Experimental Studies and Numerical Simulation on the Nitriding Process of Grain-Oriented Silicon Steel
Received date: 2016-10-18
Online published: 2017-03-13
Grain-oriented silicon steel (GOSS) is an important functional material used as lamination cores in various transformers. Its magnetic properties are strongly dependent on the sharpness of Goss texture, which is developed during the secondary recrystallization annealing of product. In order to save energy and reduce cut-down operation costs, Nippon steel first lowered the slab-reheating temperature from 1350~1400 ℃ to 1150 ℃ and adopted the nitriding process to form nitride inhibitors before recrysta-llization annealing in 1970s. In this new process, nitriding is the critical process because it controls the size, distribution and volume fraction of nitride precipitates, which then determines the subsequent deve-lopment of Goss texture. Although it is of great importance for good quality control of industrial GOSS product, unfortunately, a quantitative mathematic modeling on nitriding kinetics is still in lack. In this work, nitriding kinetics were both measured experimentally and simulated by modeling. The N contents after various nitriding periods and N concentration gradient across thickness were both measured. It has been found that the N content increases slowly at the beginning of 60 s and then much more rapidly during nitriding. There exists a sharp N concentration gradient within the depth of 0.03 mm to the steel sheet surface, which diminishes after about 0.04 mm depth. With the different assumptions on N-transfer coefficient from gas to the steel matrix, the first mathematic modeling on nitriding kinetics of GOSS has been successfully established and solved numerically. The simulation results suggest that only when the N-transfer coefficient, f, changes with time following the Avrami function, f=A(1-exp(-ktn)), the calculated nitriding kinetics are consistent with the measurements. Such an Avrami-type dependence results from the reduction kinetics of oxide layer on the surface of silicon steel sheet during nitriding, in which both plate-like and spherical oxides were observed at the beginning but most of them became spherical after nitriding.
Key words: grain-oriented silicon steel; numerical simulation; nitriding; kinetics; diffusion
Guimin ZENG , Haiwen LUO , Jun LI , Jian GONG , Xianhao LI , Xianhui WANG . Experimental Studies and Numerical Simulation on the Nitriding Process of Grain-Oriented Silicon Steel[J]. Acta Metall Sin, 2017 , 53(6) : 743 -750 . DOI: 10.11900/0412.1961.2016.00463
| [1] | He Z Z, Zhao Y, Luo H W.Electrical Steel [M]. Beijing: Metallurgical Industry Press, 2012: 1 |
| [1] | (何忠治, 赵宇, 罗海文. 电工钢[M]. 北京: 冶金工业出版社, 2012: 1) |
| [2] | Ushigami Y, Mizokami Y, Fujikura M, et al. Recent development of low-loss grain-oriented silicon steel [J]. J. Magn. Magn. Mater., 2003, 254-255: 307 |
| [3] | Goss N P.Electrical sheet and method and apparatus for its manufacture and test [P]. US Pat, 1965559A, 1934 |
| [4] | Li J, Sun Y, Zhao Y.Development of low temperature slab reheating technique for grain-oriented silicon steel[J]. Iron Steel, 2007, 42(10): 72 |
| [4] | (李军, 孙颖, 赵宇. 取向硅钢低温铸坯加热技术的研发进展[J]. 钢铁, 2007, 42(10): 72) |
| [5] | Kumano T, Haratani T, Fujii N.Effect of nitriding on grain oriented silicon steel bearing aluminum[J]. ISIJ Int., 2005, 45: 95 |
| [6] | Lee S C, Han C H, Woo J S, et al.Hot rolling annealing; cold rolling decarbonization; controlling concentration [P]. US Pat, 6451128, 2002 |
