weld metal toughness in a submerged arc welded HSLA line-pipe steel[J]. J. Mater. Process. Technol., 2006, 173: 92 |
| [8] | Zhang M, Yao C W, Fu C, et al.Submerged arc welding wire matched with X80 pipeline steel[J]. Trans. China Weld. Inst., 2006, 27(4): 64 |
| [8] | (张敏, 姚成武, 付翀等. X80管线钢埋弧焊匹配焊丝研制[J]. 焊接学报, 2006, 27(4): 64) |
| [9] | Pan X, Wang Y B, Zhang Y.Development of submerged arc welding wire for third generation pipeline X90 [A]. The National Metal Products Information Network Twenty-Third Annual Meeting and the 2013 Metal Products Industry Information Technology Symposium[C]. Wuxi: The Chinese Society for Metals, 2013 |
| [9] | (潘鑫, 王银柏, 张宇. 第三代管线X90用埋弧焊丝研制 [A]. 全国金属制品信息网第23届年会暨2013金属制品行业技术信息交流会论文集[C]. 无锡: 中国金属学会, 2013) |
| [10] | Bi Z Y, Liu H Z, Jing X T, et al.Research on submerged arc welding wire for X100 pipeline steel[J]. China Weld., 2011, 20(2): 56 |
| [11] | Zhang X L, Liu Y L, Feng Y R, et al.Relationship of microstructure and toughness index of reheated high grade pipeline steels[J]. Dev. Appl. Mater., 2008, 23(1): 1 |
| [12] | Arai Y, Kondo K, Hirata H, et al.Metallurgical design of newly developed material for seamless pipes of X80-X100 grades [A]. ASME 2007 26th International Conference on Offshore Mechanics and Arctic Engineering Volume 4: Materials Technology; Ocean Engineering[C]. San Diego, California, USA: ASME, 2007, 37 |
| [13] | Wu D Y, Han X L, Tian H T, et al.Microstructural characterization and mechanical properties analysis of weld metals with two Ni contents during post-weld heat treatments[J]. Metall. Mater. Trans., 2015, 46A: 1973 |
| [14] | Yang W W, Zhao J, Jiao B, et al.Analysis and comparison of the K65 steel grade standards[J]. Weld. Pipe Tube, 2013, 36(7): 67 |
| [14] | (杨玮玮, 赵晶, 焦斌等. K65钢级标准的分析和对比[J]. 焊管, 2013, 36(7): 67) |
| [15] | Qian B N, Guo X M, Li J L, et al.Welding text of X80 high strength pipeline steel[J]. Weld. Join., 2002, (8): 14 |
| [15] | (钱百年, 国旭明, 李晶丽等. 高强度管线钢X80的焊接研究[J]. 焊接, 2002, (8): 14) |
| [16] | Wang X L, Dong L M, Yang W W, et al.Effect of Mn, Ni, Mo proportion on micro-structure and mechanical properties of weld metal of K65 pipeline steel[J]. Acta Metall. Sin., 2016, 52: 649 |
| [16] | (王学林, 董利明, 杨玮玮等. Mn/Ni/Mo配比对K65管线钢焊缝金属组织与力学性能的影响[J]. 金属学报, 2016, 52: 649) |
| [17] | Abson D J, Pargeter R J.Factors influencing as-deposited strength, microstructure, and toughness of manual metal arc welds suitable for C-Mn steel fabrications[J]. Int. Met. Rev., 1986, 31: 141 |
| [18] | Babu S S.The mechanism of acicular ferrite in weld deposits[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 267 |
| [19] | Li Y, Baker T N.Effect of morphology of martensite-austenite phase on fracture of weld heat affected zone in vanadium and niobium microalloyed steels[J]. Mater. Sci. Technol., 2010, 26: 1029 |
| [20] | Thomas G.Retained austenite and tempered martensite embrittlement[J]. Metall. Mater. Trans., 1978, 9A: 439 |
| [21] | Hwang B, Kin Y G, Lee S, et al.Effective grain size and charpy impact properties of high-toughness X70 pipeline steels[J]. Metall. Mater. Trans., 2005, 36A: 2107 |
| [22] | Padap A K, Chaudhari G P, Pancholi V, et al.Microstructural evolution and mechanical behavior of warm multi-axially forged HSLA steel[J]. J. Mater. Sci., 2012, 47: 7894 |
| [23] | Yan W, Zhu L, Sha W, et al.Change of tensile behavior of a high-strength low-alloy steel with tempering temperature[J]. Mater. Sci. Eng., 2009, A517: 369 |
| [24] | Edmonds D V, He K, Rizzo F C, et al. Quenching and partitioning martensite——A novel steel heat treatment [J]. Mater. Sci. Eng., 2006, A438-440: 25 |
| [25] | Yang J R, Yang C C, Huang C Y.The coexistence of acicular fe-rrite and bainite in an alloy-steel weld metal[J]. J. Mater. Sci. Lett., 1992, 11: 1547 |
| [26] | Yang J R, Huang C Y, Huang C F, et al.Influence of acicular fe-rrite and bainite microstructures on toughness for an ultra-low-carbon alloy steel weld metal[J]. J. Mater. Sci. Lett., 1993, 12: 1290 |
/
| 〈 |
|
〉 |