Orginal Article

Effect of Alternating Current on Corrosion Behavior of X80 Pipeline Steel in Near-Neutral Environment

  • Hongxia WAN ,
  • Dongdong SONG ,
  • Zhiyong LIU ,
  • Cuiwei DU ,
  • Xiaogang LI
Expand
  • 1 Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China
    2 Aerospace Research Institute of Materials & Processing Technology, Beijing 100076, China
    3 Ningbo Institute of Material Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China

Received date: 2016-11-10

  Online published: 2017-02-14

Supported by

Supported by National Natural Science Foundation of China (Nos.51371036, 51131001 and 51471034)

Abstract

The rapid development of energy, electricity, and transportation industries has created a market for steel pipes; however, buried steel pipelines near high-voltage transmission lines and electrified railways often experience alternating current (AC) corrosion at the damaged coating of pipelines; such phenomenon is mostly due to the resistance between the capacitance and inductance coupling, especially for long-distance pipelines in parallel operation. AC corrosion can cause pipeline corrosion perforation and stress corrosion cracking (SCC) in some cases, which has been a vital threat to the pipeline safety. In this work, the influence of AC on corrosion behavior of X80 pipeline steel was investigated in NS4 near-neutral solution by data acquisition technique, electrochemical test, immersion tests and surface analysis techniques. Results show that with the increasing of AC density, corrosion morphology changed from uniform corrosion to localized corrosion with many pits. Under the full AC interference, X80 steel occurred cathodic and anodic polarization which resulted in iron dissolution and hydrogen precipitation. The negative half wave AC would lead to hydrogen evolution and hydrogen induced anodic dissolution, the pits in X80 steel surface present sharp. However, under disturbance of positive half-wave AC, only anodic dissolution occurred and the pitting appeared spill shape and smoothly. Under various AC waveform interference, the corrosion products of X80 steel surface were different. Under full AC wave and positive half-wave interference, the corrosion products were loose, had have no α-FeOOH and occurred cracks; however, under negative half-wave AC interference, the corrosion products were denser and contained α-FeOOH which has protective effect on substrates.

Cite this article

Hongxia WAN , Dongdong SONG , Zhiyong LIU , Cuiwei DU , Xiaogang LI . Effect of Alternating Current on Corrosion Behavior of X80 Pipeline Steel in Near-Neutral Environment[J]. Acta Metall Sin, 2017 , 53(5) : 575 -582 . DOI: 10.11900/0412.1961.2016.00500

