Orginal Article

Preparation of Micro Porous Stainless Steel by Physical Vacuum Dealloying

  • Jun LI ,
  • Wenpeng LIU ,
  • Yibin REN ,
  • Minggang SHEN ,
  • Ke YANG
Expand
  • 1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 School of Materials Science and Engineering, University of Science and Technology of China, Hefei 230026, China
    3 School of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051, China

Received date: 2016-06-27

  Online published: 2017-02-24

Supported by

Supported by National Natural Science Foundation of China (No.31370976) and National Basic Research Program of China (No.2012CB619101)

Abstract

More and more attentions have been paid to porous stainless steel, as the excellent performance in the physical, chemical and mechanical properties, in the field of solid oxide fuel cell, medical drug for implantable devices and so on. In this work, a new method called physical vacuum dealloying has been applied to produce porous stainless steel. Firstly, 316L-50Mn initial alloy was successfully melted by vacuum induction furnace, then the porous stainless steel was developed by 316L-50Mn after heat treatment in vacuum environment in this experiment. SEM, EDS and XRD were used to analyze the porous stainless steel made by physical vacuum dealloying method. Meanwhile, the effects of temperature and time on the formation, development and morphology of pores during the dealloying process were also studied. The results show that it was effective to produce porous stainless steel by physical vacuum dealloying method. The porosity of micro pores in porous stainless steel is 30%~60%, with 0.5~3 μm pore size, and the 15~60 μm thickness. The temperature mainly affects the hole formation and development by influencing the evaporation and bulk diffusion rate of Mn element, and time plays a major role in the thickness of the porous layer in the process of preparing porous stainless steel.

Cite this article

Jun LI , Wenpeng LIU , Yibin REN , Minggang SHEN , Ke YANG . Preparation of Micro Porous Stainless Steel by Physical Vacuum Dealloying[J]. Acta Metall Sin, 2017 , 53(5) : 524 -530 . DOI: 10.11900/0412.1961.2016.00260

