Orginal Article

Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel

  • Hai ZHANG ,
  • Shilei LI ,
  • Gang LIU ,
  • Yanli WANG
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2016-07-20

  Online published: 2017-02-23

Supported by

Supported by National Natural Science Foundation of China (No.51601013) and State Key Lab for Advanced Metals and Materials (No.2015-ZD09)

Abstract

Duplex stainless steels are widely used in nuclear industry for their excellent mechanical behavior, good weldability and superior ressistance to corrosion, the fracture toughness of which will be deteriorated with ageing time, as they are exposed to a certain temperature (204~538 ℃). In the present work, hot forging will be employed to induce the change of ferrite grain orientation and refinement of austenite grains; it is expected to improve the impact toughness after long-term thermal ageing. The microstructure and impact surface morphology of Z3CN20-09M duplex stainless steel were investigated by using SEM and EBSD. The micro-mechanical properties and impact properties of Z3CN20-09M duplex stainless steel at different thermal ageing time were tested by a nano-indenter and an instrumented impact tester. The results show that the crystal orientation of ferrite changes obviously and the austenite is changed from the original coarse columnar grains to the fine equiaxed grains after hot working. The im pact toughness of cast materials and forged materials decreases greatly with ageing time. The charpy impact energy of both aged and unaged forged-materials is higher than that of cast material. Cast material and forged material exhibit microvoid coalescence fracture in the early of thermal ageing; after 3000 h thermal ageing, the impact fracture features changes from ductile dimples to brittle cleavages in ferrites and tearings or dimples in austenites. However, cleavage features in forged material are significantly less than those in cast material due to the difference in ferrite crystal orientation.

Cite this article

Hai ZHANG , Shilei LI , Gang LIU , Yanli WANG . Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel[J]. Acta Metall Sin, 2017 , 53(5) : 531 -538 . DOI: 10.11900/0412.1961.2016.00321