| [7] | Takahashi N, Harase J. Recent development of technology of grain oriented silicon steel [J]. Mater. Sci. Forum, 1996,204-206: 143 |
| [8] | Kubota T, Fujikura M, Ushigami Y. Recentprogress and future trend on grain-oriented silicon steel [J]. J. Magn. Magn. Mater., 2000, 215-216: 69 |
| [9] | Lobanov M L.Nitriding of Fe-3%Si alloy[J]. Steel Trans., 2015, 45: 94 |
| [10] | Morawiec A.On abnormal growth of Goss grains in grain-oriented silicon steel[J]. Scr. Mater., 2011, 64: 466 |
| [11] | Kumano T, Ohata Y, Fujii N, et al.Effect of nitriding on grain oriented silicon steel bearing aluminum (the second study)[J]. J. Magn. Magn. Mater., 2006, 304: e602 |
| [12] | Abbruzzese G, Campopiano A.A general theory of secondary recrystallization in grain oriented Fe-Si: Metallurgical parameters controlling the microstructural evolution[J]. J. Magn. Magn. Mater., 1994, 133: 123 |
| [13] | Thermocalc: thermo-calc software TCFE8 steel/Fe-database. Version2015b [EB/OL]. 2015, |
| [14] | Wang R P, Liu J, Mao J H, et al.Influence of nitriding modes and ammonia on nitrogen content of oriented silicon steel[J]. Heat Treat. Met., 2009, 34(10): 69 |
| [14] | (王若平, 刘静, 毛炯辉等. 渗氮方式及氨气对取向硅钢氮含量的影响[J]. 金属热处理, 2009, 34(10): 69) |
| [15] | Toda H, Sato K, Komatsubara M.Characterization of internal oxide layers in 3%Si grain-oriented steel by electrochemical methods[J]. J. Mater. Eng. Perform, 1997, 6: 722 |
| [16] | Song H J, Yang P, Mao W M.Nitrogen behavior during nitriding treatment of electrical steel[J]. Heat Treat. Met., 2012, 37(1): 38 |
| [16] | (宋惠军, 杨平, 毛卫民. 电工钢渗氮的氮行为[J]. 金属热处理, 2012, 37(1): 38) |
| [17] | Yan G C, He C X, Meng L, et al.Structure of surface oxide layer and effect on nitriding of grain-oriented silicon steel[J]. J. Mater. Eng., 2015, 43(12): 89 |
| [17] | (严国春, 何承绪, 孟力等. 取向硅钢表面氧化层的结构及其对渗氮的影响[J]. 材料工程, 2015, 43(12): 89) |
| [18] | Jung S, Kwon M S, Park J, et al.A TEM study of oxide layers formed during decarburization annealing of electrical steel[J]. ISIJ Int., 2011, 51: 1163 |
| [19] | Guan C, Li J, Tan N, et al.Reduction of oxide scale on hot-rolled steel by hydrogen at low temperature[J]. Int. J. Hydrogen Energy, 2014, 39: 15116 |
| [20] | Hudson R M.Nonacidic descaling of hot band——Part II: Reduction of scale by hydrogen or carbon[J]. Met. Finish., 1985, 83(12): 59 |
| [21] | Hudson R M.Nonacidic descaling of hot band: Reduction of scale by hydrogen or carbon[J]. Met. Finish., 1985, 83(11): 73 |
| [22] | Sproge L, ?gren J.Experimental and theoretical studies of gas consumption in the gas carburizing process[J]. J. Heat Treat., 1988, 6: 9 |
| [23] | Hillert M, translated by Lai H Y, Liu G X. Diffusion in Alloys and Thermodynamics [M]. Beijing: Metallurgy Industry Press, 1984: 6 |
| [23] | (Hillert M著, 赖和怡, 刘国勋译. 合金扩散和热力学 [M]. 北京: 冶金工业出版社, 1984: 6) |
| [24] | Rozendaal H C F, Mittemeijer E J, Colijn P F, et al. The development of nitrogen concentration profiles on nitriding iron[J]. Metall. Trans., 1983, 14A: 395 |
| [25] | Nakada N, Tsuboi K, Onomoto T, et al.Thermodynamics and kinetics of solution nitriding[J]. Calphad, 2014, 47: 168 |
| [26] | Pineau A, Kanari N, Gaballah I.Kinetics of reduction of iron oxides by H2: Part I: Low temperature reduction of hematite[J]. Thermochim. Acta, 2006, 447: 89 |
| [27] | Liao C C, Hou C K.Effect of nitriding time on secondary recrystallization behaviors and magnetic properties of grain-oriented electrical steel[J]. J. Magn. Magn. Mater., 2010, 322: 434 |
/
| 〈 |
|
〉 |