Structure-Property Correlation of High Fe-ContentFe-B-Si-Hf Bulk Glassy Alloys

  • Yaoxiang GENG ,
  • Zhijie ZHANG ,
  • Yingmin WANG ,
  • Jianbing QIANG ,
  • Chuang DONG ,
  • Haibin WANG ,
  • Ojied TEGUS
Expand
  • 1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China
    2 Key Lab of Materials Modification by Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China
    3 Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials, Inner Mongolia Normal University, Hohhot 010022, China

Received date: 2016-07-05

  Online published: 2016-12-07

Supported by

Supported by National Natural Science Foundation of China (Nos.51671045 and 51601073), National Magnetic Confined Fusion Energy Development (Nos.2013GB107003 and 2015GB105003) and Fundamental Research Funds for the Central Universities (No;DUT16ZD209)

Abstract

Fe-based amorphous alloys are well known for their good magnetic properties. But these alloys were only prepared into ribbon form in early times due to their insufficient glass-forming abilities (GFAs). After first synthesized of Fe-(Al, Ga)-P-C-B bulk glassy alloy, many Fe-based bulk metallic glasses (BMGs) were synthesized. Compared with amorphous alloy ribbons, the GFA of these alloys was significantly improved, but the saturation magnetization (Bs) was less than 1.5 T. To achieve higher Bs in Fe-based amorphous alloys, the Fe content should be maximized and the metalloid and alloying elements contents should be minimized, but it makes glass formation difficult. It is difficult to reveal the effect mechanism of Fe atoms in high Fe-content amorphous alloys, due to the complexity of the amorphous structure. The present work focuses on explores the structure-property correlations of high Fe-content Fe-B-Si-Hf multi-component glassy alloys with an amorphous structure model. A series of high Fe-content alloys with the composition of [Si-B2Fe7.7Hf0.3]Fe+Fex (x=0, 1.5, 2, 2.5 and 3) was produced by adding Fe atoms to the ideal cluster formula, which is based on the composition with the best glass-forming ability of [Si-B2Fe7.7Hf0.3]Fe (Fe72.5B16.7Si8.3Hf2.5) for Fe-B-Si-Hf quaternary alloys. Liquid quench, thermal analysis and magnetic measurement results show that the critical rod size for glassy alloys gradually decreases from 2.5 mm to 1 mm as the number of Fe atoms increases from 0 to 2. The [Si-B2Fe7.7Hf0.3]Fe+Fe2 (Fe76.4B14.3Si7.1Hf2.2) bulk glassy alloy has a high saturation magnetization of 1.58 T and a low coercive force of 2.8 A/m. The decreasing of the glass transition temperature, the thermal stability, the glass-forming ability and the Curie temperature with increasing Fe content in Fe-B-Si-Hf glassy alloys was evaluated using a “dual-cluster” ({[Si-B2Fe7.7Hf0.3]+[Fe-Fe14]x/15}Fe) amorphous structure model. The result shows that the [Fe-Fe14] cluster from the α-Fe phase plays an important role in determining the properties change for this series high Fe-content Fe-B-Si-Hf glassy alloys.

Cite this article

Yaoxiang GENG , Zhijie ZHANG , Yingmin WANG , Jianbing QIANG , Chuang DONG , Haibin WANG , Ojied TEGUS . Structure-Property Correlation of High Fe-ContentFe-B-Si-Hf Bulk Glassy Alloys[J]. Acta Metall Sin, 2017 , 53(3) : 369 -375 . DOI: 10.11900/0412.1961.2016.00281

