Orginal Article

Recrystallization Texture and Magnetostriction in Binary Fe81Ga19 Sheets

  • Quan FU ,
  • Yuhui SHA ,
  • Zhenghua HE ,
  • Fan LEI ,
  • Fang ZHANG ,
  • Liang ZUO
Expand
  • Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China

Received date: 2016-07-01

  Online published: 2016-11-18

Supported by

Supported by National Natural Science Foundation of China (No.51671049) and Fundamental Research Funds for the Central Universities (No.L1502019)

Abstract

Fe-Ga alloys are attractive magnetostrictive materials due to large magnetostriction along <100> direction and high mechanical strength. However, sharp Goss ({110}<001>) texture and large magnetostriction coefficients were conventionally achieved by secondary recrystallization with centimeter-sized grains under the effects of inhibitor and surface energy, resulting in deteriorated mechanical properties. Texture optimization in relatively fine grained microstructure is an effective way to obtain excellent comprehensive properties. Cold rolling process can determine the difference in number and size of primary recrystallization grains among various texture components, and further influence the texture and grain size evolution during subsequent high temperature annealing. The present work aims to produce strong η texture (<001>//RD, rolling direction) in binary Fe-Ga sheet with relatively fine recrystallization grains by cold rolling parameter modification. Macro- and micro-texture analysis was applied to investigate the effects of primary recrystallization states on texture and grain size evolution during high temperature annealing in binary Fe-Ga sheet. The η grains can gain more numbers and relatively larger sizes in primary recrystallization stage, and preferably grow even abnormally during high temperature annealing. A sharp η texture and large magnetostriction coefficient are successfully developed in primarily and secondarily recrystallized sheets with relatively fine grains. The results provide a prospective route for the efficient recrystallization texture and grain size optimization in binary Fe-Ga and other bcc alloys.

Cite this article

Quan FU , Yuhui SHA , Zhenghua HE , Fan LEI , Fang ZHANG , Liang ZUO . Recrystallization Texture and Magnetostriction in Binary Fe81Ga19 Sheets[J]. Acta Metall Sin, 2017 , 53(1) : 90 -96 . DOI: 10.11900/0412.1961.2016.00271

References

[1] Clark A E, Hathaway K B, Wun-Fogle M, et al.Extraordinary magnetoelasticity and lattice softening in bcc Fe-Ga alloys[J]. J. Appl. Phys., 2003, 93: 8621
[2] Na S M, Flatau A B.Single grain growth and large magnetostriction in secondarily recrystallized Fe-Ga thin sheet with sharp Goss (011)[100] orientation[J]. Scr. Mater., 2012, 66: 307
[3] Na S M, Flatau A B.Surface-energy-induced selective growth of (001) grains in magnetostrictive ternary Fe-Ga-based alloys[J]. Smart Mater. Struct., 2012, 21: 055024
[4] Yuan C, Li J H, Zhang W L, et al.Sharp Goss orientation and large magnetostriction in the rolled columnar-grained Fe-Ga alloys[J]. J. Magn. Magn. Mater., 2015, 374: 459
[5] Na S M, Flatau A B.Global Goss grain growth and grain boundary characteristics in magnetostrictive Galfenol sheets[J]. Smart Mater. Struct., 2013, 22: 125026
[6] Kellogg R A, Flatau A B, Clark A E, et al.Texture and grain morphology dependencies of saturation magnetostriction in rolled polycrystalline Fe83Ga17[J]. J. Appl. Phys., 2003, 93: 8495
[7] Summers E M, Meloy R, Na S M. Magnetostriction and texture relationships in annealed Galfenol alloys [J]. J. Appl. Phys., 2009, 105: 07A922
[8] Li J H, Yuan C, Zhang W L, et al.Retaining the <001> orientation from initial columnar grains and magnetostriction in binary Fe-Ga alloy sheets[J]. Mater. Trans., 2015, 56: 1940
[9] Park J T, Szpunar J A.Evolution of recrystallization texture in nonoriented electrical steels[J]. Acta Mater., 2003, 51: 3037
[10] Srisukhumbowornchai N, Guruswamy S.Crystallographic textures in rolled and annealed Fe-Ga and Fe-Al alloys[J]. Metall. Mater. Trans., 2004, 35A: 2963
[11] Na S M, Flatau A B.Texture evolution and probability distribution of Goss orientation in magnetostrictive Fe-Ga alloy sheets[J]. J. Mater. Sci., 2014, 49: 7697
[12] Yuan C, Li J H, Bao X Q, et al.Influence of annealing process on texture evolution and magnetostriction in rolled Fe-Ga based alloys[J]. J. Magn. Magn. Mater., 2014, 362: 154
[13] Na S M, Yoo J H, Flatau A B.Abnormal (110) grain growth and magnetostriction in recrystallized Galfenol with dispersed niobium carbide[J]. IEEE Trans. Magn., 2009, 45: 4132
[14] Rios P R.Abnormal grain growth in pure materials[J]. Acta Metall. Mater., 1992, 40: 2765
[15] Hayakawa Y, Omura T, Imamura T.Onset of secondary recrystallization in high purity 3.3% Si steel[J]. ISIJ Int., 2014, 54: 2385
[16] Sha Y H, Sun C, Zhang F, et al.Strong cube recrystallization texture in silicon steel by twin-roll casting process[J]. Acta Mater., 2014, 76: 106
[17] Park J T, Szpunar J A.Texture development during grain growth in nonoriented electrical steels[J]. ISIJ Int., 2005, 45: 743
[18] Samajdar I, Cicale S, Verlinden B, et al.Primary recrystallization in a grain oriented silicon steel: on the origin of Goss {110}<001> grains[J]. Scr. Mater., 1998, 39: 1083
[19] Paolinelli S D C, da Cunha M A, de Dafe S S F, et al. Study of the simultaneous effects of the hot band grain size and cold rolling reduction on the structure and magnetic properties of nonoriented 3% Si steel[J]. IEEE Trans. Magn., 2012, 48: 1401
[20] de Dafe S S F, Paolinelli S D C, Cota A B. Influence of thermomechanical processing on shear bands formation and magnetic properties of a 3% Si non-oriented electrical steel[J]. J. Magn. Magn. Mater., 2011, 323: 3234
[21] Lee S, de Cooman B C. Effect of warm rolling on the rolling and recrystallization textures of non-oriented 3% Si steel[J]. ISIJ Int., 2011, 51: 1545
[22] Nave M D, Barnett M R, Beladi H.The influence of solute carbon in cold-rolled steels on shear band formation and recrystallization texture[J]. ISIJ Int., 2004, 44: 1072
[23] H?lscher M, Raabe D, Lücke K.Rolling and recrystallization textures of bcc steels[J]. Steel Res. Int., 1991, 62: 567
[24] de Campos M F, Landgraf F J G, Takanohashi R, et al. Effect of the hot band grain size and intermediate annealing on the deformation and recrystallization textures in low silicon electrical steels[J]. ISIJ Int., 2004, 44: 591
[25] Park J T, Szpunar J A.Effect of initial grain size on texture evolution and magnetic properties in nonoriented electrical steels[J]. J. Magn. Magn. Mater., 2009, 321: 1928
[26] Liu J L, Sha Y H, Zhang F, et al.Development of {210}<001> recrystallization texture in Fe-6.5wt.% Si thin sheets[J]. Scr. Mater., 2011, 65: 292
Outlines

/