References

[1] Tribollet B, Meyer M.2-AC-induced corrosion of underground pipelines [A]. Orazem M. Undergr Pipeline Corrosion [M]. Amsterdam: Woodhead Publishing Limited, 2014: 35
[2] Roger F.Testing and mitigation of AC corrosion on 8 line: a field study [A]. Corrosion 2004[C]. New Orleans, Louisiana: NACE International, 2004
[3] Zhang R, Vairavanathan P R, Lalvani S B.Perturbation method analysis of AC-induced corrosion[J]. Corros. Sci., 2008, 50: 1664
[4] Wakelin R G, Sheldon C.Investigation and mitigation of AC corrosion on a 300 MM natural gas pipeline [A]. Corrosion 2004[C]. New Orleans, Louisiana: NACE International, 2004: 972
[5] Zhu M, Du C W, Li X G, et al.Effect of AC current density on stress corrosion cracking behavior of X80 pipeline steel in high pH carbonate/bicarbonate solution[J]. Electrochim. Acta, 2014, 117: 351
[6] Tang D Z, Du Y X, Li X X, et al.Effect of alternating current on the performance of magnesium sacrificial anode[J]. Mater. Des., 2016, 93: 133
[7] Zhu M, Du C W, Li X G, et al.Effect of AC on stress corrosion cracking behavior and mechanism of X80 pipeline steel in carbonate/bicarbonate solution[J]. Corros. Sci., 2014, 87: 224
[8] Zhu M, Liu Z Y, Du C W, et al.Effects of alternating current on corrosion behavior of X80 pipeline steel in acid soil environment[J]. J. Mater. Eng., 2015, 43: 85
[8] (朱敏, 刘智勇, 杜翠薇等. 交流电对X80钢在酸性土壤环境中腐蚀行为的影响[J]. 材料工程, 2015, 43: 85)
[9] Lalvani S B, Zhang G.The corrosion of carbon steel in a chloride environment due to periodic voltage modulation: Part I[J]. Corros. Sci., 1995, 37: 1567
[10] Jones D A.Effect of alternating current on corrosion of low alloy and carbon steels[J]. Corrosion, 1978, 34: 428
[11] Kulman F E.Effects of alternating currents in causing corrosion[J]. Corrosion, 1961, 17: 34
[12] Bosch R W, Bogaerts W F.A theoretical study of AC-induced corrosion considering diffusion phenomena[J]. Corros. Sci., 1998, 40: 323
[13] Nielsen L V.Role of alkalization in AC induced corrosion of pipelines and consequences hereof in relation to CP requirements [A]. Corrosion 2005[C]. Houston, Texas: NACE International, 2005
[14] Xu L Y, Su X, Yin Z X, et al.Development of a real-time AC/DC data acquisition technique for studies of AC corrosion of pipelines[J]. Corros. Sci., 2012, 61: 215
[15] Lalvani S B, Lin X A.A theoretical approach for predicting AC-induced corrosion[J]. Corros. Sci., 1994, 36: 1039
[16] Lalvani S B, Lin X.A revised model for predicting corrosion of materials induced by alternating voltages[J]. Corros. Sci., 1996, 38: 1709
[17] Fu A Q, Cheng Y F.Effects of alternating current on corrosion of a coated pipeline steel in a chloride-containing carbonate/bicarbonate solution[J]. Corros. Sci., 2010, 52: 612
[18] Linhardt P, Ball G.AC corrosion: results from laboratory investigations and from a failure analysis [A]. Proceedings of the NACE International Corrosion/2006 Conference Papers on CD-ROM[C]. San Diego, CA: NACE, 2006
[19] Goidanich S, Lazzari L, Ormellese M.AC corrosion. Part 2: Parameters influencing corrosion rate[J]. Corros. Sci., 2010, 52: 916
[20] Jiang Z T, Du Y X, Dong L, et al.Effect of AC current on corrosion potential of Q235 steel[J]. Acta Metall. Sin., 2011, 47: 997
[20] (姜子涛, 杜艳霞, 董亮等. 交流电对Q235钢腐蚀电位的影响规律研究[J]. 金属学报, 2011, 47: 997)
[21] Yang Y, Li Z L, Wen C.Effects of alternating current on X70 steel morphology and electrochemical behavior[J]. Acta Metall. Sin., 2013, 49: 43
[21] (杨燕, 李自力, 文闯. 交流电对X70钢表面形态及电化学行为的影响[J]. 金属学报, 2013, 49: 43)
[22] Wan H X, Du C W, Liu Z Y, et al.The effect of hydrogen on stress corrosion behavior of X65 steel welded joint in simulated deep sea environment[J]. Ocean Eng., 2016, 114: 216
[23] Li M C, Cheng Y F.Mechanistic investigation of hydrogen-enhanced anodic dissolution of X-70 pipe steel and its implication on near-neutral pH SCC of pipelines[J]. Electrochim. Acta, 2007, 52: 8111
[24] Fu A Q, Cheng Y F.Effect of alternating current on corrosion and effectiveness of cathodic protection of pipelines[J]. Can. Metall. Quart., 2012, 51: 81
[25] Zhang G A, Cheng Y F.On the fundamentals of electrochemical corrosion of X65 steel in CO2-containing formation water in the presence of acetic acid in petroleum production[J]. Corros. Sci., 2009, 51: 87
[26] Kuang D, Cheng Y F.Understand the AC induced pitting corrosion on pipelines in both high pH and neutral pH carbonate/bicarbonate solutions[J]. Corros. Sci., 2014, 85: 304
Outlines

/