Precipitation Behavior of
Received date: 2016-11-14
Online published: 2017-02-17
Supported by
Supported by National Natural Science Foundation of China (No.51661019) and Science and Technology Project of Gansu Province (No.145RTSA004)
GH3625 alloy is a wrought nickel-based superalloy mainly used in aeronautical, aerospace, chemical, nuclear, petrochemical, and marine applications industry due to its good mechanical properties, processability, weldability and resistance to high-temperature corrosion on prolonged exposure to aggressive environments. However, in medium and high temperature environment during long-term service, the γ'' is a metastable phase, easily transformed into stable δ phase, or δ phase directly formed in the γ matrix so that alloy performance was deteriorated, leading to the result of alloy failure. At the present work, mass fraction of δ phase in GH3625 superalloy hot-extruded tube cold deformed to different reductions and then aged at 800 ℃ for different times, were measured by XRD. The effect of cold deformation on the law and kinetics of δ phase precipitation was investigated by SEM, EDS and Image-Pro Plus metallographic analysis. The results show that δ phase first precipitates at the deformation twin and grain boundaries as well as deformation bands, and then precipitates in the grains. The amount of δ phase at the deformation bands increases with the increase of cold deformation. The morphologies of δ phase change gradually from needles to spheroids or rodlike with increasing cold deformation. With the extend of ageing time, the average size of δ phase increases which grows according to LSW theory. At 800 ℃, the relationship between the precipitation content of δ phase and ageing time follows Avrami equation. As cold deformation increases, the content of δ phase increases, the time index n decreases, whereas the δ phase precipitation rate increases. Cold deformation promotes the precipitation of δ phase. The solute drags of Nb in soild solution and pinning of δ phase inhibits the grain growth during ageing process of cold deformed GH3625 superalloy hot-extruded tube. The hardness of the alloy increases with the extension of the holding time at ε =35% but no obvious change at ε ≥50%.
Key words: GH3625 superalloy; cold deformation; δphase; precipitation behavior; kinetics
Yutian DING
,
Yubi GAO
,
Zhengyi DOU
,
Xin GAO
,
Dexue LIU
,
Zhi JIA
. Precipitation Behavior of
| [1] | Guo J T.Materials Science and Engineering for Superalloys (Book 1) [M]. Beijing: Science Press, 2008: 342 |
| [1] | (郭建亭. 高温合金材料学(上册) [M]. 北京: 科学出版社, 2008: 342) |
| [2] | Murr L E, Martinez E, Gaytan S M, et al.Microstructural architecture, microstructures, and mechanical properties for a nickel-base superalloy fabricated by electron beam melting[J]. Metall. Mater. Trans., 2011, 42A: 3491 |
| [3] | China Aeronautical Materials Handbook Compile Committee. China Aeronautical Materials Handbook [M]. 2nd Ed., Beijing: Standards Press of China, 2002 |
| [3] | (中国航空材料手册编委会. 中国航空材料手册 [M]. 第2版, 北京: 中国标准出版社, 2002) |
| [4] | Paul C P, Ganesh P, Mishra S K, et al.Investigating laser rapid manufacturing for Inconel-625 components[J]. Opt. Laser Technol., 2007, 39: 800 |
| [5] | Mittra J, Dubey J S, Banerjee S.Acoustic emission technique used for detecting early stages of precipitation during aging of Inconel 625[J]. Scr. Mater., 2003, 49: 1209 |
| [6] | Ye J.Nickel Base Superalloy [M]. Beijing: Science Press, 1978: 228 |
| [6] | (冶军. 美国镍基高温合金 [M]. 北京: 科学出版社, 1978: 228) |
| [7] | Zhang H B.Inconel 625 alloy progress abroad[J]. Spec. Steel Technol., 2000(3): 69 |
| [7] | (张红斌. 国外Inconel 625合金的进展[J]. 特钢技术, 2000(3): 69) |
| [8] | Cortial F, Corrieu J M, Vernot-Loier C.Influence of heat treatments on microstructure, mechanical properties, and corrosion resistance of weld alloy 625[J]. Metall. Mater. Trans., 1995, 26A: 1273 |
