Research on Austenite Transformation of FB2 Heat-Resistant Steel During Welding Heating Process
Received date: 2016-11-21
Online published: 2017-02-27
Supported by
Supported by Science and Technology Research Program of Shanghai Science and Technology Committee (No.13DZ1101502) and Tribology Science Fund of State Key Laboratory of Tribology of Tsinghua University (No.SKLT2015A02)
The improvement of steam parameters in fossil power plants requires the development of new kinds of 9% Cr martensitic heat-resistant steels, among which FB2 steel is a 100×10-6 (mass fraction) boron-containing steel and mainly used for manufacturing components with thick walls operating at high temperatures above 600 ℃. In the alloy system of martensitic heat-resistant steels, boron plays an important role in suppressing type IV crack of weld joints by the formation of heat affected zone (HAZ) with no fine grains in the normalized and intercritical zones, where there exhibit fine grains in conventional 9%Cr heat-resistant steels with no boron such as P91 steel. In this work, the formation process of HAZ in FB2 steel was investigated. The microstructures before and after thermal simulation were compared using OM and SEM. It was concluded that the austenization of FB2 steel at rapid heating rates (≥100 ℃/s) took place by shear mechanism, demonstrating austenite memory effect; while at slow heating rates (≤5 ℃/s), the austenization was by atom short range diffusion mechanism, without austenite memory effect. The special phase transformation of austenization is the main cause for the formation of HAZ with no coarsened grain in the overheated zone. Based on the previous results reported by other researchers, a preliminary model was proposed to describe how boron atoms change the austenite transformation type of FB2 steel during heating process, which developed the previous ideas about the phenomenon.
Key words: FB2 steel; welding; martensitic transformation; austenite memory effect; boron
Kejian LI , Zhipeng CAI , Yao WU , Jiluan PAN . Research on Austenite Transformation of FB2 Heat-Resistant Steel During Welding Heating Process[J]. Acta Metall Sin, 2017 , 53(7) : 778 -788 . DOI: 10.11900/0412.1961.2016.00521
| [1] | Lo K H, Shek C H, Lai J K L. Recent developments in stainless steels[J]. Mater. Sci. Eng., 2009, R65: 39 |
| [2] | Fujita T.Current progress in advanced high Cr ferritic steels for high-temperature applications[J]. ISIJ Int., 1992, 32: 175 |
| [3] | Semba H, Abe F.Alloy design and creep strength of advanced 9%Cr USC boiler steels containing high concentration of boron[J]. Energy Mater., 2006, 1: 238 |
| [4] | Albert S K, Kondo M, Tabuchi M, et al.Improving the creep properties of 9Cr-3W-3Co-NbV steels and their weld joints by the addition of boron[J]. Metall. Mater. Trans., 2005, 36A: 333 |
| [5] | Abe F, Tabuchi M, Tsukamoto S, et al. Microstructure evolution in HAZ and suppression of type IV fracture in advanced ferritic power plant steels [J]. Int. J. Press. Vessels Piping, 2010, 87: 598 |
| [6] | Kondo M, Tabuchi M, Tsukamoto S, et al.Suppressing type IV failure via modification of heat affected zone microstructures using high boron content in 9Cr heat resistant steel welded joints[J]. Sci. Technol. Weld. Join., 2006, 11: 216 |
| [7] | Abson D J, Rothwell J S.Review of type IV cracking of weldments in 9-12%Cr creep strength enhanced ferritic steels[J]. Int. Mater. Rev., 2013, 58: 437 |
| [8] | Francis J A, Mazur W, Bhadeshia H K D H. Review type IV cracking in ferritic power plant steels[J]. Mater. Sci. Technol., 2006, 22: 1387 |
| [9] | Shirane T, Tsukamoto S, Tsuzaki K, et al.Ferrite to austenite reverse transformation process in B containing 9%Cr heat resistant steel HAZ[J]. Sci. Technol. Weld. Join., 2009, 14: 698 |
| [10] | Das C R, Albert S K, Swaminathan J, et al.Transition of crack from type IV to type II resulting from improved utilization of boron in the modified 9Cr-1Mo steel weldment[J]. Metall. Mater. Trans., 2012, 43A: 3724 |
| [11] | Das C R, Bhaduri A K, Lakshmi S, et al.Influence of boron and nitrogen on microstructure and hardness of heat-affected zone of modified 9Cr-1Mo steel——gleeble simulation study[J]. Weld. World, 2015, 59: 513 |
| [12] | Mayr P.Evolution of microstructure and mechanical properties of the heat affected zone in B-containing 9% chromium steels [D]. Graz: Graz University of Technology, 2007 |
| [13] | Kimmins S T, Gooch D J.Austenite memory effect in 1Cr-1Mo-0.75V(Ti, B) steel[J]. Met. Sci., 1983, 17: 519 |
| [14] | Cai Q G, Zhu J, He C Z.Aging structure of maraging steel[J]. Acta Phys. Sin., 1974, 23: 178 |
| [14] | (蔡其巩, 朱静, 何崇智. 马氏体时效钢的时效结构[J]. 物理学报, 1974, 23: 178) |
| [15] | Kessler H, Pitsch W.On the nature of the martensite to austenite reverse transformation[J]. Acta Metall., 1967, 15: 401 |
| [16] | Banerjee B R, Hauser J J, Capenos J M.Role of cobalt in the marage-type alloy matrix[J]. Met. Sci. J., 1968, 2: 76 |
| [17] | Apple C A, Krauss G.The effect of heating rate on the martensite to austenite transformation in Fe-Ni-C alloys[J]. Acta Metall., 1972, 20: 849 |
| [18] | Lee S J, Park Y M, Lee Y K.Reverse transformation mechanism of martensite to austenite in a metastable austenitic alloy[J]. Mater. Sci. Eng., 2009, A515: 32 |
| [19] | Liu Z C, Ren H P, An S L, et al.Martensite Transformation [M]. Beijing: Science Press, 2012: 25 |
| [19] | (刘宗昌, 任慧平, 安胜利等. 马氏体相变 [M]. 北京: 科学出版社, 2012: 25) |
| [20] | Karlyn D A, Cahn J W, Cohen M.The massive transformation in copper-zinc alloys [A]. The Selected Works of John W. Cahn[M]. Warrendale, Pennsylvania: TMS, 1969: 237 |
| [21] | Dayananda M A.6.2 Solutions of diffusion equations for constant ternary interdiffusion coefficients [A]. Mehrer H. Diffusion in Solid Metals and Alloys[M]. Berlin Heidelberg: Springer, 1990, 26: 372. |
| [22] | Zhao L, Jing H Y, Xu L Y, et al.Investigation on mechanism of type IV cracking in P92 steel at 650 ℃[J]. J. Mater. Res., 2011, 26: 934 |
| [23] | Abe F, Kern T U, Viswanathan R.Creep-Resistant Steels [M]. New York: CRC Press, 2008: 243 |
| [24] | Zhou Z F, Zhang W Y.Welding Metallurgy and Metal Weldability [M]. 2nd Ed., Beijing: China Machine Press, 1988: 207 |
| [24] | (周振丰, 张文钺. 焊接冶金与金属焊接性 [M]. 第2版, 北京: 机械工业出版社, 1988: 207) |
| [25] | Abe F.Effect of boron on microstructure and creep strength of advanced ferritic power plant steels[J]. Procedia Eng., 2011, 10: 94 |
| [26] | Wang X M, He X L.Effect of boron addition on structure and properties of low carbon bainitic steels[J]. ISIJ Int., 2002, 42: S38 |
/
| 〈 |
|
〉 |