References

[1] Kato K, Yamamoto K, Ochiai S, et al.Cytocompatibility and mechanical properties of novel porous 316 L stainless steel[J]. Mater. Sci. Eng., 2013, C33: 2736
[2] Yu Z J, Chen Y Q, Yang X D.Effective adsorption of functional biological macromolecules on stainless steel surface with micro/nanoporous texture[J]. Acta Phys.-Chim. Sin., 2013, 29: 1595
[3] Molin S, Gazda M, Kusz B, et al.Evaluation of 316 L porous stainless steel for SOFC support[J]. J. Eur. Ceram. Soc., 2009, 29: 757
[4] Xu G R, Peng M Z, Tang A P, et al.Fabrication and capacitive characteristics of a porous stainless steel-supported MnO2 thin film electrode[J]. Chin. J. Appl. Chem., 2011, 28: 815
[4] (徐国荣, 彭满芝, 唐安平等. 多孔不锈钢基二氧化锰薄膜电极的制备及电容特性[J]. 应用化学, 2011, 28: 815)
[5] Luiten-Olieman M W J, Winnubst L, Nijmeijer A, et al. Porous stainless steel hollow fiber membranes via dry-wet spinning[J]. J. Membr. Sci., 2011, 370: 124
[6] Li Z J, Jin Q L, Yang T W, et al.Fabrication of lotus-type porous Cu-Zn alloys with the Gasar continuous casting process[J] Acta. Metall. Sin., 2013, 49: 757
[6] (李再久, 金青林, 杨天武等. Gasar连铸工艺制备藕状多孔Cu-Zn合金[J]. 金属学报, 2013, 49: 757)
[7] Gao H Y, Jia Y H, Shen P Z, et al.Preparation of porous FeAl material[J]. Chin. J. Mater. Res., 2008, 22: 485
[7] (高海燕, 贾跃辉, 沈培智等. FeAl金属间化合物多孔材料的制备[J]. 材料研究学报, 2008, 22: 485)
[8] Bakan H I.A novel water leaching and sintering process for manufacturing highly porous stainless steel[J]. Scr. Mater., 2006, 55: 203
[9] Chi Y D, Tang H P, Wang Q B, et al.Preparation of stainless steel porous filter tube by powder extrusion molding and sintering[J]. Powder Metall. Technol., 2011, 29: 34
[9] (迟煜頔, 汤慧萍, 汪强兵等. 增塑挤压法制备不锈钢多孔过滤管[J]. 粉末冶金技术, 2011, 29: 34)
[10] Shen Y F, Wu P, Gu D D, et al.Micropore structures of lotus-type porous 316 stainless steel prepared by laser sintering[J]. Acta Aeronaut. Astronaut. Sin., 2007, 28: 1236
[10] (沈以赴, 吴鹏, 顾冬冬等. 激光烧结制备藕状316不锈钢多孔材料的微孔结构特征[J]. 航空学报, 2007, 28: 1236)
[11] Wada T, Kato H.Three-dimensional open-cell macroporous iron, chromium and ferritic stainless steel[J]. Scr. Mater., 2013, 68: 723
[12] Tsuchiya H, Suzumura T, Terada Y, et al.Formation of self-organized pores on type 316 stainless steel in organic solvents[J]. Electrochim. Acta, 2012, 82: 333
[13] Wang Y J, Ma X X, Tang G Z, et al.Forming micro-pores for drug loading on medical 316L stainless steel[J]. Bull. Chin. Ceram. Soc., 2009, 28(spec. issue): 29
[13] (王玉江, 马欣新, 唐光泽等. 医用316L不锈钢表面载药微孔制备技术[J]. 硅酸盐通报, 2009, 28(特刊): 29)
[14] Ren Y B, Tong M, Xiao K S, et al.Preparation method for novel porous iron-base alloy [P]. Chin Pat., 201410182792.9, 2014
[14] (任伊宾, 佟敏, 肖克沈等. 一种新型多孔铁基合金的制备方法 [P]. 中国专利, 201410182792.9, 2014)
[15] Sun Y X, Ren Y B, Yang K.New preparation method of micron porous copper through physical vacuum dealloying of Cu-Zn alloys[J]. Mater. Lett., 2016, 165: 1
[16] Sun Y X, Ren Y B.New preparation method of porous copper powder through vacuum dealloying[J]. Vacuum, 2015, 122: 215
[17] Ren H L.Technology of Metallographic Experiment [M]. Beijing: Metallurgical Industry Press, 1992: 1
[17] (任怀亮. 金相实验技术 [M]. 北京: 冶金工业出版社, 1992: 1)
[18] Lu X, Sun Z, Li Z Q, et al.Study of Ni-Mn alloy dealloying[J]. J. Dalian Jiaotong Univ., 2012, 33(6): 81(陆兴, 孙钊, 李志强等. Ni-Mn合金的去合金化 [J]. 大连交通大学学报, 2012, 33(6): 81)
[19] Erlebacher J, Aziz M J, Karma A, et al.Evolution of nanoporosity in dealloying[J]. Nature, 2001, 410: 450
[20] Ma W J, Ke C B, Zhou M B, et al.Phase-field crystal simulation on evolution and growth kinetics of kirkendall voids in interface and intermetallic compound layer in Sn/Cu soldering system[J]. Acta. Metall. Sin., 2015, 51: 873
[20] (马文婧, 柯常波, 周敏波等. Sn/Cu互连体系界面和金属间化合物层Kirkendall空洞演化和生长动力学的晶体相场法模拟[J]. 金属学报, 2015, 51: 873)
[21] Kubaschewski O, Evans E L, Alcock C B.Metallurgical Thermochemistry [M]. 4th Ed., London: Pergamon Press, 1967: 5
[22] Paul A, van Dal1 M J H, Kodentsov A A, et al. The Kirkendall effect in multiphase diffusion[J]. Acta Mater., 2004, 52: 623
[23] Shi Q Y, Li X H, Zheng Y R, et al.Formation of solidification and homogenisation micropores in two single crystal superalloys produced by HRS and LMC processes[J]. Acta. Metall. Sin., 2012, 48: 1237
[23] (石倩颖, 李相辉, 郑运荣等. HRS和LMC工艺制备的两种镍基单晶高温合金铸态及固溶微孔的形成[J]. 金属学报, 2012, 48: 1237)
[24] Guo J J, Fu H Z.Alloy Melt and Its Treatment [M]. Beijing: Chinese Machine Press, 2005: 97
[24] (郭景杰, 傅恒志. 合金熔体及其处理 [M]. 北京: 机械工业出版社, 2005: 97)
[25] Brandes E A, Brook G B.Smithells Metals Reference Book[M]. 7th Ed., Boston: Butterworth-Heinemann, 1998: 1
[26] Yu Y N.Principles of Metallurgy [M]. Beijing: Metallurgical Industry Press, 2000: 210
[26] (余永宁. 金属学原理 [M]. 北京: 冶金工业出版社, 2000: 210)
[27] Honig R E, Kramer D A.Vapor Pressure Data for the Solid and Liquid Elements[M]. New York: RCA Laboratories, David Sarnoff Research Center, 1969: 285
Outlines

/