Effect of Sb-Rich Intermetallic Phase on the CorrosionResistance of Zn Alloy in Near-Neutral and Acidic Solutions
Received date: 2016-09-21
Online published: 2016-12-23
Supported by
Supported by National Natural Science Foundation of China (No.51571201)
In the process of hot-dip galvanizing, some beneficial alloying elements are deliberately added to the molten Zn bath, in order to improve the coating properties, such as formability and corrosion resistance. Sb is one of the interesting alloying additions to the Zn bath, as it can decrease the viscosity and the surface tension of the molten Zn, contributing to producing a uniform Zn coating. Due to the low solid solubility of Sb in molten Zn at galvanising temperature, Sb-rich intermetallic particles were always found in the galvanized layers. The presence of Sb-rich phases may affect the structural properties and corrosion performance of galvanized coating. In the literature, it was reported that small addition of Sb has no significant effect on the structure and growth of galvanized layers, but a higher amount (>1%, mass fraction) of Sb can promote the dendritic solidification of Zn. In order to understand the mechanism of Sb addition on the structure and growth of galvanized coating, it is essential to identify the crystal structure of Sb-rich phases. It was reported that the Sb-rich phases found in the η layer of a galvanized coating corresponds to the electron diffraction patterns of Sb2Zn3. However, some researchers hold that the Sb2Zn3 compound does not exist at room temperature, since it can transform to Sb3Zn4 and Zn at some elevated temperature. Consequently, in this work, the structure of Sb-rich intermetallic phase in the Zn-1.2Sb (1.2%Sb) alloy has been investigated by SEM and TEM. SEM/EDS showed that Sb is present in the form of Sb-rich intermatallic phase and there is no detectable Sb in the Zn solid solution. Transmission electron diffractions analysis and EDS results indicated that the composition of Sb-rich intermatallic phases is close to that of Sb2Zn3, whereas the structure is totally different from the latter. The corrosion resistance of Zn-1.2Sb alloy has been analysed by electrochemcial polarization measurements in the different solutions. The analysed results showed that the Sb-rich phase has no obvious effect on the oxygen reduction reaction, in the aerated 0.1 mol/L NaCl (pH=6.5) solution. However, the Sb-rich phase can promote the hydrogen evolution reaction, in the deaerated acidic solution (0.1 mol/L NaCl, pH=3). Corrosion pits were found in the Zn matrix around the Sb-rich phases by SEM observations, which indicate that Zn has higher activity than Zn-Sb phase.
Xiuling SHANG , Bo ZHANG , Wei KE . Effect of Sb-Rich Intermetallic Phase on the CorrosionResistance of Zn Alloy in Near-Neutral and Acidic Solutions[J]. Acta Metall Sin, 2017 , 53(3) : 351 -357 . DOI: 10.11900/0412.1961.2016.00419
| [1] | Frydrych D J.Corrosion mechanisms of zinc-rich organic coatings on steel [D]. Pennsylvania: University of Pennsylvania, 1987 |
| [2] | Zhu L.Hot Dip Galvanizing of Steels [M]. Beijing: Chemical Industry Press, 2005: 28 |
| [2] | (朱立. 钢材热镀锌 [M]. 北京: 化学工业出版社, 2005: 28) |
| [3] | Hosking N C, Str?m M A, Shipway P H, et al.Corrosion resistance of zinc-magnesium coated steel[J]. Corros. Sci., 2007, 49: 3669 |
| [4] | Ramanauskas R, Muleshkova L, Maldonado L, et al.Characterization of the corrosion behaviour of Zn and Zn alloy electrodeposits: Atmospheric and accelerated tests[J]. Corros. Sci., 1998, 40: 401 |