| [9] | Suave L M, Cormier J, Villechaise P, et al.Microstructural evolutions during thermal aging of alloy 625: Impact of temperature and forming process[J]. Metall. Mater. Trans., 2014, 45A: 2963 |
| [10] | Sundararaman M, Mukhopadhyay P, Banerjee S.Precipitation of the δ-Ni3Nb phase in two nickel base superalloys[J]. Metall. Mater. Trans., 1988, 19A: 453 |
| [11] | Di X J, Xing X X, Wang B S.Nucleation and coarsening mechanism of δ phase in Inconel 625 deposited metal[J]. Acta Metall. Sin., 2014, 50: 323 |
| [11] | (邸新杰, 邢希学, 王宝森. Inconel 625熔敷金属中δ相的形核与粗化机理[J]. 金属学报, 2014, 50: 323) |
| [12] | Chen M H, He Y Q.Quantitative phase analysis of γ''-Ni3Nb、δ-Ni3Nb and other phases in superalloy GH-625 by X-ray diffraction[J]. Metall. Anal., 1989, 9(2): 1 |
| [12] | (陈名浩, 何银秋. 镍基合金中γ''-Ni3Nb和δ-Ni3Nb等相的衍射定量相分析[J]. 冶金分析, 1989, 9(2): 1) |
| [13] | Zhao Y X.Cold deformation behaviors of GH625 alloy and their effects on the mechanical properties[J]. J. Mater. Eng., 2000, (9): 36 |
| [13] | (赵宇新. GH625合金的冷变形及其对力学性能的影响[J]. 材料工程, 2000, (9): 36) |
| [14] | Floreen S, Fuchs G E, Yang W J.The metallurgy of alloy 625 [A]. Superalloys 718625706 and Various Derivatives[M]. Warrendale, PA: TMS, 1994: 13 |
| [15] | Shoemaker L E.Alloys 625 and 725: Trends in properties and applications [A]. Superalloys 718, 625, 706 and Derivatives 2005[M]. Warrendale, PA: TMS, 2005: 409 |
| [16] | Liu W C, Xiao F R, Yao M, et al.Quantitative phase analysis of Inconel 718 by X-ray diffraction[J]. J. Mater. Sci. Lett., 1997, 16: 769 |
| [17] | Singh R P, Hyzak J M, Howson T E, et al.Recrystallization behavior of cold rolled alloy 718 [A]. Superalloys 718 and 625 and Various Derivatives[C]. Warrendale, PA: TMS, 1991: 205 |
| [18] | Liu W C, Yao M, Chen Z L, et al.Niobium segregation in Inconel 718[J]. J. Mater. Sci., 1999, 34: 2583 |
| [19] | Liu W C, Chen Z L, Xiao F R, et al.Effect of cold rolling on the precipitation behavior of δ phase and γ'' phase in Inconel 718[J]. Acta Aeronaut. Astronaut. Sin., 1999, 20: 279 |
| [19] | (刘文昌, 陈宗霖, 肖福仁等. 冷轧变形对Inconel 718合金δ相γ''相析出行为的影响[J]. 航空学报, 1999, 20: 279) |
| [20] | Ka?etas P J P, Osorio L A R, Mata M P G, et al. Influence of the delta phase in the microstructure of the Inconel 718 subjected to "delta-processing" heat treatment and hot deformed[J]. Proc. Mater. Sci., 2015, 8: 1160 |
| [21] | Liu W C, Yao M, Xiao F R, et al.Determination of δ phase fraction and precipitation behaviour of δ phase in Inconel 718 alloy[J]. Iron Steel, 1997, 32(5): 55 |
| [21] | (刘文昌, 姚枚, 肖福仁等. Inconel 718合金δ相含量的测定及δ相析出[J]. 钢铁, 1997, 32(5): 55) |
| [22] | Footner P K, Richards B P.Long-term growth of superalloy γ'′ particles[J]. J. Mater. Sci., 1982, 17: 2141 |
| [23] | Smallman R E, translated by Zhang R J. Modern Physical Metallurgy [M]. Beijing: Metallurgical Industry Press, 1980: 176 |
| [23] | (Smallman R E著, 张人佶译. 现代物理冶金学 [M]. 北京: 冶金工业出版社, 1980: 176) |
| [24] | Avrami M.Kinetics of phase change. II Transformation-time relations for random distribution of nuclei[J]. J. Chem. Phys., 1940, 8: 212 |
| [25] | Yuan Z J, Liu J S, Zhang S H.Research on precipitation kinetics of δ-phase in GH4169 alloy[J]. J. Shenyang Ligong Univ., 2010, 29(2): 23 |
| [25] | (袁兆静, 刘劲松, 张士宏. GH4169合金δ相的析出动力学研究[J]. 沈阳理工大学学报, 2010, 29(2): 23) |
| [26] | Liu W C, Chen Z L, Xiao F R, et al.Effect of cold rolling on the kinetics of δ phase precipitation in Inconel 718[J]. Acta Metall. Sin., 1998, 34: 1049 |
| [26] | (刘文昌, 陈宗霖, 肖福仁等. 冷轧变形对Inconel 718合金δ相析出动力学的影响[J]. 金属学报, 1998, 34: 1049) |
| [27] | Cahn J W.Coherent fluctuations and nucleation in isotropic solids[J]. Acta Metall., 1962, 10: 907 |
| [28] | Smith C S.Grains, phases, and interphases: an interpretation of microstructure[J]. Met. Technol., 1948, 175: 15 |
/
| 〈 |
|
〉 |