References

[1] Egami T.Magnetic amorphous alloys: Physics and technological applications[J]. Rep. Prog. Phys., 1984, 47: 1601
[2] McHenry M E, Willard M A, Laughlin D E. Amorphous and nanocrystalline materials for applications as soft magnets[J]. Prog. Mater. Sci., 1999, 44: 291
[3] Hasegawa R.Amorphous magnetic materials——A history[J]. J. Magn. Magn. Mater., 1991, 100: 1
[4] Inoue A, Shinohara Y, Gook J S.Thermal and magnetic properties of bulk Fe-based glassy alloys prepared by copper mold casting[J]. Mater. Trans. JIM, 1995, 36: 1427
[5] Makino A, Kubota T, Chang C T, et al.Fe-metalloids bulk glassy alloys with high Fe content and high glass-forming ability[J]. J. Mater. Res., 2008, 23: 1339
[6] Liu F J, Yao K F, Ding H Y.Fe-based glassy alloys with high iron content and high saturation magnetization[J]. Intermetallics, 2011, 19: 1674
[7] Meng S Y, Ling H B, Li Q, et al.Development of Fe-based bulk metallic glasses with high saturation magnetization[J]. Scr. Mater., 2014, 81: 24
[8] Suryanarayana C, Inoue A.Bulk Metallic Glasses [M]. Boca Raton, FL: CRC Press, 2011: 460
[9] Miracle D B.A structural model for metallic glasses[J]. Nat. Mater., 2004, 3: 697
[10] Han G, Qiang J B, Li F W, et al.The e/a values of ideal metallic glasses in relation to cluster formulae[J]. Acta Mater., 2011, 59: 5917
[11] Luo L J, Chen H, Wang Y M, et al.24 electron cluster formulas as the 'molecular' units of ideal metallic glasses[J]. Philos. Mag., 2014, 94: 2520
[12] Geng Y X, Wang Y M, Qiang J B, et al.Composition formulas of Fe-B binary amorphous alloys[J]. J. Non-Cryst. Solids, 2016, 432: 453
[13] Geng Y X, Wang Y M, Qiang J B, et al.Fe-B-Si-Zr soft magnetic bulk glassy alloys[J]. Intermetallics, 2015, 67: 138
[14] Geng Y X, Wang Y M, Wang Z R, et al.Formation and structure-property correlation of new bulk Fe-B-Si-Hf metallic glasses[J].
[14] Mater. Des., 2016, 106: 69
[15] Geng Y X, Han K M, Wang Y M, Q et al. Composition design of Fe-B-Si-Ta bulk amorphous alloys based on cluster+glue atom model[J]. Acta Metall. Sin., 2015, 51: 1017
[15] (耿遥祥, 韩凯明, 王英敏等. 基于团簇+连接原子模型的Fe-B-Si-Ta块体非晶合金的成分设计[J]. 金属学报, 2015, 51: 1017)
[16] Geng Y X, Wang Y M, Qiang J B, et al.Composition design and optimization of Fe-B-Si-Nb bulk amorphous alloys[J]. Acta Metall. Sin., 2016, 52: 1459
[16] (耿遥祥, 王英敏, 羌建兵等. Fe-B-Si-Nb块体非晶合金的成分设计与优化[J]. 金属学报, 2016, 52: 1459)
[17] Inoue A, Shen B L.Soft magnetic bulk glassy Fe-B-Si-Nb alloys with high saturation magnetization above 1.5 T[J]. Mater. Trans., 2002, 43: 766
[18] Inoue A, Shen B L.Formation and soft magnetic properties of Fe-B-Si-Zr bulk glassy alloys with high saturation magnetization above 1.5 T[J]. Mater. Trans., 2002, 43: 2350
[19] Miracle D B.The density and packing fraction of binary metallic glasses[J]. Acta Mater., 2013, 61: 3157
[20] Takeuchi A, Inoue A.Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element[J]. Mater. Trans., 2005, 46: 2817
[21] Stillinger F H.Relaxation and flow mechanisms in "fragile" glass-forming liquids[J]. J. Chem. Phys., 1988, 89: 6461
[22] Ediger M D.Spatially heterogeneous dynamics in supercooled liquids[J]. Annu. Rev. Phys. Chem., 2000, 51: 99
[23] Tanaka H.Two-order-parameter model of the liquid-glass transition. II. Structural relaxation and dynamic heterogeneity[J]. J. Non-Cryst. Solids, 2005, 351: 3385
[24] Bakonyi I.Relevance of Fe atomic volumes for the magnetic properties of Fe-rich metallic glasses[J]. J. Magn. Magn. Mater., 2012, 324: 3961
[25] Durand J.Magnetic properties of metallic glasses [A]. Glassy Metals II[M]. Berlin, Heidelberg: Springer-Verlag, 1983: 343
Outlines

/