Preparation and Activation Mechanism of Pd Colloid with High Concentration and Performance
Received date: 2016-08-26
Online published: 2016-12-14
Supported by
Supported by National Natural Science Foundation of China (No.51471180) and Science and Technology Program of Shenyang (No.F16-205-1-18)
The non-conductive substrate is often metallized through electroless plating method. Prior to the electroless plating, the substrate surfaces need to be firstly Pd activation pre-treated. The traditional "two-step" activation process, i.e., sensitization-activation, has been gradually obsoleted because of poor controllability and uniformity. A "one-step" activation process using Pd colloid has been widely used in industry, especially for the microvia metallization treatment in printed circuit board (PCB) fabrication. The bottleneck problem of this technology is the preparation of the Pd colloid solution with high concentration and excellent catalytic activity. The aim of this work is to develop a preparation method of the Pd colloid with high concentration and high quality. Pd colloid was prepared by a continuous reduction reaction with minor content. By mean of this process, the Pd concentration of the prepared colloid can exceed 2%. The morphology, microstructure and composition of the Pd colloid were characterized by SEM, TEM, XRD and XPS, respectively. The activate ability of the Pd colloid was examined by electroless Cu and electrochemical test. It was found that the average diameter of the Pd particles was less than 4 nm. Even if the concentration of Pd was less than 25 mg/L, this Pd colloid still had good activation ability for electro less Cu. The result demonstrated that the shell structure of the Pd micelle played a key role for the activation ability. The shell of Pd micelle was consisted of Sn2+, Sn4+ and Cl-, and generally formed two structures, [PdSn2]Cl6 and [PdSn3]Cl8. For the structure of [PdSn3]Cl8, the failure of the hydrolysis could lead to the loss of activation. The preparation method in this work can effectively avoid the occurrence of [PdSn3]Cl8, which greatly improved the activation ability of the Pd colloid.
Key words: Pd colloidal; electroless Cu; activation
Shuoshuo QU , Qingsheng ZHU , Yadong GONG , Yuying YANG , Caifu LI , Shian GAO . Preparation and Activation Mechanism of Pd Colloid with High Concentration and Performance[J]. Acta Metall Sin, 2017 , 53(4) : 487 -493 . DOI: 10.11900/0412.1961.2016.00388
| [1] | Lee C H, Hwang S, Kim S C, et al.Cu electroless deposition onto Ta substrates[J]. Electrochem. Solid-State Lett., 2006, 9: C157 |
| [2] | Lee C H, Lee S C, Kim J J.Bottom-up filling in Cu electroless deposition using bis-(3-sulfopropyl)-disulfide (SPS)[J]. Electrochim. Acta, 2005, 50: 3563 |
| [3] | Smy T, Tan L, Dew S K, et al.Simulation of electroless deposition of Cu thin films for very large scale integration metallization[J]. J. Electrochem. Soc., 1997, 144: 2115 |
| [4] | Torres J.Advanced copper interconnections for silicon CMOS technologies[J]. Appl. Surf. Sci., 1995, 91: 112 |
| [5] | Kim K, Jin S, Kwon O J.Effect of Pd precursor status on sonochemical surface activation in Cu electroless deposition[J]. Appl. Surf. Sci., 2016, 364: 45 |
| [6] | Lee C L, Huang Y C, Kuo L C.Catalytic effect of Pd nanoparticles on electroless copper deposition[J]. J. Solid State Electrochem., 2007, 11: 639 |
| [7] | Zabetakis D, Dressick W J.Selective electroless metallization of patterned polymeric films for lithography applications[J]. ACS Appl. Mater. Interfaces, 2009, 1: 4 |
