Design Standard and Analysis of Ageing Process in High Co-Ni Secondary Hardening Steel
Received date: 2016-05-03
Online published: 2016-11-25
Supported by
Supported by National Natural Science Foundation of China (Nos.51171087 and 51471094)
High Co-Ni secondary hardening steels have received great attention for a long time. In several decades, many previous studies were made to improve their strength, toughness, corrosion resistance ability and even stress corrosion sensibility. Although many new kinds of high Co-Ni secondary hardening steels were developed by researchers, the mechanisms of strength and toughness were still a problem, which would inhibit the further development of high Co-Ni secondary hardening steels. In this work, both microstructure and mechanical properties of high Co-Ni secondary hardening steels were analyzed by simulation and experiment. The strengthening and toughening mechanism was explained, which included the transformation induced plasticity (TRIP) effect of austenite layer in nanometer size and the precipitation of M2C in nanometer size. According to the previous studies about AerMet100 steel, the design standard for high Co-Ni secondary hardening steels was established, which included the mole volume change for austenite, the stability of austenite, the austenite thickness, the austenite equilibrium content, the M2C size, the M2C equilibrium content and cost control. Based on this design standard, the ageing process for a new high Co-Ni secondary hardening steel was analyzed. By controlling the ageing process as 515 ℃ for 10 h, based on the design standard, M2C with the size of 1~5 nm and austenite layers with the thickness of 10~20 nm was formed in new high Co-Ni secondary hardening steels. The equilibrium content of M2C and austenite layers were controlled as 19.5% and 3.8%, respectively. The simulation results were basically consistent with the microstructure observation results. The high Co-Ni secondary hardening steel treated by the designed heat treatment process has considerable strength (2021 MPa) and toughness (115 MPam1/2). Both simulation and experimental results showed that this design standard of ageing process for high Co-Ni secondary hardening steels can help to obtain steels with high strength and toughness.
Key words: austenite layer; M2C precipitation; coarsen kinetics; ageing process
Chenchong WANG , Chi ZHANG , Zhigang YANG , Jie SU , Yuqing WENG . Design Standard and Analysis of Ageing Process in High Co-Ni Secondary Hardening Steel[J]. Acta Metall Sin, 2017 , 53(2) : 175 -182 . DOI: 10.11900/0412.1961.2016.00167
| [1] | Hu Z F, Wu X F, Wang C X.Coarsening kinetics of multi-component M2C precipitates in secondary hardening alloy steels[J]. Acta Metall. Sin., 2003, 39: 585 |
| [1] | (胡正飞, 吴杏芳, 王春旭. 二次硬化合金钢中多组元强化相M2C碳化物的粗化动力学研究[J]. 金属学报, 2003, 39: 585) |
| [2] | Ling B, Zhong P, Zhong B W, et al.TEM observation of the secondary hardening process in Ni10Co14 steels[J]. Acta Metall. Sin., 1995, 31: 209 |
| [2] | (凌斌, 钟平, 钟炳文等. Ni10Co14钢的二次硬化过程的TEM观察[J]. 金属学报, 1995, 31: 209) |
| [3] | Ayer M, Machmeier P.On the characteristics of M2C carbides in the peak hardening regime of AerMet 100 steel[J]. Metall. Mater. Trans., 1998, 29A: 903 |
| [4] | Wang C C, Zhang C, Yang Z G.Austenite layer and precipitation in high Co-Ni maraging steel[J]. Micron, 2014, 67: 112 |