References

[1] Wu J.Duplex Stainless Steel [M]. Beijing: Metallurgy Industry Press, 1991: 1
[1] (吴玖. 双相不锈钢 [M]. 北京: 冶金工业出版社, 1991: 1)
[2] Chung H M.Aging and life prediction of cast duplex stainless steel components[J]. Int. J. Pressure Vessels Piping, 1992, 50: 179
[3] Hau?ild P, Berdin C, Bompard P, et al.Ductile fracture of duplex stainless steel with casting defects[J]. Int. J. Pressure Vessels Piping, 2001, 78: 607
[4] Clark C A, Guha P.Improvements in corrosion resistance, mechanical properties, and weldability of duplex austenitic/ferritic steels[J]. Mater. Corros., 1983, 34: 27
[5] Tucker J D, Miller M K, Young G A.Assessment of thermal embrittlement in duplex stainless steels 2003 and 2205 for nuclear power applications[J]. Acta Mater., 2015, 87: 15
[6] Weng K L, Chen H R, Yang J R.The low-temperature aging embrittlement in a 2205 duplex stainless steel[J]. Mater. Sci. Eng., 2004, A379: 119
[7] Yao Y H, Wei J F, Wang Z P, et al.Effect of long-term thermal aging on the mechanical properties of casting duplex stainless steels[J]. Mater. Sci. Eng., 2012, A551: 116
[8] Here?ú S, Sennour M, Balbi M, et al.Influence of dislocation glide on the spinodal decomposition of fatigued duplex stainless steels[J]. Mater. Sci. Eng., 2011, A528: 7636
[9] Li S L, Wang Y L, Li S X, et al.Microstructures and mechanical properties of cast austenite stainless steels after long-term thermal aging at low temperature[J]. Mater. Des., 2013, 50: 886
[10] Miller M K, Hyde J M, Cerezo A, et al.Comparison of low temperature decomposition in Fe-Cr and duplex stainless steels[J].
[10] Appl. Surf. Sci., 1995, 87-88: 323
[11] Sahu J K, Krupp U, Ghosh R N, et al.Effect of 475 ℃ embrittlement on the mechanical properties of duplex stainless steel[J]. Mater. Sci. Eng., 2009, A508: 1
[12] Kawaguchi S, Sakamoto N, Takano G, et al.Microstructural changes and fracture behavior of CF8M duplex stainless steels after long-term aging[J]. Nucl. Eng. Des., 1997, 174: 273
[13] Li S L.Thermal aging of Z3CN20-09M steels in the primary circuit piping of nuclear power plants [D]. Beijing: University of Science and Technology Beijing, 2013
[13] (李时磊. 核电站一回路管道Z3CN20-09M不锈钢的热老化研究 [D]. 北京: 北京科技大学, 2013)
[14] Li S L, Wang Y L, Zhang H L, et al.Microstructure evolution and impact fracture behaviors of Z3CN20-09M stainless steels after long-term thermal aging[J]. J. Nucl. Mater., 2013, 433: 41
[15] Kokawa H, Shimada M, Michiuchi M, et al.Arrest of weld-decay in 304 austenitic stainless steel by twin-induced grain boundary engineering[J]. Acta Mater., 2007, 55: 5401
[16] West E A, Was G S.IGSCC of grain boundary engineered 316L and 690 in supercritical water[J]. J. Nucl. Mater., 2009, 392: 264
[17] Shi F, Li X W, H Y T, et al. Optimization of grain boundary character distribution in Fe-18Cr-18Mn-0.63N high-nitrogen austenitic stainless steel[J]. Acta Metall. Sin.(Engl. Lett.), 2013, 26: 497
[18] Shimada M, Kokawa H, Wang Z J, et al.Optimization of grain boundary character distribution for intergranular corrosion resistant 304 stainless steel by twin-induced grain boundary engineering[J]. Acta Mater., 2002, 50: 2331
[19] Tsurekawa S, Nakamichi S, Watanabe T.Correlation of grain boundary connectivity with grain boundary character distribution in austenitic stainless steel[J]. Acta Mater., 2006, 54: 3617
[20] Hu G X, Cai X, Rong Y H.Fundamentals of Materials Science [M]. 3rd Ed., Shanghai: Shanghai Jiao Tong University Press, 2010: 3
[20] (胡赓祥, 蔡珣, 戎咏华. 材料科学基础 [M]. 第3版, 上海: 上海交通大学出版社, 2010: 3)
[21] Li S L, Wang Y L, Wang X T, et al.Effects of ferrite content on the mechanical properties of thermal aged duplex stainless steels[J]. Mater. Sci. Eng., 2015, A625: 186
[22] Timofeev B T, Nikolaev Y K.About the prediction and assessment of thermal embrittlement of Cr-Ni austenitic-ferritic weld metal and castings at the ageing temperatures 260-425 ℃[J]. Int. J. Pressure Vessels Piping, 1999, 76: 849
[23] Li S L, Wang Y L, Zhang H L, et al.Effects of prior solution treatment on thermal aging behavior of duplex stainless steels[J]. J. Nucl. Mater., 2013, 441: 337
[24] Pettersson N, Wessman S, Thuvander M, et al.Nanostructure evolution and mechanical property changes during aging of a super duplex stainless steel at 300 ℃[J]. Mater. Sci. Eng., 2016, A647: 241
[25] Li S L, Wang Y L, Li S X, et al.Effect of long term aging on the microstructure and mechanical properties of cast austenitic stainless steels[J]. Acta Metall. Sin., 2010, 46: 1186
[25] (李时磊, 王艳丽, 李树肖等. 长期热老化对铸造奥氏体不锈钢组织和性能的影响[J]. 金属学报, 2010, 46: 1186)
[26] Zheng K, Wang Y L, Li S L, et al.The microstructure and tensile fracture behavior of long term thermal aged Z3CN20-09M stainless steel[J]. Acta Metall. Sin., 2013, 49: 175
[26] (郑凯, 王艳丽, 李时磊等. 长期热老化后Z3CN20-09M不锈钢的微观组织与拉伸断裂行为[J]. 金属学报, 2013, 49: 175)
[27] Ghosh A, Kundu S, Chakrabarti D.Effect of crystallographic texture on the cleavage fracture mechanism and effective grain size of ferritic steel[J]. Scr. Mater., 2014, 81: 8
Outlines

/