| [5] | Hosny A Y, El-Rafei M E, Ramadan T A, et al. Corrosion resistance of zinc coatings produced from a sulfate bath[J]. Met. Finish., 1995, 93: 55 |
| [6] | Fratesi R, Roventi G, Branca C, et al.Corrosion resistance of Zn-Co alloy coatings[J]. Surf. Coat. Technol., 1994, 63: 97 |
| [7] | Diaz-Ballote L, Ramanauskas R.Improving the corrosion resistance of hot dip galvanized zinc coatings by alloying[J]. Corros. Rev., 1999, 17: 411 |
| [8] | Boshkov N.Galvanic Zn-Mn alloys——electrodeposition, phase composition, corrosion behaviour and protective ability[J]. Surf. Coat. Technol., 2003, 172: 217 |
| [9] | Münz R, Wolf G K, Guzman L, et al.Zinc/manganese multilayer coatings for corrosion protection[J]. Thin Solid Films, 2004, 459: 297 |
| [10] | Leidheiser H Jr, Suzuki I.Technical note: Towards a more corrosion resistant galvanized steel[J]. Corrosion, 1980, 36: 701 |
| [11] | Shang X L, Zhang B, Han E H, et al.The effect of 0.4 wt.% Mn addition on the localized corrosion behaviour of zinc in a long-term experiment[J]. Electrochim. Acta, 2012, 65: 294 |
| [12] | Shang X L, Zhang B, Han E H, et al.Effect of small addition of Mn on the passivation of Zn in 0.1M NaOH solution[J]. Electrochim. Acta, 2011, 56: 1417 |
| [13] | Marder A R.The metallurgy of zinc-coated steel[J]. Prog. Mater. Sci., 2000, 45: 191 |
| [14] | Zhang B, Zhou H B, Han E H, et al.Effects of a small addition of Mn on the corrosion behaviour of Zn in a mixed solution[J]. Electrochim. Acta, 2009, 54: 6598 |
| [15] | Sebisty J J, Palmer R H.The influence of combined additions of tin, cadmium, antimony and copper on the structure and properties of galvanized coatings [A]. Proceedings of 6th International Conference on Hot Dip Galvanizing[C]. London: Zinc Development Association, 1961: 215 |
| [16] | Fasoyino F A, Weinberg F.Spangle formation in galvanized sheet steel coatings[J]. Metall. Trans., 1990, 21B: 549 |
| [17] | Rdeker W, Friehe W. Effect of alloy additions on the properties of hot galvanized coatings [A]. Proceedings of 7th International Conference on Hot Dip Galvanizing [C]. Paris: Pergamon Press, 1964: 167 |
| [18] | Chang S, Shin J C.The effect of antimony additions on hot dip galvanized coatings[J]. Corros. Sci., 1994, 36: 1425 |
| [19] | Hansen M, Elliott R P, Shunk F A.Constitution of Binary Alloys[M]. New York: McGraw-Hill Book Co., 1958: 1 |
| [20] | Hanna F, Nassif N.Factors affecting the quality of hot-dip-galvanized steel sheets[J]. Surf. Technol., 1984, 21: 27 |
| [21] | Adjadj F, Belbacha E D, Bouharkat M, et al.Crystallographic study of the intermediate compounds SbZn, Sb3Zn4 and Sb2Zn3[J]. J. Alloys Compd., 2006, 419: 267 |
| [22] | Izard V, Record M C, Tedenac J C.Mechanical alloying of a new promising thermoelectric material, Sb3Zn4[J]. J. Alloys Compd., 2002, 345: 257 |
| [23] | El-Egamy S S. Electrochemical behavior of antimony and antimony oxide films in acid solutions[J]. Corrosion, 2006, 62: 739 |
| [24] | Cané E, Fusina L, Tarroni R, et al.High resolution infrared study of SbHD2: The ground state and the Sb-H stretching bands v1 and 2v1[J]. J. Mol. Spectrosc., 2011, 265: 1 |
| [25] | Xu R, Ma K, Guo Z.Activation mechanism of Sb2O3 during removal of cobalt from zinc sulphate solution[J]. Hydrometallurgy, 2006, 82: 150 |
| [26] | Li H, Zhang B, Wang J Q, et al.Effect of Sb and Mn additions on the corrosion behaviour of Zn[J]. J. Chin. Soc. Corros. Prot., 2008, 28: 257 |
| [26] | (李红, 张波, 王俭秋等. 合金元素Sb和Mn对Zn腐蚀的影响. 中国腐蚀与防护学报, 2008, 28: 257) |
/
| 〈 |
|
〉 |