| [5] | Olson G B. Advances in theory: Martensite by design[D] [J]. Mater. Sci. Eng., 2006, A438-440: 48 |
| [6] | Olson G B.Genomic materials design: The ferrous frontier[J]. Acta Mater., 2013, 61: 771 |
| [7] | Olson G B, Kuehmann C J.Materials genomics: From CALPHAD to flight[J]. Scr. Mater., 2014, 70: 25 |
| [8] | Yoo C H, Lee H M, Chan J W, et al.M2C precipitates in isothermal tempering of high Co-Ni secondary hardening steel[J]. Metall. Mater. Trans., 1996, 27A: 3466 |
| [9] | Ayer M, Machmeier P M.Transmission electron microscopy examination of hardening and toughening phenomena in Aermet 100[J]. Metall. Trans., 1993, 24A: 1943 |
| [10] | Wang C C, Zhang C, Yang Z G, et al.Analysis of fracture toughness in high Co-Ni secondary hardening steel using FEM[J]. Mater. Sci. Eng., 2015, A646: 1 |
| [11] | Wang C C, Zhang C, Yang Z G, et al.Multi-scale simulation of hydrogen influenced critical stress intensity in high Co-Ni secondary hardening steel[J]. Mater. Des., 2015, 87: 501 |
| [12] | Olson G B, Cohen M.Stress-assisted isothermal martensitic transformation: Application to TRIP steels[J]. Metall. Trans., 1982, 13A: 1907 |
| [13] | Olson G B, Cohen M.A general mechanism of martensitic nucleation: Part I. General concepts and the FCC→HCP transformation[J]. Metall. Trans., 1976, 7A: 1897 |
| [14] | Ghosh G, Olson G B.Kinetics of F.C.C. →B.C.C. heterogeneous martensitic nucleation—I. The critical driving force for athermal nucleation[J]. Acta Metall. Mater., 1994, 42: 3361 |
| [15] | Lifshitz I M, Slyozov V V.The kinetics of precipitation from supersaturated solid solutions[J]. J. Phys. Chem. Solids, 1961, 19: 35 |
| [16] | Wagner C.Theory of precipitate change by redis-solution (Ostwald ripening)[J]. Z. Elektrochem., 1961, 65: 581 |
| [17] | Lee H M, Allen S M, Gruicic M.Coarsening resistance of M2C carbides in secondary hardening steels: Part I. Theoretical model for multicomponent coarsening kinetics[J]. Metall. Trans., 1991, 22A: 2863 |
| [18] | Wang Z Q, Sun X J, Yang Z G, et al.Carbide precipitation in austenite of a Ti-Mo-containing low-carbon steel during stress relaxation[J]. Mater. Sci. Eng., 2013, A573: 84 |
| [19] | Xia Z X, Zhang C, Lan H, et al.Effect of magnetic field on interfacial energy and precipitation behavior of carbides in reduced activation steels[J]. Mater. Lett., 2011, 65: 937 |
| [20] | Tao P, Zhang C, Yang Z G, et al.Evolution and coarsening of carbides in 2.25Cr-1Mo steel weld metal during high temperature tempering[J]. J. Iron Steel Res. Int., 2010, 17: 74 |
| [21] | Wang J S, Mulholland M D, Olson G B, et al.Prediction of the yield strength of a secondary-hardening steel[J]. Acta Mater., 2013, 61: 4939 |
| [22] | Scandella F, Atamert S, Knowles D M.Evaluation of hot strip mill backup roll cladding[J]. J. Mater. Sci. Technol., 2000, 16: 491 |
| [23] | Wang X R, Yan M F, Meng Q C.TEM observation of precipitation phase produced during tempering of steel AerMet100 and first principles calculations of phase evolution[J]. Rare Met., 2007, 26: 326 |
| [24] | He Y, Yang K, Qu W S, et al.Strengthening and toughening of a 2800-MPa grade maraging steel[J]. Mater. Lett., 2002, 56: 763 |
| [25] | Leitner H, Schober M, Schnitzer R, et al.Strengthening behavior of Fe-Cr-Ni-Al-(Ti) maraging steels[J]. Mater. Sci. Eng., 2011, A528: 5264 |
| [26] | Morral J E, Purdy G R.Particle coarsening in binary and multicomponent alloys[J]. Scr. Metall. Mater., 1994, 30: 905 |
/
| 〈 |
|
〉 |