| [8] | Yang C C, Wan C C, Wang Y Y.Synthesis of Ag/Pd nanoparticles via reactive micelles as templates and its application to electroless copper deposition[J]. J. Colloid Interface Sci., 2004, 279: 433 |
| [9] | Zhang Y H, Yan T T, Yu S Q, et al.Electroless copper deposition in the photographic gelatin layer[J]. J. Electrochem. Soc., 1999, 146: 1270 |
| [10] | Lo S H Y, Wang Y Y, Wan C C. Long-term stability of Cu/Pd nanoparticles and their feasibility for electroless copper deposition[J]. Electrochim. Acta, 2008, 54: 727 |
| [11] | Fujiwara Y, Kobayashi Y, Kita K, et al.Ag nanoparticle catalyst for electroless Cu deposition and promotion of its adsorption onto epoxy substrate[J]. J. Electrochem. Soc., 2008, 155: D377 |
| [12] | Hutchings G J.Nanocrystalline gold and gold palladium alloy catalysts for chemical synthesis[J]. Chem. Commun., 2008, 1148 |
| [13] | Nicolas-Debarnot D, Pascu M, Vasile C, et al.Influence of the polymer pre-treatment before its electroless metallization[J]. Surf. Coat. Technol., 2006, 200: 4257 |
| [14] | Hsu H H, Teng C W, Lin S J, et al.Sn/Pd catalyzation and electroless Cu deposition on TaN diffusion barrier layers[J]. J. Electrochem. Soc., 2002, 149: C143 |
| [15] | Okada S, Kamegawa T, Mori K, et al.An electroless deposition technique for the synthesis of highly active and nano-sized Pd particles on silica nanosphere[J]. Catal. Today, 2012, 185: 109 |
| [16] | Charbonnier M, Goepfert Y, Romand M, et al.Electroless plating of glass and silicon substrates through surface pretreatments involving plasma-polymerization and grafting processes[J]. J. Adhes., 2004, 80: 1103 |
| [17] | Osaka T, Takamatsu H, Nihei K.A Study on activation and acceleration by mixed PdCl2/SnCl2 catalysts for electroless metal deposition[J]. J. Electrochem. Soc., 1980, 127: 1021 |
| [18] | O'Sullivan E J M, Horkans J, White J R, et al. Characterization of PdSn catalysts for electroless metal deposition[J]. IBM J. Res. Dev., 1988, 32: 591 |
| [19] | Cui X Y, Hutt D A, Scurr D J, et al.The evolution of Pd/Sn catalytic surfaces in electroless copper deposition[J]. J. Electrochem. Soc., 2011, 158: D172 |
| [20] | Svendsen L G, Osaka T, Sawai H.Behavior of Pd/Sn and Pd catalysts for electroless plating on different substrates investigated by means of rutherford backscattering spectroscopy[J]. J. Electrochem. Soc., 1983, 130: 2252 |
| [21] | Froment M, Queau E, Martin J R, et al.Structural and analytical characteristics of adsorbed Pd-Sn colloids[J]. J. Electrochem. Soc., 1995, 142: 3373 |
| [22] | Chen L J, Wan C C, Wang Y Y.Chemical preparation of Pd nanoparticles in room temperature ethylene glycol system and its application to electroless copper deposition[J]. J. Colloid Interface Sci., 2006, 297: 143 |
| [23] | Harraz F A, El-Hout S E, Killa H M, et al. Palladium nanoparticles stabilized by polyethylene glycol: Efficient, recyclable catalyst for hydrogenation of styrene and nitrobenzene[J]. J. Catal., 2012, 286: 184 |
| [24] | Kondo K, Ishikawa J, Takenaka O, et al.Electroless copper plating in the presence of excess triethanol amine[J]. J. Electrochem. Soc., 1990, 137: 1859 |
| [25] | Nicolas-Debarnot D, Pascu M, Vasile C, et al.Influence of the polymer pre-treatment before its electroless metallization[J]. Surf. Coat. Technol., 2006, 200: 4257 |
| [26] | Rene E, Van G, Andrzej A.Handbook of X-Ray Spectrometry Version 2, 2002 |
| [27] | Shukla S, Seal S, Akesson J, et al.Study of mechanism of electroless copper coating of fly-ash cenosphere particles[J]. Appl. Surf. Sci., 2001, 181: 35 |
/
| 〈 |
|
〉 |